CN102671771A - Method for floating and separating zinc silicate and kutnahorite - Google Patents
Method for floating and separating zinc silicate and kutnahorite Download PDFInfo
- Publication number
- CN102671771A CN102671771A CN2012101331110A CN201210133111A CN102671771A CN 102671771 A CN102671771 A CN 102671771A CN 2012101331110 A CN2012101331110 A CN 2012101331110A CN 201210133111 A CN201210133111 A CN 201210133111A CN 102671771 A CN102671771 A CN 102671771A
- Authority
- CN
- China
- Prior art keywords
- mineral
- zinc
- zinc silicate
- mangandolomite
- scanned
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Abstract
The invention discloses a method for floating and separating zinc silicate and kutnahorite, wherein sodium carbonate is used as a pH value regulator, water glass and hydroxymethyl cellulose are used as inhibitor of manganese dolomite minerals, sodium sulphide is used as activator of zinc mineral silicates, and oxygen fossils preserved soap is used as collecting agent of the zinc mineral silicate. The method for floating and separating the zinc silicate and kutnahorite can float and separate the zinc silicate and the kutnahorite, and effectively recovers the zinc mineral silicate, and zinc concentrations having a mineral zinc content of 25.38%-26.75% and a recovery rate of 72.51%-76.44% is obtained through floatation separation under the conditions of 7.85%-10.39% of mineral zinc content.
Description
One, technical field
The present invention relates to a kind of floatation separating method for mineral, the flotation separation method of particularly a kind of zinc silicate and mangandolomite.
Two, background technology
In the FLOTATION SEPARATION process of zinc silicate mineral and mangandolomite, the floatability of mangandolomite and zinc silicate is approaching, causes its FLOTATION SEPARATION difficulty; Again since when broken, ore grinding manganese carbonate, dolomitic gangue mineral become very thin particle easily; Form a large amount of sludges, disturb the recovery of zinc silicate mineral, not only make the flotation flowsheet complex structure; Make that with medicament is many, production cost is high; Mineral processing automation is difficult to realize, causes the zinc silicate mineral rate of recovery not high, has also limited the development and utilization of zinc silicate.
Three, summary of the invention
The object of the present invention is to provide the flotation separation method of a kind of zinc silicate and mangandolomite, it can reclaim the zinc silicate mineral, obtains the higher grade and the rate of recovery.
The present invention adopts following technical scheme to achieve the above object: the flotation separation method of a kind of zinc silicate and mangandolomite; Adopt sodium carbonate do pH value adjust agent, waterglass and CMC as inhibitor, the vulcanized sodium of mangandolomite mineral do the zinc silicate mineral activator, make the collecting agent of zinc silicate mineral with oxidation paraffin wax soap, concrete steps and regime of agent are following:
(1) using during flotation sodium carbonate to transfer slurry pH is 9~10,
(2) with waterglass and CMC inhibitor as the mangandolomite mineral,
(3) make the activator of zinc silicate mineral with vulcanized sodium,
(4) in the floatation process; After ore ore grinding to mineral monomer dissociated; After adding sodium carbonate adjustment slurry pH and being 9~10, add waterglass and CMC inhibition mangandolomite mineral then, add vulcanized sodium again the zinc silicate mineral are carried out activation; The last cured soap of oxygenation fossil carries out collecting to the zinc silicate mineral and gets the zinc concentrate product
(4) the total consumption of medicament is:
Sodium carbonate 2000~4000g/t
Waterglass is roughly selected 1000~3000g/t and is scanned the selected 500~1000g/t of 300~600g/t
CMC roughly selects 200~300g/t and scans the selected 100~200g/t of 50~150g/t
Vulcanized sodium is roughly selected 1000~4000g/t and is scanned 500~2000g/t
Oxidation paraffin wax soap is roughly selected 400~500g/t and is scanned 100~200g/t
During use, said medicament is mixed with following concentration expressed in percentage by weight earlier:
Outstanding advantage of the present invention is:
1, zinc silicate is separated with the mangandolomite mineral floating, obtaining zinc content is 25.38%~26.75%, and the rate of recovery is 72.51%~76.44% zinc concentrate.
2, flowage structure of the present invention is simple, and dosing is few, and less energy consumption can reclaim resource comprehensive.
Four, the specific embodiment
Embodiment 1
1. raw mineral materials:
The content of zinc is 7.85% in the used raw mineral materials, manganese content is 1.73%, calcium carbonate content is 10.69%, magnesium carbonate content is 15.22%; Show through material phase analysis; Zinc mainly exists with the zinc silicate form, and gangue mineral mainly exists with carbonate form, and other has a small amount of silica mineral.
