CN107024805A - A kind of display panel to cassette method and display panel - Google Patents

A kind of display panel to cassette method and display panel Download PDF

Info

Publication number
CN107024805A
CN107024805A CN201710427600.XA CN201710427600A CN107024805A CN 107024805 A CN107024805 A CN 107024805A CN 201710427600 A CN201710427600 A CN 201710427600A CN 107024805 A CN107024805 A CN 107024805A
Authority
CN
China
Prior art keywords
liquid crystal
substrate
display panel
state
solid
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201710427600.XA
Other languages
Chinese (zh)
Inventor
袁旭晨
刘汉青
张乐
刘泽
李鑫
朱红
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
BOE Technology Group Co Ltd
Beijing BOE Optoelectronics Technology Co Ltd
Original Assignee
BOE Technology Group Co Ltd
Beijing BOE Optoelectronics Technology Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by BOE Technology Group Co Ltd, Beijing BOE Optoelectronics Technology Co Ltd filed Critical BOE Technology Group Co Ltd
Priority to CN201710427600.XA priority Critical patent/CN107024805A/en
Publication of CN107024805A publication Critical patent/CN107024805A/en
Pending legal-status Critical Current

Abstract

The present invention disclose a kind of display panel to cassette method, the display panel includes first substrate and second substrate, and methods described includes, the sprinkling solid-state liquid crystal on the first substrate;Sealant is coated in the neighboring area of the second substrate;The first substrate and the second substrate are carried out to box;The sealant is subjected to curing process;Wherein, it is described to box and the curing process during the liquid crystal be in solid-state.By the sprinkling of solid-state liquid crystal on the first substrate, and keeping liquid crystal to be in solid-state box and curing process process, can effectively prevent to box and to box into solidification process due to puncture phenomenon that the mobility of liquid crystal is caused to sealant.

