CN107962764A - Double water route stamping dies - Google Patents
Double water route stamping dies Download PDFInfo
- Publication number
- CN107962764A CN107962764A CN201711450795.6A CN201711450795A CN107962764A CN 107962764 A CN107962764 A CN 107962764A CN 201711450795 A CN201711450795 A CN 201711450795A CN 107962764 A CN107962764 A CN 107962764A
- Authority
- CN
- China
- Prior art keywords
- water route
- thermal cycle
- plate
- sapmac method
- lower template
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
The invention discloses a kind of double water route stamping dies,Including board gland,Upper mounted plate,Stretching head,Cope plate,Lower template and bottom plate,The board gland is fixed on upper mounted plate top,Through hole is equipped among the cope plate,The upper mold plate bolt is fixed on upper mounted plate lower part,The stretching head is arranged in cope plate through hole and is fixed on upper mounted plate lower part,The lower template is fixed on bottom plate top,The lower template is arranged on immediately below cope plate,Fixed plate corner is to having guide post,The bottom plate corner is equipped with guide sleeve upwards,The guide post can slide up and down in guide sleeve,Fixed plate and upper stretching head are internally provided with the first thermal cycle water route and the first SAPMAC method water route,The lower template is internally provided with the second thermal cycle water route and the second SAPMAC method water route,Die cavity is offered between the stretching head and lower template.A kind of double water route stamping dies provided by the invention, improve the formed precision of sheeting.
Description
Technical field
The present invention relates to technical field of mold, specifically, is related to a kind of double water route stamping dies.
Background technology
Existing plastic tab does moulding, is generally produced by the way of injection molded, deflection after injection is very
Greatly, it is difficult to reach required requirement, moulding is directly typically now carried out using impact style, but material deforms in punching course
Place is internal to have stress concentration, has stress bounce-back after normal cooling after mould molding, causes lamina dimensions to change, into
Dimensional accuracy is small after type, causes the finished product after punching press not meet actual operation requirements, and particularly mobile phone PET protection film is this kind of to making
The higher sheet product of molded dimension.
The content of the invention
It is an object of the invention to provide a kind of double water route stamping dies, the formed precision of sheeting is improved.
Technical solution is used by double water route stamping dies disclosed by the invention:A kind of double water route stamping dies, including
Board gland, upper mounted plate, stretching head, cope plate, lower template and bottom plate, the board gland are fixed on fixation
Plate top, the cope plate centre are equipped with through hole, and the upper mold plate bolt is fixed on upper mounted plate lower part, and the stretching head is arranged on
In cope plate through hole and upper mounted plate lower part is fixed on, the lower template is fixed on bottom plate top, and the lower template is arranged on
Immediately below cope plate, to guide post is had, the bottom plate corner is equipped with guide sleeve upwards, described to lead for fixed plate corner
Column can slide up and down in guide sleeve, and fixed plate and upper stretching head are internally provided with the first thermal cycle water route and the first SAPMAC method
Water route, the lower template is internally provided with the second thermal cycle water route and the second SAPMAC method water route, between the stretching head and lower template
Offer die cavity.
Preferably, the first SAPMAC method water route is arranged on below the first thermal cycle water route inside stretching head, institute
The second SAPMAC method water route is stated to be arranged on above the second thermal cycle water route inside lower template.
Preferably, location hole is offered below the cope plate, positioning pin is equipped with above above-mentioned lower template.
Preferably, the stretching head and the interface in upper mounted plate the first SAPMAC method water route and the first thermal cycle water route
Place is equipped with water proof ring.
Preferably, the cope plate is equipped with elastic component with fixed plate screw connection.
Preferably, the first thermal cycle water route and the first SAPMAC method water route are respectively made of and lead to a plurality of aquaporin
Cross the connection of inlet and outlet pipeline, the first thermal cycle water route and the first SAPMAC method water route are in concave shape, first heat recirculated water
Road is arranged in the second SAPMAC method water route groove.
