CN104413823A - Clothes and production method thereof - Google Patents

Clothes and production method thereof Download PDF

Info

Publication number
CN104413823A
CN104413823A CN201310406276.5A CN201310406276A CN104413823A CN 104413823 A CN104413823 A CN 104413823A CN 201310406276 A CN201310406276 A CN 201310406276A CN 104413823 A CN104413823 A CN 104413823A
Authority
CN
China
Prior art keywords
hot melt
adhesive tape
melt adhesive
fabric
clothes
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201310406276.5A
Other languages
Chinese (zh)
Inventor
秦卫平
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Toray Fibers and Textiles Research Laboratories China Co Ltd
Original Assignee
Toray Fibers and Textiles Research Laboratories China Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Toray Fibers and Textiles Research Laboratories China Co Ltd filed Critical Toray Fibers and Textiles Research Laboratories China Co Ltd
Priority to CN201310406276.5A priority Critical patent/CN104413823A/en
Publication of CN104413823A publication Critical patent/CN104413823A/en
Pending legal-status Critical Current

Abstract

The invention discloses a piece of clothes and a production method thereof. At least one part of the clothes is sutured; a seam of the sutured part is a single-layer or multi-layer fabric, and the sewing wrinkle grade at the seam can still reach over 3.5 levels after household cleaning is performed for five times according to a GB/T8629 5A program. A hot melt adhesive tape is firstly adhered to the sutured seam or/and an adhesive is coated, and then suturing and ironing are performed; or suturing and ironing are performed firstly, and then the hot melt adhesive tape is firstly adhered to the sutured seam or/and the adhesive is coated. The flatness of the seam of the clothes after washing is improved.

