CN105128401A - Medical sterilized package adhesive coating technology based on silk screen printing - Google Patents
Medical sterilized package adhesive coating technology based on silk screen printing Download PDFInfo
- Publication number
- CN105128401A CN105128401A CN201510488307.5A CN201510488307A CN105128401A CN 105128401 A CN105128401 A CN 105128401A CN 201510488307 A CN201510488307 A CN 201510488307A CN 105128401 A CN105128401 A CN 105128401A
- Authority
- CN
- China
- Prior art keywords
- adhesive
- screen printing
- solvent
- coating technique
- medical
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
The invention relates to a medical sterilized package adhesive coating technology based on silk screen printing. Mixed adhesives, assistant agent and solvent are utilized, the adhesives coat a single paper sheet through a silk screen printing plate, then the single paper sheet and another paper sheet without the adhesives are combined together in a cold press, adhesion and solidification mode through a cold press machine so that a bag can be formed, and the whole bag is placed into a pressure steam sterilization instrument to be sterilized at a high temperature so that a finished product can meet the requirements that when the product is used, an adhesive layer is completely stripped, and paper fibers cannot be drawn out. According to the invention, due to the fact that the medical sterilized package adhesive coating technology is implemented on the surface of a paper material in a silk screen printing mode, the problem that when a medical sterilized package is stripped, paper fibers on the surface of the paper material are prone to being drawn out is solved, and the adhesion performance of the medical sterilized adhesives in special fields is improved through the medical sterilized package adhesive coating technology.
Description
Technical field
The present invention relates to a kind of package printing process, particularly relate to a kind of packaging material, silk screen coating technique, coupling between adhesive-preparing technology and sterilization process.
Background technology
Along with the raising day by day of China's medical level, more and more higher to the packing instructions of curable product.Meanwhile, consider the needs of environmental protection, praise highly in the world with paper for the packaged form moulded.Medical sterilization paper bag generally adopts high surface tension material, and as paper, leaching membrane paper or lacquer painting paper are composited, it has the advantages that sealing reliably, is easily torn.Medical sterilization has at least a surface to be can pass through water or steam under being packaged in steam sterilizing, and medical sterilization coated paper envelope is required to the interface absolute cleanliness of stripping in use.For these requirements of medical sterilization coated paper envelope, just need to select special water soluble adhesive, thus make product meet sealing property, under high-temp steam sterilizing, adhesive has good temperature stability, easily from bonding paper splitting, performance requirement not inter-adhesive after stripping.Current medical sterilization coated paper envelope generally adopts in the side of medico paper around edge frame gluing, reserved to put into packing material, covers paper, cold pressing bonding, cut, thus formed paper bag, sealing, sterilizing, as long as peel off at paper bag opening end can open from two layers of paper bonding place during use.But medical sterilization packaging bag is on the market after pressuresteam sterilization, easily produces fiber during stripping and extract out, peel off the problems such as unclean, safety problem during use can be affected.
Summary of the invention
For the problems referred to above, the invention provides a kind of medical sterilization based on serigraphy packaging coating technique, to packaging material, silk screen coating technique, the special process parameter of mating between adhesive-preparing technology and sterilization process and component ratio relation, thus after solution pressuresteam sterilization, stripping occurs that paper fiber is extracted out, peels off the problems such as unclean.
To achieve these goals, the technical scheme of employing is as follows in the present invention:
A kind of packaging of the medical sterilization based on serigraphy coating technique, utilize adhesive and auxiliary agent, the solvent of allotment, by screen printing forme, adhesive is coated in sheet-fed surface, then gluing paper non-with another is colded pressing together with adhering and solidifying by machine of colding pressing, it is made to become bag, entirety is put into pressuresteam sterilization instrument high-temperature sterilization again, when making finished product reach use, glue-line is peeled off clean, and paper fiber can not be drawn out of.
The mesh number of the screen printing forme of the gluing employing of described screen printing forme selects 200 orders, and material is nylon wire, and spread is 24.928 ~ 67.343g/m
2.
