CN101347275A - Method for controlling quality of molded shoes with cloth cover - Google Patents

Method for controlling quality of molded shoes with cloth cover Download PDF

Info

Publication number
CN101347275A
CN101347275A CNA2008103037106A CN200810303710A CN101347275A CN 101347275 A CN101347275 A CN 101347275A CN A2008103037106 A CNA2008103037106 A CN A2008103037106A CN 200810303710 A CN200810303710 A CN 200810303710A CN 101347275 A CN101347275 A CN 101347275A
Authority
CN
China
Prior art keywords
shoe
footwear
appearance
less
place
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CNA2008103037106A
Other languages
Chinese (zh)
Inventor
杜江
陈松雄
邓时军
周川泉
晋齐怀
杨东
田吉
王永生
彭德彪
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Jihua 3537 Shoe Making Co Ltd
Original Assignee
Jihua 3537 Shoe Making Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Jihua 3537 Shoe Making Co Ltd filed Critical Jihua 3537 Shoe Making Co Ltd
Priority to CNA2008103037106A priority Critical patent/CN101347275A/en
Publication of CN101347275A publication Critical patent/CN101347275A/en
Pending legal-status Critical Current

Abstract

The invention discloses a quality controlling method for a pair of cloth cover moulded shoes. The method consists of the control to raw materials, appearance and physical and mechanical properties, wherein, the raw materials comprise standard natural ruuber, carbon soot with high wear resistance, zinc oxide, stearic acid, accelerant DM, accelerant M, sulfur, space-variant terylene filament canvas and terylene filament flat hair plush; the appearance comprises the appearance of an upper semifinished product and the appearance of a finished shoe; the physical and mechanical properties comprise the bond strength of the upper with a foxing, the wear-resisting performance of external bottom, the strength and elongation performance of the external bottom, the hardness of a glue component, aging performance of glue stuff and the air permeability and the moisture permeability of the upper. The invention establishes a novel quality controlling method for a pair of cloth cover moulded shoes, improves the quality control standard of moulded shoes and ensures the performances of the moulded shoes better, such as the comfortableness for wearing, the wearing resistance, etc.

Description

Method for controlling quality of molded shoes with cloth cover
Technical field
The present invention relates to the molded shoes with cloth cover technical field, particularly relate to the method for quality control of molded shoes with cloth cover.
Background technology
Molded shoes with cloth cover is the molded vulcanization structure, comprises single footwear of cloth cover mold pressing and cloth cover mold pressing cotton-padded shoes, because its practicality comfortable and easy to wear, light, and the outward appearance leisure is generous, and be subjected to consumer's favor deeply.
The preparation method of cemented shoe is:
1, make semi-finished product: the textile material that will meet specification requirement is made upper of a shoe, is used for the moulding manufacturing through after the assay was approved; Simultaneously, the chemical raw material and the rubber that are up to the standards are made cemented shoe glue component elastomeric compound on rubber mixing machine, make semi-finished product film and bonding rubber cement with elastomeric compound afterwards.
2, the moulding manufacturing of cemented shoe: earlier the end in qualified upper of a shoe and the nonwoven is sewed up, then the upper of a shoe of sewing up is enclosed within on the shoe tree through processing such as typing, swabbings.Again the swabbing upper of a shoe is enclosed within on the sulfuration shoe tree, stick the semi-finished product glue component after, under uniform temperature and pressure, the sulfuration of glue component and upper of a shoe is fixed together, form moulded footwear.At last moulded footwear is modified the making that cemented shoe is promptly finished in processing.
The shaping characteristic of cemented shoe is a sulfidization molding, saves space, simplifies working process, and has energy-conservation, characteristics of high efficiency, and the processing technical parameter is 6~7 minutes molding sulfuration time, and sulfide stress 12~17MPa, curing temperature are 140~155 ℃.
At present, what the quality control of molded shoes with cloth cover was adopted is the national standard of ordinary movement footwear, because ordinary movement footwear national standard is a kind of extensive adaptive standard, specific aim is not strong, performance requirement to footwear is not high, have only two to three months by the cemented shoe life-span of this standard production, and the life requirements of cemented shoe is more than 6 months.Do not meet the client to the cemented shoe outward appearance and wear the demand in life-span according to the cemented shoe of the standard production of ordinary movement footwear, can not form the market competitiveness, value of the product is low, and the various performances of molded shoes with cloth cover comprise that degree comfortable and easy to wear and anti-wear performance etc. all have much room for improvement.Also there is not authoritative method for controlling quality of molded shoes with cloth cover at present.
