Prior art keywords
mud
polyacrylamide
water
calcium oxide
aluminum chloride
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Active
Application number
CN201310496503.8A
Other languages
English (en)
Other versions
CN103524015A (zh
Inventor
秦广山
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
RENQIU LVBANG ENVIRONMENT PROTECTION TECHNOLOGY CO., LTD.
Original Assignee
秦广山
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by 秦广山 filed Critical 秦广山
Priority to CN201310496503.8A priority Critical patent/CN103524015B/zh
Publication of CN103524015A publication Critical patent/CN103524015A/zh
Application granted granted Critical
Publication of CN103524015B publication Critical patent/CN103524015B/zh
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Links

Landscapes

  • Treatment Of Sludge (AREA)

Abstract

一种泥浆固化剂及其制备方法,其特征在于,包括下列用量的原料:聚丙烯酰胺2%-3%、聚合氯化铝7%-8%、氧化钙20%-28%、四氧化三铁8%-15%、余量为泥浆;将2.5%的聚丙烯酰胺、7.2%的聚合氯化铝、24%的氧化钙、11%的四氧化三铁加入放有一定量水的加药罐内搅拌,稀释后的药与泥浆池内的泥浆均匀混合送至破胶絮凝反应管内反应后,使泥浆固化。所述加药罐内放置水的多少取决于泥浆的用量。本发明的有益效果是,比常规水处理方法的净水能力提高20%以上,在污水处理中可以增加水循环使用率,更可提高泥浆脱水性,使泥浆固液分离,加快固体沉降,提高滤液清澈度。

Description

一种泥浆固化剂及其制备方法
技术领域
本发明涉及一种泥浆固化剂及其制备方法,属于油田地质钻井方面的技术领域。
背景技术
石油开采或地质勘探都离不开钻井作业,而钻井作业对环境污染主要来源于废弃钻井液,如果大量的废弃钻井液不进行处理,可能外溢流入农田、河流或渗入地下,钻井液中的有害物质对土壤、地下水和当地的自然环境产生严重影响。
发明内容
本发明的目的在于,提供一种泥浆固化剂及其制备方法。
一种泥浆固化剂,由2%-3%的聚丙烯酰胺、7%-8%的聚合氯化铝、20%-28%的氧化钙、8%-15%的四氧化三铁和余量的泥浆组成。
由2.5%的聚丙烯酰胺、7.2%的聚合氯化铝、24%的氧化钙、11%的四氧化三铁和余量的泥浆组成。
一种泥浆固化剂及其制备方法,将一定量的水加入到加药罐内,再将2.5%的聚丙烯酰胺、7.2%的聚合氯化铝、24%的氧化钙、11%的四氧化三铁放入加药罐内进行搅拌,搅拌稀释后与泥浆池内的泥浆均匀混合后通过专用泵输送至破胶絮凝反应罐内进行反应,使成品泥浆固化。
在加药罐内放置水的多少取决于成品泥浆的需用量。
所述成品泥浆的固化分为三种:A.在车载泥水分离***使用时,药物稀释后与泥浆均匀混合即可;B.在废弃钻井液处理***使用时,药物稀释后与泥浆均匀混合后,进行破胶絮凝反应即可;C.在井场使用时,只需将药物放入泥浆池内与泥浆均匀混合后,进行破胶絮凝反应后,直接固化、填埋。
本发明的有益效果是,比常规水处理方法的净水能力提高20%以上在污水处理中可以增加水循环使用率,更可提高泥浆脱水性,使泥浆固液分离,加快固体沉降,提高滤液清澈度。
具体实施方式
本发明由聚丙烯酰胺、聚合氯化铝、氧化钙、四氧化三铁组成。
各原料的重量百分比为:
一般配比:
聚丙烯酰胺2%-3%;聚合氯化铝7%-8%;氧化钙20%-28%;四氧化三铁8%-15%;余量为泥浆。
优选配比:
聚丙烯酰胺是2.5%;聚合氯化铝是7.2%;氧化钙是24%;四氧化三铁是11%;余量为泥浆。
钻井剂的制备方法:先在加药罐中倒入一定量的水,将2.5%的聚丙烯酰胺、7.2%的聚合氯化铝、24%的氧化钙、11%的四氧化三铁放入加药罐内搅拌,然后把稀释后的药通过泵输送到泥浆池内与泥浆混合均匀后,再通过泵输送至破胶絮凝反应管内反应后,使泥浆固化,其固化程度是:1.放在车载和泥浆不落地设备中只需搅拌均匀即可;2.单独在井场使用需等40-90分钟即可。
所述加药罐内放置水的多少取决于泥浆的用量。
所述成品泥浆的固化分为三种:A.在车载泥水分离***使用时,药物稀释后与泥浆均匀混合即可;B.在废弃钻井液处理***使用时,药物稀释后与泥浆均匀混合后,进行破胶絮凝反应即可;C.在井场使用时,只需将药物放入泥浆池内与泥浆均匀混合后,进行破胶絮凝反应后,直接固化、填埋。

Claims (5)

