The formula of the tackiness agent of the fragrant use of a kind of novel system
Technical field
The invention belongs to novel material technical field of chemistry, relate to a kind of formula of tackiness agent of the fragrant use of a kind of novel system of utilizing plant sizing material to be mixed to be developed into.
Background technology
For many years, make fragrant adhesive therefor and mainly continue to use the fragrant plant tamanori of using of tradition system--be the sticky powder of elm skin, continuous expansion due to the fragrant industry of system, there is the situation that supply falls short of demand in the sticky powder of elm skin, in addition in recent years cultivated area fewer and feweri, close hillsides to facilitate afforestation, fell the reasons such as restricted, cause the source of goods in short supply, elm skin glues powder price increase, and fragrant cost is improved.For solving the source of the sticky powder of plant, reduce fragrant cost, the regeneration product of finding the sticky powder of new elm skin has become the task of top priority.
Summary of the invention
The present invention is in order to solve the sticky powder situation that supply falls short of demand of elm skin of the fragrant use of tradition system, designed the formula of the tackiness agent of the fragrant use of a kind of novel system, the tackiness agent that utilizes the sticking natural plant composition of tool and macromolecule component to be mixed into the fragrant use of system substitutes the sticky powder of elm skin, efficiently solves the sticky powder situation that supply falls short of demand of elm skin.
The technical solution used in the present invention is: the formula of the tackiness agent of the fragrant use of a kind of novel system, key is: above-mentioned tackiness agent be take white glue powder as base-material, be aided with wood powder, arborvitae powder, modified starch, methylcellulose gum and polyacrylamide and be mixed and form, in the formula of above tackiness agent, the weight percent of each moiety is respectively:
White glue powder 60 ~ 80%,
Wood powder 5 ~ 15%
Arborvitae powder 5 ~ 15%,
Modified starch 3 ~ 8%,
Methylcellulose gum 2 ~ 5%,
Polyacrylamide 3 ~ 7%.
The invention has the beneficial effects as follows: the tackiness agent that utilizes formula of the present invention to make has that the cold water of being dissolved in is fast, consumption is little, viscosity is high, thickening effectiveness is good, nontoxic, long preservative period, purposes is wide, cost is low, processing, accumulating, the advantage such as easy to use, is applicable to produce various incense products.
Embodiment
The formula of the tackiness agent of the fragrant use of a kind of novel system, importantly: above-mentioned tackiness agent be take white glue powder as base-material, be aided with wood powder, arborvitae powder, modified starch, methylcellulose gum and polyacrylamide and be mixed and form, in the formula of above tackiness agent, the weight percent of each moiety is respectively:
White glue powder 60 ~ 80%,
Wood powder 5 ~ 15%
Arborvitae powder 5 ~ 15%,
Modified starch 3 ~ 8%,
Methylcellulose gum 2 ~ 5%,
Polyacrylamide 3 ~ 7%.
In above-mentioned formula, the effect of major ingredient white glue powder is the viscosity that increases tackiness agent, and the effect of wood powder is the burning of supporting the fragrant bar made with its tackiness agent, has used in addition arborvitae powder in order to tart up in formula.
The model of described modified starch is WS-603.
In the formula of tackiness agent, the particle fineness of each moiety is not less than 80 orders.
In the specific implementation, respectively white glue powder, arborvitae powder, modified starch, methylcellulose gum, polyacrylamide and weighting agent pulverizing, processing grinding to particle fineness are not less than to 80 orders, wherein grinding temperature is below 200 ℃, the moisture of its each component should be controlled at below 10%, weighing to be in proportion mixed again forms, and the storage condition of the tackiness agent finished product that forms of being mixed is answered lucifuge, ventilation, dry.
Provide the specific embodiment that in tackiness agent, each component is measured by weight percentage below: