CN103015228A - Rayon knitted coating digitalization printing process - Google Patents

Rayon knitted coating digitalization printing process Download PDF

Info

Publication number
CN103015228A
CN103015228A CN2012105462686A CN201210546268A CN103015228A CN 103015228 A CN103015228 A CN 103015228A CN 2012105462686 A CN2012105462686 A CN 2012105462686A CN 201210546268 A CN201210546268 A CN 201210546268A CN 103015228 A CN103015228 A CN 103015228A
Authority
CN
China
Prior art keywords
coating
people
numberization
kinds
red
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
CN2012105462686A
Other languages
Chinese (zh)
Other versions
CN103015228B (en
Inventor
吴锋
胡兴娣
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Shaoxing Dingji Printing And Dyeing Technology Co ltd
Original Assignee
SHAOXING DIGITEX PRINTING AND DYEING CO Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by SHAOXING DIGITEX PRINTING AND DYEING CO Ltd filed Critical SHAOXING DIGITEX PRINTING AND DYEING CO Ltd
Priority to CN201210546268.6A priority Critical patent/CN103015228B/en
Publication of CN103015228A publication Critical patent/CN103015228A/en
Application granted granted Critical
Publication of CN103015228B publication Critical patent/CN103015228B/en
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

The invention discloses a rayon knitted coating digitalization printing process. The rayon knitted coating digitalization printing process consists of the following steps: 1) manufacturing a halftone; 2) modulating colorant; 3) scraping and printing; 4) drying; and 5) shaping to obtain the finished product. According to the rayon knitted coating digitalization printing process provided by the invention, the halftone is subjected to color separation by utilizing an eight-color principle and the printing method of the coating is adopted, so that the pattern is more lifelike, the moire fringe transition of the pattern is more natural and closer to the true graphical effect, the additional value of the product is increased, and energy is saved.

Description

The printing technology of the cotton knitting coating numberization of a kind of people
?
Technical field
The present invention relates to the printing technology of the cotton knitting coating numberization of a kind of people.
 
Background technology
The cotton knitted cloth of people now is when stamp, because technical reason adopts common PLATE SCREAM PRINTING usually.But its flower type weak effect of common PLATE SCREAM PRINTING, aberration are obvious, and also there is obvious stamp idea in the moire place.
 
Summary of the invention
For addressing the above problem, the object of the present invention is to provide the printing technology of the cotton knitting coating numberization of a kind of people, it utilizes eight chromogens reason that half tone is carried out color separation, stamp mode by coating, make colored type seem that effect is more true to nature, the moire transition of flower type is more natural, more presses close to the reality pictures effect, energy savings when improving added value of product.
The present invention is the purpose that reaches above-mentioned, and the present invention adopts following technical scheme:
The printing technology of the cotton knitting coating numberization of a kind of people is comprised of following steps:
1) make web plate: according to concrete colored type, by retouching the original text color separation, make respectively 8 plain net half tones, these 8 plain net half tones are used for the mill base coated with lower 8 kinds of colors: blue or green, red, yellow, black, shallow green grass or young crops, pale red, somber, tangerine; Select 200 purpose grenadines;
2) modulation mill base: difference modulation step 1) described 8 kinds of mill bases, the prescription of mill base is to contain 14-24 parts in adhesive in per 100 weight portions, 67-73 parts of emulsion thickenings, surplus are respectively a kind of coating in blue or green, red, yellow, black, shallow green grass or young crops, pale red, somber, 8 kinds of colors of tangerine; 8 kinds of color mill bases after modulating evenly are coated on respectively on 8 plain net half tones;
3) scrape: during printing the cotton knitted cloth of people is scraped mill base through the plain net half tone of blue or green, red, yellow, black, shallow green grass or young crops, pale red, somber, these 8 kinds of color mill bases of tangerine successively, finish stamp;
4) oven dry: the cotton knitted cloth of people that will finish behind the stamp is put into drying machine drying, and temperature is 80-120 ℃, and the time is 1-5 minutes;
5) typing: the cotton knitted cloth of the people behind the drying machine drying is carried out shaping and drying under 130-150 ℃ temperature, drying time is 2-3 minutes, becomes finished product after the oven dry.
The prescription of described mill base is to contain 20 parts in adhesive in per 100 weight portions, 69.5 parts of emulsion thickenings, 10.5 parts of coating.
Described step 2) adhesive adopts the adhesive of BINDER 734ELF in, and its production firm is DIC chemical industry Co., Ltd..
Described step 2) emulsion thickening forms by the configuration of following percentage by weight raw material in: emulsifying agent 4%-6%, white kerosene 25%-40%(are purchased from Kaifeng Liu Yuan petrochemical plant), water 60%-70%.
Described emulsifying agent adopts the emulsifying agent of CONC 400HENF, and its production firm is DIC chemical industry Co., Ltd..
The drying machine drying temperature is 100 ℃ in the described step 4), and the time is 1-3 minutes.
Beneficial effect of the present invention is: the printing technology that the invention provides the cotton knitting coating numberization of a kind of people, it utilizes eight chromogens reason that half tone is carried out color separation, stamp mode by coating, make colored type seem that effect is more true to nature, the moire transition of flower type is more natural, more press close to the reality pictures effect, energy savings when improving added value of product.
 
