Prior art keywords
impervious material
parts
seepage
preparation
viscosity
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Active
Application number
CN201210166839.3A
Other languages
English (en)
Other versions
CN102690079A (zh
Inventor
刘阳生
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Peking University
Original Assignee
Peking University
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Peking University filed Critical Peking University
Priority to CN201210166839.3A priority Critical patent/CN102690079B/zh
Publication of CN102690079A publication Critical patent/CN102690079A/zh
Application granted granted Critical
Publication of CN102690079B publication Critical patent/CN102690079B/zh
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Links

Images

Landscapes

  • Processing Of Solid Wastes (AREA)

Abstract

本发明公开了一种粘性防渗材料的制备方法及其用途。制备方法以粉煤灰0-5份、高岭土30-60份、膨润土40-80份、聚丙烯酸1-3份、聚丙烯酰胺0-3份、聚丙烯酸酯0-3份和十六烷基三甲基氯化铵0-2份为原料,用重量计,经充分搅拌混合均匀后即得到防渗材料,密度为1.15-1.20g/cm3。粘性防渗材料的用途,主要做“三明治”型防渗***的防渗材料。本发明优点是具有优异的防渗性能和自我修复功能,结构简单,价格便宜,施工方便,对环境不会造成二次污染。

Description

粘性防渗材料的制备方法及其用途
技术领域
本发明涉及环境保护材料的制备方法,具体地说是涉及一种粘性防渗材料的制备方法及其用途。
背景技术
随着我国城市化进程的加快以及经济的快速增长,城市垃圾、工业固体废物以及各种矿山固体废物的产生量与日俱增。城市垃圾填埋仍然是我国主要的垃圾处置方式。工业固体废物以及矿山固体废物中由于存在各种有害成分(如有机污染物、重金属等),填埋处置已经成为这两类固体废物的主要处置方式。
不管是城市垃圾填埋场还是工业固体废物、矿山固体废物填埋场,在封场之后均需要进行表面防渗覆盖和生态恢复。
目前常用的表层防渗***主要是由1.0-1.5mm厚低密度聚乙烯LDPE膜层和50cm厚粘土层组成。由于LDPE膜层通常由无数块小的LDPE膜拼接而成,既容易受到应力集中的破坏,也容易被生态修复***的树根扎破,使得整个防渗***在填埋场的后期运行过程中受到破坏,而且难以弥补,导致整个填埋场防身***的崩溃、渗滤液增多,对环境造成二次污染。
发明内容
本发明的目的在于克服现有技术中存在的不足之处,而提供了一种粘性防渗材料的制备方法及其用途,具有自我修复功能的粘性防渗***。
本发明目的可以通过下述方式来实现:粘性防渗材料的制备方法,该方法以粉煤灰0-5份、高岭土30-60份、膨润土40-80份、聚丙烯酸1-3份、聚丙烯酰胺0-3份、聚丙烯酸酯0-3份和十六烷基三甲基氯化铵0-2份为原料,用重量计,经充分搅拌混合均匀后即得到防渗材料,密度为1.15-1.20g/cm3
所述的粘性防渗材料的用途,主要做“三明治”型防渗***的防渗材料,它由两层压实粘土层和防渗材料层组成“三明治”型防渗结构:底部10-20cm压实粘土层、中间2-3cm防渗材料层、顶部10-20cm压实粘土层,防渗***的渗透系数1×10-10cm/s,用于各种固体废物填埋场的顶部防渗。
本发明与现有技术相比,具有如下优点:
(1)两层压实粘土层和防渗材料层组成“三明治”型防渗结构,渗透系数1×10-10cm/s,具有优异的防渗性能。
(2)“三明治”型防渗结构具有自我修复功能,在顶层粘土层出现穿孔的情况下,中间防渗材料能够吸水膨胀堵住漏洞。
(3)结构简单,价格便宜,施工方便,对环境不会造成二次污染。
附图说明
图1是本发明粘性防渗材料的制备方法示意图。
图中:1.顶部10-20cm压实粘土层,2.2-3cm防渗材料层,3.底部10-20cm压实粘土层,4.填埋的所要处理的废物层。
具体实施方式
下面列举3个实施例,对本发明加以进一步说明,但本发明不只限于这些实施例。
实施例1
粉煤灰1公斤、高岭土30公斤、膨润土80公斤、聚丙烯酸2公斤、聚丙烯酰胺2公斤、聚丙烯酸酯1公斤和十六烷基三甲基氯化铵2公斤为原料,经充分搅拌混合均匀后即得到防渗材料,密度为1.15g/cm3
实施例2
粉煤灰2公斤、高岭土60公斤、膨润土40公斤、聚丙烯酸1公斤、聚丙烯酸酯2公斤和十六烷基三甲基氯化铵2公斤为原料,经充分搅拌混合均匀后即得到防渗材料,密度为1.20g/cm3
实施例3
粉煤灰5公斤、高岭土40公斤、膨润土50公斤、聚丙烯酸2公斤、聚丙烯酰胺2公斤和十六烷基三甲基氯化铵2公斤为原料,经充分搅拌混合均匀后即得到防渗材料,密度为1.18g/cm3
粘性防渗材料的用途,如图1所示,在填埋的所要处理的废物层4的表面,铺设10-20cm厚的粘土层,粘土层含水率为20-23%,往返三次碾压压实,得到底部压实粘土层3;然后铺设2-3cm厚度的本发明的防渗材料2,最后铺设10-20cm厚的粘土层,含水率为20-23%,往返三次碾压压实,得到顶部压实粘土层1。这种“三明治”型粘性防渗***的渗透系数1×10-10cm/s。

