CN107323064A - A kind of Anti-bubble pastes the processing technology of more convenient decorative patch - Google Patents
A kind of Anti-bubble pastes the processing technology of more convenient decorative patch Download PDFInfo
- Publication number
- CN107323064A CN107323064A CN201710636532.8A CN201710636532A CN107323064A CN 107323064 A CN107323064 A CN 107323064A CN 201710636532 A CN201710636532 A CN 201710636532A CN 107323064 A CN107323064 A CN 107323064A
- Authority
- CN
- China
- Prior art keywords
- base stock
- square meter
- lines
- grams
- facestock
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
The invention discloses the processing technology that a kind of Anti-bubble pastes more convenient decorative patch, comprise the following steps:The PE films of base stock:Film machine is adjusted to low corona, temperature setting is at 200 degree, first pass takes plastic pellet to carry out first time film to base stock according to every 13 grams of square meter, then base stock is waited to take plastic pellet to carry out second of film to base stock for 6.5 grams per square meter after drying, base stock takes plastic pellet to carry out third time film to base stock for 2 grams per square meter after drying;Base stock is embossed;Facestock is embossed:With customization texturizing equipment, with the second lines mould, the lines of the lines of the second lines mould and the first lines mould is just fastened, and needs the place embossed to emboss base stock;Base stock applies silicone oil;Base stock gluing;Base stock and facestock are compound.Above-mentioned technical proposal, solves general decor patch because causing the caducous drawback that is pasted not strongly between facestock and base stock because there is bubble, the product bubble-free of this technique is produced, facestock and base stock stickup it is firm.
Description
Technical field
The present invention relates to decorative paste technical field, and in particular to a kind of Anti-bubble pastes the processing work of more convenient decorative patch
Skill.
Background technology
Wall paster, is the call that wall is attached to foreign countries!Teacher of the being designed's design exhibition in French household fair in 06 year of wall paster
Go out!Dealer is adornd by getting home from this and wall patch fan is pursued!Become much more popular all the way!Domestic wall patch is that occurred simultaneously since 07 year
Come into vogue, wall paster is currently most popular local decoration in the world!
Existing general decor patch goes back Shortcomings:Because between facestock and base stock when existing general decor is attached to processing
There is bubble and cause to be pasted not strongly, easy to fall off, service life is short, poor practicability.
The content of the invention
In view of the deficienciess of the prior art, being produced it is an object of the invention to provide bubble-free between a kind of facestock and base stock
Raw, facestock and base stock firm pasting, Anti-bubble easy to operate, high in machining efficiency paste the processing technology of more convenient decorative patch.
To achieve the above object, the invention provides following technical scheme:A kind of Anti-bubble pastes more convenient decorative patch
Processing technology, comprises the following steps:
(1) the PE films of base stock:Film machine is adjusted to low corona, temperature setting at 200 degree, first pass take plastic pellet by
First time film is carried out to base stock according to every 13 grams of square meter, then waits base stock to take plastic pellet per 6.5 grams of square meter to base stock after drying
Second of film is carried out, base stock takes plastic pellet to carry out third time film to base stock for 2 grams per square meter after drying;
(2) base stock is embossed:With customization texturizing equipment, the place embossed is needed to press base stock with the first lines mould
Line;
(3) facestock is embossed:With customization texturizing equipment, with the second lines mould, the lines and first of the second lines mould
The lines of lines mould is fastened, and needs the place embossed to emboss base stock;
(4) base stock applies silicone oil:The temperature for customizing texturizing equipment is set as 155 degree, it is every 3.5 grams of square meter to take silicone oil amount,
It is per 2 grams of square meter that silicone oil amount is taken after being dried Deng base stock;
(5) base stock gluing:The temperature of glue application device is set as 155 degree, taking adhesive waits base stock to dry per 32 grams of square meter
Afterwards, taking adhesive is per 10 grams of square meter;
(6) base stock and facestock are compound:Equipment complex temperature is set as 155 degree, pressure is 2.5-3.5Pa.
By using above-mentioned technical proposal, general decor patch is solved because being made between facestock and base stock because there is bubble
Into being pasted not strongly, caducous drawback is easy to operate, high in machining efficiency, without gas between the product facestock and base stock that process
Bubble is produced, facestock and base stock firm pasting, service life length, practicality are good.
The present invention is further arranged to:Step (2), texturizing equipment pressure is set in 2.5-3.5Pa, and the time is set as 1.3
- 1.5 seconds second.By this setting, the lines pressed out is unlikely to deform, restored, and shape is consolidated.
The present invention is further arranged to:Step (3), texturizing equipment pressure is set in 2.5-3.5Pa, and the time is set as 1.3
- 1.5 seconds second.By this setting, bubble-free generation, facestock and base stock firm pasting between facestock and base stock.