Summary of the invention
Technical problem to be solved by this invention is to overcome the defective that the various performances that do not have special method for controlling quality of molded shoes with cloth cover, molded shoes with cloth cover in the prior art have much room for improvement, a kind of special method of quality control at molded shoes with cloth cover is provided, this method has improved the quality of cemented shoe in all its bearings, better guarantee the performances such as degree comfortable and easy to wear, wearability of cemented shoe, can be used as the standard of producing that instructs.
In order to solve the problems of the technologies described above, the present invention adopts following technical scheme:
Method for controlling quality of molded shoes with cloth cover is by the outward appearance of raw material, footwear and the quality control of its physical and mechanical properties are formed, wherein, to raw-material quality control be the quality of control criterion natural rubber, high wear-resistant carbon black, zinc oxide, stearic acid, altax, captax, sulphur, space-variant polyester filament canvas and polyester filament straight snips suede; The control of footwear outward appearance comprises the check control to upper of a shoe semi-finished product outward appearance and product shoes outward appearance; Control to the physical and mechanical properties of footwear is the control of bonding strength, outer bottom anti-wear performance, outer bottom strength and extension property, glue component hardness, sizing material ageing properties, upper of a shoe permeability and water vapour permeability to upper of a shoe and foxing.
The control of the physical and mechanical properties described in the above-mentioned method for controlling quality of molded shoes with cloth cover is formed by following:
The bonding strength of upper of a shoe and foxing is not less than 5.0KN/m; (GB/T 532)
The outer bottom anti-wear performance: the Akron wear volume is not more than 0.8cm 3/ 1.61km; (GB/T 1689)
Outer bottom strength and extension property: hot strength 〉=13.0MPa, elongation at break 〉=450%; (GB/T 528)
Glue component hardness: 57 ± 5 degree (Shao Er A type hardness tester); (GB/T 531)
Sizing material ageing properties: i.e. percentage rate of change after the 100 ℃ * 12h hot air aging, hot strength 〉=-20%, elongation at break 〉=-35%; (GB/T 3512)
Upper of a shoe air penetrability 〉=45mm/s; (GB/T 5453)
Upper of a shoe or insole sock vapor transfer rate 〉=4500g/m 2D.(GB/T12701)
More than the control of various performances all be to adopt state's calibration method, the method code name is seen in the bracket.
The control of footwear outward appearance described in the aforementioned method for controlling quality of molded shoes with cloth cover is formed by following:
Upper of a shoe semi-finished product outward appearance
(1) upper of a shoe: 1. the aberration of together two footwear is in 4 grades; 2. obvious position free from smutting during, the stain at less important position is no more than 1 place, and its area is no more than 150mm 23. vamp cloth and flap face cloth do not have breakage; 4. the no wrong number of group before and after; 5. the askew and askew 5mm that is no more than of heel bar of both wings; 6. shoe lining does not have dead pleat; 7. counter the telling of eye lining at system mouthful place is not more than 1.0mm;
(2) suture: 1. turn over line and be no more than 4 pins, even turn over and be no more than 2 pins; 2. obviously the position does not have wire jumper, and less important position wire jumper is no more than 3 pins, and inaccurate the company jumps; 3. do not have suture and exceed the bounds and break, cross spider is pricked disconnected 1 pin that is no more than; 4. heavy line dislocation-free; 5. there is not the sewing thread of exposing the end of a thread;
(3) eyelet: non-loosening and fall lacquer; Eyelet crooked can not obviously influence attractive in appearance and wear shoestring;
The product shoes outward appearance
(1) overall appearance: 1. smooth, cleaning, symmetry, cover group rectifies; 2. upper of a shoe, sole and shoe lining do not have obvious variable color; 3. there are not the group's of revealing pin, bloom and obviously wounded or disabled; 4. shoe-pad is smooth, and footwear sizes is arranged, and footwear sizes is error-free;
