- tungstate
- hours
- dielectric ceramic
- sintering
- li3r3w2o12
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Abstract
Description
Claims (1)