ito
laser
silver slurry
induced thermal
touch screen
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201410077026.6A
Other languages
English (en)
Inventor
许国武
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
JIANGXI TIANYI PHOTOELECTRIC Co Ltd
Original Assignee
JIANGXI TIANYI PHOTOELECTRIC Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by JIANGXI TIANYI PHOTOELECTRIC Co Ltd filed Critical JIANGXI TIANYI PHOTOELECTRIC Co Ltd
Priority to CN201410077026.6A priority Critical patent/CN103846555A/zh
Publication of CN103846555A publication Critical patent/CN103846555A/zh
Pending legal-status Critical Current

Links

Classifications

    • BPERFORMING OPERATIONS; TRANSPORTING
    • B23MACHINE TOOLS; METAL-WORKING NOT OTHERWISE PROVIDED FOR
    • B23KSOLDERING OR UNSOLDERING; WELDING; CLADDING OR PLATING BY SOLDERING OR WELDING; CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING; WORKING BY LASER BEAM
    • B23K26/00Working by laser beam, e.g. welding, cutting or boring
    • B23K26/36Removing material
    • B23K26/361Removing material for deburring or mechanical trimming
    • BPERFORMING OPERATIONS; TRANSPORTING
    • B23MACHINE TOOLS; METAL-WORKING NOT OTHERWISE PROVIDED FOR
    • B23KSOLDERING OR UNSOLDERING; WELDING; CLADDING OR PLATING BY SOLDERING OR WELDING; CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING; WORKING BY LASER BEAM
    • B23K26/00Working by laser beam, e.g. welding, cutting or boring
    • B23K26/60Preliminary treatment

Landscapes

  • Engineering & Computer Science (AREA)
  • Physics & Mathematics (AREA)
  • Optics & Photonics (AREA)
  • Plasma & Fusion (AREA)
  • Mechanical Engineering (AREA)
  • Manufacturing Of Printed Circuit Boards (AREA)

Abstract

一种电容触摸屏激光蚀刻工艺,首先把ITOfilm上的耐酸油墨图案印刷蚀刻好,避开bonding区,在印刷完成的ITOfilm上印刷银浆线路,用激光蚀刻机按照设计好的激光蚀刻线蚀刻出银浆线路及下方ITO。解决了激光蚀刻工艺中银浆线路断线的问题,具有工艺简单、容易实现、成本较低的特点。

Description

一种电容触摸屏激光蚀刻工艺
技术领域
本发明涉及一种电容触摸屏激光蚀刻工艺。 
背景技术
激光蚀刻工艺作为目前主流的几种电容式触摸屏生产工艺之一,应用的领域涵盖各个层级客户,传统激光蚀刻工艺银浆线路下方没有ITO,一直存在激光蚀刻后银浆线路断线的问题,导致功能不良。 
发明内容
   本发明其目的就在于提供一种电容触摸屏激光蚀刻工艺,解决了激光蚀刻工艺中银浆线路断线的问题,具有工艺简单、容易实现、成本较低的特点。 
实现上述目的而采取的技术方案,首先把ITO film上的耐酸油墨图案印刷蚀刻好,避开bonding区,在印刷完成的ITO film上印刷银浆线路,用激光蚀刻机按照设计好的激光蚀刻线蚀刻出银浆线路及下方ITO。 
    与现有技术相比本发明具有以下优点。 
     通过在银浆线路下方增加ITO,彻底解决了激光蚀刻工艺中银浆线路断线的问题,具有工艺简单、容易实现、成本较低的特点。 
具体实施方式
    首先把ITO film上的耐酸油墨图案印刷蚀刻好,避开bonding区,在印刷完成的ITO film上印刷银浆线路,用激光蚀刻机按照设计好的激光蚀刻线蚀刻出银浆线路及下方ITO。 
   所述银浆线路下方ITO外扩到激光蚀刻线的距离不小于0.03mm,银浆线路下方ITO到通道ITO的距离不小于0.3mm,银浆线路下方ITO到银浆线路bonding区距离不小于0.3mm。 
   所述耐酸油墨选用绿固GC-UV-A60油墨,银浆线路选用贝特利SF-2772X银浆油墨。 
通过在银浆线路下方增加ITO,彻底解决电容屏激光蚀刻工艺生产中银浆线路断线现象。 
包括ITO film,ITO film上印刷耐酸油墨,通过酸碱蚀刻将多余的ITO蚀刻掉,保留银浆线路下方的ITO,但银浆线路的bonding区下方不可有ITO,通过激光蚀刻线蚀刻掉多余的银浆线路及下方ITO。 
    通过用耐酸油墨保护金属引线下方ITO,在酸碱蚀刻时隔离酸与ITO的接触以达到保留金属引线下方ITO的目的,在金属引线受到各种原因造成的断路时,下方ITO起到金属引线断裂处的桥接作用,以达到生产工艺没有影响,外观没有影响,杜绝由于金属引线断裂造成功能不良的效果。 
首先把ITO film上的耐酸油墨图案印刷蚀刻好,注意避开bonding区,在印刷完成的ITO film上印刷银浆线路,用激光蚀刻机按照设计好的激光蚀刻线蚀刻出银浆线路及下方ITO。 
耐酸油墨选用绿固GC-UV-A60油墨,银浆线路选用贝特利SF-2772X银浆油墨,印刷网版选用聚酯网版,印刷机台选用大震斜臂印刷机,激光蚀刻机台选用盛雄激光蚀刻机,印刷压力、速度,激光蚀刻参数等根据实际情况调试,通过CCD自动抓靶方式,在已印刷好银胶、ITO的ITO film上进行激光蚀刻。 
    所述ITO film为氧化铟锡透明导电膜; 
         Bonding为绑定;
         ITO为氧化铟锡;
         CCD为电荷耦合元件图像传感器。

