Prior art keywords
steel plate
metal composite
board
main body
protective layer
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CNA2008101556457A
Other languages
English (en)
Inventor
杨建丰
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Changzhou Changsong Metal Composite Material Co Ltd
Original Assignee
Changzhou Changsong Metal Composite Material Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Changzhou Changsong Metal Composite Material Co Ltd filed Critical Changzhou Changsong Metal Composite Material Co Ltd
Priority to CNA2008101556457A priority Critical patent/CN101396886A/zh
Publication of CN101396886A publication Critical patent/CN101396886A/zh
Pending legal-status Critical Current

Links

Landscapes

  • Coating With Molten Metal (AREA)

Abstract

本发明涉及一种金属复合板,尤其是涉及一种铝锌金属复合钢板,其具有钢板主体,钢板主体外包覆有铝锌合金板耐蚀保护层,所述的铝锌合金板耐蚀保护层是由按重量百分比5%-25%的铝、1%-3%的镁、1.5%的硅、0.3%的稀土以及余量的锌合成的。该铝锌金属复合钢板在苛刻的腐蚀环境下仍能发挥其优异的耐腐蚀性,产品耐刮耐磨,能适应多种加工,使用寿命长,完全可以取代目前的采用先成形加工再经热浸镀锌的后浸镀金属板产品进行使用。

Description

铝锌金属复合钢板
技术领域
本发明涉及一种金属复合板,尤其是涉及一种铝锌金属复合钢板。
背景技术
提高钢板的耐蚀性的传统做法是在成形钢板上热浸镀锌。这种热浸镀锌板的耐腐蚀性能有限,使用寿命不长,不能够适应较为苛刻的腐蚀环境,且镀锌层的耐刮耐磨性不佳,很容易造成破损使得内层的钢板失去耐蚀层的保护。另外热浸镀锌的工艺也较复杂。
发明内容
本发明公开了一种铝锌金属复合钢板,其可以取代目前传统的热浸镀锌板进行使用,克服热浸镀锌板耐腐蚀性能有限、使用寿命短、不能够适应较为苛刻的腐蚀环境,且镀锌层耐刮耐磨性不佳的缺陷。
本发明采用的技术方案是:一种铝锌金属复合钢板,具有钢板主体,钢板主体外包覆有铝锌合金板耐蚀保护层,所述的铝锌合金板耐蚀保护层是由按重量百分比5%-25%的铝、1%-3%的镁、1.5%的硅、0.3%的稀土以及余量的锌合成的。
本发明的有益效果是:该铝锌金属复合钢板在苛刻的腐蚀环境下仍能发挥其优异的耐腐蚀性,产品耐刮耐磨,能适应多种加工,使用寿命长,完全可以取代目前的采用先成形加工再经热浸镀锌的后浸镀金属板产品进行使用。
具体实施方式
实施例1:
铝锌金属复合钢板,具有钢板主体,钢板主体外包覆有铝锌合金板耐蚀保护层,所述铝锌合金板耐蚀保护层由按重量百分比5%的铝、1%的镁、1.5%的硅、0.3%的稀土以及余量的锌合成。
实施例2:
铝锌金属复合钢板,具有钢板主体,钢板主体外包覆有铝锌合金板耐蚀保护层,所述铝锌合金板耐蚀保护层由按重量百分比15%的铝、2%的镁、1.5%的硅、0.3%的稀土以及余量的锌合成的。
实施例3:
铝锌金属复合钢板,具有钢板主体,钢板主体外包覆有铝锌合金板耐蚀保护层,所述铝锌合金板耐蚀保护层由按重量百分比25%的铝、3%的镁、1.5%的硅、0.3%的稀土以及余量的锌合成的。
实施例4:
铝锌金属复合钢板,具有钢板主体,钢板主体外包覆有铝锌合金板耐蚀保护层,所述铝锌合金板耐蚀保护层由按重量百分比5%的铝、3%的镁、1.5%的硅、0.3%的稀土以及余量的锌合成的。
实施例5:
铝锌金属复合钢板,具有钢板主体,钢板主体外包覆有铝锌合金板耐蚀保护层,所述铝锌合金板耐蚀保护层由按重量百分比25%的铝、1%的镁、1.5%的硅、0.3%的稀土以及余量的锌合成的。

Claims (1)

1.一种铝锌金属复合钢板,其特征在于:具有钢板主体,钢板主体外包覆有铝锌合金板耐蚀保护层,所述的铝锌合金板耐蚀保护层是由按重量百分比5%-25%的铝、1%-3%的镁、1.5%的硅、0.3%的稀土以及余量的锌合成的。
CNA2008101556457A 2008-10-10 2008-10-10 铝锌金属复合钢板 Pending CN101396886A (zh)

Priority Applications (1)

Application Number Priority Date Filing Date Title
CNA2008101556457A CN101396886A (zh) 2008-10-10 2008-10-10 铝锌金属复合钢板

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
CNA2008101556457A CN101396886A (zh) 2008-10-10 2008-10-10 铝锌金属复合钢板

Publications (1)

Publication Number Publication Date
CN101396886A true CN101396886A (zh) 2009-04-01

Family

ID=40515843

Family Applications (1)

