CN101585987A - Raw material prescription of the heat preserving waterproof paint and method of preparing the same - Google Patents
Raw material prescription of the heat preserving waterproof paint and method of preparing the same Download PDFInfo
- Publication number
- CN101585987A CN101585987A CNA2009102031802A CN200910203180A CN101585987A CN 101585987 A CN101585987 A CN 101585987A CN A2009102031802 A CNA2009102031802 A CN A2009102031802A CN 200910203180 A CN200910203180 A CN 200910203180A CN 101585987 A CN101585987 A CN 101585987A
- Authority
- CN
- China
- Prior art keywords
- parts
- waterproof paint
- insulating type
- thermal
- type waterproof
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
The invention belongs to a heat preserving waterproof paint for structures such as exterior wall of building, thin roofing, and metal tank housing and so on and fabricating method thereof. Raw material prescription of the heat preserving waterproof paint of the invention based on weight is: 10 parts to 90 parts of water, 10 parts to 90 parts of elastic polyacrylic emulsion, 10 parts to 50 parts of filler, 1 part to 10 parts of propylene glycol, 1 part to 10 parts of thickener, 1 part to 10 parts of rutile type titanium dioxide, 1 part to 3 parts of water- and stain-proofing agent of exterior wall. The paint of the invention is great in heat preservation, waterproofing property, self-cleaning property, filling property, radioresistance and sun protection and has long service life.
Description
Technical field
The invention belongs to a kind of structural thermal-insulating type waterproof paint and manufacture method thereof such as skin, slim roofing and metal can shell of being used for.
Background technology
Skin is subjected to weather temperature difference influences such as spring, summer, autumn, winter, daytime, night bigger, and natures such as frost, dew, mist corrode, wind, the complicated environmental conditions such as attack and UV sunlight radiation that drench with rain influence, objectively require insulation, the water-repellancy of skin higher, and the insulation with waterproof be two of different nature converse to kenel, waterproof type in the market or thermal-insulating type coating are more, but the net effect of its insulation, thermal insulation, waterproof is undesirable.
Summary of the invention
Purpose of the present invention provides a kind of heat retaining property, water-repellancy, self-cleaning, fillibility and radioprotective and sun-proof better performances, the thermal-insulating type waterproof paint and the manufacture method thereof of long service life.
Thermal-insulating type waterproof paint of the present invention, its starting raw material prescription is by weight:
10~90 parts in water
10~90 parts of elastomeric propylene yogurt liquid
10~50 parts of fillers
1~10 part of propylene glycol
1~10 part of thickening material
1~10 part of Rutile type Titanium Dioxide
1~30 part of external wall waterproof stain control agent
Described filler is at least a or multiple in lime carbonate, wilkinite, activated clay, silicon powder, talcum powder, polystyrene foam powder, wood shavings powder, the pearlstone.
Described thickening material is at least a or multiple in sodium polyacrylate, polyoxyethylene, polyvinylpyrrolidone, polyvinyl alcohol, low-molecular polyethylene wax, polyacrylamide, the Natvosol.
The making method of thermal-insulating type waterproof paint of the present invention may further comprise the steps:
A. will mix in 10~90 parts in water and 10~90 parts of suction multifunctional mixers of elastomeric propylene yogurt liquid, about rotating speed 250rpm, add 1~10 part of propylene glycol in batches, 1~10 part of Rutile type Titanium Dioxide, 1~10 part of 1~30 part of external wall waterproof stain control agent and filler, fully stirred 1~3 hour rotating speed 200~500rpm.
B. above-mentioned material is moved on to sand milling in the sealed horizontal formula sand mill, the sand milling while cooling off, staving pressure remains on about 0.1MPa in the sand mill, and sand milling finishes material is moved on in the multifunctional mixer, add 1~10 part of thickening material while stirring, obtain the thermal-insulating type waterproof paint after the increase denseness.