Description

A kind of display panel to cassette method and display panel
Technical field
The present invention relates to display technology field, more particularly to a kind of display panel to cassette method and display panel.
Background technology
Available liquid crystal panel product to the general use liquid crystal of box technique be added dropwise (one drop fill, ODF) → vacuum pair Box → UV solidifies the technological process of sealant, and whole process is carried out at normal temperatures substantially.
In liquid crystal dropping apparatus, liquid crystal is instilled on array or color membrane substrates with the state of liquid crystal state, sealant coating Onto another substrate.Then the liquid crystal that will instil respectively is transmitted with being coated with the color film of sealant with array base palte by manipulator To vacuum in cartridge device, the two is completed to box in sealed vacuum chamber, then discharges vacuum pressure.The preliminary base completed to box The solidification of sealant is completed in the equipment that plate circulation solidifies to UV.
Due to liquid crystal by the mobility of itself full of space in box, box is near completion to UV this section before solidifying when In, liquid crystal can cause certain impact to surrounding sealant, and now sealant is uncured soft state, and chemistry is living Jerk is high, and easily being impacted by liquid crystal is influenceed, and forms the hole of internal thorn-like, is referred to as interior puncture.Puncture can cause it is a series of not It is good, such as break glue, liquid crystal leakage, electrostatic breakdown.
The content of the invention
The invention provides a kind of display panel to cassette method and display panel, to solve display panel in the prior art The problem of sealant is punctured during to box.
In a first aspect, the present invention provide a kind of display panel to cassette method, including:Sprayed on the first substrate solid State liquid crystal;
Sealant is coated in the neighboring area of the second substrate;
The first substrate and the second substrate are carried out to box;
The sealant is subjected to curing process;
Wherein, it is described to box and the curing process during the liquid crystal be in solid-state.
Alternatively, it is described that box and the curing process process are carried out in the cryogenic vacuum chamber of same equipment.
Alternatively, it is described to box and the solidification process after the completion of, the chamber recovers normal temperature and pressure state, makes described solid State liquid crystalline transition is liquid crystal state and the space formed full of the first substrate, the sealant and the second substrate.
Alternatively, the environment temperature in the cryogenic vacuum chamber is less than -40 DEG C.
Alternatively, the environment temperature in the cryogenic vacuum chamber is less than -50 DEG C.
Alternatively, the solid-state liquid crystal is in powdered, and the diameter of the powder of the solid-state liquid crystal is less than 3um.
Alternatively, the diameter of the powder of the solid-state liquid crystal is less than 1um.
Alternatively, it is described that the sealant is subjected to curing process, including:
Ultraviolet light UV solidifications are carried out to the sealant.
Second aspect, the present invention provides the display panel that a kind of use above method is made.
Compared with prior art, the embodiment of the present invention has advantages below:
By the sprinkling of solid-state liquid crystal on the first substrate, and liquid crystal is being kept to be in solid-state in box and curing process process, Can effectively prevent to box and to box into solidification process due to puncture phenomenon that the mobility of liquid crystal is caused to sealant.
Brief description of the drawings
Fig. 1 show a kind of display panel provided in an embodiment of the present invention to cassette method flow chart;
Fig. 2 show another display panel provided in an embodiment of the present invention to cassette method flow chart;
The technological process to cassette method that Fig. 3 a~d show a kind of display panel provided in an embodiment of the present invention is illustrated Figure.
Embodiment
Below in conjunction with the accompanying drawing in the embodiment of the present invention, the technical scheme in the embodiment of the present invention is carried out clear, complete Site preparation is described, it is clear that described embodiment is a part of embodiment of the invention, rather than whole embodiments.Based on this hair Embodiment in bright, those of ordinary skill in the art's every other implementation acquired under the premise of creative work is not made Example, belongs to the scope of protection of the invention.
The embodiment that the present invention is provided, reference picture 1 and Fig. 3 a~d, wherein Fig. 1 is one kind provided in an embodiment of the present invention Display panel to cassette method flow chart, Fig. 3 a~d is a kind of display panel provided in an embodiment of the present invention to cassette method Process flow diagram.
The embodiment comprises the following steps:
Step 101, solid-state liquid crystal is sprayed on the first substrate.
The liquid crystal of liquid crystal state has stronger mobility, causes to wear because the flowing of liquid crystal can carry out impact to sealant Thorn, and the liquid crystal mobility of solid-state is weaker, it is not easy to sealant impact is caused to puncture.
Liquid crystal state is under liquid crystal normal temperature, but at low temperature, when temperature is less than -40 DEG C, liquid crystal presented solid-state, because This, sprinkling solid-state liquid crystal needs to keep ambient temperature to be less than -40 DEG C.In order to ensure that liquid crystal is fully in solid-state, it is preferable that Ambient temperature is kept to be less than -50 DEG C.
During solid-state liquid crystal is sprayed at into first substrate, influence can be produced on the surface of first substrate because of friction, Therefore the diameter that the powder of solid-state liquid crystal may be selected is less than 3um, to weaken due to the shadow that the surface rubbed to first substrate is caused Ring.Certainly, the diameter of the powder of solid-state liquid crystal is the smaller the better, it is therefore preferable that diameter is less than 1um solid-state liquid crystal powder.
Step 102, sealant is coated in the neighboring area of the second substrate.
In the step, the neighboring area of the second substrate of sealant coating corresponds to the non-display area of display panel.
After step 101 and step 102, the structure of formation can refer to shown in Fig. 3 a.
Step 103, the first substrate and the second substrate are carried out to box.
The side of second substrate coating sealant is carried out pair to the side that liquid crystal is sprayed to first substrate in cartridge device Box.
Step 104, the sealant is subjected to curing process.
Because liquid crystal state liquid crystal can be punctured caused by mobility is to sealant, therefore, in above-mentioned steps 103 and step 104 In, liquid crystal is still to keep solid-state.
In step 103, two substrates are carried out in the vacuum chamber to cartridge device to box, due to needing to keep liquid Crystalline substance is in solid-state, therefore the chamber also needs to keep low temperature environment.Equally, at step 104, when being solidified, still also need Keep low temperature environment.Above-mentioned low temperature environment preferable temperature is less than -50 DEG C, to ensure that liquid crystal is fully in solid-state.
Structure by step 103 and step 104 formation can refer to shown in Fig. 3 b and 3c.
Wherein, after step 103 terminates, it can discharge in vacuum pressure, recovery to atmospheric pressure state, step 104, as long as keeping Low-temperature condition, you can avoid because of liquid crystal mobility in the curing process to the puncture caused by sealant.
By the above, the embodiment of the present invention has advantages below:
By the sprinkling of solid-state liquid crystal on the first substrate, and liquid crystal is being kept to be in solid-state in box and curing process process, Can effectively prevent to box and to box into solidification process due to puncture phenomenon that the mobility of liquid crystal is caused to sealant.
However, the negative pressure of vacuum chamber can be being discharged to the complete preliminary completion rear chamber of box, during pressure is discharged, greatly The periphery that gas flows into impact sealant is measured, because sealant now is uncured soft state, sealant is easily caused Outer puncture phenomenon;And curing apparatus is being transferred to two substrates of the preliminary completion of box, solidification process is carried out to sealant In, the environment that continue holding low temperature is relatively difficult, if low temperature environment can not be kept, solid-state liquid crystal can be transformed into liquid crystal State, and then due to its mobility, sealant impact is caused to puncture.