(2) vamp:, do not have breakage, dew group pin, bloom and obviously wounded or disabled 1. with color and luster, thickness, fine hair thickness and the decorative pattern color and luster basically identical of two footwear same area; 2. appear the position free from smutting during, the stain at less important position is no more than 1 place, and its area is no more than 150mm 23. the askew and askew 5mm that is no more than of heel bar of both wings; 4. pleat and shelling: substantially flat does not affect the appearance and wears; 5. eye serves as a contrast counter telling: a system mouthful place is not more than 1.0mm, and other position does not allow; 6. footwear ear out-of-flatness: slight, do not affect the appearance and wear;
(3) main root and packet header: 1. main root and packet header rectify, be convinced, symmetry and putting in place; 2. there is not soft, the shelling of main root; 3. main root and packet header are askew partially not obvious with gauffer;
(4) rim of the mouth: 1. neatly tight, no-sundries; 2. the every place of starved area is less than 6mm 2, accumulative total is less than 40mm 2, be no more than 150mm deeply 2
(5) the interior end: 1. do not have wrong number; 2. appearing the position does not have spot, and less important position spot is no more than a place and area is no more than 150mm 23. appear the position and do not have breakage;
(6) outer bottom: 1. with two footwear outer bottom same area color and lusters, decorative pattern unanimity, pattern depth is less than 1/3rd of outsole thickness; 2. the every place of starved area is less than 10mm 2, accumulative total is less than 70mm 2, be no more than 1.5mm deeply; 3. the foreign material cumulative area is no more than 20mm 2, be no more than 1mm deeply; 4. do not have come unglued, spongy, no bloom, the end in not revealing; 5. bubble is no more than 3 places and every place area is no more than 5mm 2
(7) suture: 1. neat, pin sign indicating number evenly, bottom surface line degree of tightness unanimity, no suture is exceeded the bounds and break, and cross spider breaks and is no more than 1 pin; 2. main position do not have wire jumper, heavy pin, break, turn over line, burst at the seams and wire jumper heavy pin in the 3. less important position of the end of a thread can have a place, turns over line and is no more than 4 pins and connects to turn over and be no more than 2 pins, and wire jumper is no more than three pins and must not even jumps;
(8) flanging bead: neat evenly slick and sly, no clip exposes, no breach;
(9) accessory: symmetry, firmly;
(10) with two footwear sizes: the 1. long franchise 3mm of toe lasting, the high franchise 5mm of back group; 2. crooked franchise 5mm is stitched in heel bar or back; 3. outer bottom length franchise 2mm, width franchise 1.5mm, thickness franchise 1.5mm;
(11) eyelet: 1. skewness can not influence attractive in appearance and wear shoestring, non-loosening; 2. fall to coat with lacquer to be no more than 4 places and not locate area and be no more than 2mm 2
(12) shoe lining: 1. do not have breakage, do not have dead pleat; 2. there is not obvious seep through; 3. the above adhesive-free spot in the end in the sponge;
(13) rubber cement: no rubber cement pimple, reveal slurry 0~2mm.
Main raw-material control is as follows described in the aforementioned method for controlling quality of molded shoes with cloth cover:
(1) standard natural rubber: the rubber breaking strength is not less than 19.6MPa, and elongation at break is not less than 680%;
(2) high wear-resistant carbon black: a) pure carbon black laboratory indexes: pH value 7~9.5, oil factor 0.90~1.15, DPG sorption rate 4~8%, 100 screen residues are less than 0.02%; B) (press the physical property of the prepared film of following proportioning: smoked sheet 300g, stearic acid 9g, age resistor CD 3g, zinc oxide 15g, captax 1.8g, pine tar 9g, sulphur 9g, high wear-resistant carbon black 150g add up to 496.8g to physical performance index.): breaking strength 〉=24.5MPa, elongation at break 〉=470%, 300% stretching strength 〉=11.76MPa, Akron wear volume≤0.22cm 3/ 1.61km;
(4) zinc oxide: content 〉=95.0%, 100 screen residues≤0.02%;
(5) stearic acid: iodine number (g/100g)≤8.0, saponification number (mg/g) 193~220, acid number (mg/g) 192~218, freezing point (℃) 〉=52; As 800 type stearic acid;
(6) altax: fusing point 〉=160 ℃, residue on sieve≤0.10%, ash≤0.70%;
(7) captax: fusing point 〉=170 ℃, residue on sieve≤0.10%, ash≤0.30%;
(8) sulphur: sulfur content 〉=99.00%, moisture content 1.00%, fusing point 〉=110 ℃, do not have 120 screen residues; As industrial sulphur;
(9) space-variant polyester filament canvas: specification 4 * 4;
(10) space-variant polyester filament straight snips suede: specification 4 * 4.
