cavity
joggle
battery case
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Active
Application number
CN 200910180047
Other languages
English (en)
Other versions
CN101704048A (zh
Inventor
周勤勇
杨建林
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Wuxi Jinyang New Materials Co., Ltd.
Original Assignee
WUXI CITY JINGYANG NEW TYPE POWER SUPPLY CO Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by WUXI CITY JINGYANG NEW TYPE POWER SUPPLY CO Ltd filed Critical WUXI CITY JINGYANG NEW TYPE POWER SUPPLY CO Ltd
Priority to CN 200910180047 priority Critical patent/CN101704048B/zh
Publication of CN101704048A publication Critical patent/CN101704048A/zh
Application granted granted Critical
Publication of CN101704048B publication Critical patent/CN101704048B/zh
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Links

Images

Landscapes

  • Sealing Battery Cases Or Jackets (AREA)

Abstract

一种阶梯模具冲压薄壁电池壳的工艺及阶梯模具,将坯料切成圆形的毛坯,将毛坯安装在阶梯模具上,通过阶梯模具冲压形成电池壳的外壳,通过圆柱状的冲杆冲压阶梯上凹模和阶梯下凹模的圆形模腔,将毛坯从阶梯下凹模的圆形模腔中冲压出来,所述圆柱状的冲杆上具有环切凹槽,同时在阶梯上凹模和阶梯下凹模的交界处形成圆弧过渡带,过渡带的下部壳体的壁厚较薄,过渡带的上部壳体壁厚较厚,但整个壳体的内径是相同的,这样也就在保证了整体强度的前提下,可以节省生产下部壳体所需要的材料,节省了材料成本,并使材料的相对电池容量增大。

Description

一种阶梯模具冲压薄壁电池壳的工艺及阶梯模具
技术领域
本发明涉及一种电池壳的生产工艺,具体的说是一种采用冲压模具生产薄壁电池壳的工艺。
背景技术
传统的压铸模具包括普通的型模、锻压模和一些特殊的模具如挤压模、拔模等。本发明设计了一种新型的阶梯状冲压模具。
常用的模具所生产的电池壳的壁厚较大,一般为壁厚均匀的电池壳。但经过研究发现,电池壳的开口处需要向内折边,一般对结构的强度要求较大,而电池壳的大部分壳体除了承受电池材料的张力外,不承受其他结构应力。所以在生产的过程中是可以将电池壳的壳体部分的壁厚设计成比开口处的壁厚更薄的结构,在保证开口处的结构强度的条件下即可满足电池壳的使用需要。而与此同时,如果降低了壁厚也可以节省生产电池壳所需要的耗材,并且相对的增加了电池壳的内部容量,增大了电池的电量。
发明内容
本发明的目的是提供一种阶梯模具冲压薄壁电池壳的工艺及阶梯模具,采用新型的冲压方式成型电池壳。
本发明的目的是通过以下技术方案来实现:
一种阶梯模具冲压薄壁电池壳的工艺,将坯料切成圆形的毛坯,将毛坯安装在阶梯模具上,通过阶梯模具冲压形成电池壳的外壳,通过圆柱状的冲杆冲压阶梯上凹模和阶梯下凹模的圆形模腔,将毛坯从阶梯下凹模的圆形模腔中冲压出来,所述圆柱状的冲杆上具有环切凹槽,同时在阶梯上凹模和阶梯下凹模的交界处形成圆弧过渡带,过渡带的下部壳体的壁厚较薄,过渡带的上部壳体壁厚较厚,但整个壳体的内径是相同的,这样也就在保证了整体强度的前提下,可以节省生产下部壳体所需要的材料,节省了材料成本,并使材料的相对电池容量增大,同时圆弧过渡带可以解决应力集中带来的结构问题。
上述工艺所采用的冲压电池壳的阶梯模具,包括阶梯上凹模、阶梯下凹模和冲杆,阶梯上凹模和阶梯下凹模有对接平面,对接平面是阶梯上凹模的下表面和阶梯下凹模的上表面,阶梯上凹模和阶梯下凹模的对应位置设有同心的圆形模腔,圆形模腔用于冲压使用,并且阶梯上凹模的圆形模腔的孔径略大于阶梯下凹模的圆形模腔的孔径,阶梯上凹模的圆形模腔用于固定电池壳的坯料,阶梯下凹模的圆形模腔用于支撑坯料并且配合冲杆成型电池壳,所述冲杆冲压坯料进入圆形模腔中,冲杆的外径小于圆形模腔的孔径,冲杆外径与阶梯下凹模的圆形模腔的距离就是所要成型的电池壳的厚度。
附图说明
下面根据附图和实施例对本发明作进一步详细说明。
图1是本发明实施例所述的阶梯模具冲压薄壁电池壳的工艺的阶梯上凹模和阶梯下凹模外形结构图;
图2是本发明所述的冲杆的结构图;
图3是本发明所述的薄壁电池壳的结构图。
图中:
1、阶梯上凹模;2、阶梯下凹模;3、冲杆;4、圆形模腔;5、凹槽;6、薄壁电池壳。
具体实施方式
如图3所示,本发明所述的阶梯模具冲压薄壁电池壳6的工艺,将坯料切成圆形的毛坯,将毛坯安装在阶梯模具上,通过阶梯模具冲压形成电池壳的外壳,通过圆柱状的冲杆冲压阶梯上凹模和阶梯下凹模的圆形模腔,将毛坯从阶梯下凹模2的圆形模腔4中冲压出来,所述圆柱状的冲杆3上具有环切凹槽5,同时在阶梯上凹模1和阶梯下凹模2的交界处形成圆弧过渡带,过渡带的下部壳体6的壁厚较薄,过渡带的上部壳体6壁厚较厚,但整个壳体6的内径是相同的,这样也就在保证了整体强度的前提下,可以节省生产下部壳体所需要的材料,节省了材料成本,并使材料的相对电池容量增大,同时圆弧过渡带可以解决应力集中带来的结构问题。
如图1所示,本发明所述的阶梯模具冲压薄壁电池壳的工艺,包括阶梯上凹模1、阶梯下凹模2和冲杆3,阶梯上凹模1和阶梯下凹模2有对接平面,对接平面是阶梯上凹模的下表面和阶梯下凹模的上表面,阶梯上凹模1和阶梯下凹模2的对应位置设有同心的圆形模腔4,圆形模腔4用于冲压使用,并且阶梯上凹模1的圆形模腔4的孔径A略大于阶梯下凹模2的圆形模腔4的孔径B,阶梯上凹模1的圆形模腔用于固定电池壳的坯料,阶梯下凹模2的圆形模腔4用于支撑坯料并且配合冲杆3成型电池壳,所述冲杆3冲压坯料进入圆形模腔4中,冲杆3的外径小于圆形模腔的孔径,冲杆3外径与阶梯下凹模的圆形模腔4的距离就是所要成型的电池壳的厚度。
如图2所示,本发明所述的冲杆3为圆柱形。并在圆柱形的冲杆3上环切凹槽5。
本发明设计的阶梯模可以实现对电池壳6的冲压成型,并且可以实现电池壳的多种结构成型,特别是可以实现薄壁电池壳6的成型。与通常所用的成型方法相比,本发明设计的阶梯模可以节省电池壳的耗材,并且可以增大电池壳内的装料空间,提高电池的容量。

