CN102924833A - Vibration-attenuation damping rubber product - Google Patents

Vibration-attenuation damping rubber product Download PDF

Info

Publication number
CN102924833A
CN102924833A CN 201210485555 CN201210485555A CN102924833A CN 102924833 A CN102924833 A CN 102924833A CN 201210485555 CN201210485555 CN 201210485555 CN 201210485555 A CN201210485555 A CN 201210485555A CN 102924833 A CN102924833 A CN 102924833A
Authority
CN
China
Prior art keywords
carbon black
powder
rubber product
damping rubber
rubber
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN 201210485555
Other languages
Chinese (zh)
Inventor
武献成
武献忠
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
SHANDONG ZHONGCHENG RUBBER CO Ltd
Original Assignee
SHANDONG ZHONGCHENG RUBBER CO Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by SHANDONG ZHONGCHENG RUBBER CO Ltd filed Critical SHANDONG ZHONGCHENG RUBBER CO Ltd
Priority to CN 201210485555 priority Critical patent/CN102924833A/en
Publication of CN102924833A publication Critical patent/CN102924833A/en
Pending legal-status Critical Current

Abstract

The invention relates to a rubber product for an air conditioner or other similar occasions. A vibration-attenuation damping rubber product is composed of the following components by kilograms: 3-20 kg of butyl rubber, 0.08-4 kg of terpene resin, 0.42-2.5 kg of white carbon black, 0.5-5 kg of spraying carbon black, 0.5-7 kg of highly-wear-resistant carbon black, 6.5-25 kg of 1,3-butadiene, 0.5-1.8 kg of dioctyl ester, 0.1-0.4 kg of antiager, 1.8-50 kg of calcium carbonate or barite powder or lead powder or iron powder, and 0.2-10 kg of argil or barite powder or lead powder or iron powder. The technical scheme is reasonable in prescription, high in quality, resistant to temperature, good in performance and low in price.

Description

Damping rubber product
Technical field
The present invention relates to a kind of rubber item for conditioner or other similar applications.
Background technology
Damping rubber is mainly used in cooler compressor coupling components vibration damping, and this rubber of making is at present filled a prescription unreasonable, and quality is lower, high-low temperature resistant not, and price is higher.
Summary of the invention
The object of the invention is to avoid weak point of the prior art, and a kind of have snappiness, resistant of high or low temperature is good and price is lower damping rubber product are provided.
Can take following technical scheme to realize purpose.
Damping rubber product, by kilogram weight, consist of:
Isoprene-isobutylene rubber 3-20 terpine resin 0.08-4 white carbon black 0.42-2.5
Spray carbon black 0.5-5 high wear-resistant carbon black 0.5-7 1,3-butadiene 6.5-25
Dioctyl ester 0.05-1.8 anti-aging agent 0.1-0.4
Light beggar or ground barium sulfate or lead powder or iron powder 1.8-50
Potter's clay or ground barium sulfate or lead powder or iron powder 0.2-10.
Preparation technology: 1, with the open type rubber mixing machine with the isoprene-isobutylene rubber raw material bag roller of getting on the bus; 2, terpine resin and anti-aging agent are pulverized, 200 orders that sieve drop in the sizing material; 3, use white carbon black, wait additive and tackifier, dioctyl ester stirs the companion and adds gradually. treat all to add, adjust and roll roll spacing: thin-thick-thin-thick---; Be placed on not on the sticky paper depending on mixing getting off after evenly, advance Rubber Extruder further mixing, extrude the certain specification product through the shape of the mouth as one speaks.
The relative prior art of the technical program has following advantage and effect:
Prescription is reasonable, high-and low-temperature resistance, and performance is good and price is lower.
Embodiment
Embodiment 1, damping rubber product, by kilogram weight, consist of:
Isoprene-isobutylene rubber 3-20 terpine resin 0.08-4 white carbon black 0.42-2.5
Spray carbon black 0.5-5 high wear-resistant carbon black 0.5-7 1,3-butadiene 6.5-25
Dioctyl ester 0.05-1. anti-aging agent 0.1-0.4
Light beggar or ground barium sulfate or lead powder or iron powder 1.8-50
Potter's clay or ground barium sulfate or lead powder or iron powder 0.2-10.
Be fit to make various cooler compressor coupling components damping components.
Embodiment 2, be used for the process of preparing of described damping rubber product, 1, with the open type rubber mixing machine with the isoprene-isobutylene rubber raw material bag roller of getting on the bus; 2, terpine resin and anti-aging agent are pulverized, 200 orders that sieve drop in the sizing material; 3, use white carbon black, wait additive and tackifier, dioctyl ester stirs the companion and adds gradually. treat all to add, adjust and roll roll spacing: thin-thick-thin-thick---; Be placed on not on the sticky paper depending on mixing getting off after evenly, advance Rubber Extruder further mixing, extrude the certain specification product through the shape of the mouth as one speaks.
Embodiment 3, damping rubber product, on embodiment 1 plinth, by kilogram weight, consist of:
Isoprene-isobutylene rubber 5 terpine resins 0.24 white carbon black 1.8
Spray carbon black 3 high wear-resistant carbon blacks 2 1,3-butadienes 4
Dioctyl ester 1.8 anti-aging agent 0.12 200 order iron powder 40.
This rubber proportion 2.6 is particularly suitable for the cabinet air-conditioner compressor as connecting damping component.
Embodiment 4, damping rubber product, on embodiment 1 plinth, by kilogram weight, consist of:
Isoprene-isobutylene rubber 4 terpine resins 0.2 white carbon black 0.3
Spray carbon black 9 high wear-resistant carbon blacks 6 1,3-butadienes 6.5
Dioctyl ester 0.15 anti-aging agent 0.1 potter's clay 1.5
Light beggar 20.
This rubber proportion 1.3 is particularly suitable for split type window air conditioner, as connecting damping component.

Claims (1)

1. damping rubber product, it is characterized in that by kilogram weight, consist of: isoprene-isobutylene rubber 3-20 terpine resin 0.08-4 white carbon black 0.42-2.5 spray carbon black 0.5-5 high wear-resistant carbon black 0.5-71, the 3-divinyl 6.5-25 dioctyl ester 0.05-1.8 light beggar of anti-aging agent 0.1-0.4 or ground barium sulfate or lead powder or iron powder 1.8-50 potter's clay or ground barium sulfate or lead powder or iron powder 0.2-10.
CN 201210485555 2012-11-26 2012-11-26 Vibration-attenuation damping rubber product Pending CN102924833A (en)