CN100453654C - Production of waistbands from cattle hide - Google Patents

Production of waistbands from cattle hide Download PDF

Info

Publication number
CN100453654C
CN100453654C CNB200410024212XA CN200410024212A CN100453654C CN 100453654 C CN100453654 C CN 100453654C CN B200410024212X A CNB200410024212X A CN B200410024212XA CN 200410024212 A CN200410024212 A CN 200410024212A CN 100453654 C CN100453654 C CN 100453654C
Authority
CN
China
Prior art keywords
waistband
agent
leather
tinting material
cowhells
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CNB200410024212XA
Other languages
Chinese (zh)
Other versions
CN1584055A (en
Inventor
邹福智
张元杰
邹瑞锋
邹瑞东
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Individual
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Individual filed Critical Individual
Priority to CNB200410024212XA priority Critical patent/CN100453654C/en
Publication of CN1584055A publication Critical patent/CN1584055A/en
Application granted granted Critical
Publication of CN100453654C publication Critical patent/CN100453654C/en
Anticipated expiration legal-status Critical
Expired - Fee Related legal-status Critical Current

Abstract

The present invention relates to a method for producing a cow tendon waistband, which comprises the steps that cow leather is used as the raw material and put into an alkali soak solution to be soaked; then the hair of the cow leather is removed, and the cow leather without hair is put into an acid solution having the concentration of 1.5 to 4.5% to be soaked for 2 to 8 hours after the cow leather is taken out of the alkali soak solution; then the cow leather is dried in the sun until about 60% to 70% of the cow leather are dried and cut to form leather lines after being taken out of the acid solution; then the leather lines are dried in the sun to become the finished product lines; the finished product lines are braided to form a waistband with holes, and then the waistband with holes is put into a coloring agent to be soaked, softened and colored for 5 to 50 minutes according to the pattern requirement of the specifications; the coloring agent is prepared from acid stain and leather color-change agent according to the proportion of 1:10 to 40; then the waistband with holes is shaped and ground into the product after being taken out. The waistband manufactured by the method of the present invention has the positive effect of medium hardness, good hand feeling, no paint flavor, no decolorization, etc., and furthermore, the product quality of the waistband is greatly enhanced.