Experimental example one, and relatively with the performance of the molded shoes with cloth cover of standard fabrication described in the method for quality control of the present invention with the molded shoes with cloth cover of the standard fabrication of ordinary movement footwear:
Figure A20081030371000081
The screening of experimental example two, physical and mechanical properties index
The inventor is an object with the molded shoes with cloth cover of different physical and mechanical properties, has studied its service life and degree comfortable and easy to wear etc., enumerates typical a few example below:
The experiment in service life of the molded shoes with cloth cover of table 1 different physical characteristics
Figure A20081030371000091
As can be seen from Table 1, be index with the physical and mechanical properties of No. 17 molded shoes with cloth cover, it wears the life-span and wearing conditions can meet the demands, and is method of quality control of the present invention so select to be not less than No. 17 physical and mechanical properties.
Table 2 footwear Air permenbility and vapor transfer rate and wear effect
Figure A20081030371000102
As can be seen from Table 2, be index with the upper of a shoe Air permenbility and the vapor transfer rate of No. 4 molded shoes with cloth cover, it is better that it wears effect, so the standard of selecting to be not less than No. 4 molded shoes with cloth cover in the table 2 is a method of quality control of the present invention.
Compared with prior art, the present invention has set up the method for quality control of new molded shoes with cloth cover, this method comprises the cemented shoe raw material, the control of the physical and mechanical properties of cemented shoe outward appearance and cemented shoe, short with the time of wearing that solves the molded shoes with cloth cover that adopts the production of ordinary movement footwear quality control standard, outward appearance is coarse, problems such as the high-class product rate is low, after adopting method provided by the present invention, the high-class product rate of molded shoes with cloth cover reaches more than 98%, qualification rate reaches more than 99.8%, effectively improved the quality of cemented shoe, better guaranteed the degree comfortable and easy to wear of cemented shoe, performances such as wearability are a kind of scientific and reasonable method of quality control.
The specific embodiment
Preferred implementation of the present invention:
With examined product is a collection of, therefrom extracts three pairs and tests.
At first be major-minor raw-material Properties Control:
(1) standard natural rubber: the rubber breaking strength is not less than 19.6MPa, and elongation at break is not less than 680%;
(2) high wear-resistant carbon black: a) pure carbon black laboratory indexes: pH value 7~9.5, oil factor 0.90~1.15, DPG sorption rate 4~8%, 100 screen residues are less than 0.02%; B) (press the physical property of the prepared film of following proportioning: smoked sheet 300g, stearic acid 9g, age resistor CD 3g, zinc oxide 15g, captax 1.8g, pine tar 9g, sulphur 9g, high wear-resistant carbon black 150g add up to 496.8g to physical performance index.): breaking strength 〉=24.5MPa, elongation at break 〉=470%, 300% stretching strength 〉=11.76MPa, Akron wear volume≤0.22cm 3/ 1.61km;
(4) zinc oxide: content 〉=95.0%, 100 screen residues≤0.02%;
(5) stearic acid: iodine number (g/100g)≤8.0, saponification number (mg/g) 193~220, acid number (mg/g) 192~218, freezing point (℃) 〉=52; As 800 type stearic acid;
(6) altax: fusing point 〉=160 ℃, residue on sieve≤0.10%, ash≤0.70%;
(7) captax: fusing point 〉=170 ℃, residue on sieve≤0.10%, ash≤0.30%;
(8) sulphur: sulfur content 〉=99.00%, moisture content 1.00%, fusing point 〉=110 ℃, do not have 120 screen residues; As industrial sulphur;
(9) space-variant polyester filament canvas: specification 4 * 4, fabric width 150 ± 12cm;
(10) space-variant polyester filament straight snips suede: specification 4 * 4, fabric width, 155 ± 12cm.