Preferably, the second thermal cycle water route and the second SAPMAC method water route are respectively made of and lead to a plurality of aquaporin
The connection of inlet and outlet pipeline is crossed, the second thermal cycle water route and the second SAPMAC method water route are in respectively bamboo row-like arrangement.
Preferably, the first thermal cycle water route inlet and outlet are arranged on upper mounted plate the same side, and second heat is followed
Ring water route inlet and outlet are arranged on lower template the same side.
Preferably, the first SAPMAC method water route, which is imported and exported, is arranged on the opposite both sides of upper mounted plate, and described second
SAPMAC method water route inlet and outlet set the opposite both sides of template.
Preferably, the first thermal cycle water route and the second thermal cycle water route lead to hot steam, and described first cold follows
Ring water route and the second SAPMAC method water route lead to cold air.
The beneficial effect of double water route stamping dies disclosed by the invention is:Board gland is fixed on forcing press, will be thin
Sheet material is positioned in the die cavity of lower template, and forcing press drives stretching head to press down, and connects the first thermal cycle water route and the second heat
Circulation waterway, heats to stretching head and the die cavity of lower template, makes sheet soft, and stretching head is continued to press on to moving down by forcing press
It is dynamic, by stretching head and the die cavity of lower template by slice forming, stop the first thermal cycle water route and the second thermal cycle water route plus
Heat, connects the first SAPMAC method water route and the second SAPMAC method water route, is cooled down to stretching head and the die cavity of lower template, makes thin slice cooling simultaneously
The inside bending stress of releasable material, after thin slice cooling, stops the cooling in the first SAPMAC method water route and the second SAPMAC method water route,
Forcing press drives stretching head and cope plate to move up, and takes out the thin slice after shaping, completes a punching press, what thin slice was produced by deformation
Internal stress in die cavity cool down when discharge, take out the thin slice finished product after mould deformation it is small so that improve sheeting into
Type precision.
Brief description of the drawings
Fig. 1 is the structure diagram of double water routes stamping die of the invention;
Fig. 2 is thermal cycle water route and the SAPMAC method water route arrangement schematic diagram of double water routes stamping die of the invention;
Fig. 3 is the exploded view of the upper mounted plates of water routes stamping dies of the invention double, stretching head and cope plate;
Fig. 4 is thermal cycle water route and the SAPMAC method water route arrangement schematic diagram of double water routes stamping die of the invention.
Embodiment
The present invention is further elaborated and illustrated with reference to specific embodiment and Figure of description:Please refer to Fig.1, scheme
2nd, Fig. 3 and Fig. 4, a kind of double water route stamping dies, including board gland 13, upper mounted plate 14, bottom plate 17, cope plate
18th, lower template 21 and stretching head 24, board gland 13 are fixed on 14 top of upper mounted plate, through hole are equipped among cope plate 18,
18 screw of cope plate is fixed on 14 lower part of upper mounted plate, and stretching head 24 is arranged in 18 through hole of cope plate and is fixed on upper mounted plate 14
Lower part, lower template 21 are fixed on 17 top of bottom plate, and lower template 21 is arranged on immediately below cope plate 18, and upper mounted plate 14 4 is angular
Guide post 15 is had, 17 4 jiaos of bottom plate is equipped with guide sleeve 16 upwards, and guide post 15 can slide up and down in guide sleeve 16, pass through guide post
15 and guide sleeve 16 carry out the guiding of open mold, upper mounted plate 14 and upper stretching head 24 are internally provided with the first thermal cycle water route 11 and the
One SAPMAC method water route 12, lower template 21 are internally provided with the second thermal cycle water route 20 and the second thermal cycle water route 19,24 He of stretching head
Offer die cavity between lower template 21, forcing press be fixed on by board gland 13, by forcing press drive upper mounted plate 14,
Stretching head 24 and cope plate 18 move down, and are closed stretching head 24 and 21 die cavity of lower template, pass through the first thermal cycle water route 11
Heated with the second thermal cycle water route 20 to stretching head 24 and 21 die cavity of lower template, the sheeting in die cavity is softened, can
Destruction to sheeting when reducing punching press, the generation for phenomena such as preventing uniaxial direct tensile first 24 from thrusting sheeting, thin slice into
After type, cooled down by the first SAPMAC method water route 12 and the second thermal cycle water route 19 to stretching head 24 and lower template 21, by thin slice temperature
Degree is reduced to below room temperature, and the internal stress for making thin slice be produced by deformation and heating, discharges during cooling.
