Surface has the air-entrained concrete building block production method of cavity with inside grooves
Technical field
Present invention is mainly used for air-entrained concrete building block production.
Background technique
Current air-entrained concrete building block cut after be all smooth surface, especially air-entrained concrete building block front and back
Surface be it is smooth, it is totally unfavorable to the attachment of plastering mortar, plastering sand pulp layer easily generate hollowing, shelling phenomenon, simultaneously plus
Gas concrete segment be it is solid, weight is big, it has not been convenient to carry and build.
Summary of the invention
The present invention solves the above problem, it is that multiple inflations are installed in mold before the casting of air entrained concrete idiosome
Film stick A can form the table of air-entrained concrete building block along multiple aerated film stick A cutting in the cutting of air entrained concrete idiosome
Face groove, considerably increases the plastering mortar adhesive force on air-entrained concrete building block surface, and plastering sand pulp layer will not generate hollowing, take off
Shell phenomenon, while increasing multiple vertical pneumatic film stick B in air-entrained concrete building block, the weight of building block is alleviated, carries and builds
It builds all easily;Main production method of the invention is: the filament (7) at the both ends multiple aerated film stick A(1) is hung over mold (2)
On the hook (8) of both ends side wall, make multiple aerated film stick A(1) center spacing in left and right directions with air-entrained concrete building block (5)
Equivalent width, the aerated film stick A(1 being arranged above and below) center line be exactly air entrained concrete idiosome (3) cutting line (4), it is multiple
Aerated film stick A(1) it is not required in short transverse, the air-entrained concrete building block (5) if short transverse spacing is small, after cutting
The groove (6) of front and rear surfaces is more, air-entrained concrete building block (5) front and rear surfaces if short transverse spacing is big, after cutting
Groove (6) is few, while fixed multiple vertical pneumatic film stick B(9), upper and lower multiple vertical pneumatic film stick B(9) it is connected with cord (7),
For fixing means as the fixing means of aerated film stick A(1), air entrained concrete idiosome (3) is cut into single aerating coagulation
After earth building blocks (5), multiple vertical pneumatic film stick B(9) it is located at the middle part of air-entrained concrete building block (5), multiple vertical pneumatic film stick B
(9) it does not appear up and down in air-entrained concrete building block (5), when building air-entrained concrete building block (5), masonry mortar will not in this way
Fall into aerated film stick B(9) cavity in, then by existing technical method carry out air-entrained concrete building block production,
Build air-entrained concrete building block when, tear aerated film stick A(1) film can be carried out plastering construction;It needs to illustrate: left and right two
The vertical setting of types aerated film stick A(1 on side) center line be also required to cut, aerated film stick A(1) and aerated film stick B(9) be filled with pressure sky
The thin-film rod of gas.
Detailed description of the invention
Description of symbols: 1- aerated film stick A, 2- mold, 3- air entrained concrete idiosome, 4- cutting line, 5- aerating coagulation
Earth building blocks, 6- half slot, 7- filament, 8- hook, 9- aerated film stick B.
Fig. 1 is the facade section that aerated film stick is fixed in mold 2.
Fig. 2 is the top view that aerated film stick is fixed in mold 2.
Fig. 3 is the schematic diagram after air entrained concrete idiosome 3 is cut.
Fig. 4 is the facade section of the air-entrained concrete building block 5 after the completion of cutting.
Fig. 5 is the cross-sectional view of aerated film stick A1.
Fig. 6 is that aerated film stick A1 hangs over the elevational schematic view linked up on 8.
Fig. 7 is the horizontal sectional drawing of the air-entrained concrete building block 5 after the completion of cutting.
Specific embodiment
Referring to Fig. 1 to Fig. 7, the filament 7 at multiple both ends aerated film stick A1 is hung on the hook 8 of 2 both ends side wall of mold, is made
The center spacing of the multiple aerated film stick A1 equivalent width with air-entrained concrete building block 5 in left and right directions, the inflation being arranged above and below
Film stick A1 center line is exactly the cutting line 4 of air entrained concrete idiosome 3, and multiple aerated film stick A1 are not required in short transverse, such as
Fruit short transverse spacing is small, then the groove more than 6 of 5 front and rear surfaces of air-entrained concrete building block after cutting, if short transverse spacing
Greatly, then the groove 6 of 5 front and rear surfaces of air-entrained concrete building block after cutting is few, while fixed multiple vertical pneumatic film stick B9, up and down
Multiple vertical pneumatic film stick B9 are connected with cord 7, and fixing means is as the fixing means of aerated film stick A1, air entrained concrete embryo
After body 3 is cut into single air-entrained concrete building block 5, multiple vertical pneumatic film stick B9 are located in air-entrained concrete building block 5
Portion, multiple vertical pneumatic film stick B9 do not appear up and down in air-entrained concrete building block 5, are building air-entrained concrete building block 5 in this way
When masonry mortar will not fall into the cavity of aerated film stick B9, then carry out air-entrained concrete building block by existing technical method
Production, when building air-entrained concrete building block, the film for tearing aerated film stick A1 can be carried out plastering construction;It needs
Bright: the present invention has been merely given as a kind of method that aerated film stick A1 is fixed with mold 2, other methods can also be used aerated film
Stick A1 and aerated film stick B9 are fixed.