Be the control of upper of a shoe semi-finished product outward appearance then:
(1) upper of a shoe: 1. the aberration of together two footwear is in 4 grades; 2. obvious position free from smutting during, the stain at less important position is no more than 1 place, and its area is no more than 150mm 23. vamp cloth and flap face cloth do not have breakage; 4. the no wrong number of group before and after; 5. the askew and askew 5mm that is no more than of heel bar of both wings; 6. shoe lining does not have dead pleat; 7. counter the telling of eye lining at system mouthful place is not more than 1.0mm;
(2) suture: 1. turn over line and be no more than 4 pins, even turn over and be no more than 2 pins; 2. obviously the position does not have wire jumper, and less important position wire jumper is no more than 3 pins, and inaccurate the company jumps; 3. do not have suture and exceed the bounds and break, cross spider is pricked disconnected 1 pin that is no more than; 4. heavy line dislocation-free; 5. there is not the sewing thread of exposing the end of a thread;
(3) eyelet: non-loosening and fall lacquer; Eyelet crooked can not obviously influence attractive in appearance and wear shoestring;
The control of product shoes outward appearance:
(1) overall appearance: 1. smooth, cleaning, symmetry, cover group rectifies; 2. upper of a shoe, sole and shoe lining do not have obvious variable color; 3. there are not the group's of revealing pin, bloom and obviously wounded or disabled; 4. shoe-pad is smooth, and footwear sizes is arranged, and footwear sizes is error-free;
(2) vamp:, do not have breakage, dew group pin, bloom and obviously wounded or disabled 1. with color and luster, thickness, fine hair thickness and the decorative pattern color and luster basically identical of two footwear same area; 2. appear the position free from smutting during, the stain at less important position is no more than 1 place, and its area is no more than 150mm 23. the askew and askew 5mm that is no more than of heel bar of both wings; 4. pleat and shelling: substantially flat does not affect the appearance and wears; 5. eye serves as a contrast counter telling: a system mouthful place is not more than 1.0mm, and other position does not allow; 6. footwear ear out-of-flatness: slight, do not affect the appearance and wear;
(3) main root and packet header: 1. main root and packet header rectify, be convinced, symmetry and putting in place; 2. there is not soft, the shelling of main root; 3. main root and packet header are askew partially not obvious with gauffer;
(4) rim of the mouth: 1. neatly tight, no-sundries; 2. the every place of starved area is less than 6mm 2, accumulative total is less than 40mm 2, be no more than 150mm deeply 2
(5) the interior end: 1. do not have wrong number; 2. appearing the position does not have spot, and less important position spot is no more than a place and area is no more than 150mm 23. appear the position and do not have breakage;
(6) outer bottom: 1. with two footwear outer bottom same area color and lusters, decorative pattern unanimity, pattern depth is less than 1/3rd of outsole thickness; 2. the every place of starved area is less than 10mm 2, accumulative total is less than 70mm 2, be no more than 1.5mm deeply; 3. the foreign material cumulative area is no more than 20mm 2, be no more than 1mm deeply; 4. do not have come unglued, spongy, no bloom, the end in not revealing; 5. bubble is no more than 3 places and every place area is no more than 5mm 2
(7) suture: 1. neat, pin sign indicating number evenly, bottom surface line degree of tightness unanimity, no suture is exceeded the bounds and break, and cross spider breaks and is no more than 1 pin; 2. main position do not have wire jumper, heavy pin, break, turn over line, burst at the seams and wire jumper heavy pin in the 3. less important position of the end of a thread can have a place, turns over line and is no more than 4 pins and connects to turn over and be no more than 2 pins, and wire jumper is no more than three pins and must not even jumps;
(8) flanging bead: neat evenly slick and sly, no clip exposes, no breach;
(9) accessory: symmetry, firmly;
(10) with two footwear sizes: the 1. long franchise 3mm of toe lasting, the high franchise 5mm of back group; 2. crooked franchise 5mm is stitched in heel bar or back; 3. outer bottom length franchise 2mm, width franchise 1.5mm, thickness franchise 1.5mm;
(11) eyelet: 1. skewness can not influence attractive in appearance and wear shoestring, non-loosening; 2. fall to coat with lacquer to be no more than 4 places and not locate area and be no more than 2mm 2
(12) shoe lining: 1. do not have breakage, do not have dead pleat; 2. there is not obvious seep through; 3. the above adhesive-free spot in the end in the sponge;
(13) rubber cement: no rubber cement pimple, reveal slurry 0~2mm.