Claims (3)

1.一种电容触摸屏激光蚀刻工艺,其特征在于,首先把ITO film上的耐酸油墨图案印刷蚀刻好,避开bonding区,在印刷完成的ITO film上印刷银浆线路,用激光蚀刻机按照设计好的激光蚀刻线蚀刻出银浆线路及下方ITO。
2.根据权利要求1所述的一种电容触摸屏激光蚀刻工艺,其特征在于,所述银浆线路下方ITO外扩到激光蚀刻线的距离不小于0.03mm,银浆线路下方ITO到通道ITO的距离不小于0.3mm,银浆线路下方ITO到银浆线路banding区距离不小于0.3mm。
3.根据权利要求1所述的一种电容触摸屏激光蚀刻工艺,其特征在于,所述耐酸油墨选用绿固GC-UV-A60油墨,银浆线路选用贝特利SF-2772X银浆油墨。
CN201410077026.6A 2014-03-05 2014-03-05 一种电容触摸屏激光蚀刻工艺 Pending CN103846555A (zh)

Priority Applications (1)

Application Number Priority Date Filing Date Title
CN201410077026.6A CN103846555A (zh) 2014-03-05 2014-03-05 一种电容触摸屏激光蚀刻工艺

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
CN201410077026.6A CN103846555A (zh) 2014-03-05 2014-03-05 一种电容触摸屏激光蚀刻工艺

Publications (1)

Publication Number Publication Date
CN103846555A true CN103846555A (zh) 2014-06-11

Family

ID=50854933

Family Applications (1)

Application Number Title Priority Date Filing Date
CN201410077026.6A Pending CN103846555A (zh) 2014-03-05 2014-03-05 一种电容触摸屏激光蚀刻工艺

Country Status (1)

Country Link
CN (1) CN103846555A (zh)

Cited By (1)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN108845716A (zh) * 2018-09-07 2018-11-20 芜湖伦丰电子科技有限公司 一种新型的触摸屏制作方法

