CN105904171A - Housing, and preparation method and application thereof - Google Patents

Housing, and preparation method and application thereof Download PDF

Info

Publication number
CN105904171A
CN105904171A CN201610222399.7A CN201610222399A CN105904171A CN 105904171 A CN105904171 A CN 105904171A CN 201610222399 A CN201610222399 A CN 201610222399A CN 105904171 A CN105904171 A CN 105904171A
Authority
CN
China
Prior art keywords
housing
preparation
narrow limit
present
narrow
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201610222399.7A
Other languages
Chinese (zh)
Inventor
李庆良
王叶
范金林
张吉祥
张飞
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
LeTV Holding Beijing Co Ltd
LeTV Mobile Intelligent Information Technology Beijing Co Ltd
Original Assignee
LeTV Holding Beijing Co Ltd
LeTV Mobile Intelligent Information Technology Beijing Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by LeTV Holding Beijing Co Ltd, LeTV Mobile Intelligent Information Technology Beijing Co Ltd filed Critical LeTV Holding Beijing Co Ltd
Priority to CN201610222399.7A priority Critical patent/CN105904171A/en
Publication of CN105904171A publication Critical patent/CN105904171A/en
Pending legal-status Critical Current

Abstract

The present invention relates to the field of electronic equipment. A preparation method of a housing comprises the following steps of processing chamfers and/or rounds on first edges of a housing opening, and forming first narrow edges; forming a protection layer on the housing body, and performing first coloring on the first narrow edges; processing chamfers and/or rounds on second edges of the housing opening, and forming second narrow edges; and performing second coloring on the second narrow edges and the housing body. The preparation method of the housing is simple in process, the accuracy requirement is low, the visual effect that edges of a screen are free of frames when a portable electronic device is viewed from the front side can be achieved, and a series of related tests of the whole machine can be satisfied due to the fact that the housing has the narrow edges.