Description

A kind of clothes and production method thereof
Technical field
The present invention relates to the production method of a kind of clothes and this clothes.Being specifically related to one has at least a place to employ suture, and the good clothes of the wrinkling washing resistance of the seam crossing of suture and production method thereof.
Background technology
At present, the clothes that market is sold adopts conventional sewing tech to produce mostly, wherein infirmity, the sleeve gram husband of the collar of upper dress, inner placket width, sleeve, latasuture, the bottom, front and back take charge of again and lower dress the place such as the waist of trousers, front and back crotch seam, latasuture, pin mouth especially easily wrinkling, be not convinced, the rear planarization of washing is poorer.This is mainly because when adopting plane fabric to make relief clothes, need have the fabric of curve shape to splice with polylith, oblique silk will be had like this through broadwise, particularly woven, easily stretch after the craspedodrome tissue of broadwise deforms, make and just become difficulty, when adding suture, eedle insertion fabric, the configuration of surface of fabric changes, and suture place is smooth not.Even if make moderate progress after flatiron, the effect after washing is also not fully up to expectations.
Disclose the novel shirt of a kind of anti-wrinkle shrink-proof in patent document CN2569576Y, by set in the positions such as seam at the bottom of the infirmity seam of the sleeve of shirt, side seam and sleeve adhesive plaster belt (double-faced adhesive tape) realize Machine Washable, wrinkle resistant, easily the object such as to arrange; And for example disclose a kind of resistance to deformation wash-and-wear of shirt in patent document CN201754769U, be embedded two-sided fusible interlining filler rod at the side seam of shirt, infirmity seam of tucking inside the sleeve, front yoke seam, rear seam, pocket seam, inner towel seam and the sleeve vent seam place of taking charge of again, realize non-ironing effect.But above-mentioned patent does not all relate to the washing resistance problem of seam crossing, although employ double-faced adhesive tape or two-sided fusible interlining filler rod, stitch because it is positioned at, if it is not good to set fastness, after more easily reducing initial stage and washing, make wrinkling grade.
Summary of the invention
The object of the invention is to overcome the problems referred to above, even if provide a kind of by the continuous home washings of GB/T8629 standard 5 times, seam crossing make clothes and the production method thereof that wrinkling grade still can reach more than 3.5 grades.
For achieving the above object, clothes of the present invention has at least a place to employ suture, and the seam crossing at above-mentioned suture position is single or multiple lift fabric, and suture position is pasted with hot melt adhesive tape and/or is coated with adhesive glue.Preferred suture position entirety or local coating adhesive glue.Adhesive glue just no longer melts once solidify, and has irreversibility; Use position feel more soft than hot melt adhesive tape; Adhesive glue working procedure of coating is simple, be easy to operate (step completes).
As preferably, hot melt adhesive tape and/or adhesive glue are positioned at the table side of seam crossing, are also pasted with one deck ornamental tape or fabric above it; Or hot melt adhesive tape and/or adhesive glue are positioned at the inboard of seam crossing, are also pasted with one deck ribbon or fabric above it.
Fabric of the present invention, hot melt adhesive tape, adhesive glue, ornamental tape or ribbon have antibacterial deodourizing and/or fragrance.The imparting of antibacterial deodourizing mainly by adding antibacterial deodourizing auxiliary agent when aft-loaded airfoil, suppresses the generation of the bacterium such as staphylococcus, Moraxella with this; The imparting of fragrance is by selecting in spinning process the yarn that adds fragrance particle or selecting the fiber that easily absorbs fragrance or add perfume microcapsule when aft-loaded airfoil.
As preferably, suture site portion uses hot melt adhesive tape or adhesive glue.
As preferably, in order to make this invention outward appearance and ordinary coat not have difference, hot melt adhesive tape and/or adhesive glue are used in the middle of the fabric at suture position.Hot melt adhesive tape due to through HTHP consolidation process, even if also can not peel off with fabric through repeatedly high strength washing, thus improves the initial stage and makes wrinkling grade after washing.
As preferably, in order to increase ornamental or change clothes fashion, hot melt adhesive tape and/or adhesive glue are used in the table side of seam crossing, and are also pasted with one deck ornamental tape or fabric above it.Ornamental tape can be selected as required.
As preferably, to be rubbed the uncomfortable property that skin brings by seam to eliminate, hot melt adhesive tape and/or adhesive glue are positioned at the inboard of seam crossing, and are also pasted with one deck ribbon or fabric above it.Ribbon can be selected as required.
Above-mentioned stickup fabric both first cannot can not do loosely limit process, can first press into the vertical bar not having burr after cutting yet when being cut into vertical bar, and then used.
As preferably, clothes of the present invention the making wrinkling grade and still can reach more than 3.5 grades of seam crossing after 60 degree of high strength industrials wash 5 times.
Above-mentioned hot melt adhesive tape is the double-side hot-melt adhesive film of TPU composition (TPUE), usually first fix with flatiron and then carry out hot pressing reinforcing with hot press, when usual hot pressing is reinforced, the condition of hot press is set as: temperature 110 ~ 180 degree, pressure 2 ~ 3kg, time 5 ~ 30s.Above-mentioned adhesive glue is liquid polyurethane adhesive glue, and the glue spraying cementing machine using Brother Industries Ltd to produce applies, and not only can decline and harden by Yin Wendu, also can react with the moisture in air, promote adhesion strength further after coating.Coating condition is upper roller work feed speed/lower work feed band work feed speed is 0.5 ~ 10m/min, bonded adhesives thickness 50 ~ 300 μm, the gap 0 ~ 2.6mm between nozzle and lower work feed band, roller pressure 15 ~ 20N, application width 6 ~ 20mm.
Beneficial effect of the present invention: suture position of the present invention is pasted with hot melt adhesive tape and/or is coated with adhesive glue, improves the flatness after the washing of clothes seam crossing.By pasting one deck ornamental tape or fabric again in the table side of seam crossing, hot melt adhesive tape and/or adhesive glue, clothes fashion can be changed, increases aesthetic feeling.By pasting one deck ribbon or fabric again in the inboard of seam crossing, hot melt adhesive tape and/or adhesive glue, the uncomfortable property brought by seam friction skin can also be eliminated.
