CN106876620A - Secondary battery filling hole sealing assembly - Google Patents

Secondary battery filling hole sealing assembly Download PDF

Info

Publication number
CN106876620A
CN106876620A CN201510928855.5A CN201510928855A CN106876620A CN 106876620 A CN106876620 A CN 106876620A CN 201510928855 A CN201510928855 A CN 201510928855A CN 106876620 A CN106876620 A CN 106876620A
Authority
CN
China
Prior art keywords
injection hole
sealing
secondary cell
liquid injection
seal assembly
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
CN201510928855.5A
Other languages
Chinese (zh)
Other versions
CN106876620B (en
Inventor
温裕乾
林文法
李宗法
阳超
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Contemporary Amperex Technology Co Ltd
Original Assignee
Contemporary Amperex Technology Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Contemporary Amperex Technology Co Ltd filed Critical Contemporary Amperex Technology Co Ltd
Priority to CN201510928855.5A priority Critical patent/CN106876620B/en
Publication of CN106876620A publication Critical patent/CN106876620A/en
Application granted granted Critical
Publication of CN106876620B publication Critical patent/CN106876620B/en
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

The invention provides a sealing component for a liquid injection hole of a secondary battery, which is used for sealing the liquid injection hole arranged on a top cover of the secondary battery and comprises: sealing nails and sealing films. The sealing nail is plugged into the liquid injection hole to seal the liquid injection hole for one time; the sealing film completely covers the liquid injection hole and is bonded on the top cover in a hot melting sealing mode so as to perform secondary sealing on the liquid injection hole. In the secondary battery injection hole sealing assembly according to the present invention, the sealing nail is inserted into the injection hole to perform primary sealing of the injection hole, and the sealing film completely covering the injection hole is subjected to a hot-melting process to be sealingly bonded to the top cap, thereby performing secondary sealing of the injection hole. The hot-melting connection method is adopted to replace a welding mode in the traditional technology, so that the problems of welding pinholes, explosion points, cracks and the like caused by welding are avoided, and the hot-melting sealing process is simple, convenient and reliable.