Application Number Title Priority Date Filing Date
CNA2008101556457A Pending CN101396886A (zh) 2008-10-10 2008-10-10 铝锌金属复合钢板

Country Status (1)

Country Link
CN (1) CN101396886A (zh)

Cited By (7)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN101736274B (zh) * 2009-12-28 2011-06-29 江苏麟龙新材料股份有限公司 含铝-硅-锌-稀土-铁-锰-铬的热浸镀合金及其制备方法
CN101736224B (zh) * 2009-12-28 2011-06-29 江苏麟龙新材料股份有限公司 含铝-硅-锌-稀土-锰的热浸镀合金及其制备方法
CN103660428A (zh) * 2013-11-27 2014-03-26 常熟华冶薄板有限公司 含有稀土的镀铝锌合金钢板及其生产方法
CN105648273A (zh) * 2016-01-27 2016-06-08 浙江华达新型材料股份有限公司 一种添加稀土的锌铝镁镀层钢板
CN108407670A (zh) * 2018-03-30 2018-08-17 中铁第四勘察设计院集团有限公司 一种用于接触网的防腐型钢腕臂定位装置
CN108422902A (zh) * 2018-03-30 2018-08-21 中铁第四勘察设计院集团有限公司 一种用于接触网的具有复合涂层的钢腕臂定位装置
CN108707806A (zh) * 2018-06-04 2018-10-26 芜湖征途电子科技有限公司 一种无人机用多金属复合板

Cited By (7)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN101736274B (zh) * 2009-12-28 2011-06-29 江苏麟龙新材料股份有限公司 含铝-硅-锌-稀土-铁-锰-铬的热浸镀合金及其制备方法
CN101736224B (zh) * 2009-12-28 2011-06-29 江苏麟龙新材料股份有限公司 含铝-硅-锌-稀土-锰的热浸镀合金及其制备方法
CN103660428A (zh) * 2013-11-27 2014-03-26 常熟华冶薄板有限公司 含有稀土的镀铝锌合金钢板及其生产方法
CN105648273A (zh) * 2016-01-27 2016-06-08 浙江华达新型材料股份有限公司 一种添加稀土的锌铝镁镀层钢板
CN108407670A (zh) * 2018-03-30 2018-08-17 中铁第四勘察设计院集团有限公司 一种用于接触网的防腐型钢腕臂定位装置
CN108422902A (zh) * 2018-03-30 2018-08-21 中铁第四勘察设计院集团有限公司 一种用于接触网的具有复合涂层的钢腕臂定位装置
CN108707806A (zh) * 2018-06-04 2018-10-26 芜湖征途电子科技有限公司 一种无人机用多金属复合板

Similar Documents

Publication Publication Date Title
CN101396886A (zh) 铝锌金属复合钢板
CN101402267A (zh) 多金属复合板
CN100580133C (zh) 纳米多元合金共渗防腐涂层的制备工艺
CN102206797B (zh) 一种抗海洋腐蚀与热腐蚀的复合涂层及其制备方法
WO2012091385A3 (en) High corrosion resistant hot dip zn alloy plated steel sheet and method of manufacturing the same
MX365825B (es) Composición de pretratamiento para metales que contiene zirconio, cobre, zinc, y nitrato y revestimientos relacionados sobre substratos de metal.
CN102260888A (zh) 一种金属表面镀饰锌镍合金及三价铬钝化的方法
CN102676971A (zh) 一种球墨铸铁管外表面复合涂层的制备方法
CN101186998B (zh) 一种输电线路杆塔长效防腐合金镀层及其制备工艺
CN101984130A (zh) 一种紧固件高耐腐蚀性热浸镀合金镀层及其制备工艺
CN201390000Y (zh) 复合钢板
JP7114914B2 (ja) 防錆処理された金属部材およびコート塗料
CN102464902B (zh) 一种钕铁硼永磁材料的铬锌涂层的表面处理方法
CN1271235C (zh) 一种油管的锌铝稀土合金化防腐工艺
CN201317140Y (zh) 一种镀锌工件
CN103966614A (zh) 一种金属表面镀饰锌铁合金及三价铬钝化的方法
CN210065618U (zh) 一种用于铁制工艺品的金属效果水性涂料涂层
JP2014202266A (ja) 高耐食性セルフタッピングねじ及びその製造方法
JP6265050B2 (ja) 優れた耐食性と塗料密着性を有する溶融Sn−Znめっき鋼板とその製造方法
CN201264401Y (zh) 铝锌复合钢板
CN110698899A (zh) 一种防锈蚀程度较高的金属材料涂层
CN113789506A (zh) 一种金属板、建筑及金属板的制备方法
CN102285187A (zh) 一种化学防护的牺牲性保护涂层
CN201390001Y (zh) 多金属复合钢板
CN102260865A (zh) 一种金属表面镀饰锌铁合金及三价铬钝化的方法

Legal Events

Date Code Title Description
C06 Publication
PB01 Publication
C10 Entry into substantive examination
SE01 Entry into force of request for substantive examination
C02 Deemed withdrawal of patent application after publication (patent law 2001)
WD01 Invention patent application deemed withdrawn after publication

Open date: 20090401