2. floating agent and operating condition:
Sodium carbonate 2000g/t
Waterglass is roughly selected 1000g/t and is scanned the selected 500g/t of 300g/t
CMC is roughly selected 200g/t and is scanned the selected 100g/t of 50g/t
Vulcanized sodium is roughly selected 1000g/t and is scanned 500g/t
Oxidation paraffin wax soap is roughly selected 400g/t and is scanned 100g/t
During use, said medicament is mixed with following concentration expressed in percentage by weight earlier:
After during flotation ore ore grinding to mineral monomer being dissociated; Adding sodium carbonate adjustment slurry pH is 9~10; In the floatation process; Add waterglass and CMC and suppress the mangandolomite mineral, add vulcanized sodium again the zinc silicate mineral are carried out activation, the last cured soap of oxygenation fossil carries out collecting to the zinc silicate mineral and gets the zinc concentrate product.Showing by above-mentioned technological parameter and medicament condition through test and can effectively reclaim the zinc silicate mineral, is being under 7.85% condition giving ore deposit zinc content, through one roughing scan for twice twice selected, obtaining zinc content is 25.38%, the zinc concentrate of the rate of recovery 72.51%.
Embodiment 2
1. raw mineral materials:
Zinc content is 10.39% in the used ore; Manganese content 2.42%, calcium carbonate content are 13.12%, magnesium carbonate content is 17.18%, and material phase analysis shows that zinc mainly exists with the zinc silicate form; Gangue mineral mainly exists with carbonate form, and other has a small amount of silica mineral.
2. floating agent and operating condition:
Sodium carbonate 4000g/t
Waterglass is roughly selected 3000g/t and is scanned the selected 1000g/t of 600g/t
CMC is roughly selected 300g/t and is scanned the selected 200g/t of 150g/t
Vulcanized sodium is roughly selected 4000g/t and is scanned 2000g/t
Oxidation paraffin wax soap is roughly selected 500g/t and is scanned 200g/t.
During use, said medicament is mixed with following concentration expressed in percentage by weight earlier:
After during flotation ore ore grinding to mineral monomer being dissociated; Adding sodium carbonate adjustment slurry pH is 9~10; In the floatation process; Add waterglass and CMC and suppress the mangandolomite mineral, add vulcanized sodium again the zinc silicate mineral are carried out activation, the last cured soap of oxygenation fossil carries out collecting to the zinc silicate mineral and gets the zinc concentrate product.Showing by above-mentioned technological parameter and medicament condition through test and can effectively reclaim the zinc silicate mineral, is being under 10.39% condition giving ore deposit zinc content, through one roughing scan for twice twice selected, obtaining zinc content is 26.75%, the zinc concentrate of the rate of recovery 76.44%.
Embodiment 3
1. raw mineral materials:
Zinc content is 8.57% in the used ore; Manganese content 2.04%, calcium carbonate content are 12.48%, magnesium carbonate content is 15.66%, and material phase analysis shows that zinc mainly exists with the zinc silicate form; Gangue mineral mainly exists with carbonate form, and other has a small amount of silica mineral.
2. floating agent and operating condition:
Sodium carbonate 3000g/t
Waterglass is roughly selected 2000g/t and is scanned the selected 700g/t of 500g/t
CMC is roughly selected 250g/t and is scanned the selected 150g/t of 100g/t
Vulcanized sodium is roughly selected 3000g/t and is scanned 1000g/t
Oxidation paraffin wax soap is roughly selected 450g/t and is scanned 150g/t.
During use, said medicament is mixed with following concentration expressed in percentage by weight earlier:
After during flotation ore ore grinding to mineral monomer being dissociated; Adding sodium carbonate adjustment slurry pH is 9~10; In the floatation process; Add waterglass and CMC and suppress the mangandolomite mineral, add vulcanized sodium again the zinc silicate mineral are carried out activation, the last cured soap of oxygenation fossil carries out collecting to the zinc silicate mineral and gets the zinc concentrate product.Showing by above-mentioned technological parameter and medicament condition through test and can effectively reclaim the zinc silicate mineral, is being under 8.57% condition giving ore deposit zinc content, through one roughing scan for twice twice selected, obtaining zinc content is 25.44%, the zinc concentrate of the rate of recovery 73.55%.
Claims (2)
1. the flotation separation method of zinc silicate and mangandolomite; It is characterized in that; This method adopt sodium carbonate do pH value adjust agent, waterglass and CMC as inhibitor, the vulcanized sodium of mangandolomite mineral do the zinc silicate mineral activator, make the collecting agent of zinc silicate mineral with oxidation paraffin wax soap, concrete steps and regime of agent are following:
(1) using during flotation sodium carbonate to transfer slurry pH is 9~10,
(2) with waterglass and CMC inhibitor as the mangandolomite mineral,
(3) make the activator of zinc silicate mineral with vulcanized sodium,
(4) in the floatation process; After ore ore grinding to mineral monomer dissociated; After adding sodium carbonate adjustment slurry pH and being 9~10, add waterglass and CMC inhibition mangandolomite mineral then, add vulcanized sodium again the zinc silicate mineral are carried out activation; The last cured soap of oxygenation fossil carries out collecting to the zinc silicate mineral and gets the zinc concentrate product
(5) the total consumption of medicament is:
Sodium carbonate 2000~4000g/t
Waterglass is roughly selected 1000~3000g/t and is scanned the selected 500~1000g/t of 300~600g/t
CMC is roughly selected 200~300g/t and is scanned the selected 100~200g/t of 50~150g/t
Vulcanized sodium is roughly selected 1000~4000g/t and is scanned 500~2000g/t
Oxidation paraffin wax soap is roughly selected 400~500g/t and is scanned 100~200g/t.