Accompanying drawing explanation
Fig. 1 is single-layer fabric, and hot melt adhesive tape and/or adhesive glue are used for doing seam inner side.
Fig. 2 is double-layer fabric, and hot melt adhesive tape and/or adhesive glue are used for doing seam inner side.
Fig. 3 is single-layer fabric, and hot melt adhesive tape and/or adhesive glue are positioned at the table side of seam crossing, and are also pasted with one deck ornamental tape or fabric above it.
Fig. 4 is double-layer fabric, and hot melt adhesive tape and/or adhesive glue are positioned at the table side of seam crossing, and are also pasted with one deck ornamental tape or fabric above it.
Fig. 5 is single-layer fabric, and hot melt adhesive tape and/or adhesive glue are positioned at the inboard of seam crossing, and is also pasted with one deck ribbon or fabric above it.
Fig. 6 is double-layer fabric, and hot melt adhesive tape and/or adhesive glue are positioned at the inboard of seam crossing, and is also pasted with one deck ribbon or fabric above it.
Wherein in Fig. 1 ~ 6 for hot melt adhesive tape or adhesive glue; for ribbon or fabric; for ornamental tape or fabric.
Detailed description of the invention
The method of testing of each parameter of the present invention is as follows.
(1) home washings
According to GB/T8629 Textile Test home washings and drying program.
(2) wrinkling grade is made
With reference to " outward appearance is made wrinkling Pyatyi sample and is shone ".
(3) industrial washing
Use washing machine Miele, option program cotton (1 time wash time: add laundry detergents wash about 54 minutes, rinsing 16 minutes, to dry about 38 minutes), cleaning solution temperature 60 degree, revolution 1600 revs/min, washing intensity common, laundry weight 2kg, laundry detergents be industrial washing washing powder () 15g+ nine water sodium silicate 20g.
Below in conjunction with embodiment and comparative example, the invention will be further described.
Embodiment 1
Make a shirt, mainly comprise following step:
Step 1: select materials: fabric is the plain cloth that 45 polyester-cotton blend (65:35) scribbleds are formed, its thread count 110/inch × 86 piece/inch, grammes per square metre 103g/m 2, size changing rate-0.4% ×-0.1% after home washings 5 times.
Step 2: plate-making, core version, according to model cutting.
Step 3: make, press
Step 4: coating adhesive glue, stickup ribbon: apply one deck adhesive glue and paste one deck ribbon on the suture of the suture site of shirt inboard.The glue spraying cementing machine that during coating bonded adhesives, the Brother Industries Ltd that uses produces, imposes a condition as: upper roller work feed speed/lower work feed band work feed speed is respectively 2.30m/min and 2.50m/min, bonded adhesives thickness 50 μm, gap 1.3mm, roller pressure 18.5N, application width 1cm between nozzle and lower work feed band.The width using ribbon is 1cm.
Step 5: flatiron
Through the obtained clothes of above-mentioned steps after continuous home washings 5 times, allly make making wrinkling grade and all reaching more than 4 grades of position.
Embodiment 2
Make a shirt, the coating adhesive glue in embodiment 1 step 4, stickup ribbon are changed to bonding hot melt adhesive tape, paste fabric, and all the other steps are with embodiment 1.The specific practice of step 4 is:
Step 4: bonding hot melt adhesive tape, stickup fabric: press one deck hot melt adhesive tape on the suture of the suture site of shirt inboard, then paste one deck fabric on adhesive tape.Then with hot press, hot pressing laminating is carried out to this suture site.During hot pressing laminating, the condition of seamless hot press is set as: temperature 150 degree, pressure 3kg, time 15s.Use fabric identical with fabric, be first cut into the slanted bar of wide 2cm before using, then scald into the vertical bar of clear span 1cm with flatiron.
Through the obtained clothes of above-mentioned steps after continuous home washings 5 times, allly make making wrinkling grade and all reaching more than 4 grades of position.
Embodiment 3
Make gym shorts, mainly comprise following step:
Step 1: select materials: select the spandex undershirt cloth tissue fabric processed through moisture absorbing and sweat releasing process of resin and fragrance formed by 30 polyester-cotton blend spun yarns (washing 65 cottons 35), 30D spandex, its grammes per square metre 210g/m 2, the vertical close 40/inch of close 68/inch × horizontal stroke, after home washings 5 times, size changing rate be longitudinal direction-3.5% × transverse direction-3.0%.
Step 2: plate-making, core version, according to model cutting.
Step 3: make, press
Step 4: outside is pasted hot melt adhesive tape, pasted ornamental tape: the side seam line outside sport pants presses one deck hot melt adhesive tape, then paste one deck ornamental tape on adhesive tape.Then with hot press, hot pressing reinforcing is carried out to latasuture.During hot pressing laminating, the condition of seamless hot press is set as: temperature 150 degree, pressure 3kg, time 15s.
Step 5: inboard stickup hot melt adhesive tape, stickup ribbon: press one deck hot melt adhesive tape on the front and back crotch seam, pin mouth folding line of sport pants inboard, then paste one deck ribbon on adhesive tape.Then hot pressing reinforcing is carried out with hot press.When hot pressing is reinforced, the condition of seamless hot press is set as: temperature 150 degree, pressure 3kg, time 15s.
Step 6: flatiron
Through the obtained clothes of above-mentioned steps after continuous home washings 5 times, allly make making wrinkling grade and all reaching more than 4 grades of position.
Embodiment 4
Make gym shorts, the outside in embodiment 3 step 4 is pasted hot melt adhesive tape, stickup ornamental tape is changed to outside and applies adhesive glue, pastes ornamental tape; Inboard in embodiment 3 step 5 is pasted hot melt adhesive tape, stickup ribbon is changed to inboard coating adhesive glue, bond ribbon, all the other steps are with embodiment 3.Step 4 and 5 specific practice be:
Step 4: outside coating adhesive glue, stickup ornamental tape: the side seam line outside sport pants applies one deck adhesive glue and paste one deck ornamental tape.The glue spraying cementing machine that during coating bonded adhesives, the Brother Industries Ltd that uses produces, imposes a condition as: upper roller work feed speed/lower work feed band work feed speed is respectively 2.30m/min and 2.50m/min, bonded adhesives thickness 50 μm, gap 1.3mm, roller pressure 18.5N, application width 1cm between nozzle and lower work feed band.The width using ornamental tape is 1cm.
