CN104036693B - A kind of preparation method of baking vanish silk-screen Sign Board - Google Patents

A kind of preparation method of baking vanish silk-screen Sign Board Download PDF

Info

Publication number
CN104036693B
CN104036693B CN201410174028.7A CN201410174028A CN104036693B CN 104036693 B CN104036693 B CN 104036693B CN 201410174028 A CN201410174028 A CN 201410174028A CN 104036693 B CN104036693 B CN 104036693B
Authority
CN
China
Prior art keywords
screen frame
picture
text
screen
cloth
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Active
Application number
CN201410174028.7A
Other languages
Chinese (zh)
Other versions
CN104036693A (en
Inventor
张建新
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
ANHUI STARLIGHT LOGO SYSTEMS CO., LTD.
Original Assignee
张建新
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by 张建新 filed Critical 张建新
Priority to CN201410174028.7A priority Critical patent/CN104036693B/en
Publication of CN104036693A publication Critical patent/CN104036693A/en
Application granted granted Critical
Publication of CN104036693B publication Critical patent/CN104036693B/en
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

The invention discloses a kind of preparation method of baking vanish silk-screen Sign Board, taking acryl plates as substrate, complete by substrate procedure of processing, picture and text plate-making procedure of processing and serigraphy step. Beneficial effect of the present invention: use the preparation method of this baking vanish silk-screen Sign Board, step is simple, easy to operate. The label picture and text made are clear, eye-catching, flatness is good, and decorative effect is good, can meet the advantages such as the instructions for use of different places.

Description

A kind of preparation method of baking vanish silk-screen Sign Board
Technical field
The present invention relates to the making field of roasting Sign Board, especially relate to the preparation method of baking vanish silk-screen Sign Board.
Background technology
At present, label is mainly the effect that shows it by vision, has the function of symbol, directionality, hint etc. Along with the demand of social construction, label manufacturing industry will have the status of oneself. The identification label more label of scale has met all demands of the high-tech modern automation society of today substantially. The preparation method of present baking vanish silk-screen Sign Board of today: exist base-plate cleaning surface residue many, baking vanish face coat variable thickness, top-coat paint film should smoothly be prone to current mark, wrinkle, tangerine peel, bubble, be mingled with etc. affects the defect of decorative effect. And screen printing pattern has distortion and presents the defects such as sawtooth.
Summary of the invention
The object of this invention is to provide a kind of preparation method of baking vanish silk-screen Sign Board, solve the making problem of low quality of existing baking vanish silk-screen Sign Board.
The technical solution adopted for the present invention to solve the technical problems is: a kind of preparation method of baking vanish silk-screen Sign Board, complete by substrate procedure of processing, picture and text plate-making procedure of processing and serigraphy step, and specifically comprise the following steps:
Described substrate procedure of processing comprises
The first step: material is prepared: spray gun, air pump, dust removing cloth, sand paper, material to be sprayed and substrate, paint, curing agent, diluent, baking box, sanitary cup, engineer's scale, screen pack, clean cloth;
Second step: clean: check that substrate surface is whether totally clean, substrate surface spot, oil stain, wax stain are washed away with cleaning fluid;
The 3rd step: polishing: be placed in water surface of the work is polished flat with sand paper more than 300 orders, be put on grill air-dry stand-byly, be polished to smooth seamlessly, hand is touched smooth, without any uneven;
The 4th step: rust cleaning: with dimethylbenzene, surface of the work is washed to rust, the workpiece of serious rust stain need first be polished and be cleaned; 2 refine polishing;
The 5th step: oil removing: wipe on substrate surface with cleaning cloth adhesional wetting degreaser and also dry with cleaning cloth at once;
The 6th step: spraying priming paint: according to 4:1:2 capacity ratio, spray dried for standby behind 2 to 3 roads with epoxy primer, epoxy primer curing agent, epoxy primer diluent;
The 7th step: scrape ash: ash is scraped in surface of the work out-of-flatness, crackled place, parch more than rear use 800 orders sand paper Deng atomized ash and be placed in water surface of the work is polished flat, be put on grill air-dry stand-byly, be polished to smooth seamless, hand is touched smooth, without any uneven sense;
The 8th step: polishing: the workpiece of scraping after ash is polished, first dry grinding, then machine mill, then water mill, then fine grinding;
The 9th step: micro-filling out: with filling out eye ash, micro-pinprick, sand paper trace and scratch filled out, dry grinds after filling up again;
The tenth step: need oil removing and dedusting according to spraying;
The 11 step: middle painting: with the spraying 2-3 time that primes in 2 grams, every all over being separated by 5-10 minutes; With the spraying 2-3 time that primes in 1 gram, between every time, leave standstill 3-5 minute;
