CN105862435A - 一种疏水耐洗羽绒的处理方法 - Google Patents

一种疏水耐洗羽绒的处理方法 Download PDF

Info

Publication number
CN105862435A
CN105862435A CN201610249673.XA CN201610249673A CN105862435A CN 105862435 A CN105862435 A CN 105862435A CN 201610249673 A CN201610249673 A CN 201610249673A CN 105862435 A CN105862435 A CN 105862435A
Authority
CN
China
Prior art keywords
eider down
processing method
nano
fibers
processing
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201610249673.XA
Other languages
English (en)
Inventor
周务农
周茂林
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
ANHUI WANLING DOWN AND FEATHER PRODUCTS Co Ltd
Original Assignee
ANHUI WANLING DOWN AND FEATHER PRODUCTS Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by ANHUI WANLING DOWN AND FEATHER PRODUCTS Co Ltd filed Critical ANHUI WANLING DOWN AND FEATHER PRODUCTS Co Ltd
Priority to CN201610249673.XA priority Critical patent/CN105862435A/zh
Publication of CN105862435A publication Critical patent/CN105862435A/zh
Pending legal-status Critical Current

Abstract

本发明公开了一种疏水耐洗羽绒的处理方法,该处理方法分为三个步骤,先利用前处理液对羽绒进行微蚀处理,增加蛋白纤维的反应活性,在交联改性处理过程中利用戊二醛与羽绒纤维接枝并引入纳米硅,使得纳米硅可牢固的结合在纤维上,较之直接添加纳米材料更为安全高效,同时纳米硅多孔的结构不会影响羽绒的保暖透气性,反倒改善了羽绒纤维疏水性,提高耐洗刷能力,同时具备优良的吸附性,降低羽绒的飘散。本发明工艺与现有技术相比更为高效,且生产工艺简单,原料健康环保,改善了传统羽绒吸水易飘散的缺陷,可制得轻薄保暖的羽绒服饰。

