CN106949316B - Hole measuring method is protected in one kind open loop on titanium composite panel chimney wall - Google Patents
Hole measuring method is protected in one kind open loop on titanium composite panel chimney wall Download PDFInfo
- Publication number
- CN106949316B CN106949316B CN201710173255.1A CN201710173255A CN106949316B CN 106949316 B CN106949316 B CN 106949316B CN 201710173255 A CN201710173255 A CN 201710173255A CN 106949316 B CN106949316 B CN 106949316B
- Authority
- CN
- China
- Prior art keywords
- probe tube
- wall
- flange
- titanium composite
- chimney
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Active
Abstract
The present invention relates to power plant stack gas to administer environment protection field, provides one kind open loop on titanium composite panel chimney wall and protects hole measuring method.Round measured hole is opened up in titanium composite panel chimney wall, passes through measured hole by the jacketed polytetrafluoroethylene (PTFE) soft rubber gasket of the probe tube for having welded alloy flange, then from inner wall of stack, that is, titanium liner side by the probe tube, and guarantee that inner wall of stack is close to alloy flange;On probe tube apart from the outside of chimney at siding 50mm weld a conventional carbon steel flange, single ended bolt is passed through into the simple steel flange against titanium composite flue outer wall, top nut is covered in the another side screw rod of simple steel flange simultaneously, fastening bolt and nut make screw rod hold out against chimney exterior panel, another simple steel flange is installed in the another side of probe tube, polytetrafluoroethylene (PTFE) soft rubber gasket and blind plugging plate are put on simultaneously, that is, completes installation.Technical solution of the present invention cost savings, easy for construction, weight bearing power is strong, and efficiently solves the etching problem after titanium composite panel chimney wall aperture.
Description
Technical field
The present invention relates to power plant stack gas to administer environment protection field, in particular to one kind open loop on titanium composite panel chimney wall is protected
Hole measuring method.
Background technique
Titanium composite panel (inner steel lining titanium, general titanium is with a thickness of 1.2mm) has good anti-corrosion effect, in China's thermal power generation
Factory has a large amount of titanium composite chimneys to be currently running.Since national environmental protection policy is more and more tighter, new standard and code requirement are increasingly
After height, especially minimum discharge policy implementation, newly-increased measuring point need to be needed on built titanium composite panel chimney or compares sampling hole
(gaging hole pipeline DN00 or so), is just able to satisfy code requirement.
Since titanium material can not be connect with steel plate (including steel alloy) by welding manner, titanium high temperature resistant only has 300 DEG C of left sides
The quality on the right side, temperature high titanium again will change, and the quality that common steel tube directly affects titanium is welded on titanium composite panel, thus
Influence its anti-corrosion effect.Chimney siding is routinely opened there are two types of measured hole methods: first is that the aperture on chimney, cleaning hole periphery lining
Titanium welds carbon steel measurement pipe and chimney wall carbon steel, titanium is then served as a contrast inside measurement pipe, then weld with chimney lining titanium, is formed
Obturator solves anti-corrosion.Second is that measurement pipe generally titanium, after chimney wall aperture, the titanium tube road and chimney titanium liner are welded
It connects, forms seal, solve anti-corrosion.
First method: due to gaging hole caliber very little, the requirement of titanium lined technique is high and very cumbersome, while when carbon steel welding
High temperature can damage titanium lined, influence chimney lining titanium total quality, carry out risk to anticorrosion belt.
Second method: titanium is relatively soft, and intensity is inadequate, can not the heavier measuring instrumentss of load;And titanium is expensive, sexual valence
It is higher than not;Construction is inconvenient, and titanium plate welding needs professional that could complete.
Therefore, a kind of material cheap, easy for construction is found, also wants to solve anti-corrosion with titanium interliner well
Technique is crucial.
Summary of the invention
The purpose of the present invention is to the above technical problems, provide one kind open loop on titanium composite panel chimney wall and protect gaging hole
Method, it is save the cost, easy for construction, and effectively solve etching problem.