Claims (2)

1.粘性防渗材料的制备方法,其特征在于:粘性防渗材料以粉煤灰1-5份、高岭土30-60份、膨润土40-80份、聚丙烯酸1-2份、聚丙烯酰胺0-2份、聚丙烯酸酯0-2份和十六烷基三甲基氯化铵2份为原料,用重量计,经充分搅拌混合均匀后即得到防渗材料,密度为1.15-1.20g/cm3
2.应用权利要求1所述的粘性防渗材料的用途,主要做“三明治”型防渗***的防渗材料,它由两层压实粘土层和防渗材料层组成的“三明治”型防渗结构:底部10-20cm压实粘土层、中间2-3cm防渗材料层、顶部10-20cm压实粘土层,防渗***的渗透系数1×10-10cm/s,用于各种固体废物填埋场的顶部防渗。
CN201210166839.3A 2012-05-25 2012-05-25 粘性防渗材料的制备方法及其用途 Active CN102690079B (zh)

Priority Applications (1)

Application Number Priority Date Filing Date Title
CN201210166839.3A CN102690079B (zh) 2012-05-25 2012-05-25 粘性防渗材料的制备方法及其用途

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
CN201210166839.3A CN102690079B (zh) 2012-05-25 2012-05-25 粘性防渗材料的制备方法及其用途

Publications (2)

Publication Number Publication Date
CN102690079A CN102690079A (zh) 2012-09-26
CN102690079B true CN102690079B (zh) 2014-03-26

Family

ID=46855837

Family Applications (1)

Application Number Title Priority Date Filing Date
CN201210166839.3A Active CN102690079B (zh) 2012-05-25 2012-05-25 粘性防渗材料的制备方法及其用途

Country Status (1)

Country Link
CN (1) CN102690079B (zh)

Families Citing this family (10)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN106047353A (zh) * 2016-05-31 2016-10-26 山东胜伟园林科技有限公司 一种含山楂粉的防渗材料及利用该防渗材料在盐碱地种植石榴的方法
CN107522459A (zh) * 2017-07-10 2017-12-29 浙江海洋大学 一种海泥合成的油罐地坪防渗材料及其制备方法
CN107500702A (zh) * 2017-07-10 2017-12-22 浙江海洋大学 一种临港大型原油油罐地坪自修复防渗材料及其制备方法
CN109653254B (zh) * 2017-08-06 2021-09-17 滕州道智盛智能科技有限公司 一种铺设垃圾填埋场防渗材料的方法
CN110564389A (zh) * 2018-06-06 2019-12-13 中国石油化工股份有限公司 疏水改性型吸水膨胀树脂及其制备方法
CN108996933B (zh) * 2018-09-27 2020-10-13 安徽建筑大学 一种基于建筑渣土的防渗材料及其制备方法
CN109572093A (zh) * 2018-12-29 2019-04-05 中国非金属矿工业有限公司 一种高耐蚀预水化型矿物防渗材料及其制备方法
CN109677040A (zh) * 2018-12-29 2019-04-26 中国非金属矿工业有限公司 一种抗冻型高耐蚀预水化矿物防渗材料及其制备方法
CN110683823B (zh) * 2019-11-21 2021-12-31 中蓝长化工程科技有限公司 一种盐湖盐田防渗剂及其制备与施工方法
CN112679139B (zh) * 2021-03-11 2021-05-25 湖南大学 一种耐酸碱型防渗pmsb材料及其制备方法