Description

A kind of housing and its preparation method and application
Technical field
The present invention relates to electronic device field, be specifically related to a kind of housing and its preparation method and application.
Background technology
Along with the development of science and technology, the use of smart mobile phone is more and more extensive, already takes up at present Market mainstream status, is the necessary configuration of people's routine work life.Owing to it makes expenditure high, people The highest to its requirement, not only pursue the intellectuality of mobile phone, also pursue limit ultra-thin, the narrow moulding of mobile phone Design.
At present, for promoting user's viewing experience, mobile phone screen does bigger and bigger, but bigger mobile phone screen Add frame, not only limit mobile phone products shape-designing, and be inconvenient to operate and carry.The narrowest limit Frame design or even " Rimless " design can allow mobile phone show bigger screen in the least size Area, promotes Consumer's Experience.
Adhesion ratio at present, during making Rimless mobile phone, after assembling with screen body due to metal Poor, therefore to reach Rimless effect to meet a series of dependence tests of complete machine again, mobile phone wants true Just accomplishing the effect of Rimless, there be difficulties involved when technically.Therefore, so-called " Rimless " It is the narrowest frame in fact.
When making the narrowest frame mobile phone, Digit Control Machine Tool (CNC, Computer Number Control) Chamfer surface after the processing contact surface of metal and screen (chamfer surface be) be typically case material this The color of body, and the edge of screen is usually black, in order to reach the effect of mobile phone Rimless, if adopted Machined trace can be left on chamfer surface by secondary operations, and and the most easily-controllable from the working depth of processing System, the appearance causing Rimless is poor, and product yield can reduce, thus causes cost to raise. How to provide a kind of new mobile phone to meet mobile phone giant-screen, the development trend of narrow frame is that industry urgently solves Technical problem certainly.
Summary of the invention
It is that in prior art, Rimless handset shell production technology precision is wanted to this end, to be solved by this invention Ask high, difficulty is big, yield is low problem.
For solving above-mentioned technical problem, the technical solution used in the present invention is as follows:
The preparation method of a kind of housing of the present invention, comprises the steps:
Chamfering and/or rounding on the first edge of shell nozzle, form the first narrow limit;
Enclosure body is formed protective layer, carries out described first narrow limit colouring for the first time;
Chamfering and/or rounding on the second edge of described shell nozzle, form the second narrow limit;
Described second narrow limit and described enclosure body carry out second time colour.
Alternatively, the described step forming protective layer in enclosure body, farther include:
Described first narrow limit is formed shielding layer;
In described enclosure body, described protective layer is formed for mask with described shielding layer;
Remove described shielding layer.
Alternatively, the step removing described protective layer is also included before described second time tinting steps.
Alternatively, described housing is metal shell;The most described tinting steps is anode oxidation coloration.
Alternatively, described first narrow limit is prepared by numerical control processing technology.
Alternatively, described second narrow limit is prepared by numerical control processing technology.
Alternatively, the step that described first narrow limit and/or the second narrow limit are polished also is included.
Alternatively, the coloring of described first time and/or second time are colored as black.
A kind of housing of the present invention, is prepared by the preparation method of described housing.
A kind of portable electron device of the present invention, including described housing.
The technique scheme of the present invention has the advantage that compared to existing technology
1, the preparation method of a kind of housing described in the embodiment of the present invention, comprises the steps: at housing Chamfering and/or rounding on first edge of opening, form the first narrow limit;Enclosure body is formed Protective layer, carries out described first narrow limit colouring for the first time;Second edge of described shell nozzle adds Work chamfering and/or rounding, form the second narrow limit;Described second narrow limit and described enclosure body are carried out Secondary coloring.The preparation method of described housing, not only technique is simple, required precision is low, it is possible to realize Portable electron device reaches the visual effect of screen edge Rimless in terms of front, and, housing has Narrow limit disclosure satisfy that a series of dependence tests of complete machine.
2, a kind of housing described in the embodiment of the present invention, is not only able to realize portable electron device from just The visual effect reaching screen edge Rimless is seen in face;And, production technology is simple, yield is high, cost Low.
3, a kind of portable electron device described in the embodiment of the present invention, it is possible to realize portable electron device The visual effect of screen edge Rimless is reached in terms of front;And, there is narrow limit and disclosure satisfy that complete machine A series of dependence tests.
Accompanying drawing explanation
In order to make present disclosure be more likely to be clearly understood, being embodied as below according to the present invention Example also combines accompanying drawing, and the present invention is further detailed explanation, wherein
Fig. 1 is the flow chart of the preparation method of the housing described in the embodiment of the present invention;
Fig. 2 is the structural representation of the housing described in the embodiment of the present invention;
In figure, reference is expressed as: 1-housing, the narrow limit of 2-first, the narrow limit of 3-second, 4-enclosure body.
Detailed description of the invention
In order to make the object, technical solutions and advantages of the present invention clearer, below in conjunction with accompanying drawing to this The embodiment of invention is described in further detail.
The present invention can be embodied in many different forms, and should not be construed as limited to set forth herein Embodiment.On the contrary, it is provided that these embodiments so that the disclosure will be thorough and complete, and will be The design of the present invention is fully conveyed to those skilled in the art, and the present invention will only be defined by the appended claims. In the accompanying drawings, for clarity, layer and the size in region and relative size can be exaggerated.
Embodiment
The present embodiment provides the preparation method of a kind of housing 1, as it is shown in figure 1, comprise the steps:
S1, on the first edge of housing 1 opening chamfering and/or rounding, formed the first narrow limit 2.
As one embodiment of the present of invention, the present embodiment middle shell 1 is metal shell, is chosen as aluminum and closes Gold housing, good processability, light weight, cost of material are low.As the convertible embodiment of the present invention, shell Body 1 can also be other materials, all can realize the purpose of the present invention, belong to protection scope of the present invention. Alternatively, housing 1 is the metalwork of machine-shaping substantially, its inside and outside be formed certain shape and/ Or structure, such as outside are likely to be of the arc of certain surface structure, chamfering, rounding, minute surface, frosted Face, high bright finish etc., inside be likely to be of the groove of antenna/device layout and/or connection/agree with, projection and Various snap-in structures etc., and the through hole running through inside and outside etc..Certainly, in other alternative embodiments, The internal structure of housing 1 can also reprocess molding after coloring.
As one embodiment of the present of invention, in the present embodiment, the first narrow limit 2 is by numerical control processing technology system ?.The step that the first narrow limit 2 is polished also is included so that the first narrow limit 2 after digital control processing Surface forms high bright finish, it is simple to the enforcement of tinting steps.
As one embodiment of the present of invention, the opening of the present embodiment middle shell 1 is rectangle, the first limit Along for two long limits directly contacting with screen, the second edge be not with two minor faces of screen contact.Make For the convertible embodiment of the present invention, the opening of housing 1 can also be arbitrary polygon, all can realize The purpose of the present invention, belongs to protection scope of the present invention.
S2, in enclosure body 4, form protective layer, carry out the first narrow limit 2 colouring for the first time.
As one embodiment of the present of invention, the present embodiment forms in enclosure body 4 step of protective layer Suddenly, farther include:
S21, on the first narrow limit 2 formed shielding layer;Shielding layer includes but not limited to covering of given shape Equipment, in an optional embodiment, it is possible to use cover described in the formation such as masking tape, maskant Layer;
S22, in enclosure body 4, form protective layer with shielding layer for mask;Alternatively, spraying material is used Material carries out spraying to form described protective layer, and in the alternative embodiment of the present invention, protective layer material includes But being not limited to paint, organic coating etc., generation type includes but not limited to spraying, coating, bonding etc.;
S23, removal shielding layer.
S3, on the second edge of housing 1 opening chamfering and/or rounding, formed the second narrow limit 3.
As one embodiment of the present of invention, in the present embodiment, the second narrow limit 3 is by numerical control processing technology system ?.The step that the second narrow limit 3 is polished also is included so that the second narrow limit 3 after digital control processing Surface forms high bright finish, it is simple to the enforcement of tinting steps.
S4, the second narrow limit 3 and enclosure body 4 are carried out second time colour.Enclosure body 4 is being coloured Before need to remove aforementioned protective layer, for certain material formed protective layer, measure pointedly can be taked It is removed, such as, the organic solvents such as n-Amyl acetate or ultraviolet can be used to irradiate liquid medicine (i.e. UV Liquid medicine) etc. chemical reactant aforesaid paint, organic coating etc. are removed.
In order to realize Rimless display effect, the color of tinting steps coloring for the first time is black.
As one embodiment of the present of invention, in the present embodiment, tinting steps is anode oxidation coloration.Sun Heat-tinting not only technique in pole is simple, with low cost, color is beautiful, and the coloring film formed is for converting Film, has certain hardness, wearability and corrosion resistance, disclosure satisfy that shell while having decorative effect The demand of protection.
Anode oxidation coloration needs to carry out in electrolytic solution, to this end, as one embodiment of the present of invention, In the present embodiment, protective layer is acid and alkali-resistance protective layer, and shielding layer is acid and alkali-resistance shielding layer.
As the convertible embodiment of the present invention, tinting steps can also be other any coloring process, all The purpose of the present invention can be realized, belong to protection scope of the present invention.
In the present embodiment, the preparation method of housing 1 housing 1 prepared is as shown in Figure 2.
Housing 1 may be used to portable electron device, such as mobile phone etc., it is possible to realizes Rimless display effect.
Obviously, above-described embodiment is only for clearly demonstrating example, and not to embodiment Restriction.For those of ordinary skill in the field, can also do on the basis of the above description Go out change or the variation of other multi-form.Here without also cannot all of embodiment be given exhaustive. And the obvious change thus extended out or variation still in protection scope of the present invention among.

