CN103726403A - 一种烟用白色接装纸原纸的生产方法 - Google Patents

一种烟用白色接装纸原纸的生产方法 Download PDF

Info

Publication number
CN103726403A
CN103726403A CN201310600137.6A CN201310600137A CN103726403A CN 103726403 A CN103726403 A CN 103726403A CN 201310600137 A CN201310600137 A CN 201310600137A CN 103726403 A CN103726403 A CN 103726403A
Authority
CN
China
Prior art keywords
paper
white
production method
cigarettes
cigarette
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201310600137.6A
Other languages
English (en)
Inventor
徐伟
周建芳
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
LONGYOU TEMEI PAPER PRODUCTS Co Ltd
Original Assignee
LONGYOU TEMEI PAPER PRODUCTS Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by LONGYOU TEMEI PAPER PRODUCTS Co Ltd filed Critical LONGYOU TEMEI PAPER PRODUCTS Co Ltd
Priority to CN201310600137.6A priority Critical patent/CN103726403A/zh
Publication of CN103726403A publication Critical patent/CN103726403A/zh
Pending legal-status Critical Current

Abstract

本发明涉及一种烟用白色接装纸原纸的生产方法,该方法是在生产烟用白色接装纸原纸的过程中,当纸张经过施胶后,先在纸张的表面上涂上至少一层的具有高阻隔性的丙烯酸酯类涂料,然后再继续在其表面上附着至少一层的具有高不透性≧85的白色油墨即可。采用本发明,由于具有高阻隔性的涂料和高不透性的白色油墨,可以迟滞尼古丁及焦油的渗透,防止滤嘴处的纸张变成黄褐色。

Description

一种烟用白色接装纸原纸的生产方法
技术领域
本发明涉及一种烟用白色接装纸原纸的生产方法。
背景技术
目前,经过常规工艺制得的烟用白色接装纸原纸,将其用于卷烟生产后,如果在吸烟时,卷烟滤棒处的白色接装纸原纸会迅速变成黄褐色,主要原因在于吸烟时会有大量的尼古丁及焦油,由于白色接装纸原纸的吸附性,使尼古丁及焦油由白色接装纸原纸的内表面向外表面渗透所至。
发明内容
本发明的目的是提供能在吸烟时,防止滤嘴处的纸张的外表面变成黄褐色的一种烟用白色接装纸原纸的生产方法。
本发明采取的技术方案是:一种烟用白色接装纸原纸的生产方法,其特征在于在生产烟用白色接装纸原纸的过程中,当纸张经过施胶后,先在纸张的表面上涂上至少一层的具有高阻隔性的涂料,然后再继续在其表面上附着至少一层的具有高不透性的白色油墨即可。
所述的一种烟用白色接装纸原纸的生产方法,其特征在于高阻隔性的涂料为丙烯酸酯类。
所述的一种烟用白色接装纸原纸的生产方法,其特征在于白色油墨的高不透性≧85。
采用本发明,由于具有高阻隔性的涂料和高不透性的白色油墨,可以迟滞尼古丁及焦油的渗透,防止滤嘴处的纸张变成黄褐色。
具体实施方式
下面结合实施对本发明作进一步详细说明。具体如下:
在生产烟用白色接装纸原纸的过程中,当纸张经过施胶后,先在纸张的表面上涂上至少一层的具有高阻隔性的丙烯酸酯类的涂料,然后再继续通过印刷机在其表面上附着至少一层的具有高不透性≧85的白色油墨即可。由于涂料的高阻隔性和白色油墨的高不透性,可以迟滞尼古丁及焦油的渗透,防止滤嘴处的纸张内外表面变成黄褐色。

Claims (3)

1. 一种烟用白色接装纸原纸的生产方法,其特征在于在生产烟用白色接装纸原纸的过程中,当纸张经过施胶后,先在纸张的表面上涂上至少一层的具有高阻隔性的涂料,然后再继续在其表面上附着至少一层的具有高不透性的白色油墨即可。
2.根据权利要求1所述的一种烟用白色接装纸原纸的生产方法,其特征在于高阻隔性的涂料为丙烯酸酯类。
3.根据权利要求1所述的一种烟用白色接装纸原纸的生产方法,其特征在于白色油墨的高不透性≧85。
CN201310600137.6A 2013-11-25 2013-11-25 一种烟用白色接装纸原纸的生产方法 Pending CN103726403A (zh)