CN102977609A - 一种船用耐油耐低温低烟无卤阻燃电缆料及其制备方法 - Google Patents

一种船用耐油耐低温低烟无卤阻燃电缆料及其制备方法 Download PDF

Info

Publication number
CN102977609A
CN102977609A CN2012104354909A CN201210435490A CN102977609A CN 102977609 A CN102977609 A CN 102977609A CN 2012104354909 A CN2012104354909 A CN 2012104354909A CN 201210435490 A CN201210435490 A CN 201210435490A CN 102977609 A CN102977609 A CN 102977609A
Authority
CN
China
Prior art keywords
parts
clay
cable material
potter
oxide
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
CN2012104354909A
Other languages
English (en)
Other versions
CN102977609B (zh
Inventor
姜睿
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Guangdong Lanyu Plastic Products Co ltd
Original Assignee
Anhui Jinqiao Cable Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Anhui Jinqiao Cable Co Ltd filed Critical Anhui Jinqiao Cable Co Ltd
Priority to CN201210435490.9A priority Critical patent/CN102977609B/zh
Publication of CN102977609A publication Critical patent/CN102977609A/zh
Application granted granted Critical
Publication of CN102977609B publication Critical patent/CN102977609B/zh
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

本发明提供了一种船用耐油耐低温低烟无卤阻燃电缆料,由下列重量份的原料制成:聚氨基甲酸酯20-30份、甲基乙烯基硅橡胶60-80、丁腈橡胶8-10、氢氧化镁8-10份、硬脂酸丁酯0.5-1.0份、硬脂酸钡1-3、三甘醇二异辛酸酯8-12份、氧化铜4-6份、三氧化钼0.5-1.0份、气相白炭黑30-50份、改性陶土10-13、防老剂H0.5-1.0份、防老剂AW0.1-0.3份、促进剂NOBS0.5-1.5份、硫化剂DCBP0.2-0.5、磷酸三苯酯8-10、三氧化二锑12-15、水合硼酸锌6-8。本发明的电缆料不仅具有优异阻燃性和不延燃性;燃烧时发烟量非常少,不产生有毒气体,不产生腐蚀性气体,而且同时具有良好的耐低温、耐油性、耐磨性。

Description

一种船用耐油耐低温低烟无卤阻燃电缆料及其制备方法
技术领域
  本发明涉及电缆料领域,具体涉及一种船用耐油耐低温低烟无卤阻燃电缆料及其制备方法。
背景技术
 随着全球经济的迅猛发展,及人类环保意识的增强,各领域对电线电缆的质量和性能的要求越来越高,因电线、电缆的老化而引发的火灾也越来越多,如何降低火灾的发生率及发生火灾的时的死亡率,低烟、无卤、阻燃、环保也成为电线电缆行业的发展方向。其中无卤低烟阻燃电缆料的需求量越来越大,目前无卤低烟阻燃电缆料的生产大多是在聚烯烃基材中加入大量的氢氧化镁或氢氧化镁来达到阻燃效果,然而,大量无机材料的加入,影响了电缆料的物理机械性能和加工工艺性能,其在常温下柔软性能 、耐气候性差、耐油性、耐低温性能都不是很好。
发明内容
本发明提供了一种船用耐油耐低温低烟无卤阻燃电缆料及其制备方法。
 本发明采用的技术方案为:
一种船用耐油耐低温低烟无卤阻燃电缆料,其特征在于:由下列重量份的原料制成:聚氨基甲酸酯 20-30份、甲基乙烯基硅橡胶60-80、丁腈橡胶8-10、氢氧化镁8-10份、硬脂酸丁酯0.5-1.0份、硬脂酸钡1-3、三甘醇二异辛酸酯 8-12份、氧化铜 4-6份、三氧化钼0.5-1.0份、气相白炭黑 30-50份、改性陶土10-13、防老剂H 0.5 -1.0份、防老剂AW 0.1-0.3份、促进剂NOBS 0.5-1.5份、硫化剂DCBP 0.2-0.5、磷酸三苯酯8-10、三氧化二锑12-15、水合硼酸锌6-8。 
所述的改性陶土通过以下方法制备:
(1)、陶土用10-15%盐酸浸泡3-4小时,去离子水洗涤,再用10-12%双氧水溶浸液泡3-4小时,再用去离子水洗涤至中性,烘干;
(2)、将溶于陶土加入水中,再加入相当于陶土重量2-3%的月桂醇硫酸钠、1-2%的氧化锌、2-3%的硅藻土、3-5%氢氧化铝,高速1200-1500转/分搅拌,得到分散液,分散液烘干粉碎成超细粉末
所述的船用耐油耐低温低烟无卤阻燃电缆料,其特征在于:由下列重量份的原料制成:聚氨基甲酸酯 25份、甲基乙烯基硅橡胶70、丁腈橡胶15、氢氢氧化镁9份、硬脂酸丁酯0.6份、硬脂酸钡2、三甘醇二异辛酸酯10份、氧化铜 5份、三氧化钼0.8份、气相白炭黑40份、改性陶土12、防老剂H 0.8份、防老剂AW 0.2份、促进剂NOBS 0.8份、硫化剂DCBP 0.4、磷酸三苯酯9、三氧化二锑14、水合硼酸锌7。
所述的船用耐油耐低温低烟无卤阻燃电缆料的制备方法,其特征在于:
(1)按配方比例将聚氨基甲酸酯、甲基乙烯基硅橡胶、丁腈橡胶和防老剂类投入开炼机,在80-95℃下混炼3-4分钟;
(2)将改性陶土、氧化铜、气相白炭黑等填料加入到步骤(1)的混炼胶中,继续混炼2-3分钟后,将除硫化剂、促进剂外的剩下的物料加入到混炼料中,混炼4-6分钟后,再加入硫化剂、促进剂,薄通6-7次后,挤塑机塑化造粒,即可,挤塑机的挤出温度为120-165℃。
有益效果
本发明的电缆料不仅具有优异阻燃性和不延燃性;燃烧时发烟量非常少,不产生有毒气体,不产生腐蚀性气体,而且同时具有良好的耐低温、耐油性、耐磨性。 
具体实施方式
船用耐油耐低温低烟无卤阻燃电缆料,由下列重量份的原料制成:聚氨基甲酸酯 25份、甲基乙烯基硅橡胶70、丁腈橡胶15、氢氢氧化镁9份、硬脂酸丁酯0.6份、硬脂酸钡2、三甘醇二异辛酸酯10份、氧化铜 5份、三氧化钼0.8份、气相白炭黑40份、改性陶土12、防老剂H 0.8份、防老剂AW 0.2份、促进剂NOBS 0.8份、硫化剂DCBP 0.4、磷酸三苯酯9、三氧化二锑14、水合硼酸锌7。
所述的改性陶土通过以下方法制备:
(1)、陶土用10-15%盐酸浸泡3-4小时,去离子水洗涤,再用10-12%双氧水溶浸液泡3-4小时,再用去离子水洗涤至中性,烘干;
(2)、将溶于陶土加入水中,再加入相当于陶土重量2-3%的月桂醇硫酸钠、1-2%的氧化锌、2-3%的硅藻土、3-5%氢氧化铝,高速1200-1500转/分搅拌,得到分散液,分散液烘干粉碎成超细粉末
制备方法:
(1)按配方比例将聚氨基甲酸酯、甲基乙烯基硅橡胶、丁腈橡胶和防老剂类投入开炼机,在80-95℃下混炼3-4分钟;
(2)将改性陶土、氧化铜、气相白炭黑等填料加入到步骤(1)的混炼胶中,继续混炼2-3分钟后,将除硫化剂、促进剂外的剩下的物料加入到混炼料中,混炼4-6分钟后,再加入硫化剂、促进剂,薄通6-7次后,挤塑机塑化造粒,即可,挤塑机的挤出温度为120-165℃。
用本实施例加工好的电缆料压制成试片经160℃×40min热老化后,测得其性能如下:
项目 结果
抗张强度   MPa     10.5
断裂伸长率  %     360
体积电阻率   Ω.cm     6.5×1012
氧指数% 39
135℃×168h热老化后拉伸强度≥ 20.7MPa
单位质量烟密度 14.3g
热老化质量损失 ≤ 20.8g/m2