The specific embodiment
Embodiment 1
The present embodiment provides the printing technology of the cotton knitting coating numberization of a kind of people, is comprised of following steps:
1) make web plate: according to concrete colored type, by retouching the original text color separation, make respectively 8 plain net half tones, these 8 plain net half tones are used for the mill base coated with lower 8 kinds of colors: blue or green, red, yellow, black, shallow green grass or young crops, pale red, somber, tangerine; Select 200 purpose grenadines.
2) modulation mill base: difference modulation step 1) described 8 kinds of mill bases, the prescription of mill base is to contain 20 parts in adhesive in per 100 weight portions, 69.5 parts of emulsion thickenings, 10.5 parts of coating, coating are respectively a kind of coating in blue or green, red, yellow, black, shallow green grass or young crops, pale red, somber, 8 kinds of colors of tangerine.Wherein emulsion thickening adopts the percentage by weight emulsification configuration by emulsifying agent 4%, white kerosene 29%, water 67% to form.Wherein adhesive adopts the adhesive of the BINDER 734ELF of DIC company, and emulsifying agent adopts the emulsifying agent of the CONC 400HENF of DIC company; Mill base evenly is coated on the plain net half tone.
3) scrape: during printing the cotton knitted cloth of people is scraped mill base through the plain net half tone of blue or green, red, yellow, black, shallow green grass or young crops, pale red, somber, these 8 kinds of color mill bases of tangerine successively, finish stamp.
4) oven dry: the cotton knitted cloth of people that will finish behind the stamp is put into drying machine drying, and temperature is 80 ℃, and the time is 2 minutes.
5) typing: the cotton knitted cloth of the people behind the drying machine drying is carried out shaping and drying under 130 ℃ temperature, drying time is 2 minutes, becomes finished product after the oven dry.
The printing technology of the cotton knitting coating numberization of a kind of people of the present embodiment manufacturing, it utilizes eight chromogens reason that half tone is carried out color separation, stamp mode by coating, make colored type seem that effect is more true to nature, the moire transition of flower type is more natural, more press close to the reality pictures effect, energy savings when improving added value of product.
 
Embodiment 2
The present embodiment provides the printing technology of the cotton knitting coating numberization of a kind of people, is comprised of following steps:
1) make web plate: according to concrete colored type, by retouching the original text color separation, make respectively 8 plain net half tones, these 8 plain net half tones are used for the mill base coated with lower 8 kinds of colors: blue or green, red, yellow, black, shallow green grass or young crops, pale red, somber, tangerine; Select 200 purpose grenadines.
2) modulation mill base: difference modulation step 1) described 8 kinds of mill bases, the prescription of mill base is to contain 16 parts in adhesive in per 100 weight portions, 71 parts of emulsion thickenings, 13 parts of coating, coating are respectively a kind of coating in blue or green, red, yellow, black, shallow green grass or young crops, pale red, somber, 8 kinds of colors of tangerine.Wherein emulsion thickening adopts the percentage by weight emulsification configuration by emulsifying agent 5%, white kerosene 35%, water 60% to form.Wherein adhesive adopts the adhesive of the BINDER 734ELF of DIC company, and emulsifying agent adopts the emulsifying agent of the CONC 400HENF of DIC company; Mill base evenly is coated on the plain net half tone.
3) scrape: during printing the cotton knitted cloth of people is scraped mill base through the plain net half tone of blue or green, red, yellow, black, shallow green grass or young crops, pale red, somber, these 8 kinds of color mill bases of tangerine successively, finish stamp.
4) oven dry: the cotton knitted cloth of people that will finish behind the stamp is put into drying machine drying, and temperature is 100 ℃, and the time is 3 minutes.
5) typing: the cotton knitted cloth of the people behind the drying machine drying is carried out shaping and drying under 140 ℃ temperature, drying time is 3 minutes, becomes finished product after the oven dry.
The printing technology of the cotton knitting coating numberization of a kind of people of the present embodiment manufacturing, it utilizes eight chromogens reason that half tone is carried out color separation, stamp mode by coating, make colored type seem that effect is more true to nature, the moire transition of flower type is more natural, more press close to the reality pictures effect, energy savings when improving added value of product.
 
