CN103483993A - 一种可低温固化粉末涂料 - Google Patents

一种可低温固化粉末涂料 Download PDF

Info

Publication number
CN103483993A
CN103483993A CN201310393362.7A CN201310393362A CN103483993A CN 103483993 A CN103483993 A CN 103483993A CN 201310393362 A CN201310393362 A CN 201310393362A CN 103483993 A CN103483993 A CN 103483993A
Authority
CN
China
Prior art keywords
parts
low
powder coating
powder paint
temperature curable
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
CN201310393362.7A
Other languages
English (en)
Other versions
CN103483993B (zh
Inventor
张洪滨
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Guangdong Pocket Powder Coatings Co.,Ltd.
Original Assignee
BENGBU HONGAN PRECISION MACHINERY Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by BENGBU HONGAN PRECISION MACHINERY Co Ltd filed Critical BENGBU HONGAN PRECISION MACHINERY Co Ltd
Priority to CN201310393362.7A priority Critical patent/CN103483993B/zh
Publication of CN103483993A publication Critical patent/CN103483993A/zh
Application granted granted Critical
Publication of CN103483993B publication Critical patent/CN103483993B/zh
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

本发明公开了一种可低温固化粉末涂料,它是由下述重量份的原料组成的间苯型不饱和聚酯树脂50-60、E-12环氧树脂20-25、白炭黑0.1-0.5、氧化镧3.5-4.5、活性炭粉10-13、偶氮二异丁腈1-2、硅酸钠2-3、硫酸亚铁2-3、酚醛树脂1-2、二甲基硅油0.1-1、复合填料10-20;本发明提供的可低温固化粉末涂料,透明度高,固化温度低,在喷涂过程中,对物件预热处理至50-70℃,保持5-8分钟,进行静电喷涂,再经120℃左右的热风20min,自然冷却即得,适用于木材的涂装,表面光洁无气泡,成膜性好。

Description

一种可低温固化粉末涂料
技术领域
    本发明主要涉及一种涂料,尤其涉及一种可低温固化粉末涂料。
背景技术
粉末涂料的其特性有:1、该产品不含毒性,不含溶剂和不含挥发有毒性的物质,故无中毒、无火灾、无“三废”的排放等公害的问题,完全符合国家环保法的要求。2、原材料利用率高,一些知名品牌的粉末供应商生产的粉末,其过喷的粉末可回收利用,最高的利用率甚至能达99%以上。3、被涂物前处理后, 一次性施工,无需底涂,即可得到足够厚度的涂膜,易实现自动化操作,生产效率高, 可降低成本。4、涂层致密、附着力、抗冲击强度和韧性均好,边角覆盖率高,具有优良的耐化学药品腐蚀性能和电气绝缘性能。5、粉末涂料存贮、运输安全和方便。
发明内容
本发明目的就是为了提供一种可低温固化粉末涂料。
本发明是通过以下技术方案实现的:
一种可低温固化粉末涂料,其特征在于它是由下述重量份的原料组成的:
间苯型不饱和聚酯树脂50-60、E-12环氧树脂20-25、白炭黑0.1-0.5、氧化镧3.5-4.5、活性炭粉10-13、偶氮二异丁腈1-2、硅酸钠2-3、硫酸亚铁2-3、酚醛树脂1-2、二甲基硅油0.1-1、复合填料10-20;
所述的复合填料是由下述重量份的原料组成的:
三水铝石30-40、凹凸棒土20-30、碳化硅6-10、氢氧化镁3-5、羧甲基纤维素1-2、霍霍巴油2-3;
将上述三水铝石、凹凸棒土、碳化硅混合,在600-800℃下保温煅烧2-4小时,出料冷却后送入球磨机中进行球磨混合,再加入氢氧化镁和羧甲基纤维素,继续球磨1-2小时,将霍霍巴油加热到25-30℃后加入,球磨,过80-100目筛,即得所述复合填料。
一种可低温固化粉末涂料的制备方法,包括以下步骤:
将上述除了白炭黑以外的各原料混合,送入高速混合机,800-1000转/分搅拌分散3-5分钟,送入挤出机,熔融挤出,然后置于研磨机,加入白炭黑,在1000-1200 r/min 下高速研磨,再过空隙大小为80-100μm 的筛网,即得所述可低温固化粉末涂料。
本发明的优点是:
    本发明提供的可低温固化粉末涂料,透明度高,分散性好,固化温度低,在喷涂过程中,对物件预热处理至50-70℃,保持5-8 分钟,进行静电喷涂,再经120℃左右的热风20min,自然冷却即得,适用于木材和塑料的涂装,表面光洁无气泡,成膜性好。
具体实施方式
实施例1,
一种可低温固化粉末涂料,它是由下述重量份(公斤)的原料组成的:
间苯型不饱和聚酯树脂60、E-12环氧树脂25、白炭黑0.5、氧化镧4.5、活性炭粉13、偶氮二异丁腈2、硅酸钠3、硫酸亚铁3、酚醛树脂2、二甲基硅油0.1、复合填料10-20;
所述的复合填料是由下述重量份的原料组成的:
三水铝石40、凹凸棒土30、碳化硅10、氢氧化镁5、羧甲基纤维素1、霍霍巴油3;
将上述三水铝石、凹凸棒土、碳化硅混合,在800℃下保温煅烧4小时,出料冷却后送入球磨机中进行球磨混合,再加入氢氧化镁和羧甲基纤维素,继续球磨2小时,将霍霍巴油加热到30℃后加入,球磨,过100目筛,即得所述复合填料。
一种可低温固化粉末涂料的制备方法,包括以下步骤:
将上述除了白炭黑以外的各原料混合,送入高速混合机,1000转/分搅拌分散3-5分钟,送入挤出机,熔融挤出,然后置于研磨机,加入白炭黑,在1200 r/min 下高速研磨,再过空隙大小为100μm 的筛网,即得所述可低温固化粉末涂料。
性能测试:
耐溶剂:240小时,无变化;
盐雾试验(1000h):无变化。

Claims (2)

1.一种可低温固化粉末涂料,其特征在于它是由下述重量份的原料组成的:
间苯型不饱和聚酯树脂50-60、E-12环氧树脂20-25、白炭黑0.1-0.5、氧化镧3.5-4.5、活性炭粉10-13、偶氮二异丁腈1-2、硅酸钠2-3、硫酸亚铁2-3、酚醛树脂1-2、二甲基硅油0.1-1、复合填料10-20;
所述的复合填料是由下述重量份的原料组成的:
三水铝石30-40、凹凸棒土20-30、碳化硅6-10、氢氧化镁3-5、羧甲基纤维素1-2、霍霍巴油2-3;
将上述三水铝石、凹凸棒土、碳化硅混合,在600-800℃下保温煅烧2-4小时,出料冷却后送入球磨机中进行球磨混合,再加入氢氧化镁和羧甲基纤维素,继续球磨1-2小时,将霍霍巴油加热到25-30℃后加入,球磨,过80-100目筛,即得所述复合填料。
2.一种如权利要求1所述的可低温固化粉末涂料的制备方法,其特征在于包括以下步骤:
将上述除了白炭黑以外的各原料混合,送入高速混合机,800-1000转/分搅拌分散3-5分钟,送入挤出机,熔融挤出,然后置于研磨机,加入白炭黑,在1000-1200 r/min 下高速研磨,再过空隙大小为80-100μm 的筛网,即得所述可低温固化粉末涂料。
CN201310393362.7A 2013-09-03 2013-09-03 一种可低温固化粉末涂料 Active CN103483993B (zh)