If being carried out in view of above-mentioned to box and solidification process in two equipment, keep the solid-state of liquid crystal relatively difficult, because This, will can be carried out to box and curing process process in the cryogenic chamber of same equipment, can so avoid to after the completion of box because The outer puncture for discharging vacuum chamber negative pressure and being caused to sealant, can also be avoided because being not easy to keep low-temperature condition so that solid-state liquid The interior puncture that crystalline substance is transformed into liquid crystal state liquid crystal and caused to sealant.Further, since liquid crystal is being solid-state less than -40 DEG C, therefore, Environment temperature in the cryogenic vacuum chamber of the equipment should also be below -40 DEG C.At -50 DEG C, liquid crystal can fully be in solid-state, because This, preferably the environment temperature in cryogenic vacuum chamber is less than -50 DEG C.
Another embodiment that the present invention is provided, reference picture 2 simultaneously combines Fig. 3 a~d, and wherein Fig. 2 provides for the embodiment of the present invention Another display panel to cassette method flow chart, Fig. 3 a~d is a kind of pair of display panel provided in an embodiment of the present invention The process flow diagram of cassette method.
The embodiment specific steps are as shown in Fig. 2 can include:
Step 201, solid-state liquid crystal is sprayed on the first substrate.
The liquid crystal of liquid crystal state has stronger mobility, causes to wear because the flowing of liquid crystal can carry out impact to sealant Thorn, and the liquid crystal mobility of solid-state is weaker, it is not easy to sealant impact is caused to puncture.
Liquid crystal state is under liquid crystal normal temperature, but at low temperature, when temperature is less than -40 DEG C, liquid crystal presented solid-state, because This, sprinkling solid-state liquid crystal needs to keep ambient temperature to be less than -40 DEG C.In order to ensure that liquid crystal is fully in solid-state, it is preferable that By temperature control less than -50 DEG C.
During solid-state liquid crystal is sprayed at into first substrate, influence can be produced because of the surface rubbed on first substrate, because This diameter that the powder of solid-state liquid crystal may be selected is less than 3um, to weaken due to the influence that the surface rubbed to first substrate is caused. Certainly, the diameter of the powder of solid-state liquid crystal is the smaller the better, it is therefore preferable that diameter is less than 1um solid-state liquid crystal powder.
Step 202, sealant is coated in the neighboring area of the second substrate.
In the step, the neighboring area of the second substrate of sealant coating corresponds to the non-display area of display panel.
After step 201 and step 202, the structure of formation can refer to shown in Fig. 3 a.
Step 203, the first substrate and the second substrate are carried out to box in cryogenic vacuum chamber.
The side of second substrate coating sealant is to spraying the side of liquid crystal to first substrate true to the low temperature of cartridge device Carried out in plenum chamber to box.
Step 204, curing process is carried out to sealant in cryogenic vacuum chamber.
Step 203 and step 204 are carried out in same cryogenic vacuum chamber, can so avoid to after the completion of box because The outer puncture for discharging vacuum chamber negative pressure and being caused to sealant, can also be avoided because being not easy to keep low-temperature condition so that solid-state liquid The interior puncture that crystalline substance is transformed into liquid crystal state and caused to sealant.Further, since liquid crystal-less than -40 DEG C be solid-state, therefore, should Environment temperature in the cryogenic vacuum chamber of equipment should also be below -40 DEG C.At -50 DEG C, liquid crystal can fully be in solid-state, because This, preferably the environment temperature in cryogenic vacuum chamber is less than -50 DEG C.
Structure by step 203 and step 204 formation can refer to shown in Fig. 3 b and 3c.
In above-mentioned all solidification process, alternatively, curing process is carried out to sealant using ultraviolet light UV solidifications.Ultraviolet light UV is cured as the curing commonly used in sealant solidification, implements fairly simple.
Step 205, chamber is made to recover normal temperature and pressure state, solid-state liquid crystalline transition is liquid crystal state and is full of first base The space of plate, the sealant and second substrate formation.
It is above-mentioned to box and solidification process after the completion of, solid-state liquid crystal needs to be changed into liquid crystal state, and full of two substrates with The space that sealant is surrounded, because now sealant has been cured, the liquid crystal of liquid crystal state is caused due to mobility to sealant After impact, the phenomenon of interior puncture is not resulted in yet.In addition, completed in above-mentioned same cryogenic vacuum chamber to box and solidification after, The chamber recovers during normal pressure, because sealant has been cured, after now ambient atmos impact to sealant, also will not Cause outer puncture phenomenon.
After step 205, formed shown in structure reference picture 3d.
Above-mentioned first substrate can be array base palte, and second substrate can be color membrane substrates.Alternatively, above-mentioned first base Plate can be color membrane substrates, and second substrate can be array base palte.
By the above, the embodiment of the present invention includes advantages below:
By the sprinkling of solid-state liquid crystal on the first substrate, and liquid crystal is being kept to be in solid-state in box and curing process process, Can effectively prevent to box and to box into solidification process due to puncture phenomenon that the mobility of liquid crystal is caused to sealant.Will Box and curing process process carried out in the cryogenic vacuum chamber of same equipment, it is to avoid because transfer is needed after the completion of preliminary to box The negative pressure for discharging vacuum chamber causes the outer puncture phenomenon of sealant, and in same equipment, it is to avoid branching program, section The time has been saved, the efficiency to box and solidification is improved.
The embodiment of the present invention additionally provides a kind of display panel, and it uses the display panel that above-described embodiment method is made.
Display panel provided in an embodiment of the present invention can apply to liquid crystal display, LCD TV, DPF, hand Machine, tablet personal computer etc. have the product of display function, and this present invention is not limited.
Each embodiment in this specification is described by the way of progressive, what each embodiment was stressed be with Between the difference of other embodiment, each embodiment identical similar part mutually referring to.For system embodiment For, because it is substantially similar to embodiment of the method, so description is fairly simple, referring to the portion of embodiment of the method in place of correlation Defend oneself bright.
Although having been described for the preferred embodiment of the embodiment of the present invention, those skilled in the art once know base This creative concept, then can make other change and modification to these embodiments.So, appended claims are intended to be construed to Including preferred embodiment and fall into having altered and changing for range of embodiment of the invention.
Finally, in addition it is also necessary to explanation, herein, such as first and second or the like relational terms be used merely to by One entity or operation make a distinction with another entity or operation, and not necessarily require or imply these entities or operation Between there is any this actual relation or order.Moreover, term " comprising ", "comprising" or its any other variant meaning Covering including for nonexcludability, so that process, method, article or terminal device including a series of key elements are not only wrapped Those key elements, but also other key elements including being not expressly set out are included, or also include being this process, method, article Or the intrinsic key element of terminal device.In the absence of more restrictions, by wanting that sentence "including a ..." is limited Element, it is not excluded that also there is other identical element in the process including the key element, method, article or terminal device.
The foregoing is only a specific embodiment of the invention, but protection scope of the present invention is not limited thereto, any Those familiar with the art the invention discloses technical scope in, change or replacement can be readily occurred in, should all be contained Cover within protection scope of the present invention.Therefore, protection scope of the present invention should be defined by scope of the claims.