The 12 step: face is coated with: pure color finish paint, paint adds curing agent: diluent=2:1:0.5-0.8, one pack system is 1K paint, aluminium paint, diluent=1:1, minute surface varnish will be made in aluminium paint surface, varnish: curing agent: diluent=2:1:0.5-0.8, behind spraying 2 to 3 roads, is separated by 10-15 minutes for every layer;
The 13 step: the product after spraying, should put between drying and leave standstill 2 hours, wait for that putting into baking box after surface dry toasts again, and dries through 45 minutes in the baking box of 60 DEG C;
The 14 step: waxing: the surface of the work of liniment wax is carried out to polishing grinding with sander, make last protective layer;
The 15 step: sprayed after paint at every turn, washed and spray rifle head with dimethylbenzene, must soak rifle head with dimethylbenzene on time, in order to avoid consent, in painting process, the first rear spray of spray light color is dark;
Described picture and text plate-making procedure of processing comprises
The first step, preparation: screen cloth, screen frame, nail net air gun, rifle nail, draws in the net to clamp hair-dryer, warm-air drier, photoresists, sponge, cut-off knife, scissors, film or template, printer;
Second step: select the screen frame of corresponding size according to the size of institute's impression literary composition, should notice that screen frame can not be out of shape while selecting frame, framework surrounding is smooth, framework is made firmly, if wooden frame should discharge water in advance, middle immersion re-uses after waiting after 24 hours and drying;
The 3rd step: network selection cloth, according to picture and text size and measure of precision network selection cloth, the meticulous 10mm of picture and text selects import 400 object screen cloths with planted agent;
The 4th step: screen cloth is chosen the rear screen cloth that is greater than screen frame 100mm of determining according to screen frame size;
The 5th step: air nail is put into air gun, connect the logical upper gas of air pump;
The 6th step: cover while net and should note the silking of screen cloth to become with one side of screen frame 15 to spend, first screen cloth is fixed on screen frame on one side, then fixes the screen frame of opposite side, first with drawing in the net to clamp, screen cloth is strained at when opposite side is fixing, then just nail gun is followed closely, and so way is fixed other both sides;
The 7th step: by the screen frame of fixing, should first wash away floating dust above with clear water, then dry up;
The 8th step: screen frame frictioning, when frictioning, to scrape on the two sides of screen frame, and will scrape evenly totally, glue is scraped afterwards and is dried up with hair-dryer, dryer or warm-air drier, and attention will make whole screen frame uniform drying, can not occur that some place does some local half-dried situation;
The 9th step: start to carry out layout work below: first by by the template of impression literary composition, design sketch takes out and checks, observe whether both are unified errorless, whether there are the picture and text on template to occur empty printing, should be coated with in fact at template reverse side with thin marking pen if having, whether have wrinkle phenomenon, confirm errorless after, according to drawing, the picture and text template of different colours is cut off with scissors, what picture and text size was little directly can printing down, and the template that picture and text are large should be divided on glass table and splice by design sketch;
The tenth step: the template of having spelled is ajusted, and word reverse side upward, is put on printer table top, presses screen frame, covers top cover;
The 11 step: the screen frame having shone is placed on to clear water the inside and rinses, screen frame picture and text place is rinsed with special high-pressure hydraulic giant, and washed by hand the place of being shone;
The 12 step, the screen frame surface of rinsing well is dried up or natural air drying after be put into warm-air drier fore blow to bone dry, after bone dry, screen frame is picked up facing to visible light and had or not the phenomenon of slipping through the net, if the phenomenon of slipping through the net, should be stained with photoresists with toothpick and carry out net mending, floating with hand, dry up rear use, bright in vain if picture and text do not rinse completely, application clean cloth or sponge are stained with a little diluent and carry out wiping, until picture and text are wiped brightly in vain completely;
Described serigraphy step comprises:
The first step: preparation, ink, container, splash bar, quick dry agent, drying retardant, sleaker, smears word water, clean cloth, sponge, non-wrinkle newspaper, the smooth operating table surface of having fixed screen frame folder, platen;
Second step: allotment ink, according to CMYK colour, the ink of different colours is blended in proportion, stirs, is configured, quantity of ink number be according to the demand of institute's impression literary composition from large Packaging Bottle fall some in sanitary cup;
The 3rd step: after color is chosen or mixed up, inking up diluent, in container, marginally add on a small quantity, adds diluent while stirs ink, should leave standstill 60 minutes and come into operation after being stirred;
