CN103331248A - Dispensing process - Google Patents

Dispensing process Download PDF

Info

Publication number
CN103331248A
CN103331248A CN 201310244004 CN201310244004A CN103331248A CN 103331248 A CN103331248 A CN 103331248A CN 201310244004 CN201310244004 CN 201310244004 CN 201310244004 A CN201310244004 A CN 201310244004A CN 103331248 A CN103331248 A CN 103331248A
Authority
CN
China
Prior art keywords
glue
product
baking
minutes
flame treatment
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN 201310244004
Other languages
Chinese (zh)
Inventor
周立新
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
ANHUI YANGYI PRECISE SILICON MANUFACTURE Co Ltd
Original Assignee
ANHUI YANGYI PRECISE SILICON MANUFACTURE Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by ANHUI YANGYI PRECISE SILICON MANUFACTURE Co Ltd filed Critical ANHUI YANGYI PRECISE SILICON MANUFACTURE Co Ltd
Priority to CN 201310244004 priority Critical patent/CN103331248A/en
Publication of CN103331248A publication Critical patent/CN103331248A/en
Pending legal-status Critical Current

Abstract

The invention discloses a dispensing process, which includes the steps of handling, flame treatment, baking, dust removal, dosing of treating agent, operation of a dispenser, standing and curing. The dispensing process includes the following specific steps: (1) handling: a product is taken out and put into a baking tray; (2) flame treatment: the product is treated by flame; (3) baking: the product is put into an oven and baked for 30 minutes; (4) dust removal, a piece of dustless cloth is used for remove the dust on the surface of the part on which glue needs to be dispensed; (5) dosing of treating agent: the treating agent is uniformly applied on the surface on which glue needs to be dispensed; (6) operation of the dispenser: the dispenser is used for dripping glue onto the surface of the product; (7) standing: after dispensing, the product is placed for 30 minutes; (8) curing: the product is put into the oven and cured for 15 minutes. The dispensing process has the following effects: solidification can be implemented under lower temperature; the dispensing process can be adapted to ultrahigh-speed dispensing, small-amount coating cannot lead to fiber forming and edge subsiding as well, and the glue dot can keep a good shape; the curing speed is high; the mechanical properties are high; no cured byproduct is produced; coloring is easy, and the glue dot is safe and non-toxic; the air permeability is good, the heat resistance is high, and the weatherability is excellent.

