CN103240783A - 一种重组竹管材的生产方法 - Google Patents

一种重组竹管材的生产方法 Download PDF

Info

Publication number
CN103240783A
CN103240783A CN2013102086341A CN201310208634A CN103240783A CN 103240783 A CN103240783 A CN 103240783A CN 2013102086341 A CN2013102086341 A CN 2013102086341A CN 201310208634 A CN201310208634 A CN 201310208634A CN 103240783 A CN103240783 A CN 103240783A
Authority
CN
China
Prior art keywords
bamboo
profile
reinforcement
trunk material
reorganization
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN2013102086341A
Other languages
English (en)
Inventor
白建国
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Individual
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Individual filed Critical Individual
Priority to CN2013102086341A priority Critical patent/CN103240783A/zh
Publication of CN103240783A publication Critical patent/CN103240783A/zh
Pending legal-status Critical Current

Abstract

一种重组竹管材的生产方法,它是用竹子开成竹片,经防虫、防腐处理、机械加工制成竹型材和增强竹筋,将竹型材和增强竹筋涂胶、增强竹筋围合或穿插竹型材粘合制成重组竹管材;这种重组竹管材不易开裂,易工业化、标准化、规模化生产,替代部分铁管材和塑料管材的用途,从而减少污染物的排放。

Description

一种重组竹管材的生产方法
技术领域
本发明属于竹子加工重组成新型材料领域,特别是指一种重组竹管材的生产方法。
背景技术
目前,管材多为铁管材和塑料管材,存在着生产原料用铁矿石和石油资源,破坏生态环境的不足,用竹子生产加工成重组竹管材的还不多见;本发明的技术路线是用竹子开成竹片,经防虫、防腐处理、机械加工制成竹型材和增强竹筋,将竹型材和增强竹筋涂胶、增强竹筋围合或穿插竹型材粘合制成重组竹管材;这种重组竹管材不易开裂,易工业化、标准化、规模化生产,替代部分铁管材和塑料管材的用途,从而减少污染物的排放。
发明内容
一种重组竹管材的生产方法,它是用竹子开成竹片,经防虫、防腐处理、机械加工制成竹型材和增强竹筋,将竹型材和增强竹筋涂胶、增强竹筋围合或穿插竹型材粘合制成重组竹管材;
其中所述一种重组竹管材的生产方法中,竹型材的特征在于,生产时,竹片的两侧经机械加工成外面较宽,内面较窄的梯形竹片或弧形竹片为竹型材,竹型材涂胶在环形夹具内粘合夹紧,待胶干燥后卸下环形夹具制成重组竹管材;使用增强竹筋穿插竹型材时,竹型材上分段钻孔;
其中所述一种重组竹管材的生产方法中,增强竹筋的特征在于,增强竹筋围合竹型材粘合制成重组竹管材生产时,增强竹筋是经机械加工成仿真竹凸节,仿真竹凸节的两端头切削成可搭接的斜面,经加热定型为环形仿真竹凸节,使用时,环形仿真竹凸节涂胶围合重组竹管材,用环形夹具夹紧,待胶干燥后卸下环形夹具,制成重组竹管材;用增强竹筋穿插竹型材粘合制成重组竹管材生产时,增强竹筋的直径是经机械加工成略小于竹型材上的分段钻孔的直径,增强竹筋的两端头切削成可搭接的斜面,经加热定型为环形增强竹筋,使用时,环形增强竹筋涂胶穿插竹型材上的分段钻孔,用环形夹具夹紧重组竹管材外壁,待胶干燥后卸下环形夹具,制成重组竹管材。
本发明的有益效果
1、用一种重组竹管材的生产方法生产的重组竹管材,竹型材和增强竹筋围合或穿插竹型材粘合制成不易开裂;
2、易工业化、标准化、规模化生产;
3、替代部分铁管材和塑料管材的用途,从而减少污染物的排放。
具体实施方式
制造直径120mm,长1000mm的重组竹管材,用竹子开成长1000mm、宽20mm的竹片,经去青、防虫、防腐处理,按100mm分段,在竹片的中间钻直径8mm的孔,竹片的两侧经机械加工成外面较宽,内面较窄的梯形竹片为竹型材,将竹型材的粘合面涂胶,在环形夹具内粘合夹紧,待胶干燥后卸下环形夹具制成重组竹管材;增强竹筋是用竹片经机械加工成仿真竹凸节,仿真竹凸节的两端头切削成可搭接的斜面,经加热定型为内径为120mm的环形仿真竹凸节,用环形仿真竹凸节涂胶围合重组竹管材,用环形夹具夹紧,待胶干燥后卸下环形夹具,制成重组竹管材;用增强竹筋穿插竹型材粘合制成重组竹管材实施时,增强竹筋的直径是经机械加工成略小于竹型材上的分段钻孔的直径,增强竹筋的两端头切削成可搭接的斜面,经加热定型为环形增强竹筋,将环形增强竹筋涂胶穿插竹型材上的分段孔,用环形夹具夹紧重组竹管材外壁,待胶干燥后卸下环形夹具,制成重组竹管材。

Claims (3)

1.一种重组竹管材的生产方法,它是用竹子开成竹片,经防虫、防腐处理、机械加工制成竹型材和增强竹筋,将竹型材和增强竹筋涂胶、增强竹筋围合或穿插竹型材粘合制成重组竹管材。 
2.根据权利要求1中所述一种重组竹管材的生产方法中,竹型材的特征在于,生产时,竹片的两侧经机械加工成外面较宽,内面较窄的梯形竹片或弧形竹片为竹型材,竹型材涂胶在环形夹具内粘合夹紧,待胶干燥后卸下环形夹具制成重组竹管材;使用增强竹筋穿插竹型材时,竹型材上分段钻孔。 
3.根据权利要求1中所述一种重组竹管材的生产方法中,增强竹筋的特征在于,增强竹筋围合竹型材粘合制成重组竹管材生产时,增强竹筋是经机械加工成仿真竹凸节,仿真竹凸节的两端头切削成可搭接的斜面,经加热定型为环形仿真竹凸节,使用时,环形仿真竹凸节涂胶围合重组竹管材,用环形夹具夹紧,待胶干燥后卸下环形夹具,制成重组竹管材;用增强竹筋穿插竹型材粘合制成重组竹管材生产时,增强竹筋的直径是经机械加工成略小于竹型材上的分段钻孔的直径,增强竹筋的两端头切削成可搭接的斜面,经加热定型为环形增强竹筋,使用时,环形增强竹筋涂胶穿插竹型材上的分段钻孔,用环形夹具夹紧重组竹管材外壁,待胶干燥后卸下环形夹具,制成重组竹管材。 
CN2013102086341A 2013-05-27 2013-05-27 一种重组竹管材的生产方法 Pending CN103240783A (zh)