CN104893392A - 防潮腻子粉 - Google Patents

防潮腻子粉 Download PDF

Info

Publication number
CN104893392A
CN104893392A CN201510285993.6A CN201510285993A CN104893392A CN 104893392 A CN104893392 A CN 104893392A CN 201510285993 A CN201510285993 A CN 201510285993A CN 104893392 A CN104893392 A CN 104893392A
Authority
CN
China
Prior art keywords
parts
putty powder
kilograms
dampproof
sodium chloride
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201510285993.6A
Other languages
English (en)
Inventor
梁运富
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Liuzhou Pu Ya Trade Co Ltd
Original Assignee
Liuzhou Pu Ya Trade Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Liuzhou Pu Ya Trade Co Ltd filed Critical Liuzhou Pu Ya Trade Co Ltd
Priority to CN201510285993.6A priority Critical patent/CN104893392A/zh
Publication of CN104893392A publication Critical patent/CN104893392A/zh
Pending legal-status Critical Current

Abstract

本发明公开了一种防潮腻子粉,涉及建筑材料技术领域,该防潮腻子粉采用如下重量份的原料制成:白水泥:25份至40份;坡缕石粘土:10份至15份;甘蔗渣纤维:3份至8份;羟丙基甲基纤维素:0.5份至1份;高吸水树脂:5份至10份;膨润土:2.5份至3.5份;氯化纳:0.5份至1份。本发明可以解决现有的腻子粉不耐水的问题。