Claims (2)

1.一种阶梯模具冲压薄壁电池壳的工艺,将坯料切成圆形的毛坯,将毛坯安装在阶梯模具上,通过阶梯模具冲压形成电池壳的外壳,通过圆柱状的冲杆冲压阶梯上凹模和阶梯下凹模的圆形模腔,将毛坯从阶梯下凹模的圆形模腔中冲压出来,所述圆柱状的冲杆上具有环切凹槽,同时在阶梯上凹模和阶梯下凹模的交界处形成圆弧过渡带,过渡带的下部壳体的壁厚较薄,过渡带的上部壳体壁厚较厚,但整个壳体的内径是相同的。
2.根据权利要求1所述的阶梯模具冲压薄壁电池壳的工艺,其特征在于,所采用的阶梯模具包括阶梯上凹模、阶梯下凹模和冲杆,阶梯上凹模和阶梯下凹模有对接平面,对接平面是阶梯上凹模的下表面和阶梯下凹模的上表面,阶梯上凹模和阶梯下凹模的对应位置设有同心的圆形模腔,并且阶梯上凹模的圆形模腔的孔径略大于阶梯下凹模的圆形模腔的孔径,所述冲杆冲压坯料进入圆形模腔中,冲杆的外径小于圆形模腔的孔径。
CN 200910180047 2009-10-26 2009-10-26 一种阶梯模具冲压薄壁电池壳的工艺及阶梯模具 Active CN101704048B (zh)

Priority Applications (1)

Application Number Priority Date Filing Date Title
CN 200910180047 CN101704048B (zh) 2009-10-26 2009-10-26 一种阶梯模具冲压薄壁电池壳的工艺及阶梯模具

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
CN 200910180047 CN101704048B (zh) 2009-10-26 2009-10-26 一种阶梯模具冲压薄壁电池壳的工艺及阶梯模具

