CN102423798B - 一种过共晶Al-Si合金挤压铸造成型方法及其模具 - Google Patents
一种过共晶Al-Si合金挤压铸造成型方法及其模具 Download PDFInfo
- Publication number
- CN102423798B CN102423798B CN201110380589.9A CN201110380589A CN102423798B CN 102423798 B CN102423798 B CN 102423798B CN 201110380589 A CN201110380589 A CN 201110380589A CN 102423798 B CN102423798 B CN 102423798B
- Authority
- CN
- China
- Prior art keywords
- molten metal
- mould
- hypereutectic
- billet
- alloy
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Abstract
Description
Claims (7)