Claims (3)

1.一种船用耐油耐低温低烟无卤阻燃电缆料,其特征在于:由下列重量份的原料制成:聚氨基甲酸酯 20-30份、甲基乙烯基硅橡胶60-80、丁腈橡胶8-10、氢氧化镁8-10份、硬脂酸丁酯0.5-1.0份、硬脂酸钡1-3、三甘醇二异辛酸酯 8-12份、 氧化铜 4-6份、三氧化钼0.5-1.0份、气相白炭黑 30-50份、改性陶土10-13、防老剂H 0.5 -1.0份、防老剂AW 0.1-0.3份、促进剂NOBS 0.5-1.5份、硫化剂DCBP 0.2-0.5、磷酸三苯酯8-10、三氧化二锑12-15、水合硼酸锌6-8;
所述的改性陶土通过以下方法制备:
(1)、陶土用10-15%盐酸浸泡3-4小时,去离子水洗涤,再用10-12%双氧水溶浸液泡3-4小时,再用去离子水洗涤至中性,烘干;
(2)、将溶于陶土加入水中,再加入相当于陶土重量2-3%的月桂醇硫酸钠、1-2%的氧化锌、2-3%的硅藻土、3-5%氢氧化铝,高速1200-1500转/分搅拌,得到分散液,分散液烘干粉碎成超细粉末。
2.根据权利要求1所述的船用耐油耐低温低烟无卤阻燃电缆料,其特征在于:由下列重量份的原料制成:聚氨基甲酸酯 25份、甲基乙烯基硅橡胶70、丁腈橡胶15、氢氢氧化镁9份、硬脂酸丁酯0.6份、硬脂酸钡2、三甘醇二异辛酸酯10份、氧化铜 5份、三氧化钼0.8份、气相白炭黑40份、改性陶土12、防老剂H 0.8份、防老剂AW 0.2份、促进剂NOBS 0.8份、硫化剂DCBP 0.4、磷酸三苯酯9、三氧化二锑14、水合硼酸锌7。
3.一种如权利要求1或2所述的船用耐油耐低温低烟无卤阻燃电缆料的制备方法,其特征在于:
(1)按配方比例将聚氨基甲酸酯、甲基乙烯基硅橡胶、丁腈橡胶和防老剂类投入开炼机,在80-95℃下混炼3-4分钟;
(2)将改性陶土、氧化铜、气相白炭黑等填料加入到步骤(1)的混炼胶中,继续混炼2-3分钟后,将除硫化剂、促进剂外的剩下的物料加入到混炼料中,混炼4-6分钟后,再加入硫化剂、促进剂,薄通6-7次后,挤塑机塑化造粒,即可,挤塑机的挤出温度为120-165℃。
CN201210435490.9A 2012-11-05 2012-11-05 一种船用耐油耐低温低烟无卤阻燃电缆料及其制备方法 Active CN102977609B (zh)