CN102059514A - Processing method of small-curvature and small-angle bent pipe - Google Patents
Processing method of small-curvature and small-angle bent pipe Download PDFInfo
- Publication number
- CN102059514A CN102059514A CN 201010556899 CN201010556899A CN102059514A CN 102059514 A CN102059514 A CN 102059514A CN 201010556899 CN201010556899 CN 201010556899 CN 201010556899 A CN201010556899 A CN 201010556899A CN 102059514 A CN102059514 A CN 102059514A
- Authority
- CN
- China
- Prior art keywords
- pipe
- small
- dried shrimp
- straight
- angle
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Abstract
The invention discloses a processing method of a small-curvature and small-angle bent pipe, which is characterized by comprising the following steps of: firstly replacing each straight pipe-section shrimp pipe by a circular-arc section, and segmenting the processed bent pipe into straight-pipe sections; marking a projection center line a, an outer side contour line b1, an inner side contour line b2 and a port line c of each straight pipe-section shrimp pipe for assembling the bent pip by using the processed member on a steel plate platform; sequentially positioning each straight pipe-section shrimp pipe from middle to both sides by using an angle rule; finally welding the neighboring straight pipe-section shrimp pipes in the integrally positioned straight pipe-section shrimp pipes to accomplish the connection between the neighboring straight pipe-section shrimp pipes; and then polishing edges of welding lines into smooth transition. In the method, the plurality of straight pipe-section shrimp pipes replace the circular-arc sections, the assembly of the small-curvature and small-angle bent pipe is accomplished by cutting, scribing and positioning, therefore the method is simple and rapid, and the processed small-curvature and small-angle bent pipe is especially suitable for serving as a transition section at the crossed position of two small-angle steel pipes.
Description
Technical field
The present invention relates to a kind of processing method of small curve low-angle bend pipe.
Background technology
As shown in Figure 1, the small curve low-angle bend pipe in the steel member is meant that generally material is Q345B and following grade, radius of curvature R≤500mm, angle≤50 °, the pipe fitting that can not bend in existing bending machine.
Existing pipe bending machine can only be processed the bend pipe of radius of curvature R 〉=1500mm, can't carry out the processing of small curve low-angle bend pipe; Customization must become steel-casting with molten steel casting, but this method cycle is long, expense is high.
Summary of the invention
The present invention is for avoiding above-mentioned existing in prior technology weak point, a kind of processing method of small curve low-angle bend pipe is provided so that in the specific occasion for radius of curvature R≤500mm, the processing of the bend pipe of angle≤50 ° is more quick, low-cost.
The present invention adopts following technical scheme for the technical solution problem:
The design feature of the processing method of small curve low-angle bend pipe of the present invention is to carry out as follows:
A, replace arc section with each straight length dried shrimp pipe, processed bend pipe segmentation is drawn materials is each straight length;
B, for each straight length, the length of cutting away 2mm at left end is as the fit-up gap, and forms flat mouthful of end of left end; Right-hand member cutting at each straight section forms 35 ° of periphery grooves;
C, on plate platform, mark projected centre lines a, outboard wheel profile b1, nearside wheel profile b2 and the port lines c of each the straight length dried shrimp pipe that is used to assemble bend pipe by work piece;
D, utilize angle square that each straight section dried shrimp pipe is positioned toward both sides successively from middle; During the location, aim at port lines with flat mouthful of end, and firm with plate platform spot welding, finish the integral body location of each straight section dried shrimp pipe on plate platform according to this, form the fit-up gap between the adjacent straight section dried shrimp pipe;
E is welding on the fit-up gap between the described adjacent straight section dried shrimp pipe for each straight section dried shrimp pipe of integral body location, finishes between the adjacent straight section dried shrimp pipe to connect; Again the weld seam corner angle are polished into rounding off.
The characteristics of the processing method of small curve low-angle bend pipe of the present invention also are among the described step c, and the mark on plate platform is, at first press the circular arc line, mark each straightway by Along ent again.
