CN101333577A - 降低球墨铸铁铁液中含钛量的方法 - Google Patents
降低球墨铸铁铁液中含钛量的方法 Download PDFInfo
- Publication number
- CN101333577A CN101333577A CNA2008100554098A CN200810055409A CN101333577A CN 101333577 A CN101333577 A CN 101333577A CN A2008100554098 A CNA2008100554098 A CN A2008100554098A CN 200810055409 A CN200810055409 A CN 200810055409A CN 101333577 A CN101333577 A CN 101333577A
- Authority
- CN
- China
- Prior art keywords
- iron liquid
- iron
- titanium
- nitride
- titaniferous amount
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Abstract
Description
Claims (4)