The allotment of described adhesive and auxiliary agent, solvent: adhesive
:auxiliary agent
:solvent=100
:(0.2 ~ 0.5)
:(0.4 ~ 1), wherein, solvent is alcohol solvent.
Described adhering and solidifying of colding pressing adopts normal temperature cure mode, leaves standstill adhesive solidification after 10 minutes at normal temperatures.
In described pressuresteam sterilization instrument, high-temperature sterilizing process Selecting parameter works 40 minutes under 134 DEG C of sterilizing programs, and sterilizing terminates.
The invention has the beneficial effects as follows:
1 pair of silk screen coating technique parameter is studied, and determines the matching of the parameters such as screen printing forme mesh number, spread and other relevant parameters.
The various water soluble adhesive used in 2 pairs of silk screen coating techniques and various auxiliary agent, solvent are analyzed and researched, and finally determine the proportion relation of different types of water soluble adhesive, auxiliary agent and solvent the best, guarantee the quality of medical sterilization packaging adhesive.
The various medical sterilization packaging paper used in 3 pairs of medical sterilization packaging coating techniques are analyzed and researched, and determine the matching of different paper and silk screen gluing and related process parameters.
4 pairs of medical sterilization packaging coating technique parameters are studied, and determine curing rate, the matching of the parameter such as sterilising temp and time and other relevant parameters.
Therefore, the present invention realizes medical sterilization packaging coating technique by screen printing mode on paper material surface, solves when peeling off in medical sterilization packaging and easily occurs the problems such as paper fiber extraction on paper material surface.The inventive method is utilized to improve the sticky stickiness energy of medical sterilization adhesive at special dimension.
Accompanying drawing explanation
Fig. 1 is the medical sterilization packaging coating technique flow chart based on serigraphy.
Detailed description of the invention
Below in conjunction with medical sterilization packaging coating technique parameter form and the flow chart of serigraphy, detailed elaboration is done to the present invention.
Table 1 is depicted as the medical sterilization packaging coating technique parameter form based on serigraphy, and imbody goes out each link key parameter and inner link thereof in the medical sterilization packaging coating technique based on serigraphy.
Table 1
Different types of adhesive and auxiliary agent thereof have different proportionings, have different suitabilities to coating technique parameter; The invention provides the configuration proportion of three kinds of different adhesive and auxiliary agent, and corresponding coating technique parameter.
1. the gluing of screen printing forme
The mesh number of screen printing forme selects 200 orders, and material is nylon wire.Screen printing forme make process in guarantee silk screen smooth, compact, to obtain high-quality screen printing forme.
Spread is 24.928 ~ 67.343g/m
2.
2. the allotment of adhesive and auxiliary agent, solvent
Adhesive and the necessary Selecting Complete Set of auxiliary agent, solvent is the alcohol solvent that dissolution aids is conventional.
Adhesive
:auxiliary agent
:solvent=100
:(0.2 ~ 0.5)
:(0.4 ~ 1).
Take auxiliary agent and solvent respectively by above-mentioned configuration proportion, stir certain hour after mixing and add in adhesive again to dissolving completely, after being uniformly mixed, be applied to the adhesive of medical sterilization packaging accordingly.
3. to cold pressing adhering and solidifying
The present invention adopts machine of colding pressing to carry out the bonding of coated paper envelope.
Adopt normal temperature cure mode, leave standstill adhesive solidification after 10 minutes at normal temperatures.
4. pressuresteam sterilization technological parameter is arranged
The present invention adopts pressuresteam sterilization instrument.To the packaging bag of sterilizing be needed to put into machine, select to work under 134 DEG C of sterilizing programs 40 minutes, sterilizing terminates.
For ensureing the stability of medical sterilization coated paper envelope quality, the medical sterilization packaging coating technique based on serigraphy all should carry out under constant-temperature constant-humidity environment.Different types of adhesive and auxiliary agent thereof have different proportionings, have different suitabilities to coating technique parameter; The invention provides the configuration proportion of three kinds of different adhesive and auxiliary agent, solvent, and corresponding coating technique parameter.The medical sterilization packaging paper adopted in the present invention, the quantitative of No. 1, paper is 52.8775g/m
2, the quantitative of No. 2, paper is 62.8604g/m
2.Other parameters of No. 1, paper and No. 2, paper, resistance to broken, moisture-inhibiting, ventilative, tensile strength is all different.
