CN101220238A - Method for producing solvent type energy accumulation luminescent paint - Google Patents

Method for producing solvent type energy accumulation luminescent paint Download PDF

Info

Publication number
CN101220238A
CN101220238A CNA2007101590059A CN200710159005A CN101220238A CN 101220238 A CN101220238 A CN 101220238A CN A2007101590059 A CNA2007101590059 A CN A2007101590059A CN 200710159005 A CN200710159005 A CN 200710159005A CN 101220238 A CN101220238 A CN 101220238A
Authority
CN
China
Prior art keywords
luminescent
paint
preparation
luminescent paint
organic matrix
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
CNA2007101590059A
Other languages
Chinese (zh)
Other versions
CN101220238B (en
Inventor
宁桂玲
叶俊伟
李瑞芳
庞宏昌
林�源
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Dalian University of Technology
Original Assignee
Dalian University of Technology
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Dalian University of Technology filed Critical Dalian University of Technology
Priority to CN2007101590059A priority Critical patent/CN101220238B/en
Publication of CN101220238A publication Critical patent/CN101220238A/en
Application granted granted Critical
Publication of CN101220238B publication Critical patent/CN101220238B/en
Expired - Fee Related legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

A preparation method of solvent type energy-storage luminescent paint belongs to the technical field of the production of functional coating. The invention is characterized by directly dispersing into organic matrix to prepare luminescent paint without packing aluminate energy storage luminescent power. The organic matrix, a fluidifying agent, a super-dispersant and an emulsifying agent are put into a reactor according to weight proportion, are stirred to be evenly mixed, then filled in luminescent power in batches; the mixture is stirred until being evenly dispersed, thereby obtaining the energy-storage luminescent paint. The luminescent paint prepared by the invention has bright color, is even without agglomerations, and has good liquidity, high brightness and long illumination time. The preparation technique is simple and rapid, can be produced in a factory and also can be prepared in painting site. The invention solves the problem of easy precipitation and easy failure of ordinary luminescent paint, reduces cost, simplifies production technique and greatly expands the application range of energy-storage luminescent paint. The invention can be used on luminescent safety sign, various emergency occasions, furniture decoration without need of any electricity devices, therefore, the preparation method of solvent type energy-storage luminescent paint is energy-saving and electricity -safe, reliable and beautiful.