Description

一种疏水耐洗羽绒的处理方法
技术领域
本发明涉及羽绒纤维处理技术领域,尤其涉及一种疏水耐洗羽绒的处理方法。
背景技术
羽绒纤维是一种天然动物蛋白质纤维,其轻质膨松,透气透湿,保暖效果极佳,常被用于羽绒服饰及制品。在生产过程中,羽绒原料需要经过一系列的处理后才能作为填充料使用,羽绒毛料要经过清洗、除脂、除臭、消毒、烘干等程序,如果前处理过程处置不当,将会直接影响羽绒的使用效果。
由于羽绒属于动物质类产品,其本身具有易燃、易虫蛀、易滋生微生物、产品附加值低、养护及洗涤要求高等缺点,如果能对羽绒应用一些处理手段,扬长避短,将会极大的拓宽羽绒制品的使用范围。目前报道的对羽绒进行阻燃、抗菌等处理方法,大多直接将羽绒与处理剂混合进行简单的表面处理,这样处理后产品的效果维持时间短,随着洗涤过程性能会逐渐失效。《羽绒纤维经戊二醛接枝二氰二胺处理后的阻燃性能》一文对羽绒纤维进行阻燃接枝改性处理,虽然在一定程度上提高了羽绒的阻燃时效,但是接枝的二氰二胺有一定的毒性,直接接触皮肤有危害,实际应用价值偏低。
发明内容
本发明目的就是为了弥补已有技术的缺陷,提供一种疏水耐洗羽绒的处理方法。
本发明是通过以下技术方案实现的:
一种疏水耐洗羽绒的处理方法,所述的处理方法包括以下步骤:
(1)前处理:先将羽绒进行水洗、除脂、除杂后干燥,随后将羽绒与前处理液按照1:4-5的体积比混合搅拌处理10-15h,处理结束后取出水洗3-5次后备用,其中所述的前处理液是按N,N’-二甲基甲酰胺:硫脲:去离子水=0.5:1:80-120的重量比配制而成;
(2)交联改性处理:将步骤(1)得到的羽绒投入浓度为2-5%的戊二醛水溶液中,在55-60℃条件下反应1-1.5h,反应结束后加入适量的氨水,调节溶液pH值为8-9,随后滴加正硅酸乙酯,在50-60℃条件下边滴加边超声搅拌,滴加结束后放置30-40min后过滤,过滤物在70-80℃条件下热处理1-2h后备用;
(3)后处理:将步骤(2)的产物投入后处理液中搅拌浸泡1.5-2h后取出,用去离子水清洗3-5次后烘干即得所述羽绒成品,其中所述的后处理液为聚季铵盐-6、乙醇、去离子水按照1-1.5:20-40:100-150的比例配制而成。
所述的步骤(2)中羽绒、戊二醛水溶液的体积比为1:2-3,戊二醛水溶液与正硅酸乙酯的体积比为1:0.01-0.02。
本发明先利用前处理液对羽绒进行微蚀处理,增加蛋白纤维的反应活性,在交联改性处理过程中利用戊二醛与羽绒纤维接枝并引入纳米硅,使得纳米硅可牢固的结合在纤维上,较之直接添加纳米材料更为安全高效,同时纳米硅多孔的结构不会影响羽绒的保暖透气性,反倒改善了羽绒纤维疏水性,提高耐洗刷能力,同时具备优良的吸附性,降低羽绒的飘散。本发明工艺与现有技术相比更为高效,且生产工艺简单,原料健康环保,改善了传统羽绒吸水易飘散的缺陷,可制得轻薄保暖的羽绒服饰。
具体实施方式
该实施例采用鸭羽绒毛进行处理,处理步骤为:
(1)前处理:先将羽绒进行水洗、除脂、除杂后干燥,随后将羽绒与前处理液按照1:4的体积比混合搅拌处理10h,处理结束后取出水洗3次后备用,其中所述的前处理液是按N,N’-二甲基甲酰胺:硫脲:去离子水=0.5:1:80的重量比配制而成;
(2)交联改性处理:将步骤(1)得到的羽绒投入浓度为2%的戊二醛水溶液中,在55℃条件下反应1h,反应结束后加入适量的氨水,调节溶液pH值为8,随后滴加正硅酸乙酯,在50℃条件下边滴加边超声搅拌,滴加结束后放置30min后过滤,过滤物在70℃条件下热处理1h后备用;
(3)后处理:将步骤(2)的产物投入后处理液中搅拌浸泡1.5h后取出,用去离子水清洗3次后烘干即得所述羽绒成品,其中所述的后处理液为聚季铵盐、乙醇、去离子水按照1:20:100的比例配制而成。
步骤(2)中羽绒、戊二醛水溶液的体积比为1:2,戊二醛水溶液与正硅酸乙酯的体积比为1:0.01。
处理后的鸭羽绒毛样品蓬松柔韧,水洗250次后仍具有良好的蓬松感和保暖效果,透湿量为17800WVT(g/m2.d);透气率为443.0mm/s,水滴接触60s后接触角>120℃。

Claims (2)

1.一种疏水耐洗羽绒的处理方法,其特征在于,所述的处理方法包括以下步骤:
(1)前处理:先将羽绒进行水洗、除脂、除杂后干燥,随后将羽绒与前处理液按照1:4-5的体积比混合搅拌处理10-15h,处理结束后取出水洗3-5次后备用,其中所述的前处理液是按N,N’-二甲基甲酰胺:硫脲:去离子水=0.5:1:80-120的重量比配制而成;
(2)交联改性处理:将步骤(1)得到的羽绒投入浓度为2-5%的戊二醛水溶液中,在55-60℃条件下反应1-1.5h,反应结束后加入适量的氨水,调节溶液pH值为8-9,随后滴加正硅酸乙酯,在50-60℃条件下边滴加边超声搅拌,滴加结束后放置30-40min后过滤,过滤物在70-80℃条件下热处理1-2h后备用;
(3)后处理:将步骤(2)的产物投入后处理液中搅拌浸泡1.5-2h后取出,用去离子水清洗3-5次后烘干即得所述羽绒成品,其中所述的后处理液为聚季铵盐-6、乙醇、去离子水按照1-1.5:20-40:100-150的比例配制而成。
2.如权利要求1所述的一种疏水耐洗羽绒的处理方法,其特征在于,所述的步骤(2)中羽绒、戊二醛水溶液的体积比为1:2-3,戊二醛水溶液与正硅酸乙酯的体积比为1:0.01-0.02。
CN201610249673.XA 2016-04-21 2016-04-21 一种疏水耐洗羽绒的处理方法 Pending CN105862435A (zh)