CN106948563A - 外墙涂料涂装工艺 - Google Patents
外墙涂料涂装工艺 Download PDFInfo
- Publication number
- CN106948563A CN106948563A CN201710234732.0A CN201710234732A CN106948563A CN 106948563 A CN106948563 A CN 106948563A CN 201710234732 A CN201710234732 A CN 201710234732A CN 106948563 A CN106948563 A CN 106948563A
- Authority
- CN
- China
- Prior art keywords
- exterior wall
- exterior
- paint
- coating
- base paint
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
本发明提供一种外墙涂料涂装工艺,涉及一种建筑物外墙装饰工艺类技术领域。本发明采用了以下技术方案:涂刷第一遍外墙底漆,涂刷第二遍外墙底漆,薄刮外墙腻子,清理墙面浮状物,涂装第一遍外墙面漆,涂装第二遍外墙面漆本发明的有益效果是:施工简单,减少打磨产生的粉尘对环境的污染、可彻底淘汰高耗能、脱落伤人的外墙瓷砖效果好。
Description
技术领域
本发明涉及一种建筑物外墙装饰工艺类技术领域。
背景技术
目前,我国的外墙涂料的涂装质量很差,保质期很短、不得不采用高能耗的瓷砖代替,而磁砖装饰到墙上又存在脱落伤人的安全隐患,废弃的旧料又不可降解等,还占据着建筑外墙装饰的绝对市场,近年来还有上升趋势。很不理想。
发明内容
为了克服上述不足,本发明提供一种外墙涂料涂装工艺,就能达到延长保质期,减少打磨产生的粉尘对环境的污染、可彻底淘汰高耗能、脱落伤人的外墙瓷砖的目的。
为实现上述目的,本发明外墙涂料涂装工艺采用了以下技术方案:
一:外墙抹灰的触地层三米高度内、水泥灰浆强度标号不低于100#,三米以上不低于75#,水泥灰浆内还绝对不能参入便于抹灰的混合剂(沙浆王),因为参入后会降低水泥灰浆质量。
抹灰一定要平整,阴阳角直线无缺。
二:用一比一兑水的外墙底漆充分的涂刷第一遍,在无雨的天气下二十四至四十八小时后,用兑水30%的外墙底漆涂刷第二遍。
三:待干透后批刮外墙腻子,批刮的目的是填充水泥灰浆墙体的缝隙。绝对不要留一层灰在墙面,凡是留一层灰都会降低外墙涂料的使用年限。
四:待外墙腻子干透后,约经清理,涂装选择的外墙面漆两遍。
本发明的有益效果是:施工简单,减少打磨产生的粉尘对环境的污染、延长保质期20年,可彻底淘汰高耗能、脱落伤人的外墙瓷砖效果好。
附图说明
下面结合附图和实施例对本发明作进一步说明:
图1为本发明施工方法流程图。
具体实施方式
下面将通过实施例对本发明作进一步说明。
一种外墙涂料涂装工艺,包括以下步骤:
一:外墙抹灰的触地层三米高度内水泥灰浆强度标号不低于100#,三米以上不低于75#,水泥灰浆内还绝对不能参入便于抹灰的混合剂(沙浆王),因为参入后会降低水泥灰浆质量。
抹灰一定要平整,阴阳角直线无缺。
二:用一比一兑水的外墙底漆充分的涂刷第一遍,在无雨的天气下二十四至四十八小时后用兑水30%外墙底漆涂刷第二遍。
三:待干透后批刮外墙腻子,批刮的目的是填充水泥灰浆墙体的缝隙。绝对不要留一层灰在墙面,凡是留一层灰都会降低外墙涂料的使用年限。
四:待外墙腻子干透后,约经清理,涂装选择的外墙面漆涂装两遍。
Claims (1)
1.一种外墙涂料涂装工艺,包括以下步骤,其特征在于:
(1)外墙抹灰的触地层三米高度内水泥灰浆强度标号不低于100#,三米以上不低于75#,水泥灰浆内不能参入便于抹灰的混合剂(沙浆王);
(2)用一比一兑水的外墙底漆充分的涂刷第一遍,在无雨的天气下二十四至四十八小时后用兑水30%外墙底漆涂刷第二遍;
(3)待干透后批刮外墙腻子,不能留一层灰在墙面;
(4)待外墙腻子干透后,约经清理,涂装选择的外墙面漆涂装两遍。