Description

A kind of method for preparing solvent type energy accumulation luminescent paint
Technical field
The invention belongs to the production technical field of functional paint, specially refer to a kind of preparation method of solvent type energy accumulation luminescent paint.
Background technology
Luminous paint can also be widely used in each field such as traffic, military installations, fire control equipment except the protection and decorative effect with general coating.Rare-earth activated aluminate-series luminous paint is compared not only stable performance with the sulfide luminous paint, and luminous intensity and all being significantly increased time of persistence.But the application of present rare-earth activated aluminate luminous paint only limits to some special processing technologies, because coating produces wild effects such as sedimentation or layering, and can not be as commodity selling.It is simply quick to the invention provides a kind of technology, and product performance are good, both can be in plant produced, and also can be in the preparation method of the solvent-borne type luminous paint of the on-the-spot preparation of brushing.Utilize the luminous paint of this method preparation bright-colored, evenly do not have caking, good fluidity, the luminosity height, fluorescent lifetime is long, has solved general luminous paint and has easily precipitated, deficiencies such as easy inefficacy not only have satisfactory stability and luminescent properties, have the characteristics that are coated with the smooth and beautiful appearance of wiping one's face simultaneously.
Summary of the invention
The preparation method who the purpose of this invention is to provide a kind of easy solvent type energy accumulation luminescent paint, make the luminous paint quality even, that films is highly polished, sustainable luminous more than 15 hours, be used for the luminous sign of building decoration decoration, warning mark, culture and arts product decoration and special occasions, also can be used as cove lighting and low emergency lighting.
Technical scheme of the present invention is: adopt commercially available finished product varnish and rare-earth activated aluminate long after glow luminous material to prepare the solvent-borne type luminous paint.According to proportioning, will add hyper-dispersant and emulsifying agent after the varnish dilution, fully stir dispersion agent is disperseed and emulsification complete, insert luminescent powder then in batches, stir and just can obtain luminous paint until being uniformly dispersed.Ground needs dedusting or processing of rust removing before using, and then coating is evenly applied, and seasoning is solidified.
Effect of the present invention and benefit are to adopt finished product varnish to prepare luminous paint, and luminescent powder does not need coating to handle, and preparation technology is simply quick, the luminosity height, and fluorescent lifetime is long, both can also can prepare at the brushing scene in plant produced.Solved general luminous paint and easily precipitated, easily the deficiency that lost efficacy has simplified production technique simultaneously, has reduced cost, has improved the range of application of energy-accumulating luminous paint, and especially consumed power not has certain mitigation to present energy dilemma.
Embodiment
Be described in detail the specific embodiment of the present invention and step below in conjunction with technical scheme:
The invention provides a kind of method for preparing solvent type energy accumulation luminescent paint, it is characterized in that the kind of organic matrix in the coating, long-afterglow luminous alaminate powder, hyper-dispersant, emulsifying agent and thinner and formula rate are as follows:
The organic matrix of coating is selected in commercially available finished product varnish, comprises in polyester varnish, polyurethane lacquer, the alkyd varnish one or more; Luminescent powder be a kind of be the long after glow luminous material that base material is made with the aluminate, chemical general formula is MAl 2O 4: Eu 2+, RE 3+, choose wherein one or more, wherein M is Ca, Sr or Ba, wherein RE 3+Be Dy 3+, Nd 3+And Tm 3+Hyper-dispersant is one or more among the anti-coacervation dispersion agent (polymerization degree 4~10) of polyurethane-type, the anti-coacervation dispersion agent (polymerization degree 12~18) of block polypropylene acid type polymer, the polycarboxylate sodium; Emulsifying agent is selected one or more in polyacrylic acid (polymerization degree 11~15), the tween T series non-ionic surfactants for use; T=20,40,60 or 80 wherein; Thinner is selected dehydrated alcohol, ethyl acetate, C 4~C 12In organic alcohol, ether, the sherwood oil one or more; Organic matrix, thinner, hyper-dispersant, emulsifying agent and luminescent powder part by weight are 100: 20~50: 0.5~5: 0.1~4: 10~60.The technical process of preparation is as follows:
The first step: the long-afterglow luminous alaminate powder of the technology preparation of the preparation processing of luminescent powder and the selection of organic matrix: utilize patent: ZL02109504.3, screen the particle that is of a size of 10~30 μ m with sieve before using; Organic matrix can be selected various transparencies varnish product preferably;
Second step: the preparation of luminous paint.Organic matrix, thinner, hyper-dispersant, emulsifying agent joined to stir in the reactor by weight proportion it is mixed, insert luminescent powder then in batches, stir until being uniformly dispersed, thereby obtain luminous paint; Be poured into again and seal preservation in the container;
The 3rd the step: need before the use the ground dedusting,, then luminous paint be evenly coated on the object if metal objects need eliminate rust or bonderizing, dry naturally or dry make its curing after just have good energy-accumulating luminous performance.Also can on luminescent coating, be coated with the skim clear finish again, strengthen the smooth finish and the water resisting property on top layer;
Embodiment 1
Get 500ml varnish, in the process that stirs, add 100~200ml dehydrated alcohol, 50~100ml ethyl acetate, the polymerization degree successively and be 8 the anti-coacervation dispersion agent of polyurethane-type and the polymerization degree and be 15 the anti-coacervation dispersion agent of block polypropylene acid type polymer and respectively add 1~10ml, polyacrylic acid 10~30ml, fully stirring and evenly mixing adds 10~200g SrAl again 2O 4: Eu 2+, Dy 3+Luminescent powder stirred about 10~30 minutes, moved in the container bottle sealing and standing 3~5 hours, obtain luminescent properties good, evenly do not have caking, the bottom does not have sedimentary luminous paint.Get two steel discs of handling and wood chip, the luminous paint that makes evenly is painted on the surface, after drying, the curing, obtain ganoid coating; Rayed 2~5 minutes places the dark place can be luminous more than 15 hours.

Claims (1)

1. the preparation method of a solvent type energy accumulation luminescent paint is characterized in that the kind of raw materials used and reagent and addition are as follows:
The organic matrix of coating comprises one or more in polyester varnish, polyurethane lacquer, the alkyd varnish;
Luminescent powder be a kind of be the long after glow luminous material that base material is made with the aluminate, chemical general formula is MAl 2O 4: Eu 2+, RE 3+, choose wherein one or more; Wherein M is Ca, Sr or Ba, wherein RE 3+Be Dy 3+, Nd 3+And Tm 3+
Hyper-dispersant is that the block polypropylene acid type polymer of the anti-coacervation dispersion agent of the polyurethane-type of the polymerization degree 4~10, the polymerization degree 12~18 is prevented one or more among coacervation dispersion agent, the polycarboxylate sodium;
Emulsifying agent is selected the polyacrylic acid of the polymerization degree 11~15, in the tween T series non-ionic surfactants one or more for use; T=20,40,60 or 80 wherein;
Thinner is selected dehydrated alcohol, ethyl acetate, C for use 4~C 12In organic alcohol, ether, the sherwood oil one or more;
Organic matrix, thinner, hyper-dispersant, emulsifying agent and luminescent powder operating weight ratio are 100: 20~50: 0.5~5: 0.1~4: 10~60;
Preparation flow is as follows:
The first step: the preparation processing of luminescent powder and the selection of organic matrix; Utilize patent: the technology of ZL02109504.3 prepares long-afterglow luminous alaminate powder, is of a size of the particle of 10~30 μ m before using with the sieve screening; Organic matrix is selected various transparencies varnish product preferably;
Second step: the preparation of luminous paint; Organic matrix, thinner, hyper-dispersant, emulsifying agent joined to stir in the reactor by weight proportion it is mixed, insert luminescent powder then in batches, stir, obtain luminous paint until being uniformly dispersed; Be poured into again and seal preservation in the container;
The 3rd step: need before the use the ground dedusting,, then luminous paint is evenly coated on the object, dry naturally or dry and make its curing if metal objects need eliminate rust or bonderizing.
CN2007101590059A 2007-12-15 2007-12-15 Method for producing solvent type energy accumulation luminescent paint Expired - Fee Related CN101220238B (en)