Technical problem of the invention is mainly addressed by following technical proposals:
(1) material prepares: a root timber matter is 316L, diameter 100mm, length 300mm pipeline are as probe tube, mating
316L alloy flange 1, mating simple steel flange 2, mating blind plugging plate 1, mating bolt and each 8 totally 16, nut are mating
Polytetrafluoroethylene (PTFE) soft rubber gasket 2, alloy electrode is several;
(2) it will use to be fully welded with alloy electrode between measurement probe tube one end and alloy flange and connect;
(3) measurement probe tube installation site is chosen on titanium composite panel wall, opens measured hole, size with plasma cutting machine
For 110mm;
(4) by the jacketed polytetrafluoroethylene (PTFE) soft rubber gasket of the 316L probe tube of welding alloy flange, then from chimney
The probe tube is passed through measured hole by inner wall, that is, titanium liner side, and guarantees that inner wall of stack is close to alloy flange;
(5) apart from a conventional carbon steel flange is welded on the outside of chimney at siding 50mm on 316L probe tube, by single ended bolt
The simple steel flange is passed through against titanium composite flue outer wall, while covering top nut, fastening bolt and spiral shell in the another side screw rod of simple steel flange
Mother makes screw rod hold out against chimney exterior panel, and same method installs other screw bolt and nut;
(6) another simple steel flange is installed in the another side of 316L probe tube, at the same put on polytetrafluoroethylene (PTFE) soft rubber gasket and
Blind plugging plate, that is, be installed.
The beneficial effects of the present invention are: installation is simple, without special anticorrosion process is done again, without the welding (titanium in titanium plate
Welding needs special welder, and technique is more complex);Materials are convenient, and material price is cheap, and weight bearing power is strong;It efficiently solves
The difficult point of measurement pipeline is installed in aperture additional on titanium composite panel, it is ensured that measurement pipeline and one closing of titanium liner formation are whole, solve
Etching problem after Wet chimney titanium composite panel aperture has and promotes applied value well.
Detailed description of the invention
Fig. 1 is to be installed rear structural schematic diagram using the present invention.
In figure: 1. carbon steel sidings;2. titanium liner;3. probe tube;4. alloy flange;5. gasket;6. simple steel flange;7. spiral shell
Bolt;8. nut;9. blind plugging plate.
Specific embodiment
Below with reference to the embodiments and with reference to the accompanying drawing the technical solutions of the present invention will be further described.
Hole measuring method is protected in one kind open loop on titanium composite panel chimney wall, is arranged on titanium composite panel chimney wall, the titanium is multiple
Plywood chimney wall includes outside carbon steel siding 1 and inside titanium liner 2, and the titanium composite panel chimney wall opens up round measured hole, also
Including probe tube 3, described 3 one end of probe tube is equipped with alloy flange 4 and is fully welded and connects, and the jacketed gasket of the probe tube 35 is in alloyage
Blue 4 sides, and fixed from inside to outside across measured hole, on the inside of its alloy flange 4 of probe tube 3 and titanium composite panel chimney after fixing
Titanium liner 2 is close to;The welding of simple steel flange 6 is additionally provided on the probe tube 3, which is also locked by bolt 7 and nut 8
Tight 1 outside of carbon steel siding;3 outermost end of probe tube is additionally provided with another simple steel flange 6, gasket 5 and a blind plugging plate 9.
The probe tube 3 is 316L steel pipe.The 3 internal diameter 100mm of probe tube, length 300mm.Carbon on the probe tube 3
Steel flange 6 is away from siding 50mm on the outside of chimney, and residue length is greater than 50mm after the bolt 7 passes through simple steel flange 6.The gasket 5
For soft PTFE rubber pad.
Embodiment:
By taking a piece measurement pipeline (DN100mm, length 300mm) of installation as an example:
1, material prepares:
At 55 DEG C or so, condensed water contains very high chloride ion, pH value 3 or so for wet flue gas temperature after desulfurization,
There is very strong corrosivity, it is necessary to the alloy material of 316L or more be selected just to be able to satisfy corrosion-resistant requirement.