Citations (4)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN1243858A (zh) * 1999-06-28 2000-02-09 吉林大学 干旱、半干旱地防渗保水剂
CN1730552A (zh) * 2005-08-26 2006-02-08 郑州大学 一种热塑性极性聚合物/层状粘土纳米复合材料及其制备方法
CN101429434A (zh) * 2008-09-08 2009-05-13 梁劲松 一种土壤保水防渗剂
CN102154014A (zh) * 2011-03-04 2011-08-17 长沙理工大学 一种边坡土壤改性材料及其制备方法

Patent Citations (4)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN1243858A (zh) * 1999-06-28 2000-02-09 吉林大学 干旱、半干旱地防渗保水剂
CN1730552A (zh) * 2005-08-26 2006-02-08 郑州大学 一种热塑性极性聚合物/层状粘土纳米复合材料及其制备方法
CN101429434A (zh) * 2008-09-08 2009-05-13 梁劲松 一种土壤保水防渗剂
CN102154014A (zh) * 2011-03-04 2011-08-17 长沙理工大学 一种边坡土壤改性材料及其制备方法

Also Published As

Publication number Publication date
CN102690079A (zh) 2012-09-26

Similar Documents

Publication Publication Date Title
CN102690079B (zh) 粘性防渗材料的制备方法及其用途
CN103978025B (zh) 一种可以快速稳定化含铬土壤及生活垃圾的填埋方法
CN205530203U (zh) 废物利用的生活垃圾填埋场封场结构
CN103978024B (zh) 一种可以同步稳定化含铬土壤及生活垃圾的填埋方法
CN203200794U (zh) 一种以陈旧垃圾为库底的填埋场防渗结构
CN103922620B (zh) 一种以废物为基料的卫生填埋场覆盖材料
CN107503383A (zh) 一种用于垃圾填埋场底部防渗防污的多层复合衬垫***
CN102319713A (zh) 混合卫生垃圾的填埋方法
CN203125727U (zh) 再生骨料固定式设备
CN102442008A (zh) 全自动液压式垃圾成型环保机
CN104310815B (zh) 一种水泥
CN102515696A (zh) 城市综合垃圾处理及回收制砖工艺
CN103723786A (zh) 重金属污染物场地防渗墙体自修复方法
CN205002133U (zh) 一种方便清理煤灰的锅炉
CN104830396A (zh) 一种污泥清洁燃料的制备方法
CN202483059U (zh) 一种用于框架结构填充墙的墙板
CN211171474U (zh) 防污染的生活垃圾焚烧炉渣沥青路面结构
Ismail et al. Innovative green technology and products meeting geo-environmental challenges
CN203008217U (zh) 轻质复合实心墙板
CN204626473U (zh) 地下室顶板防水结构
CN203188252U (zh) 一种应用于煤化工行业蒸发塘的防渗结构
CN103866685B (zh) 一种垃圾焚烧发电厂的多功能上料栈桥
CN104671714A (zh) 再生混凝土生产工艺及其制品
CN201713924U (zh) 渗滤液导排管装置
Xiong et al. Technology and performance analysis of preventing surface subsidence by sealing and backfilling the goaf with Urban waste

Legal Events

Date Code Title Description
C06 Publication
PB01 Publication
C10 Entry into substantive examination
SE01 Entry into force of request for substantive examination
GR01 Patent grant
GR01 Patent grant