Be the control of the physical and mechanical properties of product shoes at last:
The bonding strength of upper of a shoe and foxing is not less than 5.0KN/m; (GB/T 532)
The outer bottom anti-wear performance: the Akron wear volume is not more than 0.8cm 3/ 1.61km; (GB/T 1689)
Outer bottom strength and extension property: hot strength 〉=13.0MPa, elongation at break 〉=450%; (GB/T 528)
Glue component hardness: 57 ± 5 degree (Shao Er A type hardness tester); (GB/T 531)
Sizing material ageing properties: i.e. percentage rate of change after the 100 ℃ * 12h hot air aging, hot strength 〉=-20%, elongation at break 〉=-35%; (GB/T 3512)
Upper of a shoe air penetrability 〉=45mm/s; (GB/T 5453)
Upper of a shoe or insole sock vapor transfer rate 〉=4500g/m 2D.(GB/T12701)
More than the control of various performances all be to adopt state's calibration method, the method code name is seen in the bracket.
Adopt as above method that single footwear of cloth cover mold pressing and cloth cover mold pressing cotton-padded shoes are carried out quality control, can well guarantee the outward appearance of cemented shoe, various physical and mechanical properties, degree comfortable and easy to wear etc.

Claims (4)

1. method for controlling quality of molded shoes with cloth cover, it is characterized in that: method of quality control is by the outward appearance of raw material, footwear and the quality control of its physical and mechanical properties are formed, wherein, to raw-material quality control be the quality of control criterion natural rubber, high wear-resistant carbon black, zinc oxide, stearic acid, altax, captax, sulphur, space-variant polyester filament canvas and polyester filament straight snips suede; The control of footwear outward appearance comprises the check control to upper of a shoe semi-finished product outward appearance and product shoes outward appearance; Control to the physical and mechanical properties of footwear is the control of bonding strength, outer bottom anti-wear performance, outer bottom strength and extension property, glue component hardness, sizing material ageing properties, upper of a shoe permeability and water vapour permeability to upper of a shoe and foxing.
2. according to the described method for controlling quality of molded shoes with cloth cover of claim 1, it is characterized in that: the control of described physical and mechanical properties is formed by following:
The bonding strength of upper of a shoe and foxing is not less than 5.0KN/m;
The outer bottom anti-wear performance: the Akron wear volume is not more than 0.8cm3/1.61km;
Outer bottom strength and extension property: hot strength 〉=13.0MPa, elongation at break 〉=450%;
Glue component hardness: 57 ± 5 degree;
Sizing material ageing properties: i.e. percentage rate of change after the 100 ℃ * 12h hot air aging, hot strength 〉=-20%, elongation at break 〉=-35%;
Upper of a shoe air penetrability 〉=45mm/s;
Upper of a shoe or insole sock vapor transfer rate 〉=4500g/m2d.
3. according to the described method for controlling quality of molded shoes with cloth cover of claim 1, it is characterized in that: the control of described footwear outward appearance is formed by following:
Upper of a shoe semi-finished product outward appearance
(1) upper of a shoe: 1. the aberration of together two footwear is in 4 grades; 2. obvious position free from smutting during, the stain at less important position is no more than 1 place, and its area is no more than 150mm2; 3. vamp cloth and flap face cloth do not have breakage; 4. the no wrong number of group before and after; 5. the askew and askew 5mm that is no more than of heel bar of both wings; 6. shoe lining does not have dead pleat; 7. counter the telling of eye lining at system mouthful place is not more than 1.0mm;
(2) suture: 1. turn over line and be no more than 4 pins, even turn over and be no more than 2 pins; 2. obviously the position does not have wire jumper, and less important position wire jumper is no more than 3 pins, and inaccurate the company jumps; 3. do not have suture and exceed the bounds and break, cross spider is pricked disconnected 1 pin that is no more than; 4. heavy line dislocation-free; 5. there is not the sewing thread of exposing the end of a thread;
(3) eyelet: non-loosening and fall lacquer; Eyelet crooked can not obviously influence attractive in appearance and wear shoestring;
The product shoes outward appearance
(1) overall appearance: 1. smooth, cleaning, symmetry, cover group rectifies; 2. upper of a shoe, sole and shoe lining do not have obvious variable color; 3. there are not the group's of revealing pin, bloom and obviously wounded or disabled; 4. shoe-pad is smooth, and footwear sizes is arranged, and footwear sizes is error-free;