Citations (7)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN202548808U (zh) * 2012-01-19 2012-11-21 深圳秋田微电子有限公司 一种电容触摸屏的双面走线的结构
WO2012173455A2 (ko) * 2011-06-16 2012-12-20 솔렌시스 주식회사 터치 패널 제조 방법, 및 이를 위한 레이저 장치
CN102902389A (zh) * 2011-07-27 2013-01-30 比亚迪股份有限公司 一种触摸传感器的制作方法
CN202904547U (zh) * 2012-11-09 2013-04-24 赣州市德普特科技有限公司 电容式触摸屏
CN103150074A (zh) * 2013-03-18 2013-06-12 江西合力泰科技股份有限公司 一种先镀膜后bm方式非搭桥而实现多点触控的一体式电容屏制作方法
CN103310903A (zh) * 2012-03-08 2013-09-18 深圳欧菲光科技股份有限公司 Ito薄膜蚀刻方法
CN103605444A (zh) * 2013-11-30 2014-02-26 东莞市平波电子有限公司 一种g1f结构的触摸屏的制作工艺

Patent Citations (7)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
WO2012173455A2 (ko) * 2011-06-16 2012-12-20 솔렌시스 주식회사 터치 패널 제조 방법, 및 이를 위한 레이저 장치
CN102902389A (zh) * 2011-07-27 2013-01-30 比亚迪股份有限公司 一种触摸传感器的制作方法
CN202548808U (zh) * 2012-01-19 2012-11-21 深圳秋田微电子有限公司 一种电容触摸屏的双面走线的结构
CN103310903A (zh) * 2012-03-08 2013-09-18 深圳欧菲光科技股份有限公司 Ito薄膜蚀刻方法
CN202904547U (zh) * 2012-11-09 2013-04-24 赣州市德普特科技有限公司 电容式触摸屏
CN103150074A (zh) * 2013-03-18 2013-06-12 江西合力泰科技股份有限公司 一种先镀膜后bm方式非搭桥而实现多点触控的一体式电容屏制作方法
CN103605444A (zh) * 2013-11-30 2014-02-26 东莞市平波电子有限公司 一种g1f结构的触摸屏的制作工艺

Cited By (2)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN108845716A (zh) * 2018-09-07 2018-11-20 芜湖伦丰电子科技有限公司 一种新型的触摸屏制作方法
CN108845716B (zh) * 2018-09-07 2021-04-13 芜湖伦丰电子科技有限公司 一种触摸屏制作方法

Similar Documents

Publication Publication Date Title
WO2008099772A1 (ja) 積層セラミックコンデンサおよびその製造方法
US10503325B2 (en) Display device, touch panel and method for manufacturing the same
CN102510664B (zh) 解决pcb板线路油薄的方法
CN104407734A (zh) 触控屏的制造方法及触控屏
CN203588240U (zh) 单层玻璃电容式触摸屏
CN107493658A (zh) 一种铜厚印制电路板的制备方法及设备
CN204537103U (zh) 一种metal架桥的ogs电容触摸屏
CN103176658A (zh) 镜面液晶显示器及其制造方法
CN104345985A (zh) 触控基板及其制备方法、触控显示面板、触控显示装置
CN103846555A (zh) 一种电容触摸屏激光蚀刻工艺
CN203405799U (zh) 一种ogs结构电容触控屏及触控屏手机
CN103699268A (zh) 用于触摸屏的环保型干法蚀刻方法
CN103862897A (zh) 触摸屏ito玻璃丝印工艺
CN104503644A (zh) 一种电容式触控面板及制作方法
CN204331654U (zh) 触控屏
CN203930778U (zh) 一种投射式电容屏
CN204087173U (zh) 新型结构的电容式触摸屏
CN203675430U (zh) 柔性印制电路板
CN104859327A (zh) Bm工艺光刻胶绝缘减少针孔短路的制作方法
CN203894732U (zh) Ito架桥的ogs电容触摸屏
CN104156115A (zh) 一种单层膜多点触控的触摸屏及其生产方法
CN106739493A (zh) 一种在盖板的油墨层镭射开孔的方法
CN203101786U (zh) 一种液晶显示器的阵列基板
CN205566789U (zh) 一种印刷电路板
CN105677079A (zh) 触摸屏的制作方法

Legal Events

Date Code Title Description
C06 Publication
PB01 Publication
C10 Entry into substantive examination
SE01 Entry into force of request for substantive examination
RJ01 Rejection of invention patent application after publication
RJ01 Rejection of invention patent application after publication

Application publication date: 20140611