Description

Secondary cell fluid injection bore seal assembly
Technical field
The present invention relates to field of batteries, more particularly to a kind of secondary cell fluid injection bore seal assembly.
Background technology
In the manufacturing process of secondary cell (such as lithium ion battery), after fluid injection operation is completed, Need for the liquid injection hole O on top cover 1 to carry out laser seal welding, to prevent the leakage of electrolyte.
In the prior art, as shown in Figures 6 and 7, specific implementation process is first to follow closely 2 with T-shaped sealing to clog Liquid injection hole O on top cover 1, prevents electrolyte from overflowing pollution weld seam W, afterwards to remaining in liquid injection hole O The electrolyte of top is cleaned, and finally leads to the wall of seal cover board 6 and the formation liquid injection hole O of top cover 1 Cross the mode of laser full weld to seal, weld gestalt into full weld weld seam W.
The energy density of laser welding is very high, up to 107W/cm2, metal surface can be heated and reach More than the boiling point of material, vaporization is produced, now laser energy is delivered to metal inside, shape from metal surface Into molten bath.When molten bath is close to T-shaped plastic seal nail 2, plastic seal nail 2 is local can be by moment vapour Change, plastics steam sprays axially upward, drive molten bath weld seam W to produce pin hole, quick-fried point, split The defects such as line.Similarly, when liquid injection hole O remained on surface electrolyte is not cleaned up, in the presence of laser Also the defects such as pin hole, quick-fried point, crackle can be produced.
The content of the invention
In view of problem present in background technology, it is an object of the present invention to provide a kind of secondary cell Fluid injection bore seal assembly, its use the method for hot-melt adhesive paste solve produced by welding welding pin hole, The problems such as quick-fried point, crackle, and sealing process is simple, convenient, reliable.
To achieve these goals, the invention provides a kind of secondary cell fluid injection bore seal assembly, its use Sealed in the liquid injection hole to being arranged on the top cover of secondary cell, including:Sealing nail and diaphragm seal. Sealing nail is filled in liquid injection hole, and once sealing is carried out with to liquid injection hole;Diaphragm seal is completely covered liquid injection hole simultaneously Hot-melting sealed is bonded on top cover, and secondary seal is carried out with to liquid injection hole.
Beneficial effects of the present invention are as follows:
In secondary cell fluid injection bore seal assembly of the invention, will sealing nail fill in it is right in liquid injection hole Liquid injection hole carries out once sealing, and the diaphragm seal to being completely covered on liquid injection hole carries out hot melt treatment to seal It is bonded on top cover, so as to carry out secondary seal to liquid injection hole.The present invention is by using this hot-melt adhesive paste Method substitute the welding manner in conventional art, so as to avoid coming due to welded bands welding pin hole, The problems such as quick-fried point, crackle, and the operation of this hot-melting sealed is simple, convenient, reliable.
Brief description of the drawings
Fig. 1 is before being sealed using the secondary cell liquid injection hole of secondary cell fluid injection bore seal assembly of the invention Stereogram;
Fig. 2 is the exploded view of secondary cell fluid injection bore seal assembly of the invention;
Fig. 3 is assembling and the seal process schematic diagram of secondary cell fluid injection bore seal assembly of the invention;
Fig. 4 is the schematic diagram after secondary cell fluid injection bore seal assembly assembling of the invention and sealing;
Fig. 5 is the structural representation of the diaphragm seal of secondary cell fluid injection bore seal assembly of the invention;
Fig. 6 is the exploded view of secondary cell fluid injection bore seal assembly in the prior art;
Fig. 7 is the schematic diagram after secondary cell fluid injection bore seal assembly assembling in the prior art and sealing.
Wherein, description of reference numerals is as follows:
The heat transfer layer of 1 top cover 32
The heat-conducting layer of O liquid injection holes 33
2 sealing nails 4 heat head
The binding part of 21 insertion section 5
The seal cover board of 22 stopper section 6
3 diaphragm seal W weld seams
31 melting zones
Specific embodiment
Describe secondary cell fluid injection bore seal assembly of the invention in detail with reference to the accompanying drawings.
Referring to figs. 1 to Fig. 5, secondary cell fluid injection bore seal assembly of the invention, for setting Sealed in the liquid injection hole O on the top cover 1 of secondary cell, it includes:Sealing nail 2 and diaphragm seal 3. Sealing nail 2 is filled in liquid injection hole O, and once sealing is carried out with to liquid injection hole O;Diaphragm seal 3 covers completely Simultaneously hot-melting sealed is bonded on top cover 1 lid liquid injection hole O, and secondary seal is carried out with to liquid injection hole O.
In secondary cell fluid injection bore seal assembly of the invention, sealing nail 2 is filled in into liquid injection hole O In once sealing is carried out to liquid injection hole O, the diaphragm seal 3 to being completely covered on liquid injection hole O carries out heat Molten treatment is bonded on top cover 1 with sealing, so as to carry out secondary seal to liquid injection hole O.The present invention passes through The welding manner in conventional art is substituted using the method for this hot-melt adhesive paste, so as to avoid due to welding The problems such as welding pin hole, quick-fried point, crackle for bringing, and the operation of this hot-melting sealed it is simple, convenient, It is reliable.
Secondary cell fluid injection bore seal assembly of the invention, in one embodiment, reference picture 2 to figure 4, sealing nail 2 can be T-shaped.
In one embodiment, to Fig. 4, sealing nail 2 can have reference picture 2:Insertion section 21, insertion top In liquid injection hole O on lid 1;And stopper section 22, it is resisted against on top cover 1.In the present embodiment, The stopper section 22 of nail 2 is sealed in the liquid injection hole O that the insertion section 21 that nail 2 will be sealed is inserted on top cover 1 It is resisted against on top cover 1, can prevents electrolyte from overflowing, it is to avoid causes battery core electrolyte inside not enough and top The surface contamination of lid 1 influences the hot melt quality of diaphragm seal 3.
In one embodiment, sealing nail 2 or taper or cylinder, but not only limit in this way, can also set It is calculated as other shapes.
In one embodiment, sealing nail 2 can seal nail for plastic cement, and the material of sealing nail is not only limited such as certainly This, can also according to specific needs select other types of material.
In one embodiment, reference picture 5, diaphragm seal 3 can have:Melting zone 31, is placed on top cover 1 So that liquid injection hole O is completely covered;Heat-conducting layer 32, is laminated on melting zone 31;And heat transfer layer 33, Positioned at the superiors of diaphragm seal 3, outside heat is transferred to melting zone by heat transfer layer 32 via heat-conducting layer 32 31 melting melting zone 31.In the present embodiment, the meeting in high temperature melting of melting zone 31 of diaphragm seal 3 Closely continuous binding part 5 is formed with top cover 1, so as to liquid injection hole O is fully sealed.
In one embodiment, melting zone 31 is polypropylene layer;Heat-conducting layer 32 is aluminium foil;And heat transfer layer 33 is nylon layer, and this is the concrete structure (i.e. a kind of aluminum plastic film) of diaphragm seal of the present invention 3, But not only limit is in this way, the melting zone 31 of diaphragm seal 3, heat-conducting layer 32 and heat transfer layer 33 can also use it The material of its type is made.Wherein, in the present embodiment, heat-conducting layer 32 increased sealing using aluminium foil The bulk strength and toughness of film 3, and enhance melting zone 31 thermal conductivity and Temperature Distribution it is uniform Property, so as to improve the quality and efficiency of hot-melting sealed.
In one embodiment, the thickness of melting zone 31 can be 5 μm~15 μm.
In one embodiment, the thickness of heat-conducting layer 32 can be 5 μm~15 μm.
In one embodiment, the thickness of heat transfer layer 33 can be 5 μm~15 μm.
Remark additionally herein, above-described melting zone 31, heat-conducting layer 32 and heat transfer layer 33 Thickness range be currently preferred thickness range, based on actual demand, processing and produce, fusing The thickness range of layer 31, heat-conducting layer 32 and heat transfer layer 33 all can be adjusted suitably.
In one embodiment, reference picture 2 and Fig. 3, the diaphragm seal in secondary cell fluid injection bore seal assembly 3 can carry out hot melt treatment using heating first 4, so as to diaphragm seal 3 melts and seals be bonded on top cover 1.

