CN104862741A - Method for stopping a cell under situation of no power-off of aluminum electrolytic cell - Google Patents
Method for stopping a cell under situation of no power-off of aluminum electrolytic cell Download PDFInfo
- Publication number
- CN104862741A CN104862741A CN201510304486.2A CN201510304486A CN104862741A CN 104862741 A CN104862741 A CN 104862741A CN 201510304486 A CN201510304486 A CN 201510304486A CN 104862741 A CN104862741 A CN 104862741A
- Authority
- CN
- China
- Prior art keywords
- short
- circuit opening
- short circuit
- cell
- circuit port
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
The invention discloses a method for stopping a cell under the situation of no power-off of an aluminum electrolytic cell. The method comprises the following steps: 1), preparing a cell stopping tool; 2) replacing a short circuit port insulating rod by using an iron screw rod with an insulating sleeve; 3) viewing the horizontal bus height of the cell to be stopped; 4) taking an electrolyte and gradually reducing the cell voltage to below 1.10 V; 5) cleanly blowing accumulated dust at a short circuit port by using a high-pressure air pipe; 6) taking out an insulating plug board and remaining a transverse insulating plug board; 7) cleaning the accumulated dust at the short circuit port by using the high-pressure air pipe again; 8) measuring the pressure drop of the short circuit port; 9) taking out the transverse insulating plug board; 10) measuring the pressure drop of the short circuit port; 11) lifting anodes; 12) measuring the pressure drop of the short circuit port again; 13) picking up the tool to complete the groove stopping operation. The method disclosed by the invention is reasonable in design; all the anodes of the cell to be stopped are directly lowered, so that bottom palms of the anodes are completely immersed into molten aluminum in the cell to perform the direct short circuit operation of the short circuit port, and therefore, huge gains are brought to electrolytic aluminum production.
Description
Technical field
The invention belongs to electrolyzer field, specifically, relate to a kind of aluminium cell and not have a power failure groove method.
Background technology
Electrolyzer is after long-time running, and the breakage that cathode carbon pieces and sidepiece silica brick all will produce in various degree, therefore electrolyzer inevitably will carry out stopping groove operation.Stop groove operation to take power failure to series or use Sai Er switch circuit breaking to carry out every groove that stops to operate, series power failure is produced groove to other and is brought more negative impact, as output reduce, effect is frequent, destroy burner hearth inner mold, contaminate environment, even cause potline current to be difficult to recover the serious consequences such as ortho states, Sai Er switch circuit breaking is adopted to carry out stopping groove operation, operated as cumbersome, at substantial man power and material cost.
Summary of the invention
In order to overcome the deficiencies in the prior art, the invention provides a kind of aluminium cell not have a power failure groove method, reasonable in design, not stopping potline current, state that groove carries out power-off will be stopped without Sai Er Switch Controller under, all anodes that directly will stop groove decline, in the aluminium liquid that anode bottom is immersed in groove completely, make it to be in short-circuit condition, bath voltage at below 1.10v, and carries out the operating process of the direct short circuit of short-circuit opening, brings huge income to Aluminum Electrolysis Production.
The technical solution adopted for the present invention to solve the technical problems is:
Aluminium cell does not have a power failure groove method, it is characterized in that: step is as follows:
1), prepare to stop groove Work tool: iron screw rod, pneumatic impact wrench, fork spanner, speed wrench, volt ohm-milliammeter, change poles face shield, insulation rod, sledgehammer;
2), short circuit port insulation bar is changed with insulation thimble on iron screw rod band;
3), watching and will stop groove horizontal bus height, require to be not more than 250mm, requiring to propose bus operation to this groove as being greater than 250mm;
4), taking electrolyte, progressively reduce bath voltage to below 1.10v;
5), blow clean with the dust stratification of high-pressure air hose by short-circuit opening;
6), take out insulation insertion plate, keep lateral isolation plate;
7), with the dust stratification of high-pressure air hose to short-circuit opening place again clear up, with little bamboo chip, the foreign material in short-circuit opening gap are cleaned out;
8), measure short-circuit opening pressure drop, require to be less than 1.0v, be greater than 1.0v and require to reduce potline current;
9), lateral isolation plate is taken out, pneumatic impact wrench is used rapidly short-circuit opening to be carried out short circuit, its operation steps is: a people at the side pneumatic impact wrench of short-circuit opening by urgent for iron screw rod, two people fix iron bolt at the opposite side fork spanner of short-circuit opening, order by first and third, two, four is by urgent for iron screw rod, the like, by four short-circuit opening end of operations;
10), measure short-circuit opening pressure drop, require to be less than 15mv;
11), on lift anode, make horizontal bus be in 50mm;
12), again measure short-circuit opening pressure drop, require to be less than 20mv;
13), pack up, it is complete to stop groove operation.