1.一种泥浆固化剂,由2%-3%的聚丙烯酰胺、7%-8%的聚合氯化铝、20%-28%的氧化钙、8%-15%的四氧化三铁和余量的泥浆组成。
2.根据权利要求1所述的一种泥浆固化剂,由2.5%的聚丙烯酰胺、7.2%的聚合氯化铝、24%的氧化钙、11%的四氧化三铁和余量的泥浆组成。
3.根据权利要求1所述的一种泥浆固化剂的制备方法,其特征在于,将一定量的水加入到加药罐内,再将2.5%的聚丙烯酰胺、7.2%的聚合氯化铝、24%的氧化钙、11%的四氧化三铁放入加药罐内进行搅拌,搅拌稀释后与泥浆池内的泥浆均匀混合后通过专用泵输送至破胶絮凝反应罐内进行反应,使成品泥浆固化。
4.根据权利要求3所述的一种方法,其特征在于,在加药罐内放置水的多少取决于成品泥浆的需用量。
5.根据权利要求3所述的一种方法,其特征在于,所述成品泥浆的固化分为三种:A.在车载泥水分离***使用时,药物稀释后与泥浆均匀混合即可;B.在废弃钻井液处理***使用时,药物稀释后与泥浆均匀混合后,进行破胶絮凝反应即可;C.在井场使用时,只需将药物放入泥浆池内与泥浆均匀混合后,进行破胶絮凝反应后,直接固化、填埋。
CN201310496503.8A 2013-10-22 2013-10-22 一种泥浆固化剂及其制备方法 Active CN103524015B (zh)

Priority Applications (1)

Application Number Priority Date Filing Date Title
CN201310496503.8A CN103524015B (zh) 2013-10-22 2013-10-22 一种泥浆固化剂及其制备方法

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
CN201310496503.8A CN103524015B (zh) 2013-10-22 2013-10-22 一种泥浆固化剂及其制备方法

Publications (2)

Publication Number Publication Date
CN103524015A CN103524015A (zh) 2014-01-22
CN103524015B true CN103524015B (zh) 2015-08-19

Family

ID=49926433

Family Applications (1)

Application Number Title Priority Date Filing Date
CN201310496503.8A Active CN103524015B (zh) 2013-10-22 2013-10-22 一种泥浆固化剂及其制备方法

Country Status (1)

Country Link
CN (1) CN103524015B (zh)

Families Citing this family (4)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN105154104A (zh) * 2015-09-28 2015-12-16 江苏振宇环保科技有限公司 一种回收铁泥制备土壤粉体固化剂的方法
CN110903016A (zh) * 2019-11-01 2020-03-24 四川格英达环保科技有限公司 一种钻井水基泥浆干化剂
CN112358163A (zh) * 2020-11-13 2021-02-12 中冶集团武汉勘察研究院有限公司 一种加速泥浆脱水分离的化学试剂及方法
CN113735412B (zh) * 2021-11-05 2022-02-08 中南大学 一种基础工程废弃泥浆高效脱水固化处理剂及其使用方法

Citations (1)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN1792898A (zh) * 2005-11-22 2006-06-28 刘茂平 钻井废泥浆固化剂

Family Cites Families (1)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JPH0440248A (ja) * 1990-06-01 1992-02-10 Fujita Corp 固液分離方法

Patent Citations (1)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN1792898A (zh) * 2005-11-22 2006-06-28 刘茂平 钻井废泥浆固化剂

Also Published As

Publication number Publication date
CN103524015A (zh) 2014-01-22

Similar Documents

Publication Publication Date Title
CN110318696B (zh) 一种水基废弃钻井液无害化处理工艺
CN103524015B (zh) 一种泥浆固化剂及其制备方法
CN101475285A (zh) 天然气田污水及固体污染物综合处理工艺方法
CN204097269U (zh) 磁力混凝及分离处理矿井水装置
CN103708594A (zh) 一种高效重介质混凝沉淀水处理工艺
CN106854024A (zh) 一种油田、气田压裂返排液处理***及处理方法
CN102718341A (zh) 一种离心式不落地废弃钻井液无害化处理技术
CN104030536A (zh) 一种环保疏浚底泥一体化机械深度干化***
CN104355338A (zh) 一种移动污水处理设备用加药装置
CN102381785B (zh) 一种含磷废水回收的方法
CN207391160U (zh) 一种含芬顿反应池的地下水处理装置
CN101503237A (zh) 一种化学试剂组合及其在泥水快速分离与水质净化中的应用
CN105863563B (zh) 一种应用于油气田钻井废弃物无害化治理及可持续利用的方法及***
CN108609948A (zh) 一种高钢渣含量透水混凝土的制备方法
CN105859069B (zh) 地浸采铀钻孔泥浆无害化处理的方法
CN203960024U (zh) 一种环保疏浚底泥一体化机械深度干化***
CN103304053B (zh) 矿井疏矸排水转化为生产用水的处理***
CN1590305A (zh) 废弃水包油钻井液的处理方法和处理剂
CN104261587B (zh) 一种用于页岩气井压裂作业返排压力液的再利用处理装置
CN106277260A (zh) 一种木质纤维板生产废水污泥脱水***
CN201666145U (zh) 钻井废弃泥浆陶瓷分离装置
CN207391161U (zh) 一种含多介质过滤器的地下水处理装置
CN205999180U (zh) 一种压裂反排液环保处理***
CN202030624U (zh) 钻井废弃物处理装置
CN206089343U (zh) 一种黑臭泥水移动式应急处理***

Legal Events

Date Code Title Description
C06 Publication
PB01 Publication
C10 Entry into substantive examination
SE01 Entry into force of request for substantive examination
C14 Grant of patent or utility model
GR01 Patent grant
ASS Succession or assignment of patent right

Owner name: RENQIU GREEN NATION ENVIRONMENTAL PROTECTION TECHN

Free format text: FORMER OWNER: QIN GUANGSHAN

Effective date: 20150819

C41 Transfer of patent application or patent right or utility model
TR01 Transfer of patent right

Effective date of registration: 20150819

Address after: 062552, Hebei, Cangzhou, Renqiu North China Petroleum Bohai North District Hospital

Patentee after: RENQIU LVBANG ENVIRONMENT PROTECTION TECHNOLOGY CO., LTD.

Address before: 062550, room 4, unit 16, 202 North District, Huabei Road, Bohai Road, Renqiu, Hebei, Bohai, China

Patentee before: Qin Guangshan