Claims (10)

1. a kind of secondary cell fluid injection bore seal assembly, for the top cover (1) to being arranged at secondary cell On liquid injection hole (O) sealed, secondary cell fluid injection bore seal assembly includes:
Sealing nail (2), is filled in liquid injection hole (O), and once sealing is carried out with to liquid injection hole (O);
Characterized in that, the secondary cell fluid injection bore seal assembly also includes:
Diaphragm seal (3), is completely covered liquid injection hole (O) and hot-melting sealed is bonded on top cover (1), Secondary seal is carried out with to liquid injection hole (O).
2. secondary cell fluid injection bore seal assembly according to claim 1, it is characterised in that close Envelope nail (2) is T-shaped.
3. secondary cell fluid injection bore seal assembly according to claim 2, it is characterised in that close Envelope nail (2) has:
Insertion section (21), in the liquid injection hole (O) in insertion top cover (1);And
Stopper section (22), is resisted against on top cover (1).
4. secondary cell fluid injection bore seal assembly according to claim 1, it is characterised in that close Envelope nail (2) is taper or cylinder.
5. secondary cell fluid injection bore seal assembly according to claim 1, it is characterised in that close Envelope nail (2) is followed closely for plastic cement is sealed.
6. secondary cell fluid injection bore seal assembly according to claim 1, it is characterised in that close Sealer (3) has:
Melting zone (31), is placed on top cover (1) that liquid injection hole (O) is completely covered;
Heat-conducting layer (32), is laminated on melting zone (31);And
Heat transfer layer (33), positioned at the superiors of diaphragm seal (3), heat transfer layer (32) is by outside warm It is transferred to melting zone (31) to melt melting zone (31) via heat-conducting layer (32).
7. secondary cell fluid injection bore seal assembly according to claim 6, it is characterised in that
Melting zone (31) is polypropylene layer;
Heat-conducting layer (32) is aluminium foil;
Heat transfer layer (33) is nylon layer.
8. secondary cell fluid injection bore seal assembly according to claim 7, it is characterised in that molten The thickness for changing layer (31) is 5 μm~15 μm.
9. secondary cell fluid injection bore seal assembly according to claim 7, it is characterised in that lead The thickness of thermosphere (32) is 5 μm~15 μm.
10. secondary cell fluid injection bore seal assembly according to claim 7, it is characterised in that pass The thickness of thermosphere (33) is 5 μm~15 μm.
CN201510928855.5A 2015-12-14 2015-12-14 Secondary battery liquid injection hole sealing assembly Active CN106876620B (en)