Step 5: inboard coating adhesive glue, bonding ribbon: apply one deck adhesive glue and bond one deck ribbon on the front and back crotch seam, pin mouth folding line of sport pants inboard.The glue spraying cementing machine using Brother Industries Ltd to produce during coating bonded adhesives, imposes a condition as: upper roller work feed speed/lower work feed band work feed speed is respectively 2.30m/min and 2.50m/min, bonded adhesives thickness 50 μm, gap 1.3mm, roller pressure 18.5N, application width 1cm between nozzle and lower work feed band.The width using ribbon is 1cm.
Through the obtained clothes of above-mentioned steps after continuous home washings 5 times, allly make making wrinkling grade and all reaching more than 4 grades of position.
Embodiment 5
Make gym shorts, the outside in embodiment 3 step 4 is pasted hot melt adhesive tape, the stickup ornamental tape outside be changed in embodiment 4 step 4 applies adhesive glue, pastes ornamental tape.All the other steps are with embodiment 3.
Through the obtained clothes of above-mentioned steps after continuous home washings 5 times, allly make making wrinkling grade and all reaching more than 4 grades of position.
Embodiment 6
Make gym shorts, the inboard in embodiment 3 step 5 is pasted hot melt adhesive tape, the stickup ribbon inboard be changed in embodiment 4 step 5 applies adhesive glue, bonding ribbon.All the other steps are with embodiment 3.
Through the obtained clothes of above-mentioned steps after continuous home washings 5 times, allly make making wrinkling grade and all reaching more than 4 grades of position.
Embodiment 7
Making job takes, and mainly comprises following step:
Step 1: select materials: select the 2/1 twill tissue fabric formed by 32 polyester-cotton blend spun yarns (washing 65 cottons 35), conductive filament, its grammes per square metre 260g/m 2, thread count 100/inch × 61 piece/inch, after industrial washing 5 times, size changing rate is warp-wise-2.1% × broadwise-0.9%.
Step 2: plate-making, core version, according to model cutting.
Step 3: paste hot melt adhesive tape: stitch press one deck hot melt adhesive tape respectively along shoulder seam, rear body sheet, greatly tuck inside the sleeve sheet, inner neck, sleeve gram husband, left front.Then hot pressing reinforcing is carried out with hot press.When hot pressing is reinforced, the condition of seamless hot press is set as: temperature 150 degree, pressure 3kg, time 15s.
Step 4: make: technique spells shoulder seam, latasuture, size sleeve sheet routinely, and tangent line; Technique makes sleeve, collar, sleeve gram husband routinely.
Step 5: paste hot melt adhesive tape:, cuff infirmity along sleeve, front center stitch and press one deck hot melt adhesive tape respectively.Then hot pressing reinforcing is carried out with hot press.When hot pressing is reinforced, the condition of seamless hot press is set as: temperature 150 degree, pressure 3kg, time 15s.
Step 6: make: upper sleeve, sleeve gram husband, dress left front, upper slide fastener, and tangent line.
Step 7: flatiron
Through the obtained clothes of above-mentioned steps after continuous home washings 5 times, allly make making wrinkling grade and all reaching more than 4 grades of position; After continuous industry washs 5 times, allly make making wrinkling grade and all reaching more than 3.5 grades of position.
Embodiment 8
Making job takes, and changes the stickup hot melt adhesive tape in embodiment 7 step 3 and 5 into coating adhesive glue.All the other steps are with embodiment 7.Specific practice is:
Step 3: coating adhesive glue: do each coating one deck adhesive glue of seam along shoulder seam, rear body sheet, greatly tuck inside the sleeve sheet, inner neck, sleeve gram husband, left front.The glue spraying cementing machine using Brother Industries Ltd to produce during coating bonded adhesives, imposes a condition as: upper roller work feed speed/lower work feed band work feed speed is respectively 2.30m/min and 2.50m/min, bonded adhesives thickness 50 μm, gap 1.3mm, roller pressure 18.5N, application width 1cm between nozzle and lower work feed band.
Step 5: coating adhesive glue: do each coating one deck adhesive glue of seam along infirmity, the cuff of sleeve, front center.The glue spraying cementing machine using Brother Industries Ltd to produce during coating bonded adhesives, imposes a condition as: upper roller work feed speed/lower work feed band work feed speed is respectively 2.30m/min and 2.50m/min, bonded adhesives thickness 50 μm, gap 1.3mm, roller pressure 18.5N, application width 1cm between nozzle and lower work feed band.
Through the obtained clothes of above-mentioned steps after continuous home washings 5 times, allly make making wrinkling grade and all reaching more than 4 grades of position; After continuous industry washs 5 times, allly make making wrinkling grade and all reaching more than 3.5 grades of position.
Embodiment 9
Making job takes, and the stickup hot melt adhesive tape in embodiment 7 step 3 is changed into the coating adhesive glue in embodiment 8 step 3.All the other steps are with embodiment 7.
Through the obtained clothes of above-mentioned steps after continuous home washings 5 times, allly make making wrinkling grade and all reaching more than 4 grades of position; After continuous industry washs 5 times, allly make making wrinkling grade and all reaching more than 3.5 grades of position.
Embodiment 10
Making job takes, and the stickup hot melt adhesive tape in embodiment 7 step 5 is changed into the coating adhesive glue in embodiment 8 step 5.All the other steps are with embodiment 7.
Through the obtained clothes of above-mentioned steps after continuous home washings 5 times, allly make making wrinkling grade and all reaching more than 4 grades of position; After continuous industry washs 5 times, allly make making wrinkling grade and all reaching more than 3.5 grades of position.
Comparative example 1
Make a shirt, mainly comprise following step:
Step 1: select materials: fabric is the plain cloth that 45 polyester-cotton blend (35:65) scribbleds are formed, its thread count 110/inch × 86 piece/inch, grammes per square metre 103g/m 2, size changing rate-0.4% ×-0.1% after home washings 5 times.
Step 2: plate-making, core version, according to model cutting.
Step 3: make, press
Through the obtained clothes of above-mentioned steps after continuous home washings 5 times, the wrinkling grade of making of making position is 3 grades.
Comparative example 2
Making job takes, and mainly comprises following step:
Step 1: select materials: fabric is 2/1 twill that 32 polyester cotton blended yarns (washing 65 cottons 35) and conductive filament are formed, its grammes per square metre 260g/m 2, thread count 100/inch × 61 piece/inch, size changing rate is warp-wise-2.1% × broadwise-0.9% after industrial washing 5 times.
Step 2: plate-making, core version, according to model cutting.
Step 3: make, whole scald.
Through the obtained work clothes of above-mentioned steps after continuous industry washs 5 times, the wrinkling grade of making of making position is 2.5 grades.

