CN100363139C - 镁合金表面B4C和Al堆焊重熔方法 - Google Patents
镁合金表面B4C和Al堆焊重熔方法 Download PDFInfo
- Publication number
- CN100363139C CN100363139C CNB2005100250652A CN200510025065A CN100363139C CN 100363139 C CN100363139 C CN 100363139C CN B2005100250652 A CNB2005100250652 A CN B2005100250652A CN 200510025065 A CN200510025065 A CN 200510025065A CN 100363139 C CN100363139 C CN 100363139C
- Authority
- CN
- China
- Prior art keywords
- welding
- built
- magnesium alloy
- alloy surface
- coating
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Abstract
Description
Claims (9)