Claims (9)

1. a kind of display panel to cassette method, the display panel include first substrate and second substrate, it is characterised in that bag Include:
Solid-state liquid crystal is sprayed on the first substrate;
Sealant is coated in the neighboring area of the second substrate;
The first substrate and the second substrate are carried out to box;
The sealant is subjected to curing process;
Wherein, it is described to box and the curing process during the liquid crystal be in solid-state.
2. display panel according to claim 1 to cassette method, it is characterised in that it is described to box and the curing process Process is carried out in the cryogenic vacuum chamber of same equipment.
3. display panel according to claim 2 to cassette method, it is characterised in that also include:
It is described to box and the solidification process after the completion of, the chamber recovers normal temperature and pressure state, makes the solid-state liquid crystalline transition For liquid crystal state and full of the space of the first substrate, the sealant and second substrate formation.
4. display panel according to claim 2 to cassette method, it is characterised in that the ring in the cryogenic vacuum chamber Border temperature is less than -40 DEG C.
5. display panel according to claim 4 to cassette method, it is characterised in that the ring in the cryogenic vacuum chamber Border temperature is less than -50 DEG C.
6. display panel according to claim 1 to cassette method, it is characterised in that the solid-state liquid crystal in powdered, And the diameter of the powder of the solid-state liquid crystal is less than 3um.
7. display panel according to claim 6 to cassette method, it is characterised in that the powder of the solid-state liquid crystal it is straight Footpath is less than 1um.
8. display panel according to claim 1 to cassette method, it is characterised in that it is described to be consolidated the sealant Change is handled, including:
Ultraviolet light UV solidifications are carried out to the sealant.
9. a kind of display panel that cassette method is made of the display panel described in use claim any one of 1-8.
CN201710427600.XA 2017-06-08 2017-06-08 A kind of display panel to cassette method and display panel Pending CN107024805A (en)