CN102898908A - Waterproof coating - Google Patents
Waterproof coating Download PDFInfo
- Publication number
- CN102898908A CN102898908A CN2012103678417A CN201210367841A CN102898908A CN 102898908 A CN102898908 A CN 102898908A CN 2012103678417 A CN2012103678417 A CN 2012103678417A CN 201210367841 A CN201210367841 A CN 201210367841A CN 102898908 A CN102898908 A CN 102898908A
- Authority
- CN
- China
- Prior art keywords
- parts
- powder
- waterproof coating
- waterproof paint
- ethylene glycol
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
The invention discloses a waterproof coating, which comprises the following raw materials in parts by mass: 0.2 to 0.6 part of dibutyltin dilaurate, 1 to 3 parts of triethanolamine, 0.4 to 0.8 part of tributyl phosphate, 20 to 30 parts of quartz powder, 3 to 6 parts of stearic acid, 10 to 20 parts of polyvinyl alcohol, 3 to 5 parts of wollastonite powder, 4 to 6 parts of titanium white powder, 1 to 3 parts of talc powder, 2 to 4 parts of mica powder, 1 to 4 parts of carbon tetrachloride, 2 to 5 parts of ethylene glycol and 10 to 20 parts of soft water. The waterproof coating is convenient in construction, low in comprehensive manufacturing cost, environment-friendly, nontoxic and easy to clean.
Description
Technical field
The invention belongs to the clean-out system field, be specifically related to a kind of waterproof paint.
Background technology
At present, the water-proof material on the market is of a great variety, but the tar gas toxicity that some product volatilizees is large, the not easy-clear that has, and the then price that has is higher, and stability is also good not, uses inconvenience, can not satisfy the demands.
Summary of the invention
Goal of the invention: the present invention seeks to provides a kind of waterproof paint in order to solve the deficiency of existing waterproof paint.
Technical scheme: a kind of waterproof paint of the present invention comprises the raw material of following mass fraction: dibutyl tin laurate 0.2-0.6 part, trolamine 1-3 part, tributyl phosphate 0.4-0.8 part, silica powder 20-30 part, stearic acid 3-6 part, polyvinyl alcohol 10-20 part, wollastonite powder 3-5 part, titanium dioxide 4-6 part, talcum powder 1-3 part, mica powder 2-4 part tetracol phenixin 1-4 part, ethylene glycol 2-5 part and soft water 10-20 part.
Beneficial effect: waterproof paint of the present invention, not only easy construction, comprehensive cost are low, and environment-protecting asepsis, easy cleaning.
Embodiment
The invention will be further described below in conjunction with specific embodiment:
Embodiment 1
A kind of waterproof paint comprises the raw material of following mass fraction: 10 parts of 0.2 part of dibutyl tin laurate, 1 part of trolamine, 0.4 part of tributyl phosphate, 20 parts of silica powders, 3 parts of stearic acid, 10 parts of polyvinyl alcohol, 3 parts of wollastonite powder, 4 parts of titanium dioxides, 1 part of talcum powder, 1 part in 2 parts of tetracol phenixin of mica powder, 2 parts of ethylene glycol and soft water.
Embodiment 2
A kind of waterproof paint comprises the raw material of following mass fraction: 20 parts of 0.6 part of dibutyl tin laurate, 3 parts of trolamines, 0.8 part of tributyl phosphate, 30 parts of silica powders, 6 parts of stearic acid, 20 parts of polyvinyl alcohol, 5 parts of wollastonite powder, 6 parts of titanium dioxides, 3 parts of talcum powder, 4 parts in 4 parts of tetracol phenixin of mica powder, 5 parts of ethylene glycol and soft water.
Embodiment 3
A kind of waterproof paint comprises the raw material of following mass fraction: 15 parts of 0.4 part of dibutyl tin laurate, 2 parts of trolamines, 0.6 part of tributyl phosphate, 25 parts of silica powders, 4.5 parts of stearic acid, 15 parts of polyvinyl alcohol, 4 parts of wollastonite powder, 5 parts of titanium dioxides, 2 parts of talcum powder, 2.5 parts in 3 parts of tetracol phenixin of mica powder, 3.5 parts of ethylene glycol and soft water.
Claims (1)
1. a waterproof paint is characterized in that: the raw material that comprises following mass fraction in the described waterproof paint: dibutyl tin laurate 0.2-0.6 part, trolamine 1-3 part, tributyl phosphate 0.4-0.8 part, silica powder 20-30 part, stearic acid 3-6 part, polyvinyl alcohol 10-20 part, wollastonite powder 3-5 part, titanium dioxide 4-6 part, talcum powder 1-3 part, mica powder 2-4 part tetracol phenixin 1-4 part, ethylene glycol 2-5 part and soft water 10-20 part.