The 4th step: screen frame is fixed on fixed network device, before printing, first substrate surface is carried out to dedusting clean, again operation the substrate that will print is put on platen picture and text on screen frame under, adjust to a position accurately facing to online picture and text, surrounding at plate is made mark with pencil or double faced adhesive tape, completes location work;
The 5th step: after location, before printing, also to first try China ink, a little ink is stained with and is dripped to picture and text vicinity on screen frame with splash bar, ink is applied on picture and text lightly with sleaker, examination China ink is to be placed on below picture and text with newspaper pad, then the even scrubbing brush China ink of exerting oneself, the angle of sleaker should be 45 degree of parallel angle;
The 6th step: after substrate that a collection of ink colors is identical is printed, remaining ink in cup should be sealed and mouthful sealed up for safekeeping with adhesive tape, and write the title of beginning a project for future use on cup;
The 7th step: plate good silk-screen being put into from down to up and being dried on rack, push in baking box and toast, is to become finished product in 80 DEG C of baking boxs after baking in 30 minutes in temperature;
The 8th step: the screen frame after silk-screen is put into and washed plate intermixture pond and soak after 12 hours and carry out deinking and degumming, rinse, dry again and use.
Beneficial effect of the present invention: use the preparation method of this baking vanish silk-screen Sign Board, step is simple, easy to operate. The label picture and text made are clear, eye-catching, flatness is good, and decorative effect is good, can meet the advantages such as the instructions for use of different places.
Below with reference to embodiment, the present invention is described in detail.
Detailed description of the invention
Embodiment,
A preparation method for baking vanish silk-screen Sign Board, completes by substrate procedure of processing, picture and text plate-making procedure of processing and serigraphy step, specifically comprises the following steps:
Described substrate procedure of processing comprises
The first step: material is prepared: spray gun, air pump, dust removing cloth, sand paper, material to be sprayed and substrate, paint, curing agent, diluent, baking box, sanitary cup, engineer's scale, screen pack, clean cloth;
Second step: clean: check that substrate surface is whether totally clean, substrate surface spot, oil stain, wax stain are washed away with cleaning fluid;
The 3rd step: polishing: be placed in water surface of the work is polished flat with sand paper more than 300 orders, be put on grill air-dry stand-byly, be polished to smooth seamlessly, hand is touched smooth, without any uneven;
The 4th step: rust cleaning: with dimethylbenzene, surface of the work is washed to rust, the workpiece of serious rust stain need first be polished and be cleaned; 2 refine polishing;
The 5th step: oil removing: wipe on substrate surface with cleaning cloth adhesional wetting degreaser and also dry with cleaning cloth at once;
The 6th step: spraying priming paint: according to 4:1:2 capacity ratio, spray dried for standby behind 2 to 3 roads with epoxy primer, epoxy primer curing agent, epoxy primer diluent;
The 7th step: scrape ash: ash is scraped in surface of the work out-of-flatness, crackled place, parch more than rear use 800 orders sand paper Deng atomized ash and be placed in water surface of the work is polished flat, be put on grill air-dry stand-byly, be polished to smooth seamless, hand is touched smooth, without any uneven sense;
The 8th step: polishing: the workpiece of scraping after ash is polished, first dry grinding, then machine mill, then water mill, then fine grinding;
The 9th step: micro-filling out: with filling out eye ash, micro-pinprick, sand paper trace and scratch filled out, dry grinds after filling up again;
The tenth step: need oil removing and dedusting according to spraying;
The 11 step: middle painting: with the spraying 2-3 time that primes in 2 grams, every all over being separated by 5-10 minutes; With the spraying 2-3 time that primes in 1 gram, between every time, leave standstill 3-5 minute;
The 12 step: face is coated with: pure color finish paint, paint adds curing agent: diluent=2:1:0.5-0.8, one pack system is 1K paint, aluminium paint, diluent=1:1, minute surface varnish will be made in aluminium paint surface, varnish: curing agent: diluent=2:1:0.5-0.8, behind spraying 2 to 3 roads, is separated by 10-15 minutes for every layer;
The 13 step: the product after spraying, should put between drying and leave standstill 2 hours, wait for that putting into baking box after surface dry toasts again, and dries through 45 minutes in the baking box of 60 DEG C;
The 14 step: waxing: the surface of the work of liniment wax is carried out to polishing grinding with sander, make last protective layer;
The 15 step: sprayed after paint at every turn, washed and spray rifle head with dimethylbenzene, must soak rifle head with dimethylbenzene on time, in order to avoid consent, in painting process, the first rear spray of spray light color is dark;
Described picture and text plate-making procedure of processing comprises
The first step, preparation: screen cloth, screen frame, nail net air gun, rifle nail, draws in the net to clamp hair-dryer, warm-air drier, photoresists, sponge, cut-off knife, scissors, film or template, printer;