Description

防潮腻子粉
技术领域
本发明涉及建筑材料技术领域,尤其是一种用于墙壁的防潮腻子粉。
背景技术
随着人们生活质量的提高,家庭装修越来越得到人们的重视,腻子粉是家庭装修中不可缺少的材料,现有的腻子粉多采用的是碳酸钙、滑石粉、聚乙醇胶等原料制成,其不防潮功能差,在我国南方尤其是广西每年的3月至4月间阴雨不断,空气湿度大,家里刮了腻子的墙壁上经常会出现凝聚的水珠或流水,不但造成人体的不舒爽还造成家用电器的短路烧坏及家庭用品、家具的发霉损坏,因此提供一种无毒无害、粘结度强且环保防潮的腻子粉是本领域技术人员亟需解决的问题。
发明内容
本发明所要解决的技术问题是提供一种防潮腻子粉,它可以解决现有的腻子粉无防潮功能的问题。
为了解决上述问题,本发明的技术方案是:这种防潮腻子粉,采用如下重量份的原料制成:
白水泥:25份至40份;坡缕石粘土:10份至15份;甘蔗渣纤维:3份至8份;羟丙基甲基纤维素:0.5份至1份;高吸水树脂:5份至10份;膨润土:2.5份至3.5份;氯化纳:0.5份至1份。
上述技术方案中,更具体的方案还可以是:白水泥:29份至35份;坡缕石粘土:12份至14份;甘蔗渣纤维:5份至7份;羟丙基甲基纤维素:0.6份至0.9份;高吸水树脂:6份至8份;膨润土:2.7份至3份;氯化纳:0.6份至0.8份。
进一步的:白水泥:32份;坡缕石粘土:13份;甘蔗渣纤维:6份;羟丙基甲基纤维素:0.7份;高吸水树脂:7份;膨润土:3份;氯化纳:0.7份。
由于采用上述技术方案 ,本发明具有如下有益效果:
1、由于在白水泥中加入了坡缕石粉,其不但增加了腻子粉的粘结度和耐水性并且坡缕石粉干燥收缩率小,不产生龟裂;
2、由于加入了甘蔗渣纤维,甘蔗渣纤维作为增韧剂,其不但增加了腻子的抗裂性并且天然环保;
3、由于加入了羟丙基甲基纤维素,作为分散剂和稳定剂,使各原料在水或有机溶剂中都具有良好相溶性;
4、由于加入了高吸水树脂,起到房间空气的吸潮作用,使潮湿天气里的房间保持干燥,不但使人体感觉舒爽还保护了家用电器及家庭用品、家具的干燥,
5、由于加入了膨润土,其具有较强的吸湿性和粘接性,不但天然环保且提高了腻子的吸湿性和粘接性;
6、由于加入了氯化纳,氯化纳的亲水性和杀毒性,其不但增加了腻子粉的吸潮作用并起到消毒作用。
具体实施方式
下面用实施例对本发明进一步详述:
实施例1:
这种防潮腻子粉,采用如下重量的原料制成:
白水泥:25公斤;坡缕石粘土:10公斤;甘蔗渣纤维:3公斤;羟丙基甲基纤维素:0.5公斤;高吸水树脂:5公斤;膨润土:2.5公斤;氯化纳:0.5公斤;
包括如下步骤:
A.将坡缕石粘土置于土窑中进行烧制,时间2小时,温度280摄氏度至300摄氏度,待用;
B.将步骤A制得的坡缕石粘土放入粉碎机中进行粉碎,得粉碎料;
C.将步骤B制得的粉碎料和高吸水树脂、羟丙基甲基纤维素、膨润土、甘蔗渣纤维放入搅拌机中,以5000转/分的速度搅拌2分钟,得混合料;
D.将步骤C制得的混合料放入研磨机中进行研磨,细度为500目,即得。
实施例2:
这种防潮腻子粉,采用如下重量的原料制成:
白水泥:40公斤;坡缕石粘土:15公斤;甘蔗渣纤维:8公斤;羟丙基甲基纤维素:1公斤;高吸水树脂:10公斤;膨润土:3.5公斤;氯化纳:1公斤;其余均与实施例一相同。
实施例3:
这种防潮腻子粉,采用如下重量的原料制成:
白水泥:29公斤;坡缕石粘土:12公斤;甘蔗渣纤维:5公斤;羟丙基甲基纤维素:0.6公斤;高吸水树脂:6公斤;膨润土:2.7公斤;氯化纳:0.6公斤;氯化纳:0.6公斤;其余均与实施例一相同。
实施例4
这种防潮腻子粉,采用如下重量的原料制成:
白水泥:35公斤;坡缕石粘土:14公斤;甘蔗渣纤维7公斤;羟丙基甲基纤维素: 0.9公斤;高吸水树脂:8公斤;膨润土:3公斤;氯化纳:0.8公斤;其余均与实施例一相同。
实施例5
这种防潮腻子粉,采用如下重量的原料制成:
白水泥:32公斤;坡缕石粘土:13公斤;甘蔗渣纤维:6公斤;羟丙基甲基纤维素:0.7公斤;高吸水树脂:7公斤;膨润土:3公斤;氯化纳:0.7公斤;其余均与实施例一相同。

Claims (3)

1.一种防潮腻子粉,其特征在于:采用如下重量份的原料制成:
白水泥:25份至40份;坡缕石粘土:10份至15份;甘蔗渣纤维:3份至8份;羟丙基甲基纤维素:0.5份至1份;高吸水树脂:5份至10份;膨润土:2.5份至3.5份;氯化纳:0.5份至1份。
2.根据权利要求1所述的防潮腻子粉,其特征在于:采用如下重量份的原料制成:
白水泥:29份至35份;坡缕石粘土:12份至14份;甘蔗渣纤维:5份至7份;羟丙基甲基纤维素:0.6份至0.9份;高吸水树脂:6份至8份;膨润土:2.7份至3份;氯化纳:0.6份至0.8份。
3.根据权利要求1或2所述的防潮腻子粉,其特征在于:采用如下重量份的原料制成:
白水泥:32份;坡缕石粘土:13份;甘蔗渣纤维:6份;羟丙基甲基纤维素:0.7份;高吸水树脂:7份;膨润土:3份;氯化纳:0.7份。
CN201510285993.6A 2015-05-29 2015-05-29 防潮腻子粉 Pending CN104893392A (zh)