Embodiment 3
The present embodiment provides the printing technology of the cotton knitting coating numberization of a kind of people, is comprised of following steps:
1) make web plate: according to concrete colored type, by retouching the original text color separation, make respectively 8 plain net half tones, these 8 plain net half tones are used for the mill base coated with lower 8 kinds of colors: blue or green, red, yellow, black, shallow green grass or young crops, pale red, somber, tangerine; Select 200 purpose grenadines.
2) modulation mill base: difference modulation step 1) described 8 kinds of mill bases, the prescription of mill base is to contain 23 parts in adhesive in per 100 weight portions, 68 parts of emulsion thickenings, 9 parts of coating, coating are respectively a kind of coating in blue or green, red, yellow, black, shallow green grass or young crops, pale red, somber, 8 kinds of colors of tangerine.Wherein emulsion thickening adopts the percentage by weight emulsification configuration by emulsifying agent 6%, white kerosene 26%, water 68% to form.Wherein adhesive adopts the adhesive of the BINDER 734ELF of DIC company, and emulsifying agent adopts the emulsifying agent of the CONC 400HENF of DIC company; Mill base evenly is coated on the plain net half tone.
3) scrape: during printing the cotton knitted cloth of people is scraped mill base through the plain net half tone of blue or green, red, yellow, black, shallow green grass or young crops, pale red, somber, these 8 kinds of color mill bases of tangerine successively, finish stamp.
4) oven dry: the cotton knitted cloth of people that will finish behind the stamp is put into drying machine drying, and temperature is 120 ℃, and the time is 3 minutes.
5) typing: the cotton knitted cloth of the people behind the drying machine drying is carried out shaping and drying under 150 ℃ temperature, drying time is 3 minutes, becomes finished product after the oven dry.
The printing technology of the cotton knitting coating numberization of a kind of people of the present embodiment manufacturing, it utilizes eight chromogens reason that half tone is carried out color separation, stamp mode by coating, make colored type seem that effect is more true to nature, the moire transition of flower type is more natural, more press close to the reality pictures effect, energy savings when improving added value of product.

Claims (6)

1. the printing technology of the cotton knitting coating numberization of a people, it is characterized in that being formed by following steps: 1) make web plate: according to concrete colored type, by retouching the original text color separation, make respectively 8 plain net half tones, these 8 plain net half tones are used for the mill base coated with lower 8 kinds of colors: blue or green, red, yellow, black, shallow green grass or young crops, pale red, somber, tangerine; Select 200 purpose grenadines;
2) modulation mill base: difference modulation step 1) described 8 kinds of mill bases, the prescription of mill base is to contain 14-24 parts in adhesive in per 100 weight portions, 67-73 parts of emulsion thickenings, surplus are respectively a kind of coating in blue or green, red, yellow, black, shallow green grass or young crops, pale red, somber, 8 kinds of colors of tangerine; 8 kinds of color mill bases after modulating evenly are coated on respectively on 8 plain net half tones;
3) scrape: during printing the cotton knitted cloth of people is scraped mill base through the plain net half tone of blue or green, red, yellow, black, shallow green grass or young crops, pale red, somber, these 8 kinds of color mill bases of tangerine successively, finish stamp;
4) oven dry: the cotton knitted cloth of people that will finish behind the stamp is put into drying machine drying, and temperature is 80-120 ℃, and the time is 1-5 minutes;
5) typing: the cotton knitted cloth of the people behind the drying machine drying is carried out shaping and drying under 130-150 ℃ temperature, drying time is 2-3 minutes, becomes finished product after the oven dry.
2. the printing technology of the cotton knitting coating numberization of a kind of people according to claim 1, it is characterized in that: the prescription of described mill base is to contain 20 parts in adhesive in per 100 weight portions, 69.5 parts of emulsion thickenings, 10.5 parts of coating.
3. the printing technology of the cotton knitting coating numberization of a kind of people according to claim 1 is characterized in that: the adhesive of adhesive employing BINDER 734ELF described step 2).
4. the printing technology of cotton knitting coating numberization of a kind of people according to claim 1, it is characterized in that: emulsion thickening configures by following percentage by weight raw material and forms described step 2): emulsifying agent 4%-6%, in vain kerosene 25%-40%, water 60%-70%.
5. the printing technology of the cotton knitting coating numberization of a kind of people according to claim 4 is characterized in that: the emulsifying agent of described emulsifying agent employing CONC 400HENF.
6. the printing technology of the cotton knitting coating numberization of a kind of people according to claim 1, it is characterized in that: the drying machine drying temperature is 100 ℃ in the described step 4), the time is 1-3 minutes.
CN201210546268.6A 2012-12-17 2012-12-17 Rayon knitted coating digitalized printing process Active CN103015228B (en)