CN1075757C - Resistance plugging spot welding of vacuum pumping port with internal pressure container - Google Patents

Resistance plugging spot welding of vacuum pumping port with internal pressure container Download PDF

Info

Publication number
CN1075757C
CN1075757C CN97116094A CN97116094A CN1075757C CN 1075757 C CN1075757 C CN 1075757C CN 97116094 A CN97116094 A CN 97116094A CN 97116094 A CN97116094 A CN 97116094A CN 1075757 C CN1075757 C CN 1075757C
Authority
CN
China
Prior art keywords
spot welding
welding
vacuum pumping
plugging
pumping port
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CN97116094A
Other languages
Chinese (zh)
Other versions
CN1210049A (en
Inventor
谭文一
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
DALIAN BAOYUAN NUCLEAR EQUIPMENT CO LTD
Original Assignee
DALIAN BAOYUAN NUCLEAR EQUIPMENT CO LTD
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by DALIAN BAOYUAN NUCLEAR EQUIPMENT CO LTD filed Critical DALIAN BAOYUAN NUCLEAR EQUIPMENT CO LTD
Priority to CN97116094A priority Critical patent/CN1075757C/en
Publication of CN1210049A publication Critical patent/CN1210049A/en
Application granted granted Critical
Publication of CN1075757C publication Critical patent/CN1075757C/en
Anticipated expiration legal-status Critical
Expired - Fee Related legal-status Critical Current

Abstract

The invention discloses a resistance spot welding method for plugging a vacuum pumping port of an internal pressure container. The method adopts an SO426 type spot welding machine and special technical equipment to place a stainless steel ball for plugging on the drawing opening, and a good spot welding joint can be obtained through secondary resistance spot welding. Firstly, vacuumizing an inner cavity of an inner pressure container, filling helium to form an inner pressure of 0.103MPa, and applying pretightening force to weld by using an electrode; then, an upsetting force of 0.2 to 0.3MPa is immediately applied and welding is performed again according to the same specifications. The joint welded by the method has no burn-through phenomenon; the steel ball can not fly away and leak helium during repair welding, and the method can meet the manufacturing requirement of the cadmium sleeve for the nuclear power station and can be applied to the aspect of plugging a container with pressure.

Description

The resistance shutoff spot welding of the vacuum pumping port of band inner pressure vessel
The present invention relates to a kind of welding method, relate in particular to a kind of method of the aperture resistance shutoff spot welding of on the container of band internal pressure, implementing.
The alleged method of the present invention is to put forward according to the requirement of used in nuclear power station cadmium sleeve pipe manufacture process and the permission of nuclear equipment manufacturing standard.As everyone knows, because airtight cavity internal pressure greater than the atmospheric pressure in the external world, makes band press the shutoff of interior force container to be welded on generally speaking and can't to realize.Although the employing special measure has realized this welding, and the quality of its combination degree also will directly influence next procedure TIG repairing welding quality, so that cause flying ease or producing burning leakage phenomenon of shutoff steel ball.
The objective of the invention is to propose a kind of vacuumizing, fill three one step completed processes of operation of helium and resistance shutoff spot welding.
Technical scheme of the present invention is achieved in that
At first, adopt SO462 type mash welder to make welding equipment, what lucite was made finds time, and fills the special process equipment that the helium clamping device is done resistance spot welding, Φ 3-5mm austenitic stainless steel steel ball is placed on the vacuum pumping port of band inner pressure vessel, and welds by following technological parameter:
Electrode diameter (mm) Electrode pressure (Mpa) Welding current (A) Conduction time (S)
Φ10 0.1-0.3 11300 0.25
Secondly, the welding process comprises following two steps:
(1) special tooling is installed at the solder joint place, vacuumize desiring vacuum-pumping container, make residual pressure reach 1mbar, fill helium subsequently, make pressure reach 0.103MPa and afterwards the stainless steel steel ball is placed on taking out on the mouth of band internal pressure, put down top electrode, apply pretightning force 0.1MPa, turn-on current, preheating and welding.
(2) finish above-mentioned welding after, apply upset force 0.2-0.3MPa immediately, treat 5-15 slightly after second, adopt the same standard to carry out the resistance spot welding second time.
Method provided by the invention successfully is applied in the development of nuclear power station cadmium sleeve pipe.By macroscopical metallographic examination, can see that the fusion of steel ball and outer sleeve mother metal contact site is good, solder joint dye penetrant inspection is qualified, and vacuum leak hunting does not have leakage.
Embodiment used in nuclear power station cadmium bushing vacuum is taken out a mouthful stainless steel steel ball resistance shutoff spot welding.
Used in nuclear power station cadmium sleeve pipe is a Welding Structure, by inside and outside sleeve, and compositions such as rust chuck and base plate.Wherein, inner sleeve is 2mm, and outer sleeve is 0.8mm, and base plate is 28mm, and material is austenite stainless steel plate; The cadmium chuck is a 0.5mmCd-2 cadmium plate.The technological procedure regulation, the cadmium sleeve pipe puts the 0.8mm outer sleeve behind bag cadmium on the 2mm inner sleeve, and the employing of inside and outside sleeve lap-joint adds a pulse TIG welding and is connected together, and forms an airtight cavity.Owing to the needs of airtight cavity vacuum leak hunting, on the 0.8mm outer sleeve, be drilled with the aperture of a Φ 2.5mm, utilize it as vacuum pumping port, to airtight chamber vacuum.Residual pressure is filled the helium of 0.103MPa with during less than 1mbar again, gets lodged on the aperture of Φ 2.5mm with Φ 3mm stainless steel ball, puts down electrode and pushes down steel ball, adds pretightning force 0.1MPa earlier, connects power supply then, preheating and welding; Immediately add the upset force of 0.2-0.3MPa.Behind the clock, adopt identical welding conditions in several seconds, carry out the resistance spot welding second time.So, can obtain in the interlayer of cadmium sleeve pipe to keep the helium of 0.103MPa pressure, the solder joint place does not have the resistance shutoff solder joint of any leakage.
The partial sectional view of present embodiment is shown in the drawings.Wherein:
(1) inner sleeve (2) Cd-2 cadmium chuck (3) outer sleeve (4) specific welding assambly
(5) stainless steel steel ball (6) vacuum pumping port (7) battery lead plate.

Claims (1)

1. resistance shutoff spot welding with the vacuum pumping port of inner pressure vessel is characterized in that the technical process of this method comprises:
A. make welding equipment with SO462 type mash welder, what lucite was made vacuumizes, and fills helium, and clamping device is made special tooling, Φ 3-Φ 5mm austenitic stainless steel steel ball is seated on the vacuum pumping port of band inner pressure vessel, and
B. take out at this and install special tooling on mouth and begin to vacuumize, make its residual pressure reach 1mbar, fill helium subsequently, after pressure reaches 0.103MPa, put down the pole plate that diameter is Φ 10mm, add pretightning force 0.1MPa, connect power supply, keep electric current 11300 peaces, switched on 0.25 second, preheating and welding, postwelding should promptly add upset force 0.2-0.3Mpa, treats that slightly 5-15 carries out the resistance spot welding second time with the same standard after second again.
CN97116094A 1997-09-04 1997-09-04 Resistance plugging spot welding of vacuum pumping port with internal pressure container Expired - Fee Related CN1075757C (en)