CN107720714A - 一种制备羟基磷灰石的新方法 - Google Patents
一种制备羟基磷灰石的新方法 Download PDFInfo
- Publication number
- CN107720714A CN107720714A CN201711099239.9A CN201711099239A CN107720714A CN 107720714 A CN107720714 A CN 107720714A CN 201711099239 A CN201711099239 A CN 201711099239A CN 107720714 A CN107720714 A CN 107720714A
- Authority
- CN
- China
- Prior art keywords
- phosphate
- hydroxyapatite
- incrustation scale
- new method
- present
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
本发明涉及一种制备羟基磷灰石的新方法,具体产品废弃水垢、磷酸盐,用磷酸盐浸泡废弃水垢,置于混凝土标准养护箱里温度控制在25℃,湿度控制在98%,3天后取出。最后在105℃的烘箱里烘5h后取出。作为优选,本发明提供的一种磷酸盐,具体是水垢中的钙元素与磷酸盐中的磷元素摩尔比值为1.67;本发明能生成片状的纯度较高的羟基磷灰石,生成的羟基磷灰石有很好的吸附性。真正做到了以废治废,低能耗且操作简单,大大降低了成本。
Description
技术领域
本发明涉及水资源净化的领域,具体是一种制备羟基磷灰石的新方法。
背景技术
羟基磷灰石又名钙磷灰石,是一个很好的功能性材料,它与人体骨骼成分近似,具有良好的生物相容性和生物活性。同时它还有很好的吸附性,尤其是对于重金属离子的吸附。所以近年来已成为一种具有良好应用前景的新型材料,主要用于医疗,水净化方面等方面。
羟基磷灰石制备方法很多种,有固相反应法、液相沉淀法、水解法、溶胶-凝胶法、微乳液法以及机械化学法等。固相反应法是在水蒸气保护下高温煅烧,可以得到结晶度很高的羟基磷灰石晶体,但比表面积小,耗能且对设备要求高。液相沉淀法虽然工艺简单,成本低,但易混入杂质,纯度低。水解法是在高压环境下进行,虽然纯度高、分散性好的羟基磷灰石粉体,但对设备要求高,产量低。溶胶-凝胶法虽然可以获得均匀的纳米羟基磷灰石,但工艺复杂,不便操作,且制备过程中会对环境造成一定的污染。
发明内容
本发明的目的是提供一种制备羟基磷灰石的新方法;该方法利用了废水处理后的废弃水垢作为钙源来合成较高纯度的羟基磷灰石,达到了以废治废、操作简单、实用性强且能循环利用资源的目的。
本发明实现发明目的采用如下技术方案:
一种制备羟基磷灰石的新方法,具体产品废弃水垢、磷酸盐,用磷酸盐浸泡废弃水垢,置于混凝土标准养护箱里温度控制在25℃,湿度控制在98%,3天后取出。最后在105℃的烘箱里烘5h后取出。
作为优选,本发明提供的一种磷酸盐,具体是水垢中的钙元素与磷酸盐中的磷元素摩尔比值为1.67。
有益效果:
本发明与现有技术相比,其有益效果体现在:该发明能循环利用资源,变废为宝。同时实验条件简单,操作性强且耗能少。
附图说明
图1是羟基磷灰石的扫描电镜图
具体实施方式
以下通过具体实施例对本发明做进一步解释说明。
一种制备羟基磷灰石的新方法,具体产品有废弃水垢、磷酸盐。取废弃水垢放入已配置好的磷酸盐溶液里,密封。然后将烧杯置于混凝土标准养护箱里进行反应,混凝土标准养护箱的温度控制在25℃,湿度控制在98%。3天后取出烧杯,用去离子水反复冲洗处理后的废弃水垢,过滤。最后在105℃的烘箱里烘5h后取出。
作为优选,本发明提供的一种磷酸盐,具体是水垢中的钙元素与磷酸盐中的磷元素摩尔比值为1.67。
对于本领域技术人员而言,显然本发明不限于上述示范性实施例的细节,而且在不背离本发明的精神或基本特征的情况下,能够以其他的具体形式实现本发明。因此,无论从哪一点来看,均应将实施例看作是示范性的,而且是非限制性的,本发明的范围由所附权利要求而不是上述说明限定,因此旨在将落在权利要求的等同要件的含义和范围内的所有变化囊括在本发明内。不应将权利要求中的任何附图标记视为限制所涉及的权利要求。
此外,应当理解,虽然本说明书按照实施方式加以描述,但并非每个实施方式仅包含一个独立的技术方案,说明书的这种叙述方式仅仅是为清楚起见,本领域技术人员应当将说明书作为一个整体,各实施例中的技术方案也可以经适当组合,形成本领域技术人员可以理解的其他实施方式。
Claims (1)
1.一种制备羟基磷灰石的新方法,具体产品废弃水垢、磷酸盐,用磷酸盐浸泡废弃水垢,置于混凝土标准养护箱里温度控制在25℃,湿度控制在98%,3天后取出,最后在105℃的烘箱里烘5h后取出,作为优选,本发明提供的一种磷酸盐,具体是水垢中的钙元素与磷酸盐中的磷元素摩尔比值为1.67。