CN104085008A - 一种防霉竹子软化剂及其制备方法 - Google Patents

一种防霉竹子软化剂及其制备方法 Download PDF

Info

Publication number
CN104085008A
CN104085008A CN201410252911.3A CN201410252911A CN104085008A CN 104085008 A CN104085008 A CN 104085008A CN 201410252911 A CN201410252911 A CN 201410252911A CN 104085008 A CN104085008 A CN 104085008A
Authority
CN
China
Prior art keywords
mildew
softening
softener
add
resistant bamboo
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201410252911.3A
Other languages
English (en)
Inventor
王文忠
王东营
杨子成
王东宝
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
ANHUI HUAYU CRAFTS GROUP Co Ltd
Original Assignee
ANHUI HUAYU CRAFTS GROUP Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by ANHUI HUAYU CRAFTS GROUP Co Ltd filed Critical ANHUI HUAYU CRAFTS GROUP Co Ltd
Priority to CN201410252911.3A priority Critical patent/CN104085008A/zh
Publication of CN104085008A publication Critical patent/CN104085008A/zh
Pending legal-status Critical Current

Abstract

一种防霉竹子软化剂,由下列重量份的原料制成:氢氧化钠10-12、柠檬酸铵3-4、正辛醇12-14、聚乙二醇辛基苯基醚2-3、栀子5-10、苦参5-10、蛇床子5-10、薄荷3-4、聚维酮碘6-8、助剂3-4、水100。本发明使用了氢氧化钠和聚乙二醇辛基苯基醚,软化速度快,软化均匀;通过使用正辛醇,使茎条表面光滑,能提高编织效率;通过使用苦参等中草药及聚维酮碘,能防止霉变虫蛀。本发明适用于竹子软化,软化周期明显缩短。

Description

一种防霉竹子软化剂及其制备方法
技术领域
本发明涉及软化剂领域,尤其涉及一种防霉竹子软化剂及其制备方法。
背景技术
    使用植物的茎条编织成各种日常用品已经有很多年的历史了,随着人们生活水平的提高,这种编织物很多成为了艺术品,造型越来奇特复杂。在编制过程中由于茎条较硬,难以编织,需要软化,目前软化主要是传统的方法如浸泡、闷等方法,不仅耗时而且时常达不到很好的效果,需要进一步研究新的软化剂,不仅软化效果好、速度快、又能对茎条损伤小,最好能其保护作用以延长使用寿命。
发明内容
本发明的目的在于提供一种防霉竹子软化剂及其制备方法,该软化剂具有软化速度快、光滑、防霉的特点。
本发明的技术方案如下:
一种防霉竹子软化剂,其特征在于由下列重量份的原料制成:氢氧化钠10-12、柠檬酸铵3-4、正辛醇12-14、聚乙二醇辛基苯基醚2-3、栀子5-10、苦参5-10、蛇床子5-10、薄荷3-4、聚维酮碘6-8、助剂3-4、水100。所述的助剂由下列重量份的原料制成:松节油3-4、三聚氰胺甲醛树脂3-4、环烷酸钴1-2、渗透剂JFC1-2、松香4-5、月桂酸钠2-3、乙醇12-14,制备方法是将松香加入乙醇中,加热至60-70℃,再加入环烷酸钴,搅拌10-15分钟,再加入其它剩余成分,在1200-1500转/分下高速分散,冷却,即得。
所述防霉竹子软化剂的制备方法,其特征在于包括以下步骤:将栀子、苦参、蛇床子、薄荷加水煎煮,过滤得药浆,加入其他剩余成分混合搅拌,即得。
本发明的有益效果
本发明使用了氢氧化钠和聚乙二醇辛基苯基醚,软化速度快,软化均匀;通过使用正辛醇,使茎条表面光滑,能提高编织效率;通过使用苦参等中草药及聚维酮碘,能防止霉变虫蛀。本发明适用于竹子软化,软化周期明显缩短。
具体实施方式
一种防霉竹子软化剂,由下列重量份(公斤)的原料制成:氢氧化钠11、柠檬酸铵3.5、正辛醇13、聚乙二醇辛基苯基醚2.5、栀子7、苦参7、蛇床子8、薄荷3.5、聚维酮碘7、助剂3.5、水100。所述的助剂由下列重量份(公斤)的原料制成:松节油3、三聚氰胺甲醛树脂3、环烷酸钴1、渗透剂JFC1、松香4、月桂酸钠2、乙醇14,制备方法是将松香加入乙醇中,加热至60-70℃,再加入环烷酸钴,搅拌10-15分钟,再加入其它剩余成分,在1200-1500转/分下高速分散,冷却,即得。
所述防霉竹子软化剂的制备方法,包括以下步骤:将栀子、苦参、蛇床子、薄荷加水煎煮,过滤得药浆,加入其他剩余成分混合搅拌,即得。
使用该实施例的软化剂浸泡竹条,比普通软化剂浸泡的竹条编织速度提高了3%,折断现象减少了4%,表面光亮,放置30天不发霉,不蛀虫。

Claims (2)

1.一种防霉竹子软化剂,其特征在于由下列重量份的原料制成:氢氧化钠10-12、柠檬酸铵3-4、正辛醇12-14、聚乙二醇辛基苯基醚2-3、栀子5-10、苦参5-10、蛇床子5-10、薄荷3-4、聚维酮碘6-8、助剂3-4、水100;所述的助剂由下列重量份的原料制成:松节油3-4、三聚氰胺甲醛树脂3-4、环烷酸钴1-2、渗透剂JFC1-2、松香4-5、月桂酸钠2-3、乙醇12-14,制备方法是将松香加入乙醇中,加热至60-70℃,再加入环烷酸钴,搅拌10-15分钟,再加入其它剩余成分,在1200-1500转/分下高速分散,冷却,即得。
2.根据权利要求1所述防霉竹子软化剂的制备方法,其特征在于包括以下步骤:将栀子、苦参、蛇床子、薄荷加水煎煮,过滤得药浆,加入其他剩余成分混合搅拌,即得。
CN201410252911.3A 2014-06-10 2014-06-10 一种防霉竹子软化剂及其制备方法 Pending CN104085008A (zh)