CN106807756A - A kind of method and apparatus for controlling hot-strip head and tail width - Google Patents

A kind of method and apparatus for controlling hot-strip head and tail width Download PDF

Info

Publication number
CN106807756A
CN106807756A CN201710181638.3A CN201710181638A CN106807756A CN 106807756 A CN106807756 A CN 106807756A CN 201710181638 A CN201710181638 A CN 201710181638A CN 106807756 A CN106807756 A CN 106807756A
Authority
CN
China
Prior art keywords
strip
short stroke
lateral pressure
stroke curve
pressure amount
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201710181638.3A
Other languages
Chinese (zh)
Inventor
王登刚
赵志斌
付尚江
李卫平
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Pangang Group Xichang Steel and Vanadium Co Ltd
Original Assignee
Pangang Group Xichang Steel and Vanadium Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Pangang Group Xichang Steel and Vanadium Co Ltd filed Critical Pangang Group Xichang Steel and Vanadium Co Ltd
Priority to CN201710181638.3A priority Critical patent/CN106807756A/en
Publication of CN106807756A publication Critical patent/CN106807756A/en
Pending legal-status Critical Current

Abstract

This application discloses a kind of method and apparatus for controlling hot-strip head and tail width.The method chooses the strip of different lateral pressure amount specifications, rolled in the case of the short stroke function that do not come into operation, strip width data to all rollings are collected analysis, to rest in without in the case of any head and tail width control function, the true strain situation of strip head and tail width.Further, it is that different lateral pressure amounts sets up corresponding short stroke curve according to above-mentioned analysis.So, when being rolled, the difference according to lateral pressure amount chooses different short stroke curves.Compared with prior art, the present invention is adjusted according to practical condition to short stroke curve, so as to cover strip deformation end to end in all directions, reaches the purpose of effectively control strip head and tail width.