The invention provides the configuration proportion of three kinds of different adhesive and auxiliary agent, and the coating technique parameter of correspondence.Design parameter is as shown in table 1.
According to Fig. 1 in the present invention, the medical sterilization packaging coating technique operation of serigraphy is carried out in parameter preparation, can solve when peeling off in medical sterilization packaging and easily occur the problems such as paper fiber extraction on paper material surface.
The medical sterilization packaging coating technique flow process of serigraphy is described, its technological process: the allotment → silk screen gluing → adhering and solidifying → pressuresteam sterilization → finished product of colding pressing of screen printing forme → adhesive processed and auxiliary agent shown in Fig. 1.Technological process key link is described as follows:
1. screen printing forme processed
The making of screen printing forme adopts makes by hand, and material is nylon.Screen printing forme make process in guarantee silk screen smooth, compact, to obtain high-quality screen printing forme.
2. the allotment of adhesive and auxiliary agent, solvent
Adhesive and auxiliary agent must be Selecting Complete Sets.Adhesive, auxiliary agent and solvent carry out corresponding coupling according to the model of adhesive.
Take auxiliary agent and solvent respectively by configuration proportion, stir certain hour after mixing and add in adhesive again to dissolving completely, after being uniformly mixed, be applied to the adhesive of medical sterilization packaging accordingly.
3. silk screen gluing
Silk screen gluing can be manual gluing also can engine sizing-.The difference of spread, affects the adhesive strength of medical sterilization coated paper envelope, selects the mesh size of silk screen gluing according to the scope of spread.
4. to cold pressing adhering and solidifying
The present invention adopts machine of colding pressing to carry out the bonding of coated paper envelope.
Adopt normal temperature cure mode, leave standstill adhesive solidification after 10 minutes at normal temperatures.
5. pressuresteam sterilization technological parameter is arranged
The present invention adopts pressure steam sterilizer.To the packaging bag of sterilizing be needed to put into machine, select to work under 134 DEG C of sterilizing programs 40 minutes, sterilizing terminates.
For ensureing the stability of medical sterilization coated paper envelope quality, the medical sterilization packaging coating technique based on serigraphy all should carry out under constant-temperature constant-humidity environment.
Claims (5)
1. the packaging of the medical sterilization based on a serigraphy coating technique, it is characterized in that: the adhesive and auxiliary agent, the solvent that utilize allotment, by screen printing forme, adhesive is coated in sheet-fed surface, then gluing paper non-with another is colded pressing together with adhering and solidifying by machine of colding pressing, it is made to become bag, entirety is put into pressuresteam sterilization instrument high-temperature sterilization again, when making finished product reach use, glue-line is peeled off clean, and paper fiber can not be drawn out of.
2. the packaging of the medical sterilization based on serigraphy coating technique according to claim 1, is characterized in that: the mesh number of the screen printing forme of the gluing employing of described screen printing forme selects 200 orders, and material is nylon wire, and spread is 24.928 ~ 67.343g/m
2.
3. the medical sterilization based on serigraphy according to claim 1 packaging coating technique, is characterized in that: the allotment of described adhesive and auxiliary agent, solvent: adhesive
:auxiliary agent
:solvent=100
:(0.2 ~ 0.5)
:(0.4 ~ 1), wherein, solvent is alcohol solvent.
4. the medical sterilization based on serigraphy according to claim 1 packaging coating technique, is characterized in that: described in adhering and solidifying of colding pressing adopt normal temperature cure mode, leave standstill adhesive solidification after 10 minutes at normal temperatures.
5. the packaging of the medical sterilization based on serigraphy coating technique according to claim 1, is characterized in that: in described pressuresteam sterilization instrument, high-temperature sterilizing process Selecting parameter works 40 minutes under 134 DEG C of sterilizing programs, and sterilizing terminates.