The invention has the advantages that films has performances such as sunlight reflectivity height, elasticity height, tension set are big, washability, anti-contamination, self-cleaning.Be used for structures such as skin, slim roofing and metal can shell, significantly improve buildings and metallic surface heat energy, play tangible effect of heat insulation to internal delivery.
The present invention has very strong energy-conservation effect, uses the skin coating of this coating, can make buildings at room temperature decline in summer 2-4 degree, and whole buildings is turned on the aircondition and saved 20% electric energy.Can save 30% heat energy winter in the north.
Thin coating film of the present invention just can produce a desired effect, and reduces construction cost significantly, is the higher multi-use architecture coating of cost performance in the like product.
Embodiment
Below in conjunction with example product of the present invention and method are described further.
Embodiment 1
With mixing in water 50kg and the elastomeric propylene yogurt liquid 100kg suction multifunctional mixer, about rotating speed 250rpm, add propylene glycol 5kg in batches, Rutile type Titanium Dioxide 6.5kg, external wall waterproof stain control agent 10kg and polystyrene foam powder 8kg fully stirred rotating speed 300rpm 2 hours.Above-mentioned material is moved on to sand milling in the sealed horizontal formula sand mill, the sand milling while cooling off, staving pressure remains on about 0.1MPa in the sand mill, and sand milling finishes material is moved on in the multifunctional mixer, add polyoxyethylene 2.5kg while stirring, obtain the thermal-insulating type waterproof paint after the increase denseness.
Embodiment 2
With mixing in water 60kg and the elastomeric propylene yogurt liquid 150kg suction multifunctional mixer, about rotating speed 250rpm, add propylene glycol 6kg in batches, Rutile type Titanium Dioxide 5kg, external wall waterproof stain control agent 10kg and pearlstone 8.5kg fully stirred rotating speed 400rpm 3 hours.Above-mentioned material is moved on to sand milling in the sealed horizontal formula sand mill, the sand milling while cooling off, staving pressure remains on about 0.1MPa in the sand mill, and sand milling finishes material is moved on in the multifunctional mixer, add Natvosol 3.5kg while stirring, obtain the thermal-insulating type waterproof paint after the increase denseness.
Claims (4)
1, a kind of thermal-insulating type waterproof paint is characterized in that the starting raw material recipe ingredient of this coating is by weight:
10~90 parts in water
10~90 parts of elastomeric propylene yogurt liquid
10~50 parts of fillers
1~10 part of propylene glycol
1~10 part of thickening material
1~10 part of Rutile type Titanium Dioxide
1~30 part of external wall waterproof stain control agent.
2, according to the described thermal-insulating type waterproof paint of claim 1, its characteristic is that filler is at least a or multiple in lime carbonate, wilkinite, activated clay, silicon powder, talcum powder, polystyrene foam powder, wood shavings powder, the pearlstone.
3, according to the described thermal-insulating type waterproof paint of claim 1, its characteristic is that thickening material is at least a or multiple in sodium polyacrylate, polyoxyethylene, polyvinylpyrrolidone, polyvinyl alcohol, low-molecular polyethylene wax, polyacrylamide, the Natvosol.
4, the manufacture method of the described thermal-insulating type waterproof paint of a kind of claim 1 is characterized in that: may further comprise the steps,
A. will mix in 10~90 parts in water and 10~90 parts of suction multifunctional mixers of elastomeric propylene yogurt liquid, about rotating speed 250rpm, add 1~10 part of propylene glycol in batches, 1~10 part of Rutile type Titanium Dioxide, 1~10 part of 1~30 part of external wall waterproof stain control agent and filler, fully stirred 1~3 hour rotating speed 200~500rpm.
B. above-mentioned material is moved on to sand milling in the sealed horizontal formula sand mill, the sand milling while cooling off, staving pressure remains on about 0.1MPa in the sand mill, and sand milling finishes material is moved on in the multifunctional mixer, add 1~10 part of thickening material while stirring, obtain the thermal-insulating type waterproof paint after the increase denseness.