Description

A kind of method and apparatus for controlling hot-strip head and tail width
Technical field
The application is related to technical field of steel rolling, more specifically to a kind of method for controlling hot-strip head and tail width And device.
Background technology
The control of hot-strip head and tail width is a technical barrier, because strip is end to end during edge rolling, end Position is influenceed by metal deformation flow, shows irregular deformation, and then strip head and tail width narrow rule or ultra-wide is occurred Phenomenon.In order to eliminate or alleviating this phenomenon, present hot continuous rolling factory edger roll all has short stroke control function end to end, that is, exists Edge rolling strip end to end when, by the opening degree of hydraulic means dynamic regulation edger roll, so as to improve strip width end to end.
At present, all there is roughing vertical roll short stroke control function end to end substantially on hot-rolling line at home.But to band In the specific deformed shape of steel toe tail and corresponding compensation short stroke CURVE STUDY but seldom, the control of main flow is mainly 4 sections of foldings Line, simple high order curve, this method do not have all situations that all standing strip deforms end to end, can only partly compensate band steel toe , still there is strip head and tail width and does not conform in tail shape when causing the specification being not covered with.
The content of the invention
In view of this, the application provides a kind of method and apparatus for controlling hot-strip head and tail width, according to actual production Situation, is adjusted to short stroke curve, so as to cover strip deformation end to end in all directions, reaches and effectively controls strip end to end The purpose of width.
To achieve these goals, it is proposed that scheme it is as follows:
A kind of method for controlling hot-strip head and tail width, including:
Obtain the lateral pressure amount under current state;
The short stroke curve corresponding with the lateral pressure amount is transferred, the short stroke curve is based in no short stroke control Strip in different pressure measurement rollings, set up by the head and tail width variation tendency of strip under function;
Based on the short stroke curve controlled strip operation of rolling end to end.
Preferably, the process of setting up of the short stroke curve includes:
Obtain multiple strip samples generated under without short stroke control function;
The strip sample not lower to same lateral pressure amount layer is analyzed, to determine the head and tail width change to the strip sample Change trend;
Variation tendency end to end according to the strip sample sets up short stroke curve not corresponding with lateral pressure amount layer.
Preferably, the lateral pressure amount layer is an other scope of layer not with 10mm.
Preferably, the lateral pressure amount layer does not include:Less than or equal to 0,0~10mm, 10~20mm, 20~30mm, 30~ 40mm, 40~50mm, 50~60mm, 60~70mm and more than 70mm.
Preferably, the operation of rolling based on the short stroke curve controlled strip end to end, also includes afterwards:
Head and tail width to the strip after rolling is analyzed, and the ginseng of the short stroke curve is adjusted based on analysis result Number.
A kind of device of control hot-strip head and tail width, including:
Lateral pressure amount collecting unit, for obtaining the lateral pressure amount under current state;
Short stroke curve transfers unit, for transferring the short stroke curve corresponding with the lateral pressure amount, the short stroke Curve is based on the strip under no short stroke control function, and, in different pressure measurement rollings, the head and tail width variation tendency of strip is built It is vertical;
Control unit, for the operation of rolling based on the short stroke curve controlled strip end to end.
Preferably, also include:Short stroke curve sets up unit, for pre-building the short row corresponding with the lateral pressure amount Journey curve;
The short stroke curve sets up unit to be included:
Sample collection module, for obtaining multiple strip samples generated under without short stroke control function;
Head and tail width mutation analysis module, for being analyzed to the not lower strip sample of same lateral pressure amount layer, with determination To the head and tail width variation tendency of the strip sample;
Curve sets up module, for setting up not right with lateral pressure amount layer according to the variation tendency end to end of the strip sample The short stroke curve answered.
Preferably, the lateral pressure amount layer is an other scope of layer not with 10mm.
Preferably, the lateral pressure amount layer does not include:Less than or equal to 0,0~10mm, 10~20mm, 20~30mm, 30~ 40mm, 40~50mm, 50~60mm, 60~70mm and more than 70mm.
Preferably, also include:Short stroke curve adjustment unit, is divided for the head and tail width to the strip after rolling Analysis, and the parameter of the short stroke curve is adjusted based on analysis result.
Through as shown from the above technical solution, this application discloses the method and dress of a kind of control hot-strip head and tail width Put.The method chooses the strip of different lateral pressure amount specifications, is rolled in the case of the short stroke function that do not come into operation, and is rolled to all The strip width data of system are collected analysis, and to rest in without in the case of any head and tail width control function, strip is end to end The true strain situation of width.Further, it is that different lateral pressure amounts sets up corresponding short stroke curve according to above-mentioned analysis.This Sample, when being rolled, the difference according to lateral pressure amount chooses different short stroke curves.Compared with prior art, root of the present invention According to practical condition, short stroke curve is adjusted, so as to cover strip deformation end to end in all directions, reaches effectively control The purpose of strip head and tail width processed.
Brief description of the drawings
In order to illustrate more clearly about the embodiment of the present invention or technical scheme of the prior art, below will be to embodiment or existing The accompanying drawing to be used needed for having technology description is briefly described, it should be apparent that, drawings in the following description are only this Inventive embodiment, for those of ordinary skill in the art, on the premise of not paying creative work, can also basis The accompanying drawing of offer obtains other accompanying drawings.
Fig. 1 shows that a kind of flow of the method for control hot-strip head and tail width is shown disclosed in one embodiment of the invention It is intended to;
Short stroke curve map tendency when Fig. 2 shows lateral pressure amount disclosed by the invention less than 30mm;
Short stroke curve map tendency when Fig. 3 shows lateral pressure amount disclosed by the invention more than 30mm less than 50mm;
Short stroke curve map tendency when Fig. 4 shows lateral pressure amount disclosed by the invention more than 50mm;
Fig. 5 shows a kind of structure of the device of control hot-strip head and tail width disclosed in another embodiment of the present invention Schematic diagram.
Specific embodiment
Below in conjunction with the accompanying drawing in the embodiment of the present invention, the technical scheme in the embodiment of the present invention is carried out clear, complete Site preparation is described, it is clear that described embodiment is only a part of embodiment of the invention, rather than whole embodiments.Based on this Embodiment in invention, the every other reality that those of ordinary skill in the art are obtained under the premise of creative work is not made Example is applied, the scope of protection of the invention is belonged to.
A kind of stream of the method for control hot-strip head and tail width disclosed in one embodiment of the invention is shown referring to Fig. 1 Journey schematic diagram.
As shown in Figure 1, the method includes:
S101:Obtain the lateral pressure amount under current state.
S102:Transfer the short stroke curve corresponding with the lateral pressure amount.
