CN103726069A - 一种新型电解镍的生产方法 - Google Patents

一种新型电解镍的生产方法 Download PDF

Info

Publication number
CN103726069A
CN103726069A CN201210386438.9A CN201210386438A CN103726069A CN 103726069 A CN103726069 A CN 103726069A CN 201210386438 A CN201210386438 A CN 201210386438A CN 103726069 A CN103726069 A CN 103726069A
Authority
CN
China
Prior art keywords
nickel
production method
electrolytic solution
electrolyte
ion
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201210386438.9A
Other languages
English (en)
Inventor
范厚元
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
JIANGXI JIANGLI SCIENCE AND TECHNOLOGY Co Ltd
Original Assignee
JIANGXI JIANGLI SCIENCE AND TECHNOLOGY Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by JIANGXI JIANGLI SCIENCE AND TECHNOLOGY Co Ltd filed Critical JIANGXI JIANGLI SCIENCE AND TECHNOLOGY Co Ltd
Priority to CN201210386438.9A priority Critical patent/CN103726069A/zh
Publication of CN103726069A publication Critical patent/CN103726069A/zh
Pending legal-status Critical Current

Abstract

一种新型电解镍的生产方法,它涉及化工生产技术领域,它的生产方法为:(1)将含镍原料采用硫酸盐体质电解液进行电解,电解完成后加入硫酸将电解液的PH值调节为3.0-5.5;(2)然后将电解液通过离子交换树脂和活性炭将电解液中的杂质去除,用泵将电解液送入高位储液槽中,加温至55-80℃,电解液流入到隔膜袋内进行电解,电解时间为24-36个小时,获得高纯度电解镍。它采用回收的镍制品重新进行生产,生产方法简单,生产出来的电解镍纯度高,杂质少,产品能更好的应用于各个行业。

Description

一种新型电解镍的生产方法
技术领域:
本发明涉及化工生产技术领域,具体涉及一种新型电解镍的生产方法。  
背景技术:
镍是一种银白色的金属,具有机械强度高,延展性好,难熔,在空气中不易氧化等优良特性,因此,它用于制造的不锈钢和各种合金钢被广泛的应用于飞机、坦克、导弹等军用行业和工业中的机械制造和电子遥控等领域,现有的普遍电解镍的生产方法比较复杂,并且生产的电解镍纯度不高。在高纯镍的生产过程中,电解液必须循环使
用。目前国内外镍电解液净化除杂工艺大都采用以下方法,除铁采用中和水解法、黄钾铁矾法和赤铁矿法。除铜采用置换沉淀或萃取法。除钴采用中和水解、萃取或“黑镍”氧化水解法。除铅、锌采用共沉淀法、离子交换法和萃取法,但是一些杂质的萃取率还是很低。
发明内容:
本发明的目的是提供一种新型电解镍的生产方法,它采用回收的镍制品重新进行生产,生产方法简单,生产出来的电解镍纯度高,杂质少,产品能更好的应用于各个行业。
为了解决背景技术所存在的问题,本发明采取以下技术方案:它的生产方法为:(1)将含镍原料采用硫酸盐体质电解液进行电解,电解完成后加入硫酸将电解液的PH值调节为3.0-5.5;(2)然后将电解液通过离子交换树脂和活性炭将电解液中的杂质去除,用泵将电解液送入高位储液槽中,加温至55-80℃,电解液流入到隔膜袋内进行电解,电解时间为24-36个小时,获得高纯度电解镍。
所述的步骤(2)中的除杂具体步骤为:在室温下(25℃)进行,先采用M5640除铜离子,使得铜离子的含量小于0.1mg·L-1,然后采用P1507除对杂质离子铁、锌、铅进行去除;最后用氢氧化钠溶液均相制皂75%去除镍离子,并用pHS·3D型pH测定pH值,用原子吸收法测定各离子含量。
    本发明具有以下有益效果:它采用回收的镍制品重新进行生产,生产方法简单,生产出来的电解镍纯度高,杂质少,产品能更好的应用于各个行业。
具体实施方式:
本具体实施方式采取以下技术方案:它的生产方法为:(1)将含镍原料采用硫酸盐体质电解液进行电解,电解完成后加入硫酸将电解液的PH值调节为3.0-5.5;(2)然后将电解液通过离子交换树脂和活性炭将电解液中的杂质去除,用泵将电解液送入高位储液槽中,加温至55-80℃,电解液流入到隔膜袋内进行电解,电解时间为24-36个小时,获得高纯度电解镍。
所述的步骤(2)中的除杂具体步骤为:在室温下(25℃)进行,先采用M5640除铜离子,使得铜离子的含量小于0.1mg·L-1,然后采用P1507除对杂质离子铁、锌、铅进行去除;最后用氢氧化钠溶液均相制皂75%去除镍离子,并用pHS·3D型pH测定pH值,用原子吸收法测定各离子含量。
本具体实施方式采用回收的镍制品重新进行生产,生产方法简单,生产出来的电解镍纯度高,杂质少,产品能更好的应用于各个行业。

Claims (2)

1.一种新型电解镍的生产方法,其特征在于它的生产方法为:(1)将含镍原料采用硫酸盐体质电解液进行电解,电解完成后加入硫酸将电解液的PH值调节为3.0-5.5;(2)然后将电解液通过离子交换树脂和活性炭将电解液中的杂质去除,用泵将电解液送入高位储液槽中,加温至55-80℃,电解液流入到隔膜袋内进行电解,电解时间为24-36个小时,获得高纯度电解镍。
2.根据权利要求1所述的一种新型电解镍的生产方法,其特征在于所述的步骤(2)中的除杂具体步骤为:在室温下(25℃)进行,先采用M5640除铜离子,使得铜离子的含量小于0.1mg·L-1,然后采用P1507除对杂质离子铁、锌、铅进行去除;最后用氢氧化钠溶液均相制皂75%去除镍离子,并用pHS·3D型pH测定pH值,用原子吸收法测定各离子含量。
CN201210386438.9A 2012-10-13 2012-10-13 一种新型电解镍的生产方法 Pending CN103726069A (zh)