One root timber matter is 316L, diameter 100mm, length 300mm pipeline are as probe tube 3, mating 316L standard alloy
Flange 4 one, mating ordinary steel pipeline simple steel flange 6 two, mating blind plugging plate 9 one, mating bolt 7 and 8 each 8, nut
Totally 16, mating soft PTFE rubber pad, i.e. 5 two, gasket, alloy electrode is several.
2, measurement 3 one end of probe tube and alloy flange 4 are fully welded and are connect (with alloy electrode);
3, measurement 3 installation site of probe tube is chosen on titanium composite panel wall, opens measured hole, size with plasma cutting machine
For 110mm;
4, by 3 jacketed polytetrafluoroethylene (PTFE) cushion films 5 of the 316L probe tube of welding alloy flange 4, then out of chimney
The probe tube 3 is passed through measured hole by wall, that is, titanium liner side, and guarantees that inner wall of stack is close to alloy flange 4;
5, apart from a conventional carbon steel flange 6 is welded on the outside of chimney at siding 50mm on 316L probe tube 3, by single ended bolt
7 pass through the simple steel flange 6 against titanium composite flue outer wall, while covering top nut 8, fastening bolt in the another side screw rod of simple steel flange 6
7 and nut 8 so that screw rod is held out against chimney exterior panel, same method installs other bolts 7 and nut 8.
6, another simple steel flange 6 is installed in the another side of 316L probe tube 3, while puts on polytetrafluoroethylene (PTFE) cushion film 5 and blind
Closure plate 9, is installed.
Rui Jin power plant, applying unit implements technological transformation according to the technical program in June, 2016, examines after running half a year
It looks into, does not occur leakage, corrosion phenomenon, work well.And the gaging hole pipeline can be full with the weight of 200 ㎏ or more of load after installing
Foot intensity requirement.
The present embodiment is the exemplary embodiment of the present invention, for those skilled in the art, in the present invention
On the basis of disclosing application method and principle, it is easy to make various types of improvement or deformation, be not limited solely to the present invention
Structure described in above-mentioned specific embodiment, therefore previously described mode is preferred embodiment, and it is not restrictive
Meaning, it is all according to equivalence changes made by the present invention and modification, all in the range protection scope of claims of the present invention.
Claims (4)
1. hole measuring method is protected in one kind open loop on titanium composite panel chimney wall, which comprises the following steps:
(1) material prepares: diameter is 100mm, length 300mm alloy pipeline is as probe tube, mating alloy flange 1,
Mating simple steel flange 2, mating blind plugging plate 1, mating bolt and each 8 totally 16, nut, mating polytetrafluoroethylene (PTFE) soft rubber
2, gasket, alloy electrode is several;
(2) it will use to be fully welded with alloy electrode between probe tube one end and alloy flange and connect;
(3) probe tube installation site has been chosen on titanium composite panel wall, measured hole is opened with plasma cutting machine, having a size of 110mm;
(4) by the jacketed polytetrafluoroethylene (PTFE) soft rubber gasket of the probe tube of welding alloy flange, then from inner wall of stack, that is, titanium
The probe tube is passed through measured hole by liner side, and guarantees that inner wall of stack is close to alloy flange;
(5) apart from a simple steel flange is welded on the outside of chimney at siding 50mm on probe tube, by single ended bolt against titanium composite smoke
Pipeline outer wall passes through the simple steel flange, while covering top nut in the another side screw rod of simple steel flange, and fastening bolt and nut hold out against screw rod
Chimney exterior panel, same method install other screw bolt and nut;
(6) another simple steel flange is installed in the another side of probe tube, while puts on polytetrafluoroethylene (PTFE) soft rubber gasket and blind plugging plate, i.e.,
It is installed.
2. hole measuring method is protected in one kind according to claim 1 open loop on titanium composite panel chimney wall, which is characterized in that described
Probe tube is 316L steel pipe.
3. hole measuring method is protected in one kind according to claim 1 open loop on titanium composite panel chimney wall, which is characterized in that described
Alloy flange 316L material.
4. hole measuring method is protected in one kind according to claim 1 open loop on titanium composite panel chimney wall, which is characterized in that described
Residue length is greater than 50mm after bolt passes through simple steel flange.