First SAPMAC method water route 12 is arranged on below the first thermal cycle water route 11 inside stretching head 24, the second SAPMAC method water route
19 are arranged on above the second thermal cycle water route 20 inside the lower template 21, make in heating process, because of the first thermal cycle water route 11 and the
There is certain distance in two thermal cycle water routes 20 with die cavity, can be more uniformly distributed stretching head 24 and the heated of the die cavity of lower template 21, together
When the first SAPMAC method water route 12 and the second SAPMAC method water route 19 it is nearer from die cavity, accelerate the cooling of die cavity, accelerate sheeting
Shaping.
The lower section of cope plate 18 offers location hole, and the above-mentioned top of lower template 21 is equipped with positioning pin, is played in clamping process
Positioning action.
Stretching head 24 is equipped with anti-with the interface in 14 first SAPMAC method water route 12 of upper mounted plate and the first thermal cycle water route 11
Hydrosphere 23, increases the waterway seal between stretching head 24 and upper mounted plate 14.
Cope plate 18 is equipped with elastic component 22 with fixed plate screw connection, protrudes cope plate 18 by 22 elastic force of elastic component
Stretching head 24, elastic component 22 is spring herein, in clamping process, first passes through cope plate 18 and lower template 21 is positioned, keep away
Exempt from stretching head 24 and the die cavity of lower template 21 does not align.
First thermal cycle water route 11 and the first SAPMAC method water route 12 are respectively made of and by importing and exporting pipeline a plurality of aquaporin
Connect, the first thermal cycle water route 11 and the first SAPMAC method water route 12 are in concave shape, and the first thermal cycle water route 11 is followed arranged on the second heat
In 19 groove of ring water route, make the first thermal cycle water route 11 and the first SAPMAC method water route 12 non-intersect, and a plurality of pipeline makes first
11 and first SAPMAC method water route 12 of thermal cycle water route and 24 contact surface bigger of stretching head, make the die cavity on stretching head 24 add hot and cold
But evenly and more rapidly.
Second thermal cycle water route 20 and the second thermal cycle water route 19 are respectively made of and by importing and exporting pipeline a plurality of aquaporin
Connect, the second thermal cycle water route 20 and the second thermal cycle water route 19 are in respectively bamboo row-like arrangement, and bamboo row-like arrangement makes the second thermal cycle
20 and second thermal cycle water route 19 of water route and 21 contact surface bigger of lower template, be die cavity heating in template and cooling evenly and
More rapidly.
First thermal cycle water route 11 inlet and outlet are arranged on 14 the same side of upper mounted plate, and the second thermal cycle water route 20 inlet and outlet are arranged on
21 the same side of lower template.
First SAPMAC method water route 12 inlet and outlet are arranged on the opposite both sides of upper mounted plate 14, and the second thermal cycle water route 19 is imported and exported
Set the opposite both sides of template 21.
First thermal cycle water route 11 and the second thermal cycle water route 20 lead to hot steam, the first SAPMAC method water route 12 and second
Thermal cycle water route 19 leads to cold air, makes the heating of die cavity and cools down more rapidly.
In such scheme, board gland 13 is fixed on forcing press, sheeting is positioned over to the die cavity of lower template 21
Interior, forcing press drives stretching head 24 to press down, and the first thermal cycle water route 11 and the second thermal cycle water route 20 is connected, to stretching head 24
Heated with the die cavity of lower template 21, make sheet soft, continuing to press on stretching head 24 by forcing press moves down, and passes through stretching head
24 and lower template 21 die cavity by slice forming, stop the heating in the first thermal cycle water route 11 and the second thermal cycle water route 20, connect
Logical first SAPMAC method water route 12 and the second thermal cycle water route 19, cool down to stretching head 24 and the die cavity of lower template 21, drop thin slice
The inside bending stress of temperature and releasable material, after thin slice cooling, stops the first SAPMAC method water route 12 and the second thermal cycle water route
19 cooling, forcing press drive stretching head 24 and cope plate 18 to move up, and take out the thin slice after shaping, complete a punching press, thin slice
The internal stress produced by deformation in die cavity cool down when discharge, take out the thin slice finished product after mould deformation it is small, so as to carry
The formed precision of high sheeting.