Second step: select the screen frame of corresponding size according to the size of institute's impression literary composition, should notice that screen frame can not be out of shape while selecting frame, framework surrounding is smooth, framework is made firmly, if wooden frame should discharge water in advance, middle immersion re-uses after waiting after 24 hours and drying;
The 3rd step: network selection cloth, according to picture and text size and measure of precision network selection cloth, the meticulous 10mm of picture and text selects import 400 object screen cloths with planted agent;
The 4th step: screen cloth is chosen the rear screen cloth that is greater than screen frame 100mm of determining according to screen frame size;
The 5th step: air nail is put into air gun, connect the logical upper gas of air pump;
The 6th step: cover while net and should note the silking of screen cloth to become with one side of screen frame 15 to spend, first screen cloth is fixed on screen frame on one side, then fixes the screen frame of opposite side, first with drawing in the net to clamp, screen cloth is strained at when opposite side is fixing, then just nail gun is followed closely, and so way is fixed other both sides;
The 7th step: by the screen frame of fixing, should first wash away floating dust above with clear water, then dry up;
The 8th step: screen frame frictioning, when frictioning, to scrape on the two sides of screen frame, and will scrape evenly totally, glue is scraped afterwards and is dried up with hair-dryer, dryer or warm-air drier, and attention will make whole screen frame uniform drying, can not occur that some place does some local half-dried situation;
The 9th step: start to carry out layout work below: first by by the template of impression literary composition, design sketch takes out and checks, observe whether both are unified errorless, whether there are the picture and text on template to occur empty printing, should be coated with in fact at template reverse side with thin marking pen if having, whether have wrinkle phenomenon, confirm errorless after, according to drawing, the picture and text template of different colours is cut off with scissors, what picture and text size was little directly can printing down, and the template that picture and text are large should be divided on glass table and splice by design sketch;
The tenth step: the template of having spelled is ajusted, and word reverse side upward, is put on printer table top, presses screen frame, covers top cover;
The 11 step: the screen frame having shone is placed on to clear water the inside and rinses, screen frame picture and text place is rinsed with special high-pressure hydraulic giant, and washed by hand the place of being shone;
The 12 step, the screen frame surface of rinsing well is dried up or natural air drying after be put into warm-air drier fore blow to bone dry, after bone dry, screen frame is picked up facing to visible light and had or not the phenomenon of slipping through the net, if the phenomenon of slipping through the net, should be stained with photoresists with toothpick and carry out net mending, floating with hand, dry up rear use, bright in vain if picture and text do not rinse completely, application clean cloth or sponge are stained with a little diluent and carry out wiping, until picture and text are wiped brightly in vain completely;
Described serigraphy step comprises:
The first step: preparation, ink, container, splash bar, quick dry agent, drying retardant, sleaker, smears word water, clean cloth, sponge, non-wrinkle newspaper, the smooth operating table surface of having fixed screen frame folder, platen;
Second step: allotment ink, according to CMYK colour, the ink of different colours is blended in proportion, stirs, is configured, quantity of ink number be according to the demand of institute's impression literary composition from large Packaging Bottle fall some in sanitary cup;
The 3rd step: after color is chosen or mixed up, inking up diluent, in container, marginally add on a small quantity, adds diluent while stirs ink, should leave standstill 60 minutes and come into operation after being stirred;
The 4th step: screen frame is fixed on fixed network device, before printing, first substrate surface is carried out to dedusting clean, again operation the substrate that will print is put on platen picture and text on screen frame under, adjust to a position accurately facing to online picture and text, surrounding at plate is made mark with pencil or double faced adhesive tape, completes location work;
The 5th step: after location, before printing, also to first try China ink, a little ink is stained with and is dripped to picture and text vicinity on screen frame with splash bar, ink is applied on picture and text lightly with sleaker, examination China ink is to be placed on below picture and text with newspaper pad, then the even scrubbing brush China ink of exerting oneself, the angle of sleaker should be 45 degree of parallel angle;
The 6th step: after substrate that a collection of ink colors is identical is printed, remaining ink in cup should be sealed and mouthful sealed up for safekeeping with adhesive tape, and write the title of beginning a project for future use on cup;
The 7th step: plate good silk-screen being put into from down to up and being dried on rack, push in baking box and toast, is to become finished product in 80 DEG C of baking boxs after baking in 30 minutes in temperature;
The 8th step: the screen frame after silk-screen is put into and washed plate intermixture pond and soak after 12 hours and carry out deinking and degumming, rinse, dry again and use.
