CN105418138A - 一种建筑废料砂基透水砖及其制作方法 - Google Patents
一种建筑废料砂基透水砖及其制作方法 Download PDFInfo
- Publication number
- CN105418138A CN105418138A CN201510763158.9A CN201510763158A CN105418138A CN 105418138 A CN105418138 A CN 105418138A CN 201510763158 A CN201510763158 A CN 201510763158A CN 105418138 A CN105418138 A CN 105418138A
- Authority
- CN
- China
- Prior art keywords
- permeable brick
- sand
- dry
- water
- building waste
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Withdrawn
Abstract
本发明公开了一种建筑废料砂基透水砖,本发明将水稻秸炭化处理后添加到原料中,通过研磨将抗蚊虫粉吸附在表面提高了产品的吸附性和防蚊性能,以改性后的糖滤泥为成孔剂,将沙漠沙水洗烘干再配伍铁铝尖晶石、建筑废料、电气石粉等粗骨料在不影响砖体透水性的情况下明显提高了产品的强度和抗折性能,降低成本,利用本发明制得的砂基透水砖强度高,透水能力强,能够环保利用建筑废料,产品性能符合相关质量标准要求。
Description
技术领域
本发明涉及建筑材料技术领域,尤其涉及一种建筑废料砂基透水砖及其制作方法。
背景技术
近些年来砂基透水砖成为关注热点,这种砂基透水砖,是以沙漠里的沙子为原料,透水性能好,防滑,还不像一般透水砖那样容易被灰尘堵塞,但是成本太高,推广砂基透水砖是实现沙漠沙资源化的有效途径,一方面在矿石资源日益紧缺的情况下,可以将沙漠沙作为一种廉价的建筑用材,另一方面对于我国大面积的沙漠治理、沙漠变废为宝是有益的。然而目前关于砂基透水砖的研究较少,传统的砂基透水砖的生产工艺落后、成本高、功能单一、抗压强度和透水性能不能同时达到透水砖的行业标准。
发明内容
本发明目的就是为了弥补已有技术的缺陷,提供一种建筑废料砂基透水砖及其制作方法。
本发明是通过以下技术方案实现的:
一种建筑废料砂基透水砖,由下列重量份的原料制成:沙漠沙39-40、铁铝尖晶石10-11、建筑废料13-15、电气石粉12-14、水泥9-10、糖滤泥13-14、三元乙丙橡胶6-8、四氧化三铁2.1-2.5、硝酸钠0.6-0.8、抗蚊虫粉0.1-0.3、水稻秸秆5-7、适量水。
所述的一种建筑废料砂基透水砖的制作方法,包括以下步骤:
(1)将水稻秸秆烘干放入炭化炉中于450-500℃的温度下,隔绝空气炭化20-30分钟,冷却至室温加入抗蚊虫粉研磨40-50分钟;
(2)将糖滤泥水洗后于50-60℃温度下烘干,送入高速混合机中加入三元乙丙橡胶、四氧化三铁、硝酸钠和适量的水,以1400-1500转/min的速度高速搅拌15-20分钟,干燥,超声研磨成粉烘干;
(3)将沙漠沙水洗烘干后加入铁铝尖晶石、建筑废料、电气石粉于690-735℃高温煅烧处理后粉碎至120-140目,加入步骤(1)、(2)物料及其他剩余成分混匀,投入球磨机中球磨2-3小时,喷水造粒、陈化2天后压制成生砖坯;
(4)将生砖坯自然晾晒风干,在箱式电阻炉中于1060-1100℃烧结1-2小时,自然冷却至室温出料。
本发明的优点是:本发明将水稻秸炭化处理后添加到原料中,通过研磨将抗蚊虫粉吸附在表面提高了产品的吸附性和防蚊性能,以改性后的糖滤泥为成孔剂,将沙漠沙水洗烘干再配伍铁铝尖晶石、建筑废料、电气石粉等粗骨料在不影响砖体透水性的情况下明显提高了产品的强度和抗折性能,降低成本,利用本发明制得的砂基透水砖强度高,透水能力强,能够环保利用建筑废料,产品性能符合相关质量标准要求。
具体实施方式
一种建筑废料砂基透水砖,由下列重量份的原料制成:沙漠沙39、铁铝尖晶石10、建筑废料13、电气石粉12、水泥9、糖滤泥13、三元乙丙橡胶6、四氧化三铁2.1、硝酸钠0.6、抗蚊虫粉0.1、水稻秸秆5、适量水。
所述的一种建筑废料砂基透水砖的制作方法,包括以下步骤:
(1)将水稻秸秆烘干放入炭化炉中于450℃的温度下,隔绝空气炭化20分钟,冷却至室温加入抗蚊虫粉研磨40分钟;
(2)将糖滤泥水洗后于50℃温度下烘干,送入高速混合机中加入三元乙丙橡胶、四氧化三铁、硝酸钠和适量的水,以1400转/min的速度高速搅拌15分钟,干燥,超声研磨成粉烘干;
(3)将沙漠沙水洗烘干后加入铁铝尖晶石、建筑废料、电气石粉于690℃高温煅烧处理后粉碎至120目,加入步骤(1)、(2)物料及其他剩余成分混匀,投入球磨机中球磨2小时,喷水造粒、陈化2天后压制成生砖坯;
(4)将生砖坯自然晾晒风干,在箱式电阻炉中于1060℃烧结1小时,自然冷却至室温出料。
使用本发明生产的砂基透水砖的技术参数指标如下:抗压强度为48.2MPa,透水系数为0.052cm/s,透水砖的保水性为0.64g/cm2。
Claims (2)
1.一种建筑废料砂基透水砖,其特征在于,由下列重量份的原料制成:沙漠沙39-40、铁铝尖晶石10-11、建筑废料13-15、电气石粉12-14、水泥9-10、糖滤泥13-14、三元乙丙橡胶6-8、四氧化三铁2.1-2.5、硝酸钠0.6-0.8、抗蚊虫粉0.1-0.3、水稻秸秆5-7、适量水。
2.根据权利要求1所述的一种建筑废料砂基透水砖的制作方法,其特征在于包括以下步骤:
(1)将水稻秸秆烘干放入炭化炉中于450-500℃的温度下,隔绝空气炭化20-30分钟,冷却至室温加入抗蚊虫粉研磨40-50分钟;
(2)将糖滤泥水洗后于50-60℃温度下烘干,送入高速混合机中加入三元乙丙橡胶、四氧化三铁、硝酸钠和适量的水,以1400-1500转/min的速度高速搅拌15-20分钟,干燥,超声研磨成粉烘干;
(3)将沙漠沙水洗烘干后加入铁铝尖晶石、建筑废料、电气石粉于690-735℃高温煅烧处理后粉碎至120-140目,加入步骤(1)、(2)物料及其他剩余成分混匀,投入球磨机中球磨2-3小时,喷水造粒、陈化2天后压制成生砖坯;
(4)将生砖坯自然晾晒风干,在箱式电阻炉中于1060-1100℃烧结1-2小时,自然冷却至室温出料。