Wherein, the short stroke curve be based under no short stroke control function strip it is different pressure measurement rolling when, The head and tail width variation tendency of strip is set up.
The process of setting up of the short stroke curve includes:
A:Obtain multiple strip samples generated under without short stroke control function.
B:To same lateral pressure amount layer not under strip sample be analyzed, to determine the head and tail width to the strip sample Variation tendency.
C:Variation tendency end to end according to the strip sample sets up short stroke curve not corresponding with lateral pressure amount layer.
The strip of different lateral pressure amount specifications can be chosen in specific implementation process, in the short stroke that do not come into operation (SSC) function In the case of rolled, the strip width data to all rollings are collected analysis.Rest in without any head and tail width control In the case of function processed, the true strain situation of strip head and tail width is easy to follow-up specific aim to formulate the compensation of head and tail width control Measure.
There is following trend by the strip width tracing analysis result produced in the case of without using short stroke function, When lateral pressure amount is less than 30mm, there is different degrees of ultra-wide phenomenon in strip head and tail width;When lateral pressure amount is more than 30mm, band steel toe Tail width engenders narrow rule phenomenon, and as the increase narrow rule amplitude of lateral pressure amount increases therewith, but in strip tail end Portion has certain ultra-wide to be present.
According to the deformation rule of this rolling, with lateral pressure amount 30mm as boundary, two kinds of parameters of control mode are set out.One It is that edger roll roll gap depresses (curve is as shown in Figure 1) end to end to plant, mainly for the specification in side pressure 30mm, the actual drafts of roll gap Accurate adjustment is carried out according to layer not difference.Another kind is that roll gap increases (curve is as shown in Figure 2) end to end, is more than mainly for lateral pressure amount The specification of 30mm, the same other incrementss of different layers are according to actually carrying out accurate adjustment.Meanwhile, band when being rolled according to the super 50mm of lateral pressure amount Easy narrow rule between the 0.2-0.5m of steel end, but the phenomenon of end 0.2m or so ultra-wide, make end extruding, what middle part was opened Short stroke curve (curve is as shown in Figure 3).
Different foundation with side pressure value according to lateral pressure amount be the other model table of layer, lateral pressure amount layer not She Zhi 10mm be one The other scope of layer, scope is from lateral pressure amount less than 0mm (i.e. broadening rolling) to more than 70mm.
Specially:Less than or equal to 0,0~10mm, 10~20mm, 20~30mm, 30~40mm, 40~50mm, 50~ 60mm, 60~70mm and more than 70mm.
S103:Based on the short stroke curve controlled strip operation of rolling end to end.
S104:Head and tail width to the strip after rolling is analyzed, and it is bent to adjust the short stroke based on analysis result The parameter of line.
It should be noted that the precision in order to improve short stroke curve, in other embodiment disclosed by the invention, it is necessary to Head and tail width to the strip after rolling is analyzed, so that the parameter to short stroke curve is adjusted.
As seen from the above embodiment, this application discloses this application discloses a kind of side of control hot-strip head and tail width Method.The method chooses the strip of different lateral pressure amount specifications, is rolled in the case of the short stroke function that do not come into operation, and is rolled to all The strip width data of system are collected analysis, and to rest in without in the case of any head and tail width control function, strip is end to end The true strain situation of width.Further, it is that different lateral pressure amounts sets up corresponding short stroke curve according to above-mentioned analysis.This Sample, when being rolled, the difference according to lateral pressure amount chooses different short stroke curves.Compared with prior art, root of the present invention According to practical condition, short stroke curve is adjusted, so as to cover strip deformation end to end in all directions, reaches effectively control The purpose of strip head and tail width processed.
A kind of device of control hot-strip head and tail width disclosed in another embodiment of the present invention is shown referring to Fig. 5 Structural representation.
As shown in Figure 5, the device includes:Lateral pressure amount collecting unit 1, short stroke curve are set up unit 2, short stroke curve and are adjusted Take unit 3 and control unit 4.
Lateral pressure amount collecting unit 1 is used to obtain the lateral pressure amount under current state.
Short stroke curve sets up unit 2 for pre-building the short stroke curve corresponding with the lateral pressure amount, wherein, institute Short stroke curve is stated based on the strip under no short stroke control function in different pressure measurement rollings, the head and tail width of strip becomes Change trend is set up;.
Specifically, the short stroke curve is set up unit and is included:
Sample collection module 21, for obtaining multiple strip samples generated under without short stroke control function.
Head and tail width mutation analysis module 22, for same lateral pressure amount layer not under strip sample be analyzed, with true The fixed head and tail width variation tendency to the strip sample.
Curve sets up module 23, for being set up with lateral pressure amount layer not according to the variation tendency end to end of the strip sample Corresponding short stroke curve.
Further, short stroke curve transfers unit 3 and the short stroke corresponding with the lateral pressure amount is transferred when being rolled Curve.
Control unit 4, for the operation of rolling based on the short stroke curve controlled strip end to end.
Optionally, in order to improve the precision of short stroke curve, in other embodiment disclosed by the invention, the device is also wrapped Include:Short stroke curve adjustment unit, is analyzed for the head and tail width to the strip after rolling, and based on analysis result adjustment The parameter of the short stroke curve.
It should be noted that the system embodiment is corresponding with embodiment of the method, its implementation procedure is identical with principle is performed, Therefore not to repeat here.
Finally, in addition it is also necessary to explanation, herein, such as first and second or the like relational terms be used merely to by One entity or operation make a distinction with another entity or operation, and not necessarily require or imply these entities or operation Between there is any this actual relation or order.And, term " including ", "comprising" or its any other variant meaning Covering including for nonexcludability, so that process, method, article or equipment including a series of key elements not only include that A little key elements, but also other key elements including being not expressly set out, or also include for this process, method, article or The intrinsic key element of equipment.In the absence of more restrictions, the key element limited by sentence "including a ...", does not arrange Except also there is other identical element in the process including the key element, method, article or equipment.
Each embodiment is described by the way of progressive in this specification, and what each embodiment was stressed is and other The difference of embodiment, between each embodiment identical similar portion mutually referring to.
The foregoing description of the disclosed embodiments, enables professional and technical personnel in the field to realize or uses the present invention. Various modifications to these embodiments will be apparent for those skilled in the art, as defined herein General Principle can be realized in other embodiments without departing from the spirit or scope of the present invention.Therefore, the present invention The embodiments shown herein is not intended to be limited to, and is to fit to and principles disclosed herein and features of novelty phase one The scope most wide for causing.