Finally it should be noted that the above embodiments are merely illustrative of the technical solutions of the present invention, rather than the present invention is protected
The limitation of scope is protected, although being explained with reference to preferred embodiment to the present invention, those of ordinary skill in the art should
Work as understanding, can be to technical scheme technical scheme is modified or replaced equivalently, without departing from the reality of technical solution of the present invention
Matter and scope.
Claims (10)
- A kind of 1. double water route stamping dies, it is characterised in that including board gland, upper mounted plate, stretching head, cope plate, under Template and bottom plate;The board gland is fixed on upper mounted plate top, is equipped with through hole among the cope plate, it is described on Template screw is fixed on upper mounted plate lower part, and the stretching head is arranged in cope plate through hole and is fixed on upper mounted plate lower part, institute State lower template and be fixed on bottom plate top, the lower template is arranged on immediately below cope plate;Fixed plate corner is to dividing into Have guide post, the bottom plate corner is equipped with guide sleeve upwards, and the guide post can slide up and down in guide sleeve, fixed plate and Upper stretching head is internally provided with the first thermal cycle water route and the first SAPMAC method water route, and the lower template is internally provided with the second heat recirculated water Road and the second SAPMAC method water route, die cavity is offered between the stretching head and lower template.
- 2. a kind of double water route stamping dies as claimed in claim 1, it is characterised in that the first SAPMAC method water route is stretching Head is internal to be arranged on below the first thermal cycle water route, and the second SAPMAC method water route is arranged on the second thermal cycle water route inside lower template Top.
- 3. a kind of double water route stamping dies as claimed in claim 2, it is characterised in that offer positioning below the cope plate Hole, above-mentioned lower template top are equipped with positioning pin.
- 4. a kind of double water route stamping dies as claimed in claim 3, it is characterised in that the stretching head and upper mounted plate first The interface in SAPMAC method water route and the first thermal cycle water route is equipped with water proof ring.
- 5. double water routes stamping die as claimed in claim 4, it is characterised in that the cope plate and fixed plate screw connection Equipped with elastic component.
- 6. such as a kind of double water route stamping dies of claim 1-5 any one of them, it is characterised in that first heat recirculated water Road is respectively made of a plurality of aquaporin with the first SAPMAC method water route and is connected by importing and exporting pipeline, the first thermal cycle water route and First SAPMAC method water route is in concave shape, and the first thermal cycle water route is arranged in the second SAPMAC method water route groove.
- 7. a kind of double water route stamping dies as claimed in claim 6, it is characterised in that the second thermal cycle water route and second SAPMAC method water route is respectively made of a plurality of aquaporin and is connected by importing and exporting pipeline, and the second thermal cycle water route and second cold is followed Ring water route is in respectively bamboo row-like arrangement.
- 8. such as a kind of double water route stamping dies of claim 1-5 any one of them, it is characterised in that first heat recirculated water Road inlet and outlet are arranged on upper mounted plate the same side, and the second thermal cycle water route inlet and outlet are arranged on lower template the same side.
- 9. such as a kind of double water route stamping dies of claim 1-5 any one of them, it is characterised in that first cool circulation water Road inlet and outlet are arranged on the opposite both sides of upper mounted plate, and the second SAPMAC method water route inlet and outlet set the opposite both sides of template.
- 10. such as a kind of double water route stamping dies of claim 1-5 any one of them, it is characterised in that first thermal cycle Water route and the second thermal cycle water route lead to hot steam, and the first SAPMAC method water route and the second SAPMAC method water route lead to cold air.