Publications (2)

Publication Number Publication Date
CN101704048A CN101704048A (zh) 2010-05-12
CN101704048B true CN101704048B (zh) 2013-04-10

Family

ID=42374339

Family Applications (1)

Application Number Title Priority Date Filing Date
CN 200910180047 Active CN101704048B (zh) 2009-10-26 2009-10-26 一种阶梯模具冲压薄壁电池壳的工艺及阶梯模具

Country Status (1)

Country Link
CN (1) CN101704048B (zh)

Families Citing this family (3)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN104942112B (zh) * 2015-07-08 2017-01-18 哈尔滨工业大学 一种多杆施力的薄壁坯料逐步成形方法
CN107199287B (zh) * 2017-01-25 2019-12-10 蔡振豪 一种手机外壳的制造方法及专用模具
CN108213158A (zh) * 2017-12-25 2018-06-29 东莞捷荣技术股份有限公司 基于手机电池盖侧壁变薄的冲压成型方法、电池盖及手机

Citations (4)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN1432199A (zh) * 2000-05-26 2003-07-23 吉莱特公司 成形一个电化电池外壳的方法
CN1519965A (zh) * 2003-02-04 2004-08-11 ʯ����ƹ�ҵ��ʽ���� 电池用负极罐及其制造方法
CN101208817A (zh) * 2005-07-21 2008-06-25 松下电器产业株式会社 电池罐及其制造方法
CN101259498A (zh) * 2007-03-06 2008-09-10 昭和电工包装株式会社 电池壳体的成形方法及成形装置

Patent Citations (4)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN1432199A (zh) * 2000-05-26 2003-07-23 吉莱特公司 成形一个电化电池外壳的方法
CN1519965A (zh) * 2003-02-04 2004-08-11 ʯ����ƹ�ҵ��ʽ���� 电池用负极罐及其制造方法
CN101208817A (zh) * 2005-07-21 2008-06-25 松下电器产业株式会社 电池罐及其制造方法
CN101259498A (zh) * 2007-03-06 2008-09-10 昭和电工包装株式会社 电池壳体的成形方法及成形装置

Also Published As

Publication number Publication date
CN101704048A (zh) 2010-05-12

Similar Documents

Publication Publication Date Title
CN101716627B (zh) 一种改进的用于密封环制造的级进连续冲压模具
CN202377371U (zh) 摆动式成形模
CN101704048B (zh) 一种阶梯模具冲压薄壁电池壳的工艺及阶梯模具
CN101704049B (zh) 一种阶梯模具冲压薄壁电池壳的工艺及阶梯模具
CN201693069U (zh) 一种用于密封环制造的级进连续冲压模具
CN201175727Y (zh) 电机壳体冷挤压成型模具
CN201644616U (zh) 汽车板簧卡子下料、冲孔复合模具
CN101704050B (zh) 一种阶梯模具冲压薄壁电池壳的工艺及阶梯模具
CN201543722U (zh) 一种冲压电池壳的阶梯模具
CN205613926U (zh) 一种端盖冲压模具
CN202155921U (zh) 车门内板锁孔模具
CN201768835U (zh) U铁翻边整形模
CN201768832U (zh) 一种用于制造异径管的模具组件
CN110814168A (zh) 一种用于制造dip-6838石英晶振外壳的精密模具
CN205967027U (zh) 一种闷盖成型模具
CN202861110U (zh) 一种高精度落料冲压结构
CN202037291U (zh) 冷挤压模具
CN101704053A (zh) 一种冲压电池壳的阶梯模具
CN110886756A (zh) 一种异形偏心销柱及其生产工艺
CN205926788U (zh) 一种新型模具成形兼反向冲孔机构
CN202021222U (zh) 一种电机壳体加工装置
CN201755658U (zh) 模具
CN220387796U (zh) 薄壁直排齿环体的冷镦组合模具
CN217018229U (zh) 一种冲压拉伸件模内定位机构
CN204234580U (zh) 一种汽车横梁模具

Legal Events

Date Code Title Description
C06 Publication
PB01 Publication
C10 Entry into substantive examination
SE01 Entry into force of request for substantive examination
C14 Grant of patent or utility model
GR01 Patent grant
CP01 Change in the name or title of a patent holder
CP01 Change in the name or title of a patent holder

Address after: 214117 6 Wuxi Road, Xishan, Jiangsu.

Patentee after: Wuxi Jinyang New Materials Co., Ltd.

Address before: 214117 6 Wuxi Road, Xishan, Jiangsu.

Patentee before: Wuxi City Jingyang New Type Power Supply Co., Ltd.