CN102814880A - 永久性不粘式塑料熔接模具及其焊接机 - Google Patents
永久性不粘式塑料熔接模具及其焊接机 Download PDFInfo
- Publication number
- CN102814880A CN102814880A CN2012102739485A CN201210273948A CN102814880A CN 102814880 A CN102814880 A CN 102814880A CN 2012102739485 A CN2012102739485 A CN 2012102739485A CN 201210273948 A CN201210273948 A CN 201210273948A CN 102814880 A CN102814880 A CN 102814880A
- Authority
- CN
- China
- Prior art keywords
- hot
- mold
- plastic welding
- polytetrafluoroethylene
- stick type
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
本发明涉及一种永久性不粘式塑料熔接模具,包括热模,热模上固定有用于对焊接件进行接触加热的聚四氟乙烯加热条。所述聚四氟乙烯加热条可以嵌入热模中通过螺钉固定;也可以采用如下结构固定:热模上表面制有工字槽,聚四氟乙烯加热条的下部制有与工字槽结构相配合的工字块,聚四氟乙烯加热条与热模之间通过工字块与工字槽的配合进行固定。本发明还记载了一种安装有上述永久性不粘式塑料熔接模具的接触式热板焊接机。本发明将铁弗龙制成条状固定在热模上,既防止了热模对塑料焊接件接触加热后粘上熔融塑料,又使得铁弗龙长期固定在热模上不会掉落,与现有技术相比,大幅提高了工作效率,并保证了塑料焊接产品的质量。
Description
技术领域
本发明及一种永久性不粘式塑料熔接模具及其焊接机,属于机械技术领域。
背景技术
现有的接触式热板焊接机,工作时其热模对塑料焊接件接触加热后,往往出现焊接件上的熔融塑料粘在金属加热筋上,使得加热筋和熔融塑料无法分离。即使强行拉开后,金属加热筋上也会粘贴上塑料,需要清理,降低了工作效率。为此,本申请人曾想出在热模的金属加热筋上涂上铁弗龙(聚四氟乙烯),利用铁弗龙的不粘性,在一定程度上解决了上述问题。但仍存在如下缺陷:涂在金属加热筋上的铁弗龙容易掉落,掉落后需要再往热模上涂铁弗龙,操作麻烦,工作效率还是比较低;而且操作人员不可能一直盯着热模,导致铁弗龙掉落后很难被发现,因此焊接件上的熔融塑料还是经常粘在热模上。
发明内容
针对现有技术中的缺陷,本发明提供一种对塑料焊接件接触加热后不会粘上熔融塑料的永久性不粘式塑料熔接模具及其焊接机。
为达到上述发明目的本发明所采用的技术方案是:
永久性不粘式塑料熔接模具,包括热模,其特征在于所述热模上固定有用于对焊接件进行接触加热的聚四氟乙烯加热条。
作为对上述技术方案的进一步优化,所述热模为铝模。
作为对上述技术方案的进一步优化,所述聚四氟乙烯加热条嵌入所述热模中,并通过螺钉进行固定。
作为对上述技术方案的进一步优化,所述热模上表面制有工字槽,所述聚四氟乙烯加热条下部制有与所述工字槽结构相配合的工字块,所述聚四氟乙烯加热条与所述热模之间通过所述工字块与所述工字槽的配合进行固定。
本发明还记载了一种接触式热板焊接机,其特征在于所述焊接机机架上安装有上述永久性不粘式塑料熔接模具。
本发明将铁弗龙制成条状固定在热模上,既防止了热模对塑料焊接件接触加热后粘上熔融塑料,又使得铁弗龙长期固定在热模上不会掉落,与现有技术相比,大幅提高了工作效率,并保证了塑料焊接产品的质量。
下面结合附图对本发明的实施方式做进一步说明。
附图说明
图1是本发明一种较佳实施方式的结构示意图;
图2是图1的俯视结构示意图;
图3是图2中A-A方向的剖视图;
图4是本发明另一种较佳实施方式的聚四氟乙烯加热条与热模固定结构的示意图。
具体实施方式
实施例一:
如图1-3所示,一种永久性不粘式塑料熔接模具,包括热模1,所述热模1上固定有用于对焊接件进行接触加热的聚四氟乙烯加热条2。其中的热模1为铝模。所述聚四氟乙烯加热条2嵌入所述热模1中,在聚四氟乙烯加热条2的侧向敲入螺钉3,通过螺钉3对热模1和聚四氟乙烯加热条2进行固定。
实施例二:
本实施例与实施例一的不同之处在于聚四氟乙烯加热条2与热模1的固定方式,其具体结构为:热模1上表面制有工字槽11,所述聚四氟乙烯加热条2下部制有与所述工字槽11结构相配合的工字块21,所述聚四氟乙烯加热条2与所述热模1之间通过所述工字块21与所述工字槽11的配合进行固定。
本发明还公开了一种接触式焊接机,所述焊接机机架上安装有上述任一实施例所描述的永久性不粘式塑料熔接模具。
以上详细描述了本发明的较佳具体实施例。应当理解,本领域的普通技术无需创造性劳动就可以根据本发明的构思作出诸多修改和变化。因此,凡本技术领域中技术人员依本发明的构思在现有技术的基础上通过逻辑分析、推理或者有限的实验可以得到的技术方案,皆应落入本发明的保护范围内。
Claims (5)
1.永久性不粘式塑料熔接模具,包括热模(1),其特征在于所述热模(1)上固定有用于对焊接件进行接触加热的聚四氟乙烯加热条(2)。
2.根据权利要求1所述的永久性不粘式塑料熔接模具,其特征在于所述热模(1)为铝模。
3.根据权利要求1所述的永久性不粘式塑料熔接模具,其特征在于所述聚四氟乙烯加热条(2)嵌入所述热模(1)中,并通过螺钉(3)进行固定。
4.根据权利要求1所述的永久性不粘式塑料熔接模具,其特征在于所述热模(1)上表面制有工字槽(11),所述聚四氟乙烯加热条(2)下部制有与所述工字槽(11)结构相配合的工字块(21),所述聚四氟乙烯加热条(2)与所述热模(1)之间通过所述工字块(21)与所述工字槽(11)的配合进行固定。
5.接触式热板焊接机,其特征在于所述焊接机机架上安装有上述任一权利要求所述的永久性不粘式塑料熔接模具。