Above embodiment is described the preferred embodiment of the present invention; not scope of the present invention is limited; design under the prerequisite of spirit not departing from the present invention; various distortion and improvement that the common engineers and technicians in this area make technical scheme of the present invention, all should fall in the definite protection domain of claims of the present invention.
The part that the present invention does not relate to all prior art that maybe can adopt same as the prior art is realized.

Claims (1)

1. a preparation method for baking vanish silk-screen Sign Board, completes by substrate procedure of processing, picture and text plate-making procedure of processing and serigraphy step, specifically comprises the following steps:
Described substrate procedure of processing comprises
The first step, material are prepared: spray gun, air pump, dust removing cloth, sand paper, material to be sprayed and substrate, paint, curing agent, diluent, baking box, sanitary cup, engineer's scale, screen pack, cleaning cloth;
Second step, cleaning: check that substrate surface is whether totally clean, substrate surface spot is washed away with cleaning fluid;
The 3rd step, polishing: be placed in water surface of the work is polished flat with sand paper more than 300 orders, be put on grill air-dry stand-byly, be polished to smooth seamlessly, hand is touched smooth, without any uneven;
The 4th step, rust cleaning: with dimethylbenzene, surface of the work is washed to rust, the workpiece of serious rust stain need first be polished and be cleaned; 2 refine polishing;
The 5th step, oil removing: wipe on substrate surface with cleaning cloth adhesional wetting degreaser and also dry with cleaning cloth at once;
The 6th step, spraying priming paint: according to 4:1:2 capacity ratio, spray dried for standby behind 2 to 3 roads with epoxy primer, epoxy primer curing agent, epoxy primer diluent;
The 7th step, scrape ash: ash is scraped in surface of the work out-of-flatness, crackled place, parch more than rear use 800 orders sand paper Deng atomized ash and be placed in water surface of the work is polished flat, be put on grill air-dry stand-byly, be polished to smooth seamless, hand is touched smooth, without any uneven sense;
The 8th step, polishing: the workpiece of scraping after ash is polished, first dry grinding, then machine mill, then water mill, then fine grinding;
The 9th step, micro-filling out: with filling out eye ash, micro-pinprick, sand paper trace and scratch filled out, dry grinds after filling up again;
The tenth step, oil removing and dedusting;
The 11 step, middle painting: with the spraying 2 to 3 times of priming in 2K, every all over being separated by 5 to 10 minutes; With the spraying 2 to 3 times of priming in 1K, between every time, leave standstill 3 to 5 minutes again;
The 12 step, face are coated with: with pure color finish paint, paint and add curing agent, diluent according to 2:1:0.5-0.8 capacity ratio, with aluminium paint, diluent according to 1:1 capacity ratio, minute surface varnish is made on aluminium paint surface, with varnish, curing agent, diluent according to 2:1:0.5-0.8 capacity ratio, behind spraying 2 to 3 roads, per pass is separated by 10-15 minutes;
Product after the 13 step, spraying, should put between drying and leave standstill 2 hours, waits for that putting into baking box after surface dry toasts again, and dries through 45 minutes in the baking box of 60 DEG C;
The 14 step, waxing: the surface of the work of liniment wax is carried out to polishing grinding with sander, make last protective layer;
The 15 step, sprayed after paint at every turn, soaked rifle head with dimethylbenzene, in order to avoid consent, in painting process, first spray is dark after spray light color;
Described picture and text plate-making procedure of processing comprises
The first step, preparation: screen cloth, screen frame, nail net air gun, rifle nail, draws in the net to clamp hair-dryer, warm-air drier, photoresists, sponge, cut-off knife, scissors, template, printer;
Second step, select the screen frame of corresponding size according to the size of institute's impression literary composition, should notice that screen frame can not be out of shape while selecting frame, framework surrounding is smooth, and framework is made firmly, if wooden frame should discharge water in advance, middle immersion re-uses after waiting after 24 hours and drying;
The 3rd step, network selection cloth, according to picture and text size and measure of precision network selection cloth, the meticulous 10mm of picture and text selects import 400 object screen cloths with planted agent;
The 4th step, screen cloth are chosen the rear screen cloth that is greater than screen frame 100mm of determining according to screen frame size;
The 5th step, air nail is put into air gun, connect the logical upper gas of air pump;