Owing to have employed technique scheme, compared with prior art, the present invention is reasonable in design, not stopping potline current, state that groove carries out power-off will be stopped without Sai Er Switch Controller under, all anodes that directly will stop groove decline, in the aluminium liquid that anode bottom is immersed in groove completely, make it to be in short-circuit condition, bath voltage at below 1.10v, and carries out the operating process of the direct short circuit of short-circuit opening, brings huge income to Aluminum Electrolysis Production.
Embodiment
Aluminium cell does not have a power failure groove method, and step is as follows:
1), prepare to stop groove Work tool: iron screw rod, pneumatic impact wrench, fork spanner, speed wrench, volt ohm-milliammeter, change poles face shield, insulation rod, sledgehammer etc.
2), short circuit port insulation bar is changed with insulation thimble on iron screw rod band.
3), watching and will stop groove horizontal bus height, require to be not more than 250mm, requiring to propose bus operation to this groove as being greater than 250mm.
4), taking electrolyte, progressively reduce bath voltage to below 1.10v.
5), blow clean with the dust stratification of high-pressure air hose by short-circuit opening.
6), take out insulation insertion plate, keep lateral isolation plate.
7), with the dust stratification of high-pressure air hose to short-circuit opening place again clear up, with little bamboo chip, the foreign material in short-circuit opening gap are cleaned out.
8), measure short-circuit opening pressure drop, require to be less than 1.0v, be greater than 1.0v and require to reduce potline current.
9), lateral isolation plate is taken out, pneumatic impact wrench is used rapidly short-circuit opening to be carried out short circuit, its operation steps is: a people at the side pneumatic impact wrench of short-circuit opening by urgent for iron screw rod, two people fix iron bolt at the opposite side fork spanner of short-circuit opening, order by first and third, two, four is by urgent for iron screw rod, the like, by four short-circuit opening end of operations.
10), measure short-circuit opening pressure drop, require to be less than 15mv.
11), on lift anode, make horizontal bus be in 50mm.
12), again measure short-circuit opening pressure drop, require to be less than 20mv.
13), pack up, it is complete to stop groove operation.
The present invention is reasonable in design, not stopping potline current, state that groove carries out power-off will be stopped without Sai Er Switch Controller under, all anodes that directly will stop groove decline, in the aluminium liquid that anode bottom is immersed in groove completely, make it to be in short-circuit condition, bath voltage at below 1.10v, and carries out the operating process of the direct short circuit of short-circuit opening, brings huge income to Aluminum Electrolysis Production.
The present invention is not limited to above-mentioned preferred implementation, and anyone should learn the structural changes made under enlightenment of the present invention, and every have identical or akin technical scheme with the present invention, all belongs to protection scope of the present invention.
Claims (1)
1. aluminium cell does not have a power failure groove method, it is characterized in that: step is as follows:
1), prepare to stop groove Work tool;
2), short circuit port insulation bar is changed with insulation thimble on iron screw rod band;
3), watching and will stop groove horizontal bus height, require to be not more than 250mm, requiring to propose bus operation to this groove as being greater than 250mm;
4), taking electrolyte, progressively reduce bath voltage to below 1.10v;
5), blow clean with the dust stratification of high-pressure air hose by short-circuit opening;
6), take out insulation insertion plate, keep lateral isolation plate;
7), with the dust stratification of high-pressure air hose to short-circuit opening place again clear up, with little bamboo chip, the foreign material in short-circuit opening gap are cleaned out;
8), measure short-circuit opening pressure drop, require to be less than 1.0v, be greater than 1.0v and require to reduce potline current;
9), lateral isolation plate is taken out, pneumatic impact wrench is used rapidly short-circuit opening to be carried out short circuit, its operation steps is: a people at the side pneumatic impact wrench of short-circuit opening by urgent for iron screw rod, two people fix iron bolt at the opposite side fork spanner of short-circuit opening, order by first and third, two, four is by urgent for iron screw rod, the like, by four short-circuit opening end of operations;
10), measure short-circuit opening pressure drop, require to be less than 15mv;
11), on lift anode, make horizontal bus be in 50mm;
12), again measure short-circuit opening pressure drop, require to be less than 20mv;
13), pack up, it is complete to stop groove operation.