CN104649602A - 流化床粉煤灰激活剂 - Google Patents
流化床粉煤灰激活剂 Download PDFInfo
- Publication number
- CN104649602A CN104649602A CN201310582560.8A CN201310582560A CN104649602A CN 104649602 A CN104649602 A CN 104649602A CN 201310582560 A CN201310582560 A CN 201310582560A CN 104649602 A CN104649602 A CN 104649602A
- Authority
- CN
- China
- Prior art keywords
- fly ash
- bed fly
- fluidized bed
- activating agent
- fluidization bed
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
一种能流化床粉煤灰激活剂。主要分为成分是电厂粉煤灰与高炉炼铁产生的水渣混合而成的固体添加剂和浓度40%的氢氧化钠溶液与5%水玻璃混合的液体激活剂,能够提高流化床粉煤灰活性,使常态无活性的流化床粉煤灰强度活性指数≥70%。
Description
技术领域
本发明涉及一种流化床粉煤灰激活剂,尤其是能改变流化床粉煤灰固化性能的激活剂。
背景技术
目前,流化床粉煤灰由于其低温循环烧结的特点,导致循环流化床灰无法形成玻璃相而导致活性相对较低,加之流化床灰在烧结过程中,添加有过量的石灰,对其本身的凝胶时间和强度产生较大的影响,导致流化床粉煤灰活性较低,水化后无法凝固、产生强度,无法像常规锅炉灰一样用于铺路、建筑、固井等领域。无法进行利用的流化床粉煤灰只能使用掩埋的方式处理,产生较大的环境影响。
发明内容
为了克服现有的流化床粉煤灰无活性,无法进行常规利用的问题,本发明提供一种能有效提高流化床活性的激活剂,能改变流化床粉煤灰的固化性能,使其可以应用于于铺路、建筑、固井等领域。
本发明解决其技术问题所采用的技术方案是:在流化床粉煤灰中添加活性灰、活性颗粒,使混合灰整体形成均匀整体,通过灰中活性物质连接粉煤灰颗粒,形成粉煤灰与活性成分相连接的网状结构,通过添加碱性溶液,可使混合物质中的分子键断裂,与水进行水化反应,形成类似水泥浆的可固化结构,以此激活剂激活的粉煤,具有可固化、固化后拥有一定强度的特点。
本发明的有益效果是,解决了流化床粉煤灰无活性的问题,使得流化床粉煤灰可以固化,应用于铺路固井等领域。解决了流化床粉煤灰掩埋处理产生的环境问题。
Claims (4)
1.一种流化床粉煤灰激活剂,其特征是:提高流化床粉煤灰的活性,使原本无法固化的流化床粉煤灰可以固化。
2.根据权利要求1所述的流化床粉煤灰激活剂,其特征是:分为固体添加剂与液体碱性激活剂。
3.根据权利要求1所述的流化床粉煤灰激活剂,其特征是固体添加剂为电厂粉煤灰与高炉炼铁产生的水渣的混合物。
4.液体碱性激活剂成分为浓度40%的氢氧化钠溶液与5%水玻璃的混合溶液。