Claims (9)

1. a clothes, it is characterized in that: this clothes has at least a place to employ suture, the seam crossing at described suture position is single or multiple lift fabric and making wrinkling grade and still can reach more than 3.5 grades by seam crossing after GB/T8629 5A program home washings 5 times.
2. clothes according to claim 1, is characterized in that: described suture position is pasted with hot melt adhesive tape and/or is coated with adhesive glue.
3. clothes according to claim 2, is characterized in that: described hot melt adhesive tape and/or adhesive glue are positioned at the table side of described seam crossing, and are also pasted with one deck ornamental tape or fabric above it.
4. clothes according to claim 2, is characterized in that: described hot melt adhesive tape and/or adhesive glue are positioned at the inboard of described seam crossing, and are also pasted with one deck ribbon or fabric above it.
5. the clothes according to claim 1,2,3 or 4, is characterized in that: the fabric of this clothes, hot melt adhesive tape, adhesive glue, ornamental tape or ribbon have antibacterial deodourizing and/or fragrance.
6. a production method for clothes according to claim 1, comprises plate-making, cutting, makes, presses, it is characterized in that: when making, at least one place uses suture, and the seam crossing at suture position is single or multiple lift fabric.
7. the production method of clothes according to claim 6, is characterized in that: the seam crossing of suture first paste hot melt adhesive tape or/and coating adhesive glue, then suture, flatiron; Or first suture, flatiron, then paste hot melt adhesive tape or/and coating adhesive glue at the seam crossing of suture.
8. the production method of clothes according to claim 7, is characterized in that: described hot melt adhesive tape or/and adhesive glue is used in the table side of seam crossing, and pastes one deck ornamental tape or fabric in the above again.
9. the production method of clothes according to claim 7, is characterized in that: described hot melt adhesive tape or/and adhesive glue is used in the inboard of seam crossing, and pastes one deck ribbon or fabric in the above again.
CN201310406276.5A 2013-09-09 2013-09-09 Clothes and production method thereof Pending CN104413823A (en)