Claims (10)

1. it is a kind of control hot-strip head and tail width method, it is characterised in that including:
Obtain the lateral pressure amount under current state;
The short stroke curve corresponding with the lateral pressure amount is transferred, the short stroke curve is based on not having short stroke control function Lower strip in different pressure measurement rollings, set up by the head and tail width variation tendency of strip;
Based on the short stroke curve controlled strip operation of rolling end to end.
2. method according to claim 1, it is characterised in that the process of setting up of the short stroke curve includes:
Obtain multiple strip samples generated under without short stroke control function;
The strip sample not lower to same lateral pressure amount layer is analyzed, to determine that the head and tail width to the strip sample changes Gesture;
Variation tendency end to end according to the strip sample sets up short stroke curve not corresponding with lateral pressure amount layer.
3. method according to claim 2, it is characterised in that the lateral pressure amount layer is an other scope of layer not with 10mm.
4. method according to claim 3, it is characterised in that the lateral pressure amount layer does not include:Less than or equal to 0,0~ 10mm, 10~20mm, 20~30mm, 30~40mm, 40~50mm, 50~60mm, 60~70mm and more than 70mm.
5. method according to claim 1, it is characterised in that it is described based on the short stroke curve controlled strip end to end The operation of rolling, also includes afterwards:
Head and tail width to the strip after rolling is analyzed, and the parameter of the short stroke curve is adjusted based on analysis result.
6. it is a kind of control hot-strip head and tail width device, it is characterised in that including:
Lateral pressure amount collecting unit, for obtaining the lateral pressure amount under current state;
Short stroke curve transfers unit, for transferring the short stroke curve corresponding with the lateral pressure amount, the short stroke curve Based on the strip under no short stroke control function in different pressure measurement rollings, the head and tail width variation tendency of strip is set up;
Control unit, for the operation of rolling based on the short stroke curve controlled strip end to end.
7. device according to claim 6, it is characterised in that also include:Short stroke curve sets up unit, for building in advance The vertical short stroke curve corresponding with the lateral pressure amount;
The short stroke curve sets up unit to be included:
Sample collection module, for obtaining multiple strip samples generated under without short stroke control function;
Head and tail width mutation analysis module, for same lateral pressure amount layer not under strip sample be analyzed, to determine to institute State the head and tail width variation tendency of strip sample;
Curve sets up module, for setting up not corresponding with lateral pressure amount layer according to the variation tendency end to end of the strip sample Short stroke curve.
8. the device according to right wants 7, it is characterised in that the lateral pressure amount layer is an other scope of layer not with 10mm.
9. device according to claim 8, it is characterised in that the lateral pressure amount layer does not include:Less than or equal to 0,0~ 10mm, 10~20mm, 20~30mm, 30~40mm, 40~50mm, 50~60mm, 60~70mm and more than 70mm.
10. device according to claim 6, it is characterised in that also include:Short stroke curve adjustment unit, for rolling The head and tail width of the strip after system is analyzed, and the parameter of the short stroke curve is adjusted based on analysis result.
CN201710181638.3A 2017-03-23 2017-03-23 A kind of method and apparatus for controlling hot-strip head and tail width Pending CN106807756A (en)