It is an advantage of the invention that:Compared with prior art, solve general decor patch because between facestock and base stock because
There is bubble and cause to be pasted not strongly, caducous drawback is easy to operate, high in machining efficiency, the product facestock processed and bottom
Bubble-free generation, facestock and base stock firm pasting, service life length, practicality are good between paper.
With reference to specific embodiment, the invention will be further described.
Embodiment
A kind of Anti-bubble disclosed by the invention pastes the processing technology of more convenient decorative patch, it is characterised in that:Including following
Step:
(1) the PE films of base stock:Film machine is adjusted to low corona, temperature setting at 200 degree, first pass take plastic pellet by
First time film is carried out to base stock according to every 13 grams of square meter, then waits base stock to take plastic pellet per 6.5 grams of square meter to base stock after drying
Second of film is carried out, base stock takes plastic pellet to carry out third time film to base stock for 2 grams per square meter after drying;This technical scheme,
The transparency of base stock leaching membrane layer is very high, leaching membrane layer corrosion difficult for drop-off.
(2) base stock is embossed:With customization texturizing equipment, the place embossed is needed to press base stock with the first lines mould
Line;
(3) facestock is embossed:With customization texturizing equipment, with the second lines mould, the lines and first of the second lines mould
The lines of lines mould is fastened, and needs the place embossed to emboss base stock;
(4) base stock applies silicone oil:The temperature for customizing texturizing equipment is set as 155 degree, it is every 3.5 grams of square meter to take silicone oil amount,
It is per 2 grams of square meter that silicone oil amount is taken after being dried Deng base stock;So high temperature resistant, protection against the tide, grease proofing characteristic are optimal.
(5) base stock gluing:The temperature of glue application device is set as 155 degree, taking adhesive waits base stock to dry per 32 grams of square meter
Afterwards, taking adhesive is per 10 grams of square meter;
(6) base stock and facestock are compound:Equipment complex temperature is set as 155 degree, pressure is 2.5-3.5Pa.
As preferred, step (2), texturizing equipment pressure is set in 2.5-3.5Pa, and the time is set as 1.3 seconds -1.5
Second.By this setting, the lines pressed out is unlikely to deform, restored, and shape is consolidated.
As preferred, step (3), texturizing equipment pressure is set in 2.5-3.5Pa, and the time is set as 1.3 seconds -1.5
Second.By this setting, bubble-free generation, facestock and base stock firm pasting between facestock and base stock.
The present invention solves general decor patch because of causing to be pasted not strongly because there is bubble between facestock and base stock, easily de-
The drawbacks of falling, easy to operate, high in machining efficiency, bubble-free generation, facestock and bottom between the product facestock and base stock that process
Paper firm pasting, service life length, practicality are good.
Above-described embodiment is served only for that the present invention is further described, it is impossible to be interpreted as to the specific descriptions of the present invention
Limiting the scope of the present invention, it is non-that the technician of this area makes some according to the content of foregoing invention to the present invention
The modifications and adaptations of essence are each fallen within protection scope of the present invention.
Claims (3)
1. a kind of Anti-bubble pastes the processing technology of more convenient decorative patch, it is characterised in that:Comprise the following steps:
(1) the PE films of base stock:Film machine is adjusted to low corona, temperature setting is at 200 degree, and first pass takes plastic pellet according to every
13 grams of square meter carries out first time film to base stock, then waits base stock to take plastic pellet to be carried out per square meter to base stock for 6.5 grams after drying
Second of film, base stock takes plastic pellet to carry out third time film to base stock for 2 grams per square meter after drying;
(2) base stock is embossed:With customization texturizing equipment, the place embossed is needed to emboss base stock with the first lines mould;
(3) facestock is embossed:With customization texturizing equipment, with the second lines mould, the lines and the first lines of the second lines mould
The lines of mould is fastened, and needs the place embossed to emboss base stock;
(4) base stock applies silicone oil:The temperature for customizing texturizing equipment is set as 155 degree, it is, per 3.5 grams of square meter, to wait bottom to take silicone oil amount
Paper takes silicone oil amount to be per 2 grams of square meter after drying;
(5) base stock gluing:The temperature of glue application device is set as 155 degree, taking adhesive is waited after base stock dries per 32 grams of square meter,
Taking adhesive is per 10 grams of square meter;
(6) base stock and facestock are compound:Equipment complex temperature is set as 155 degree, pressure is 2.5-3.5Pa.
2. a kind of Anti-bubble according to claim 1 pastes the processing technology of more convenient decorative patch, it is characterised in that:Step
(2), texturizing equipment pressure is set in 2.5-3.5Pa, and the time is set as 1.3 seconds -1.5 seconds.
3. a kind of Anti-bubble according to claim 2 pastes the processing technology of more convenient decorative patch, it is characterised in that:Step
(3), texturizing equipment pressure is set in 2.5-3.5Pa, and the time is set as 1.3 seconds -1.5 seconds.