Compared with the prior art, beneficial effect of the present invention is embodied in:
The present invention replaces arc section with many straight sections dried shrimp pipe, finishes small curve low-angle bend pipe by cutting, line and location assembling, and the inventive method is simple, quick, is particularly suitable for as two low-angle steel pipe intersection changeover portions.
Description of drawings
Fig. 1 is work piece schematic diagram among the present invention.
Fig. 2 is a light plate platform mark schematic diagram of the present invention.
Fig. 3 is each straight section dried shrimp pipe location schematic diagram among the present invention.
Fig. 4 welds schematic diagram for finishing between each straight section dried shrimp pipe among the present invention.
Number in the figure: 1 processed bend pipe, 2 plate platform, a projected centre lines, b1 outboard wheel profile, b2 nearside wheel profile, c port lines, 3 angle squares.
The specific embodiment
The processing method of small curve low-angle bend pipe is to carry out as follows in the present embodiment:
1, replace arc section with each straight length dried shrimp pipe, processed bend pipe 1 segmentation is drawn materials is each straight length;
B, for each straight length, the length of cutting away 2mm at left end is as the fit-up gap, and forms flat mouthful of end of left end; Right-hand member cutting at each straight section forms 35 ° of periphery grooves;
C, as shown in Figure 2 on plate platform 2, marks projected centre lines a, outboard wheel profile b1, nearside wheel profile b2 and the port lines c of each the straight length dried shrimp pipe that is used to assemble bend pipe by work piece; Specifically the mark on plate platform is, at first presses the circular arc line, marks each straightway by Along ent again; The relevant parameter of processed bend pipe 2 shown in Figure 2: R200 is that dried shrimp center line curvature, H are that the location height of right output port, location that L is right output port are wide, the dried shrimp angle is that 35 °, external diameter are that 203mm, wall thickness are 12mm;
D, utilize 3 pairs of each straight section dried shrimp pipes of angle square to position successively toward both sides from middle; During the location, aim at port lines with flat mouthful of end, and firm with plate platform 2 spot welding, finish the integral body location of each straight section dried shrimp pipe on plate platform 2 according to this, form the fit-up gap between the adjacent straight section dried shrimp pipe;
E is for each straight section dried shrimp pipe of integral body location, welding on the fit-up gap between the adjacent straight section dried shrimp pipe, at first finish the welding of a side, the weld seam that digs dried shrimp pipe and plate platform spot welding place with carbon digs then, the dried shrimp pipe is stood up the fit-up gap of the other side of welding, and then finish overall welding; Again the weld seam corner angle are polished into rounding off at last.
In concrete the enforcement, should note:
1, get many straight lengths, corner angle are just more little so as far as possible, cross and get over slyness;
2, guarantee the internal orifice of each straight length, promptly the minor face of straight length also has 2 centimeters length after cutting periphery groove.
Claims (2)
1. the processing method of small curve low-angle bend pipe is characterized in that carrying out as follows:
A, replace arc section with each straight length dried shrimp pipe, processed bend pipe segmentation is drawn materials is each straight length;
B, for each straight length, the length of cutting away 2mm at left end is as the fit-up gap, and forms flat mouthful of end of left end; Right-hand member cutting at each straight section forms 35 ° of periphery grooves;
C, on plate platform, mark projected centre lines a, outboard wheel profile b1, nearside wheel profile b2 and the port lines c of each the straight length dried shrimp pipe that is used to assemble bend pipe by work piece;
D, utilize angle square that each straight section dried shrimp pipe is positioned toward both sides successively from middle; During the location, aim at port lines with flat mouthful of end, and firm with plate platform spot welding, finish the integral body location of each straight section dried shrimp pipe on plate platform according to this, form the fit-up gap between the adjacent straight section dried shrimp pipe;
E, for each straight section dried shrimp pipe of integral body location, welding on the fit-up gap between the described adjacent straight section dried shrimp pipe, finish between the adjacent straight section dried shrimp pipe and connect; Again the weld seam corner angle are polished into rounding off.
2. the processing method of small curve low-angle bend pipe according to claim 1 is characterized in that among the described step c, and the mark on plate platform is, at first presses the circular arc line, marks each straightway by Along ent again.