CN101205135A - 一种功能型内墙瓷砖 - Google Patents
一种功能型内墙瓷砖 Download PDFInfo
- Publication number
- CN101205135A CN101205135A CNA2006101677537A CN200610167753A CN101205135A CN 101205135 A CN101205135 A CN 101205135A CN A2006101677537 A CNA2006101677537 A CN A2006101677537A CN 200610167753 A CN200610167753 A CN 200610167753A CN 101205135 A CN101205135 A CN 101205135A
- Authority
- CN
- China
- Prior art keywords
- ceramic tile
- raw material
- product
- wall ceramic
- functional form
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
一种功能型内墙瓷砖,本发明产品其特征是它由天然非金属矿物蛋白石轻质页岩制成,经过超细粉碎、复合、造粒、成型,最终经过高温烧结制成的功能型内墙瓷砖;本发明产品使用了含有大量纳米级微孔结构的天然非金属矿石蛋白石轻质页岩为基本原料,原料本身具备吸附性强,吸水率74.4%,原料还可以持久释放负离子,对居室环境起到自然调湿、净化室内空气、消除异味异臭、防止生霉结露、防止病菌害虫、防止家中贵重物品褪色劣化、防火阻燃功能;该产品给人体健康和人们的居住环境带来一系列好处,是现有同类产品的升级和换代产品。
Description
1.技术领域
本发明产品属于新材料应用领域,是利用天然非金属矿物蛋白石轻质页岩经过精深加工,添加一定量的烧结助剂、粘结剂,再经过高温烧结制成的外观多种形状的、具备一定功能的内墙瓷砖,本产品具备极高的吸附性能,吸水率74.4%,并具备持久释放负离子功能,对居室环境起到自然调湿、净化室内空气、消除异味异臭、防止生霉结露、防止病菌害虫、防止家中贵重物品褪色劣化、防火阻燃功能。
2.背景技术
现代化住宅的发展方向是:健康、生态、环保和节能,这也是人们追求的健康生活方式,具备一定功能的室内装修用建筑陶瓷材料在国外近两年取得了快速发展。本发明产品,一种功能型内墙瓷砖,采用的是天然非金属矿石蛋白石轻质页岩为基本原料,经过超细粉碎、高温烧结制作而成,由于蛋白石轻质页岩是自然界中珍贵的具备天然纳米级微孔结构的非金属矿石,蛋白石轻质页岩具备极强吸附性能,可以吸附居室内的有毒有害气体和异味、吸附居室内空气中多余的水份,蛋白石轻质页岩具备持久释放负离子的功能,通过其释放的负离子给人们身体健康和居住环境带来了一系列的好处,本发明产品,一种功能型内墙瓷砖是现有同类产品的技术升级和换代产品。
3.技术发明 本发明产品,一种功能型内墙瓷砖,该产品是由天然非金属矿物蛋白石轻质页岩为基本原料,制造时先对原矿石进行超细粉碎至5微米以下,加入分散剂有机聚合铵盐质量百分比为0.1-0.3%,加入粘结剂聚乙烯醇质量百分比为1-3%,在搅拌磨中进行搅拌分散和混匀,经过机械造粒,颗粒大小为1-3毫米,经过机械式压力机成型,再经过高温1100℃-1250℃最终烧结制成。
其中天然非金属矿物蛋白石轻质页岩为该产品的基本材料,该产品具有的多种功能也是由蛋白石轻质页岩的自身特性而产生作用的。蛋白石(又名Opal)化学成分为SiO2·nH2O,硬度:5.5-6.5,密度:2.15-2.23g/cm3,自身组成含有大量的5-20纳米的微孔结构,吸附性极强,吸水率在74.4%,具备天然释放负离子的功能,由蛋白石轻质页岩生产制造的功能型内墙瓷砖,用于居室内装修可以起到持久释放负离子、自然调湿、净化室内空气、消除异味异臭、防止生霉结露、防止病菌害虫、防止家中贵重物品褪色劣化、防火阻燃作用。
有机聚合铵盐是超细粉体分散助剂,聚乙烯醇是成型时使用的粘结剂。
将定量的蛋白石轻质页岩超细粉体加入质量百分比为0.1-0.3%分散剂有机聚合铵盐、加入粘结剂聚乙烯醇质量百分比为1-3%、在加入质量百分比为13-17%的水,将上述原料放入搅拌磨中搅拌分散混匀;使用机械式造粒机制成1-3毫米的颗粒,使用机械式成型压力机制成不同规格的内墙瓷砖坯体;成型好的瓷砖坯体在105℃-110℃进行烘干,烘干处理好的瓷砖坯体在380℃-420℃进行预烧结,时间为45分钟至1个小时,然后在1100℃-1250℃进行终烧结,时间为2.5-3小时,通过自然冷却,就可以得到成品,一种功能型内墙瓷砖。
4.具体实施方式
将原矿石蛋白石轻质页岩使用机械式粉碎机粉碎成1-5微米的超细粉体,按配比的要求,按质量百分比分别称取一定量的蛋白石轻质页岩超细粉体、分散剂有机聚合铵盐0.1-0.3%、粘结剂聚乙烯醇1-3%,将称好的原料放入搅拌磨中,加入相当于固体份料重量13-17%的水,进行充分的搅拌,做分散和混料处理;
将混匀的原料用机械式造粒机造成1-3毫米的颗粒;
将造好粒的原料用机械式压力成型机压制成不同规格形状坯体瓷砖;
将成型好的坯体瓷砖,在105℃-110℃进行烘干,烘干处理好的瓷砖坯体在380℃-420℃进行预烧结,时间为45分钟至1个小时,然后在1100℃-1250℃进行终烧结,时间为2.5-3小时;
最后通过自然冷却,就可以得到成品——功能型内墙瓷砖。
Claims (2)
1.一种功能型内墙瓷砖,其特征是它由天然非金属矿物蛋白石轻质页岩制成,将原矿石经过超细粉碎成1-5微米的超细粉体,复合添加质量百分比为0.1-0.3%分散剂有机聚合铵盐、1-3%粘结剂聚乙烯醇。
2.实施权利要求1所用工艺,其特征是按配方配比要求,按质量百分比分别称取一定量的蛋白石轻质页岩超细粉体、分散剂有机聚合铵盐0.1-0.3%、粘结剂聚乙烯醇1-3%,将称好的原料放入搅拌磨中,加入相当于固体份料重量13-17%的水,进行充分的搅拌,做分散和混料处理;
将混匀的原料用机械式造粒机造成1-3毫米的颗粒;
将造好粒的原料用机械式压力成型机压制成不同规格形状坯体瓷砖;
将成型好的坯体瓷砖,在105℃-110℃进行烘干,烘干处理好的瓷砖在380℃-420℃进行预烧结,时间为45分钟至1个小时,然后在1100℃-1250℃进行终烧结,时间为2.5-3小时;
最后通过自然冷却,就可以得到成品,一种功能型内墙瓷砖。