Description

A kind of gluing process
Technical field
The present invention relates to a kind of gluing process.
Background technology
Point glue be called for short to drip glue, is glue curing thing surface, thereby makes surfacing, gloss excellent, is applicable to silastic product surface point seal, plays the effect of decorating with protection silastic press key surface; It and silicon rubber have firm then property, and wearability is good.
But conventional point glue process is wayward, and the poor effect of some glue.
Summary of the invention
It is a kind of easy to operate, easy to control that main purpose of the present invention is to provide, all good gluing process of some glue effect.
For addressing the above problem, the present invention adopts following technical scheme:
A kind of gluing process comprises and gets that dish, flame treatment, baking, dedusting, interpolation inorganic agent, point gum machine operation are used, sky is put, vulcanisation step, specifically may further comprise the steps:
(1) gets dish: take out product and put into baking tray;
(2) flame treatment: product is carried out flame treatment;
(3) baking: put into baking box baking 30 minutes;
(4) dedusting: carry out surperficial dedusting to dripping the glue position with non-dust cloth;
(5) add inorganic agent: inorganic agent is evenly smeared dripped the glue surface;
(6) point gum machine operation is used: use point gum machine with glue point at product surface;
(7) sky is put: the product that some glue finishes was placed 30 minutes;
(8) sulfuration: put into roasting incubator sulfuration 15 minutes.
As optimized technical scheme, described point gum machine operation is used and is divided into following steps:
(a) the size control of some glue amount: the size of glue spot diameter should be half of product spacing;
(b) control of some glue laminated power: spot gluing equipment provides certain pressure to guarantee the glue supply for needle tubing (glue rifle), and the pressure size determines for glue amount and the glue rate of outflow;
(c) pinhead-sized selection: in production operation, syringe needle internal diameter size should be 1/2 of a glue glue spot diameter;
(d) the distance control between syringe needle and the working face;
(e) viscosity of glue is selected;
(f) glue temperature control: the serviceability temperature of glue should be 23 ℃~25 ℃;
(g) produce bubble in the anti-stop glue process;
(h) set fluid;
(i) selection of glue: select to use AB glue.
The invention has the beneficial effects as follows:
(1) can under lower temperature, realize solidifying;
(2) can corresponding ultrahigh speed point glue, the wire drawing limit of collapsing, the shaping that glue point maintenance is good can not take place in the trace coating yet;
(3) curingprocess rate is fast;
(4) mechanical performance is strong;
(5) there is not the sulfuration accessory substance;
(6) easy coloring, safety non-toxic;
(7) good permeability, hear resistance is good, weather resisteant is good.
Description of drawings
In order to be easy to explanation, the present invention is done to describe in detail by following specific embodiment and accompanying drawing.
Fig. 1 is solidification temperature schematic diagram of the present invention.
The specific embodiment
A kind of gluing process of the present invention comprises and gets that dish, flame treatment, baking, dedusting, interpolation inorganic agent, point gum machine operation are used, sky is put, vulcanisation step, specifically may further comprise the steps:
(1) gets dish: take out product and put into baking tray;
(2) flame treatment: product is carried out flame treatment;
(3) baking: put into baking box baking 30 minutes;
(4) dedusting: carry out surperficial dedusting to dripping the glue position with non-dust cloth;
(5) add inorganic agent: inorganic agent is evenly smeared dripped the glue surface;
(6) point gum machine operation is used: use point gum machine with glue point at product surface;
(7) sky is put: the product that some glue finishes was placed 30 minutes;
(8) sulfuration: put into roasting incubator sulfuration 15 minutes.
As optimized technical scheme, described point gum machine operation is used and is divided into following steps:
(a) the size control of some glue amount: the size of glue spot diameter should be half of product spacing;
(b) control of some glue laminated power: spot gluing equipment provides certain pressure to guarantee the glue supply for needle tubing (glue rifle), and the pressure size determines for glue amount and the glue rate of outflow;
(c) pinhead-sized selection: in production operation, syringe needle internal diameter size should be 1/2 of a glue glue spot diameter;
(d) the distance control between syringe needle and the working face;
(e) viscosity of glue is selected;
(f) glue temperature control: the serviceability temperature of glue should be 23 ℃~25 ℃;
(g) produce bubble in the anti-stop glue process;
(h) set fluid;
(i) selection of glue: select to use AB glue.
The above only is the specific embodiment of the present invention, but protection scope of the present invention is not limited thereto, and any variation or replacement of expecting without creative work all should be encompassed within protection scope of the present invention.Therefore, protection scope of the present invention should be as the criterion with the protection domain that claims were limited.

Claims (2)

1. gluing process comprises and gets that dish, flame treatment, baking, dedusting, interpolation inorganic agent, point gum machine operation use, sky is put, vulcanisation step, it is characterized in that, specifically may further comprise the steps:
(1) gets dish: take out product and put into baking tray;
(2) flame treatment: product is carried out flame treatment;
(3) baking: put into baking box baking 30 minutes;
(4) dedusting: carry out surperficial dedusting to dripping the glue position with non-dust cloth;
(5) add inorganic agent: inorganic agent is evenly smeared dripped the glue surface;
(6) point gum machine operation is used: use point gum machine with glue point at product surface;
(7) sky is put: the product that some glue finishes was placed 30 minutes;
(8) sulfuration: put into roasting incubator sulfuration 15 minutes.
2. gluing process according to claim 1 is characterized in that: described point gum machine operation is used and is divided into following steps:
(a) the size control of some glue amount: the size of glue spot diameter should be half of product spacing;
(b) control of some glue laminated power: spot gluing equipment provides certain pressure to guarantee the glue supply for needle tubing (glue rifle), and the pressure size determines for glue amount and the glue rate of outflow;
(c) pinhead-sized selection: in production operation, syringe needle internal diameter size should be 1/2 of a glue glue spot diameter;
(d) the distance control between syringe needle and the working face;
(e) viscosity of glue is selected;
(f) glue temperature control: the serviceability temperature of glue should be 23 ℃~25 ℃;
(g) produce bubble in the anti-stop glue process;
(h) set fluid;
(i) selection of glue: select to use AB glue.
CN 201310244004 2013-06-17 2013-06-17 Dispensing process Pending CN103331248A (en)