Description

The preparation method of Cowhells waistband
Technical field
The present invention relates to daily necessities, is a kind of preparation method of Cowhells waistband.
Background technology
The applicant has been subjected to the higher geographic people of people's welcome, particularly temperature to like using since beginning to make the Cowhells waistband deeply, and it has avoided because of the temperature sultry sense of discomfort that waistband produces when higher etc.But find that in actual applications still there is some deficiency in this Cowhells waistband: the hardness of waistband is bigger, bring more inconvenience to the user, one of important quality standard that the soft durometer of Cowhells waistband becomes people to be selected when buying, also be that outlet needs one of quality product that improves, it is that those skilled in the art are all in the problem of making great efforts research.
Summary of the invention
The objective of the invention is, a kind of preparation method of Cowhells waistband is provided, it has changed the hardness of existing Cowhells waistband, makes waistband have advantages such as neither too hard, nor too soft hand feel and drape.
The present invention is in order to finish goal of the invention, following technical scheme is provided: it adopts ox-hide is raw material, ox-hide is put into alkaline soak solution to be soaked, plucking after pulling out and putting into concentration again is that the acid solution of 1.5-4.5% was soaked 2-8 hour, pull the cool solarization in back to about six, seventy percent dried cutting out and make rubber-insulated wire, drying becomes product line, according to the requirement of specification pattern, put into softening painted 5-50 minute of tinting material immersion after being woven into waistband with holes, tinting material adopts matching stain and leather color alternation agent to prepare in 1: 10~40 ratio, pulls the back shaping out and is polished into product.
The present invention is in order further to finish goal of the invention, the quality that improves waistband increases pliability and degree of staining, can also finish by the following technical programs: will soak the remollescent waistband through tinting material, use surface slip agent, laking agent and water in 1.5~4.5 again: 0.5~1.5: 1~3 the liquid swabbing of ratio furnishing, carry out the second time with the bating agent again and soften, become product with the brightening agent spary at last.Tinting material of the present invention can also adopt matching stain and leather color alternation agent to prepare in 1: 25~35 ratio.The present invention makes waistband further softening in order better to improve the quality of products, and can also will become product with the hand feeling agent spary at last through shaping polishing or the process remollescent waistband second time.Waistband of the present invention soaks softening better scope of painted time in tinting material be 20-30 minute.
Matching stain described in the preparation method of the present invention, leather color alternation agent, surface slip agent, laking agent, bating agent, brightening agent and hand feeling agent are known commodity.
The waistband that adopts method of the present invention to make has positive effects such as neither too hard, nor too soft, good hand touch, nothing lacquer flavor, nondiscoloration, has improved the quality product of waistband by a relatively large margin.
Embodiment
The invention is not restricted to the present embodiment protection domain.
Embodiment 1
Choose ox-hide and do raw material, 200 kilograms of bracket skins are put into 100 kilograms in lime, soaked 40 hours in 1500 kilograms of alkaline soak solutions of 20 kilograms in Sodium Sulphide and water, plucking after pulling out and putting into concentration again is that 3.5% acid solution was soaked 3 hours, pull out and be cut into rubber-insulated wire after the cool solarization in back is done to sixty percent, rubber-insulated wire dried to become product line standby, according to the requirement of specification pattern, after being woven into waistband with holes, put into tinting material again and soak, soften paintedly, soak time is 35 minutes, tinting material adopts matching stain and leather color alternation agent to prepare in 1: 15 ratio, pulls the back shaping out and is polished into product.
Embodiment 2
Choose ox-hide and do raw material, 100 kilograms on ox-hide is put into 50 kilograms in lime, soaked 45 hours in 800 kilograms of alkaline soak solutions of 10 kilograms in Sodium Sulphide and water, plucking after pulling out and putting into concentration again is that 2% hydrochloric acid solution soaked 5 hours, pull out and be cut into rubber-insulated wire after the cool solarization in back is done to seventy percent, rubber-insulated wire dried to become product line standby, according to the requirement of specification pattern, after being woven into waistband with holes, put into tinting material again and soak, soften paintedly, soak time is 20 minutes, tinting material adopts matching stain and leather color alternation agent to prepare in 1: 35 ratio, pull back shaping polishing out, will soak the remollescent waistband through tinting material again and use surface slip agent again, laking agent and water is in 2.8: 0.8: 2.5 ratio furnishing liquid swabbing, and it is softening to carry out the second time with the bating agent again, spary is on waistband, and spary evenly gets final product.
Embodiment 3
Choose ox-hide and do raw material, 300 kilograms on ox-hide is put into 150 kilograms in lime, soaked 35 hours in 2000 kilograms of alkaline soak solutions of 30 kilograms in Sodium Sulphide and water, plucking after pulling out and putting into concentration again is that 4% hydrochloric acid solution soaked 7 hours, pull out and be cut into rubber-insulated wire after the cool solarization in back is done to sixty percent, rubber-insulated wire dried to become product line standby, according to the requirement of specification pattern, after being woven into waistband with holes, putting into tinting material again soaks, soften paintedly, soak time is 10 minutes, and tinting material adopts matching stain and leather color alternation agent to prepare in 1: 25 ratio, pull back shaping polishing out, to soak the remollescent waistband through tinting material again and use surface slip agent again, laking agent and water is in 3: 1: 2 ratio furnishing liquid swabbing, and it is softening to carry out the second time with the bating agent again, and spary is on waistband.With brightening agent or hand feeling agent, perhaps both all use spary to become product at last.

Claims (4)

1, the preparation method of Cowhells waistband, it adopts ox-hide is raw material, ox-hide is put into alkaline soak solution immersion to be pulled out, it is characterized in that: plucking after pulling out and putting into concentration again is that the acid solution of 1.5-4.5% was soaked 2-8 hour, cool solarization is cut and is made rubber-insulated wire after pulling out, drying becomes product line, according to the requirement of specification pattern, put into softening painted 5-50 minute of tinting material immersion after being woven into waistband with holes, tinting material adopts matching stain and leather color alternation agent to prepare in 1: 10~40 ratio, pulls the back shaping out and is polished into product.
2, the preparation method of Cowhells waistband according to claim 1 is characterized in that: tinting material adopts matching stain and leather color alternation agent to prepare in 1: 25~35 ratio.
3, the preparation method of Cowhells waistband according to claim 1 is characterized in that: waistband soaks the softening painted time in tinting material be 20-30 minute.
4, the preparation method of Cowhells waistband according to claim 1, it is characterized in that: soak the remollescent waistband through tinting material, use surface slip agent, laking agent and water in 1.5~4.5 again: 0.5~1.5: 1~3 the liquid swabbing of ratio furnishing, carry out the second time with the bating agent again and soften, become product with the brightening agent spary at last.
CNB200410024212XA 2004-05-27 2004-05-27 Production of waistbands from cattle hide Expired - Fee Related CN100453654C (en)