CN103691774A - 一种无缝管的矫直方法 - Google Patents

一种无缝管的矫直方法 Download PDF

Info

Publication number
CN103691774A
CN103691774A CN201310703981.1A CN201310703981A CN103691774A CN 103691774 A CN103691774 A CN 103691774A CN 201310703981 A CN201310703981 A CN 201310703981A CN 103691774 A CN103691774 A CN 103691774A
Authority
CN
China
Prior art keywords
seamless pipe
roller
pipe
reduced
straightening
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201310703981.1A
Other languages
English (en)
Inventor
张尧
陈勇
邸军
高山
邵会勇
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Angang Steel Co Ltd
Original Assignee
Angang Steel Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Angang Steel Co Ltd filed Critical Angang Steel Co Ltd
Priority to CN201310703981.1A priority Critical patent/CN103691774A/zh
Publication of CN103691774A publication Critical patent/CN103691774A/zh
Pending legal-status Critical Current

Abstract

本发明提供一种无缝管的矫直方法,六辊矫直机矫直辊转数控制在588~592rpm,辊道频率为29~29.3Hz。本发明可在矫直时躲过无缝管端头位置,极大提高管端椭圆度控制精度,使热处理无缝管管端椭圆度由之前的1-2mm减少至1mm以内,反切率下降,合格率与成材率上升,产品质量显著提高,不仅可降低无缝管的生产成本,而且能提高用户车丝合格率,减少质量异议率。

Description

一种无缝管的矫直方法
技术领域
本发明属于轧钢工艺领域,尤其涉及一种用于无缝钢管的快开式矫直方法。
背景技术
热处理无缝管因水淬变形,调质后会出现弯曲变形及椭圆度大等缺陷,因此目前国内多数厂家均采用回火后增加定径机方式来控制椭圆度,利用后续矫直工序进行弯曲度控制。而对于没有定径工序的无缝钢管厂来说,将造成调质后的无缝管出现如下问题:
1、管端椭圆度大,平均达到1-2mm,且无法控制。
2、用户车丝后出现黑皮扣缺陷,质量异议较多。
3、对管端椭圆度大的无缝管需进行切头处理,不仅浪费热力和物力,而且直接影响成材率。
发明内容
本发明旨在提供一种可实现端头矫直位置准确控制,提高管端椭圆度控制精度,减少切头量,降低生产成本的无缝管矫直方法。
为达此目的,本发明采取了如下解决方案:
一种无缝管的矫直方法,其特征在于,通过调整六辊矫直辊转数和辊道频率,躲过无缝管端头,实现无缝管端头矫直位置控制,其六辊矫直机矫直辊转数控制在588~592rpm,辊道频率为29~29.3Hz。
本发明的有益效果为:
由于本发明在矫直时躲过无缝管端头位置,极大提高管端椭圆度控制精度,使热处理无缝管管端椭圆度由之前的1-2mm,减少至1mm以内,反切率下降,合格率与成材率上升,产品质量显著提高,不仅可降低无缝管的生产成本,而且能提高用户车丝合格率,减少质量异议率。
具体实施方式
实施例1:
本发明无缝管的矫直方法,主要是通过合理调整六辊矫直辊转数和辊道频率,实现无缝管端头矫直位置的精确控制。六辊矫直机矫直辊转数控制在589rpm,辊道频率为29Hz。实施后管端椭圆度控制在0.92mm。
实施例2:
通过合理调整六辊矫直辊转数和辊道频率,实现无缝管端头矫直位置的精确控制。六辊矫直机矫直辊转数控制在590rpm,辊道频率为29.3Hz。实施后管端椭圆度控制在0.9mm。
实施例3:
通过合理调整六辊矫直辊转数和辊道频率,实现无缝管端头矫直位置的精确控制。六辊矫直机矫直辊转数控制在592rpm,辊道频率为29.1Hz。实施后管端椭圆度控制在0.91mm。

Claims (1)

1.一种无缝管的矫直方法,其特征在于,通过调整六辊矫直辊转数和辊道频率,躲过无缝管端头,实现无缝管端头矫直位置控制,其六辊矫直机矫直辊转数控制在588~592rpm,辊道频率为29~29.3Hz。
CN201310703981.1A 2013-12-20 2013-12-20 一种无缝管的矫直方法 Pending CN103691774A (zh)