(2) vamp:, do not have breakage, dew group pin, bloom and obviously wounded or disabled 1. with color and luster, thickness, fine hair thickness and the decorative pattern color and luster basically identical of two footwear same area; 2. appear the position free from smutting during, the stain at less important position is no more than 1 place, and its area is no more than 150mm2; 3. the askew and askew 5mm that is no more than of heel bar of both wings; 4. pleat and shelling: substantially flat does not affect the appearance and wears; 5. eye serves as a contrast counter telling: a system mouthful place is not more than 1.0mm, and other position does not allow; 6. footwear ear out-of-flatness: slight, do not affect the appearance and wear;
(3) main root and packet header: 1. main root and packet header rectify, be convinced, symmetry and putting in place; 2. there is not soft, the shelling of main root; 3. main root and packet header are askew partially not obvious with gauffer;
(4) rim of the mouth: 1. neatly tight, no-sundries; 2. the every place of starved area is less than 6mm2, and accumulative total is no more than 150mm2 deeply less than 40mm2;
(5) the interior end: 1. do not have wrong number; 2. appearing the position does not have spot, and less important position spot is no more than a place and area is no more than 150mm2; 3. appear the position and do not have breakage;
(6) outer bottom: 1. with two footwear outer bottom same area color and lusters, decorative pattern unanimity, pattern depth is less than 1/3rd of outsole thickness; 2. the every place of starved area is less than 10mm2, and accumulative total is no more than 1.5mm deeply less than 70mm2; 3. the foreign material cumulative area is no more than 20mm2, is no more than 1mm deeply; 4. do not have come unglued, spongy, no bloom, the end in not revealing; 5. bubble is no more than 3 places and every place area is no more than 5mm2;
(7) suture: 1. neat, pin sign indicating number evenly, bottom surface line degree of tightness unanimity, no suture is exceeded the bounds and break, and cross spider breaks and is no more than 1 pin; 2. main position do not have wire jumper, heavy pin, break, turn over line, burst at the seams and wire jumper heavy pin in the 3. less important position of the end of a thread can have a place, turns over line and is no more than 4 pins and connects to turn over and be no more than 2 pins, and wire jumper is no more than three pins and must not even jumps;
(8) flanging bead: neat evenly slick and sly, no clip exposes, no breach;
(9) accessory: symmetry, firmly;
(10) with two footwear sizes: the 1. long franchise 3mm of toe lasting, the high franchise 5mm of back group; 2. crooked franchise 5mm is stitched in heel bar or back; 3. outer bottom length franchise 2mm, width franchise 1.5mm, thickness franchise 1.5mm;
(11) eyelet: 1. skewness can not influence attractive in appearance and wear shoestring, non-loosening; 2. fall that lacquer is no more than 4 places and every place area is no more than 2mm2;
(12) shoe lining: 1. do not have breakage, do not have dead pleat; 2. there is not obvious seep through; 3. the above adhesive-free spot in the end in the sponge;
(13) rubber cement: no rubber cement pimple, reveal slurry 0~2mm.
4. according to the described method for controlling quality of molded shoes with cloth cover of claim 1, it is characterized in that: the raw-material control of described master is as follows:
(1) standard natural rubber: the rubber breaking strength is not less than 19.6MPa, and elongation at break is not less than 680%;
(2) high wear-resistant carbon black: a) pure carbon black laboratory indexes: pH value 7~9.5, oil factor 0.90~1.15, DPG sorption rate 4~8%, 100 screen residues are less than 0.02%; B) physical performance index: breaking strength 〉=24.5MPa, elongation at break 〉=470%, 300% stretching strength 〉=11.76MPa, Akron wear volume≤0.22cm3/1.61km;
(3) zinc oxide: content 〉=95.0%, 100 screen residues≤0.02%;
(4) stearic acid: iodine number (g/100g)≤8.0, saponification number (mg/g) 193~220, acid number (mg/g) 192~218, freezing point (℃) 〉=52;
(5) altax: fusing point 〉=160 ℃, residue on sieve≤0.10%, ash≤0.70%;
(6) captax: fusing point 〉=170 ℃, residue on sieve≤0.10%, ash≤0.30%;
(7) sulphur: sulfur content 〉=99.00%, moisture content 1.00%, fusing point 〉=110 ℃, do not have 120 screen residues;
(8) space-variant polyester filament canvas: specification 4 * 4;
(9) space-variant polyester filament straight snips suede: specification 4 * 4.
CNA2008103037106A 2008-08-13 2008-08-13 Method for controlling quality of molded shoes with cloth cover Pending CN101347275A (en)