When the 6th step, illiteracy are netted, should note the silking of screen cloth to become with one side of screen frame 15 degree, first screen cloth is fixed on screen frame on one side, then fix the screen frame of opposite side, when opposite side is fixed, first with drawing in the net to clamp, screen cloth be strained at, then nail gun nail, so way is fixed other both sides;
The 7th step, by the screen frame of fixing, first wash away floating dust above with clear water, then dry up;
The 8th step, screen frame frictioning: when frictioning, will scrape on the two sides of screen frame, and will scrape evenly totally, glue is scraped afterwards and dried up with hair-dryer, dryer or warm-air drier, and attention will make whole screen frame uniform drying, can not occur that some place does some local half-dried situation;
The 9th step, start to carry out layout work below: first will be taken out and check by the template of impression literary composition, design sketch, observe both and whether unify errorlessly, whether have the picture and text on template to occur empty printing, if useful thin marking pen is coated with reality at template reverse side; Whether have wrinkle phenomenon, confirm errorless after, according to drawing, the picture and text template of different colours is cut off with scissors, what picture and text size was little directly can printing down, the template that picture and text are large should be divided on glass table and splice by design sketch;
The tenth step, the template of having spelled is ajusted, word reverse side upward, is put on printer table top, presses screen frame, covers top cover;
The 11 step, the screen frame having shone is placed on to clear water the inside rinses, screen frame picture and text place is rinsed with special high-pressure hydraulic giant, and washed by hand the place of being shone;
The 12 step, the screen frame surface of rinsing well is dried up or natural air drying after be put into warm-air drier fore blow to bone dry, after bone dry, screen frame is picked up facing to visible light and had or not the phenomenon of slipping through the net, if the phenomenon of slipping through the net, is stained with photoresists with toothpick and carries out net mending, floating with hand, dry up rear use, if it is bright in vain that picture and text do not rinse completely, application clean cloth or sponge are stained with a little diluent and carry out wiping, until picture and text are wiped brightly in vain completely;
Described serigraphy step comprises:
The first step, preparation: ink, container, splash bar, quick dry agent, drying retardant, sleaker, smears word water, clean cloth, sponge, non-wrinkle newspaper, the smooth operating table surface of having fixed screen frame folder, platen;
Second step, allotment ink: according to CMYK colour, the ink of different colours is blended in proportion, stirs, is configured, quantity of ink number be according to the demand of institute's impression literary composition from large Packaging Bottle fall some in sanitary cup;
The 3rd step, color is chosen or is mixed up after, inking up diluent, in cup, marginally add on a small quantity, adds diluent while stirs ink, is stirred rear leaving standstill and comes into operation for 60 minutes again;
The 4th step, screen frame is fixed on fixed network device, before printing, first substrate surface is carried out to dedusting clean, again operation the substrate that will print is put on platen picture and text on screen frame under, adjust to a position accurately facing to the picture and text on screen frame, surrounding at plate is made mark with pencil or double faced adhesive tape, completes location work;
Before printing after the 5th step, location, also to first try China ink, a little ink is stained with and is dripped to picture and text vicinity on screen frame with splash bar, ink is applied on picture and text lightly with sleaker, examination China ink is to be placed on below picture and text with newspaper pad, then the even scrubbing brush China ink of exerting oneself, the angle of sleaker should be 45 degree of parallel angle;
After the 6th step, the substrate that a collection of ink colors is identical are printed, remaining ink in cup should be sealed and mouthful sealed up for safekeeping with adhesive tape, and on cup, write the title of beginning a project for future use;
The 7th step, plate good silk-screen being put into from down to up and being dried on rack, push in baking box and toast, is after baking in 30 minutes, to become finished product in 80 DEG C of baking boxs in temperature;
The 8th step, the screen frame after silk-screen is put into and washed plate intermixture pond and soak after 12 hours and carry out deinking and degumming, rinse, dry again and use.
CN201410174028.7A 2014-04-28 2014-04-28 A kind of preparation method of baking vanish silk-screen Sign Board Active CN104036693B (en)