CN101004370A - 透水混凝土路面表面孔隙率与试块断面孔隙率检测方法 - Google Patents
透水混凝土路面表面孔隙率与试块断面孔隙率检测方法 Download PDFInfo
- Publication number
- CN101004370A CN101004370A CNA2007102001189A CN200710200118A CN101004370A CN 101004370 A CN101004370 A CN 101004370A CN A2007102001189 A CNA2007102001189 A CN A2007102001189A CN 200710200118 A CN200710200118 A CN 200710200118A CN 101004370 A CN101004370 A CN 101004370A
- Authority
- CN
- China
- Prior art keywords
- concrete
- paper
- trace
- porosity
- packing
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
Description
Claims (10)