Claims (10)

1. the preparation method of a housing, it is characterised in that comprise the steps:
Chamfering and/or rounding on the first edge of shell nozzle, form the first narrow limit;
Enclosure body is formed protective layer, carries out described first narrow limit colouring for the first time;
Chamfering and/or rounding on the second edge of described shell nozzle, form the second narrow limit;
Described second narrow limit and described enclosure body carry out second time colour.
The preparation method of housing the most according to claim 1, it is characterised in that described in enclosure body The step of upper formation protective layer, farther includes:
Described first narrow limit is formed shielding layer;
In described enclosure body, described protective layer is formed for mask with described shielding layer;
Remove described shielding layer.
The preparation method of housing the most according to claim 1 and 2, it is characterised in that described second time The step removing described protective layer is also included before tinting steps.
4. according to the preparation method of the housing described in any one of claim 1-3, it is characterised in that described shell Body is metal shell;The most described tinting steps is anode oxidation coloration.
5. according to the preparation method of the housing described in any one of claim 1-4, it is characterised in that described One narrow limit is prepared by numerical control processing technology.
6. according to the preparation method of the housing described in any one of claim 1-5, it is characterised in that described Two narrow limits are prepared by numerical control processing technology.
7. according to the preparation method of the housing described in claim 5 or 6, it is characterised in that also include institute State the first narrow limit and/or step that the second narrow limit is polished.
8. according to the preparation method of the housing described in any one of claim 1-7, it is characterised in that described Once coloring and/or second time are colored as black.
9. a housing, it is characterised in that by the preparation method of the housing described in any one of claim 1-8 Preparation.
10. a portable electron device, it is characterised in that include the housing described in claim 9.
CN201610222399.7A 2016-04-11 2016-04-11 Housing, and preparation method and application thereof Pending CN105904171A (en)