CN102492354B - 一种用于防盗门的水性烘烤涂料及其制备方法和应用 - Google Patents
一种用于防盗门的水性烘烤涂料及其制备方法和应用 Download PDFInfo
- Publication number
- CN102492354B CN102492354B CN201110379083.6A CN201110379083A CN102492354B CN 102492354 B CN102492354 B CN 102492354B CN 201110379083 A CN201110379083 A CN 201110379083A CN 102492354 B CN102492354 B CN 102492354B
- Authority
- CN
- China
- Prior art keywords
- weight
- water
- aminoresin
- baking
- paint
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Active
Abstract
Description
Claims (3)